Basf Ultradur Pbt Gf B4300g6 Bk

BASF Ultradur® PBT+GF B4300G6 BK

    • Product Name: BASF Ultradur® PBT+GF B4300G6 BK
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 583914
    Polymer Type PBT
    Glass Fiber Content 30% by weight
    Color Black
    Density 1.53 g/cm³
    Tensile Modulus 9500 MPa
    Tensile Strength 135 MPa
    Elongation At Break 2.5%
    Charpy Impact Strength 23 C Unnotched 45 kJ/m²
    Charpy Notched Impact Strength 23 C 8 kJ/m²
    Hdt A 1 8 Mpa 205 °C
    Hdt B 0 45 Mpa 220 °C
    Melting Temperature Dsc 223 °C
    Water Absorption Saturation 0.4%
    Equilibrium Water Absorption 23 C 50 Rh 0.2%
    Molding Shrinkage Parallel 0.3%
    Molding Shrinkage Normal 0.8%
    Melt Volume Flow Rate 190 C 2 16 Kg 12 cm³/10 min
    Processing Method Injection molding
    Ul 94 Flammability Rating HB

    As an accredited BASF Ultradur® PBT+GF B4300G6 BK factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-barrier bags, palletized for safe storage and handling of BASF Ultradur® PBT+GF B4300G6 BK.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized, shrink-wrapped 25 kg bags of BASF Ultradur® PBT+GF B4300G6 BK, secured for ocean transport.
    Shipping Shipping description: BASF Ultradur® PBT+GF B4300G6 BK, a black polybutylene terephthalate with glass fiber in pellet form. It is non-hazardous and not regulated as dangerous goods for transport. Use standard closed packaging, keep dry, avoid excessive heat, and follow the SDS and package labeling.
    Storage Store BASF Ultradur® PBT+GF B4300G6 BK in original, sealed containers in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and moisture. Protect from humid conditions and UV exposure. Keep containers closed, avoid dust generation and incompatible chemicals, and do not store near food or drink. Follow the SDS and local regulations.
    Shelf Life Shelf life is approximately five years when stored dry in original sealed packaging, protected from moisture and moderate heat.
    Free Quote

    Competitive BASF Ultradur® PBT+GF B4300G6 BK prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    BASF Ultradur® PBT+GF B4300G6 BK is an injection-molding grade of polybutylene terephthalate containing a nominal glass-fiber content of 30% by mass. The grade-code suffix G6 identifies the glass-fiber loading in BASF Ultradur nomenclature; the suffix BK designates black color. The matrix is a semicrystalline polyester produced from 1,4-butanediol and terephthalic acid. Glass fibers are retained through a silane coupling system that controls interfacial adhesion, and the compound is supplied as cylindrical pellets for screw-fed injection molding. The grade is specified where unfilled PBT lacks sufficient stiffness, creep resistance, or dimensional stability, and where electrical insulation under moderate thermal stress is required.

    What Does the 30% Glass-Fiber Reinforcement Do to the Stress-Strain Response?

    Under tensile test conditions to ISO 527-2, the representative tensile modulus is reported between 9500 MPa and 10500 MPa at 23 °C. Tensile stress at break is reported between 130 MPa and 140 MPa; tensile strain at break is typically below 3.0%. The modulus increase relative to unfilled PBT, which commonly falls between 2600 MPa and 2800 MPa, is therefore approximately threefold, while elongation declines sharply. Flexural modulus to ISO 178 is reported between 8500 MPa and 9500 MPa. Charpy notched impact strength to ISO 179-1/1eA at 23 °C is reported between 7 kJ/m² and 9 kJ/m²; subzero values are lower. These values are representative of publicly available product literature and do not replace lot-specific certificates of analysis.

    PropertyStandardRepresentative range
    DensityISO 1183-11.52–1.54 g/cm³
    Tensile modulusISO 527-29500–10500 MPa
    Tensile stress at breakISO 527-2130–140 MPa
    Tensile strain at breakISO 527-22.0–3.0 %
    Flexural modulusISO 1788500–9500 MPa
    Charpy notched impact, 23 °CISO 179-1/1eA7–9 kJ/m²
    Heat deflection temperature, 1.80 MPaISO 75-2195–205 °C
    Vicat softening temperature, B50ISO 306205–215 °C
    Melt volume-flow rate, 250 °C/2.16 kgISO 1133-110–15 cm³/10 min
    Water absorption, saturationISO 620.3–0.5 %

    Melt volume-flow rate to ISO 1133-1 is reported between 10 cm³/10 min and 15 cm³/10 min at 250 °C under 2.16 kg. The glass-fiber reinforcement increases low-shear viscosity and produces marked shear thinning in narrow gates and thin walls. Published capillary rheometry data specific to B4300G6 BK is limited; mold-filling simulation should therefore use shear-viscosity data supplied by the manufacturer rather than generic unfilled PBT datasets.

