| HS Code | 204063 |
| Grade | BASF Ultradur PBT+GF B4300G6 BK05110 |
| Polymerbase | Polybutylene terephthalate (PBT) |
| Glassfibercontent | 30% |
| Color | Black (BK05110) |
| Density | 1.53 g/cm³ |
| Tensilemodulus | 10,000 MPa |
| Tensilestrength | 140 MPa |
| Elongationatbreak | 3.0% |
| Charpynotchedimpactstrength23c | 10 kJ/m² |
| Hdt A 1 8mpa | 210 °C |
| Meltingtemperature | 220–225 °C |
| Waterabsorptionsaturation | 0.4% |
| Moldingshrinkageparallel | 0.3% |
| Moldingshrinkagenormal | 0.8% |
| Volumeresistivity | 1E15 Ω·cm |
| Processingmethod | Injection molding |
As an accredited BASF Ultradur® PBT+GF B4300G6 BK05110 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg moisture-proof paper bags, supplied on 1,000 kg pallets (40 bags per pallet). |
| Container Loading (20′ FCL) | 20′ FCL container loaded with BASF Ultradur® PBT+GF B4300G6 BK05110 in moisture-proof bags, palletized and secured for ocean shipment. |
| Shipping | BASF Ultradur® PBT+GF B4300G6 BK05110 is shipped as non-hazardous thermoplastic pellets in sealed moisture-barrier bags or octabins. Keep dry, cool, and protected from direct sunlight; avoid humidity and high temperatures. No special dangerous-goods labeling or UN number is normally required. |
| Storage | Store BASF Ultradur® PBT+GF B4300G6 BK05110 in a cool, dry, well-ventilated area away from direct sunlight, heat sources, moisture, and oxidizing agents. Keep containers tightly closed to prevent humidity absorption and contamination. Use good housekeeping and avoid dust formation. Follow local regulations and the safety data sheet for additional handling and storage requirements. |
| Shelf Life | The shelf life is 12 months from delivery when stored dry in sealed packaging at 10–30°C. |
Competitive BASF Ultradur® PBT+GF B4300G6 BK05110 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
BASF Ultradur® PBT+GF B4300G6 BK05110 is a black, 30 wt% glass-fibre-reinforced polybutylene terephthalate injection-moulding compound. The designation B4300 identifies the PBT base series, G6 denotes nominal 30 % glass-fibre reinforcement, and BK05110 specifies the black colour package. Published typical values include density of 1.53 g/cm³ to ISO 1183-1, melt volume rate of 12 cm³/10 min at 250 °C and 2.16 kg to ISO 1133-1, tensile modulus of 10,000 MPa and tensile stress at break of 135 MPa to ISO 527-2, flexural modulus of 9,000 MPa to ISO 178, and Charpy notched impact strength of 8 kJ/m² at 23 °C to ISO 179-1/1eA. The material is intended for injection-moulded technical components that require high stiffness, dimensional stability under load, and resistance to many automotive fluids, but it is not a flame-retardant grade.
| Property | Test method | Typical value |
|---|---|---|
| Density | ISO 1183-1 | 1.53 g/cm³ |
| Melt volume rate, 250 °C/2.16 kg | ISO 1133-1 | 12 cm³/10 min |
| Tensile modulus | ISO 527-2 | 10,000 MPa |
| Tensile stress at break | ISO 527-2 | 135 MPa |
| Tensile strain at break | ISO 527-2 | 2.5 % |
| Flexural modulus | ISO 178 | 9,000 MPa |
| Charpy notched impact, 23 °C | ISO 179-1/1eA | 8 kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-2 | 205 °C |
| Heat deflection temperature, 0.45 MPa | ISO 75-2 | 220 °C |
| Flammability classification at 1.6 mm | IEC 60695-11-10 | UL 94 HB |
| Volume resistivity | IEC 62631-3-1 | 1.0×1016 Ω·cm |
The critical process variable for PBT is residual moisture. Supplier guidance for glass-filled PBT grades sets a maximum moisture content of 0.02 wt% before melt plastication. Above 0.04 wt%, hydrolysis during barrel residence produces measurable loss of tensile stress at break and notched impact. Drying should be performed in a desiccant dryer with a dew point of −30 °C to −40 °C, at 80 °C to 100 °C for 4 h to 6 h. Moisture analysis is commonly performed by Karl Fischer titration or ISO 15512. On production-scale machines with hopper residence below 4 h, damp granules intermittently reach the feed throat and produce splay marks on moulded surfaces; this is the most frequently observed field failure in humid plants.
