Basf Ultradur Pbt Gf B4040g6 Bk Q29 15075

BASF Ultradur® PBT+GF B4040G6 BK Q29 15075

    • Product Name: BASF Ultradur® PBT+GF B4040G6 BK Q29 15075
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 718110
    Polymer Type PBT
    Glass Fiber Content Percent 30
    Density G Cm3 1.53
    Tensile Modulus Mpa 10000
    Tensile Strength Mpa 135
    Elongation At Break Percent 2.5
    Charpy Impact Strength 23c Kj M2 50
    Charpy Notched Impact Strength 23c Kj M2 8
    Heat Deflection Temperature A C 205
    Heat Deflection Temperature B C 220
    Melting Point C 223
    Water Absorption Percent 0.4
    Molding Shrinkage Percent 0.3-0.5
    Melt Temperature C 260-280
    Mold Temperature C 80-100
    Flammability Ul94 HB
    Processing Method injection molding

    As an accredited BASF Ultradur® PBT+GF B4040G6 BK Q29 15075 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg moisture-proof bags on pallets, BASF Ultradur® PBT+GF B4040G6 BK Q29 15075 packaging protects material during transport and storage.
    Container Loading (20′ FCL) A 20-foot FCL container is loaded with BASF Ultradur® PBT+GF B4040G6 BK Q29 15075 chemical, securely packed for shipment.
    Shipping BASF Ultradur® PBT+GF B4040G6 BK Q29 15075 is shipped as non-hazardous polymer granules in sealed bags or boxes. It is not regulated for transport under DOT, IMDG, IATA, or ADR. Keep dry, avoid excessive heat, and protect packaging from damage.
    Storage Store BASF Ultradur® PBT+GF B4040G6 BK Q29 15075 in a cool, dry, well-ventilated area, protected from direct sunlight, moisture, heat, and ignition sources. Keep in original, tightly closed containers or sealed bags, off the floor and away from strong oxidizers. Avoid prolonged moisture exposure; dry/condition before processing per BASF recommendations.
    Shelf Life Typically 24 months when stored dry in sealed original packaging below 30°C, protected from moisture and UV.
    Free Quote

    Competitive BASF Ultradur® PBT+GF B4040G6 BK Q29 15075 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    BASF Ultradur® PBT+GF B4040G6 BK Q29 15075 is a semicrystalline polybutylene terephthalate compound reinforced with 30% glass fiber by weight. The designation B4040G6 identifies the base resin and glass-fiber loading within the Ultradur® PBT+GF portfolio, while the suffix BK Q29 denotes black coloration and 15075 is the commercial variant or color-match code used for supply-chain traceability. The material is specified for injection-molded parts that require substantially higher stiffness than unreinforced PBT, lower thermal expansion, and short-term dimensional stability at elevated temperature. Representative usage includes connector bodies, sensor housings, relay bases, electronic control unit housings, headlamp bezels, mirror brackets, impeller housings, and structural underhood components. Because the glass fibers orient during melt flow, the mechanical response is anisotropic and depends strongly on gate location, wall thickness, weld-line position, and fiber-length retention in the molded part. Published data obtained from standard ISO specimens therefore cannot be transferred directly to highly oriented thin-wall sections or weld-dominated geometries without explicit validation.

    What Distinguishes This 30% Glass-Filled PBT Grade From Lower Glass Variants?

    The primary compositional distinction is the mass fraction of short glass fiber, fixed at 30%. This places B4040G6 above lower glass loadings in the Ultradur B4040G series and below specialty grades that may carry mineral fillers, flame retardants, or higher reinforcement content. The structural consequence is an increase in tensile modulus and heat deflection temperature, accompanied by lower elongation at break and higher melt viscosity. The comparative values in the table below use typical manufacturer literature values for the filled grade and general reference data for unfilled PBT; unfilled PBT is not an exact Ultradur grade but serves as a baseline for the effect of 30% glass reinforcement.

    PropertyUltradur® B4040G6 typicalUnfilled PBT referenceTest method
    Density1.55 g/cm³1.30 g/cm³ISO 1183
    Tensile modulus10,500 MPa2,600 MPaISO 527-2
    Tensile stress at break135 MPa55 MPaISO 527-2
    Flexural modulus9,000 MPa2,500 MPaISO 178
    Charpy notched impact at 23 °C9 kJ/m²4 kJ/m²ISO 179/1eA
    Heat deflection temperature A at 1.8 MPa200 °C55 °CISO 75-2
    Molding shrinkage, parallel0.4 %1.5 %ISO 294-4
    Molding shrinkage, normal1.2 %1.8 %ISO 294-4
    Melt volume-flow rate 250 °C/2.16 kg13 cm³/10 min40 cm³/10 minISO 1133-1
    Melting temperature, DSC223 °C225 °CISO 11357-3
    Moisture absorption at 23 °C/50% RH0.2 %0.2 %ISO 62
    Flammability ratingHBHBUL 94