    Before processing, the pellets are dried in a desiccant dryer with a dew point at or below -30 °C. Residual moisture must be held below 0.04% by mass; higher moisture levels cause hydrolytic cleavage at melt temperature, producing surface splay, loss of molecular weight, and reduced notched impact strength. On injection molding machines with screw diameters between 30 mm and 80 mm, the melt temperature measured at the nozzle is maintained between 250 °C and 270 °C. Mold temperature is held between 40 °C and 80 °C; the upper half of that range improves melt-front fusion and reduces post-mold anisotropy. Glass-fiber abrasion requires hardened screw flights, barrel coatings, and check ring components. Extended residence time above 270 °C should be avoided because black colorant and polyester matrix degrade under prolonged exposure.

    When This Grade Is Converted From Unfilled PBT in Existing Cavities

    Conversion from unfilled PBT to B4300G6 BK reduces mold shrinkage and increases shrinkage anisotropy. Glass fibers orient predominantly in the direction of flow, so linear mold shrinkage may be 0.2% to 0.5% in the flow direction and higher in the transverse direction. Unfilled PBT typically exhibits shrinkage between 1.5% and 2.0%. Existing cavities designed for unfilled PBT therefore require re-evaluation of gate size, runner diameter, and vent depth. If the tool is not recut, the lower shrinkage may produce ejection drag, higher clamp pressure, and flash at the parting line.

    Relative to the less-filled Ultradur B4300G2 and Ultradur B4300G4 grades, the G6 grade has higher tensile and flexural modulus, lower elongation at break, and lower unnotched impact. The material is not an impact-modified product, and subzero Charpy notched impact is below that of impact-modified PBT blends. Direct substitution into living hinges or snap-fit designs that rely on large strain recovery is not appropriate. In snap-fit arms, the maximum permissible deflection at a wall thickness of 2 mm is governed by the tensile strain at break below 3.0%; designs should convert strain energy through geometry rather than material ductility.

    Processing parameterRecommended rangeUnit or condition
    Drying temperature80°C
    Drying time4h
    Residual moisture<0.04% by mass
    Melt temperature250–270°C
    Mold temperature40–80°C
    Back pressure0.3–0.7MPa
    Cushion2–5mm

    On production machines with clamp forces from 800 kN to 12000 kN, the main process defect observed with glass-fiber PBT is fiber accumulation at the melt front, which appears as dull weld lines and reduced gloss. Increasing mold temperature to 70 °C improves melt-front fusion but adds several seconds of cycle time per 10 °C increase in cold-runner tools with wall thicknesses below 2.5 mm. The trade-off is managed by holding the mold at the upper recommended temperature for structural parts and at 50 °C for dimensionally flat covers.

    Electrical Tracking Resistance, Thermal Limits, and Hydrolytic Boundaries

    For insulating connector bodies and terminal strips, volume resistivity measured to IEC 60093 is reported in the range of 1E13 Ω·m to 1E15 Ω·m at 23 °C. Surface resistivity is similarly high. Comparative tracking index to IEC 60112 is commonly reported between 350 V and 600 V; carbon-black pigmentation may lower tracking index relative to a natural grade by at least one test-voltage step. The UL 94 rating for glass-filled PBT without flame retardants is typically HB; the current UL Yellow Card for the specific BK color and thickness should be verified because black pigmentation can alter ignition behavior.

    Thermal service is constrained by thermo-oxidative aging and hydrolysis. Published data for B4300G6 BK under long-term heat aging is limited; glass-filled PBT without special heat stabilization is generally applied in mechanical service only below 140 °C. Hydrolytic degradation accelerates in continuous hot water above 60 °C. The material is not suitable for continuous immersion in 85 °C water without part-specific validation. Contact with strong alkalis, hot mineral acids, and steam should be avoided; short-term contact with dilute mineral acids and aliphatic hydrocarbons at ambient temperature may be acceptable only after part testing.

    In Multi-Gate Housings, Weld-Line Placement Is the Controlling Variable

    In multi-cavity connector bodies and automotive sensor housings, weld-line location controls field failure. Glass fibers can align parallel to the weld line, producing a notch-sensitive plane with reduced strength. Gate placement should position the weld line outside snap-fit retention features and sealing ridges. When the tool contains more than eight cavities, mold-filling analysis with a 30% glass-fiber PBT viscosity model is used to predict fill imbalance. Process settings that increase melt temperature to 265 °C and mold temperature to 70 °C improve weld-line strength but increase cycle time and post-mold shrinkage.

    When metal contacts are insert-molded, preheating inserts to 80 °C to 100 °C reduces differential thermal shrinkage and cracking around the insert. The coefficient of linear thermal expansion of 30% GF-PBT is typically 25 µm/(m·K) to 40 µm/(m·K) in the flow direction and higher transverse to flow; this is lower than unfilled PBT but still high relative to steel. Inserts should be degreased and free of silicone mold-release agents. Regrind addition is limited to 25% by mass; higher levels reduce tensile modulus and change black color uniformity. For hot-runner tools, valve gates are preferred to open gates because they reduce fiber breakage at the gate and improve part-to-part weight consistency.

    Top