Melt temperature should be held between 250 °C and 270 °C. Extended residence above 280 °C for more than 5 min increases thermal degradation and should be avoided. Mould temperature is maintained between 60 °C and 100 °C; the upper portion of this range improves crystallinity, dimensional stability, and surface uniformity but increases cycle time. Screw geometry is normally specified with a three-zone screw of 18:1 to 20:1 L/D and a compression ratio of 2.0:1 to 2.5:1 to limit glass-fibre breakage. Back pressure at 0.3–0.7 MPa melt pressure is sufficient to homogenise glass distribution without excessive fibre fracture, and screw surface speed should remain below 0.3 m/s for the same reason.
Injection speed is set in the medium-to-high range. Excessively low speed causes premature freezing and floating glass at the surface, while linear gate velocity above approximately 400 mm/s can generate gate blush and jetting. Holding pressure is typically selected at 50 % to 70 % of injection peak pressure and held until gate freeze. Premature hold release produces sink marks behind bosses and ribs. The screw cushion should be maintained between 3 mm and 6 mm, and decompression should be limited to 2 mm to 5 mm to prevent air entrapment and burning. On cold-runner tools, runner diameter should be at least 5 mm for wall sections above 2 mm to limit pressure loss.
Mechanical data place this grade in the high-stiffness class of polybutylene terephthalate compounds. The tensile modulus of 10,000 MPa is approximately 3.8 times that of unreinforced PBT, which typically exhibits tensile modulus near 2,600 MPa under ISO 527-2. The heat deflection temperature under 1.8 MPa load is 205 °C per ISO 75-2, while unreinforced PBT typically remains near 60 °C. These differences support substitution of stamped metal and die-cast aluminium in bracketry where mass reduction is required, provided service temperature and load duration remain below the polymer’s creep limits, not simply below its HDT.
Structural parts such as sensor housings, connector bodies, enclosure frames, and motor brackets are injection-moulded from this compound when the dominant load path is flexural or torsional. However, the 30 wt% glass-fibre content introduces anisotropic mould shrinkage: values parallel to flow are typically lower than values transverse to flow, and unbalanced gating produces warpage in flat covers. Mould-filling simulations should include fibre-orientation analysis because the glass orientation tensor controls local stiffness. Published data for this specific configuration is limited, so production tools often require a first-shot correction based on measured shrinkage data from ISO 294-4 plaques.
The G6 designation indicates a nominal 30 % glass-fibre level, which provides higher stiffness and lower creep tendency than the lower glass-fibre grades in the same series. Published datasheet comparisons show tensile modulus increasing from approximately 4,500 MPa for a 10 % glass-fibre grade and 7,500 MPa for a 20 % grade to 10,000 MPa for this 30 % grade under ISO 527-2. Simultaneously, tensile strain at break declines, falling from approximately 3.5 % for the 20 % grade to 2.5 % for the 30 % grade, indicating lower ductility and greater notch sensitivity in thick, highly constrained sections.
The increased glass content also reduces mould shrinkage magnitude but increases shrinkage anisotropy. Unreinforced PBT mould shrinkage is often near 1.5 % to 2.0 %, whereas glass-reinforced grades reduce this value and shift warpage behaviour from simple isotropic contraction to orientation-dependent contraction. The trade-off is that weld lines, ribs, and bosses become more critical because the glass fibres align along flow fronts and reduce local out-of-plane strength in those regions.
Electrical connector and enclosure applications use this compound because heat deflection temperature and stiffness allow thin-wall designs with snap-fit retention. Insulation-type values are reported by the supplier under IEC 62631 methods; volume resistivity is on the order of 1.0×1016 Ω·cm. The grade carries UL 94 HB at 1.6 mm; therefore, applications requiring flame-retardant behaviour must use a V-class product or be limited by end-product enclosure rules. Where UL 94 V-0 at 1.6 mm is mandated, B4300G6 BK05110 is not an appropriate selection.
Although PBT resists aliphatic hydrocarbons, gasoline, diesel, and many automotive oils under short-term contact, the ester linkages remain vulnerable to hydrolysis. The compound is not recommended for continuous immersion in hot water above 60 °C or for steam-sterilised components. Strong alkaline media and concentrated acetic acid at elevated temperature also attack the polyester backbone. Chemical resistance should be verified by ISO 175 immersion testing or by the end-use specification, not inferred from room-temperature solvent resistance. In automotive underhood use, continuous exposure to engine coolant/water mixtures above this temperature is a process risk; a hydrolysis-resistant PBT or polyamide grade may be required.
The high glass content also reduces weld-line strength. In multi-gate tools, the meeting front of glass-filled melt has reduced fibre entanglement and produces a visible knit line. Moulded weld-line specimens tested under ISO 527-2 commonly retain only 50 % to 60 % of un-welded tensile strength for this class of material, depending on gate angle, melt temperature, and fill speed. Where load paths cross knit lines, the part should be designed with local ribs or relocated gate positions. Published data for the exact BK05110 colour grade is limited, so first-article validation should include weld-line tensile tests on production tooling.
In multi-cavity tools with hot-runner systems, cavity-to-cavity balance becomes critical. The viscosity of B4300G6 BK05110 under shear is lower than that of unfilled PBT because the rigid glass fibres increase shear heating, but the reinforcement raises gate pressure drop in small gates. Production lines with valve-gated hot runners are preferred over open hot tips to prevent stringing and drool. Typical gate diameter for a 2.0 mm wall section should not be below 0.8 mm; smaller gates generate excessive fibre breakage and surface bloom. Hot-runner manifold temperatures are set near 250 °C to 270 °C, with nozzle tip temperature no more than 10 °C above melt temperature to reduce degradation in stagnant zones.
Heat deflection temperature is a short-term, single-point test under ISO 75-2, not a continuous-use temperature rating. For load-bearing parts at elevated temperature, creep modulus is measured under ISO 899-2, and continuous-use temperature is most meaningfully assessed by the relative thermal index under UL 746B. At elevated service temperatures, glass-reinforced PBT can lose a significant fraction of initial flexural modulus under sustained load; the exact creep modulus for BK05110 should be obtained from supplier long-term ageing data. Published data for this specific configuration is limited. Therefore, a metal replacement programme should compare total deflection under sustained load, not only the short-term modulus.
Thermal ageing at the upper service range can shift colour, reduce notched impact, and increase brittleness. Applications exposed to air hotter than 140 °C for more than 500 h should be validated by accelerated ageing to ISO 188 or IEC 60216-1. The grade is typically not selected for continuous air temperatures above 150 °C without derating mechanical loads. In short-term excursions, the 205 °C HDT/A provides margin, but creep and oxidative embrittlement govern long-term design.
Impact-modified PBT grades and flame-retardant grades occupy different positions in the material portfolio. Where low-temperature notched Charpy impact above 10 kJ/m² at −30 °C is required, an impact-modified PBT or a blend may be necessary because the B4300G6 grade is stiffness-oriented rather than toughness-oriented. Where flame-retardant compliance is required, a V-class grade must be specified. The selection between B4300G6 BK05110 and these alternatives is therefore based on the flammability standard, the notched impact requirement, and the creep requirement, not stiffness alone.
Regrind use in production is limited to 20 % by shot weight for non-critical parts after drying. Fines from glass fibre are removed by a dedusting unit, and regrind moisture and bulk density variation must be controlled. Production melt pressure is monitored across the cycle as an indirect measure of viscosity loss from hydrolysed regrind. Conveying systems with sharp feed-line bends should be avoided because glass-filled pellets generate fines that segregate in hoppers and alter glass content in moulded parts.