    Compared with a PBT grade containing 20% glass fiber, B4040G6 normally exhibits higher tensile modulus, higher heat deflection temperature, and greater creep resistance, but lower melt flow length and reduced ductility. A 20% glass-filled PBT may show a tensile modulus near 7,000 MPa and an HDT/A value near 180 °C; therefore B4040G6 is preferred only where the additional stiffness and heat resistance justify reduced flow and lower elongation. Compared with unreinforced PBT, the 30% glass addition raises tensile modulus roughly 4× and shifts HDT/A from approximately 55 °C to 200 °C. The penalty is a clear transition from ductile yielding to semi-brittle fracture, especially at sub-zero temperatures. Designers should not select B4040G6 where snap-fit flexure, repeated post-mold deformation, or high weld-line strain is the dominant loading mode without verifying strain at break and weld-line strength on prototype tools.

    In a desiccant-dryer configuration with air dew point below -30 °C, pellets of B4040G6 must be dried to a residual moisture level below 0.04% before melt processing. PBT hydrolyzes at melt temperature in the presence of moisture, producing molecular-weight reduction, surface splay, reduced notched impact, and batch-to-batch viscosity drift. The manufacturer’s published drying guidance for PBT/GF30 recommends 80 °C to 100 °C for 4 h to 6 h. However, hopper dryers must deliver sufficient air flow and residence distribution. A system holding pellets at the correct setpoint but with conditioned-air flow below 1.85 m³/h per kg/h of material throughput can leave the core moisture above the specified limit and produce intermittent molding defects. Drying above 120 °C should be avoided unless explicitly validated because oxidative discoloration and additive loss may occur even below the melting point.

    At the press, melt temperature measured at the nozzle should be held between 250 °C and 270 °C. Barrel settings should be profiled so that the rear zone is 230 °C to 240 °C, the center zone 240 °C to 250 °C, the front zone 250 °C to 260 °C, and the nozzle 255 °C to 265 °C. Screw peripheral speed should be limited to 0.1 m/s to 0.3 m/s; excessive screw rotation causes glass-fiber attrition and lowers tensile strength because the residual fiber-length distribution shifts downward. Back pressure normally ranges from 5 MPa to 15 MPa; higher back pressure improves melt homogeneity but increases shear heating and residence time. Injection velocity should produce a fill time of 0.5 s to 2.0 s for thin-wall parts, with higher velocity used only when gas traps or hesitation lines appear. Mold temperature is best controlled at 80 °C to 100 °C where crystallinity and dimensional stability are critical; the lower range of 60 °C to 80 °C may be acceptable for less loaded parts but produces lower crystallinity and more post-mold shrinkage.

    Melt residence time should remain below 5 min. If the cycle is interrupted, barrel temperatures should be reduced and the machine purged with fresh material. Regrind content should not exceed 25%; each re-pass through the screw reduces glass-fiber length and therefore lowers tensile strength, fatigue strength, and notched impact. Reground sprues and runners must be dried before reuse because their increased surface area can accelerate moisture uptake. The grade is not recommended for processing on general-purpose screws with compression ratios above 2.5:1 without adjustment, because the glass-filled rigid pellets can produce excessive shear heating and fiber breakage. A medium-compression screw with L/D of 20:1 to 25:1 and wear-resistant barrel coating is preferred. Observed production-scale failure modes have included surface blistering after inadequate drying, warp reversal following mold-temperature changes, weld-line cracks in connector snap arms, and gate blush when injection speed was too high. The material is not suitable for direct contact with hot strong alkaline solutions or strong acids; it resists many automotive fuels, oils, greases, and neutral coolants under normal service conditions, but continuous immersion in hot coolant above 120 °C is not recommended.

    Mechanical and Thermal Data Must Be Interpreted With Moisture, Orientation, and Fiber-Length Effects

    Test data for B4040G6 are generated on dry-as-molded or conditioned specimens under standard ISO conditions. For tensile and flexural tests, specimens are conditioned at 23 °C and 50% relative humidity for 88 h unless otherwise specified. Because PBT absorbs limited moisture, the conditioning effect is smaller than in polyamide, but post-mold shrinkage and crystallinity continue after demolding. Measurements taken within 4 h of molding may show higher residual stress and lower dimensional stability than values measured after 24 h. For parts operating in hot dry environments, tests at 80 °C or 120 °C should be used because PBT may undergo post-crystallization and slight embrittlement. Glass-fiber orientation causes anisotropy: tensile modulus in the transverse flow direction may be significantly lower than in the parallel flow direction. Weld lines in glass-reinforced PBT typically reduce tensile strength by 30% to 50% relative to bulk material; therefore gate location and flow-front convergence must be managed in connector housings and ring-shaped parts.

    In automotive electrical distribution housings and sensor carriers, B4040G6 is typically used underhood at continuous ambient temperatures up to approximately 120 °C and short-term peaks approaching 200 °C. The black colorant package allows laser marking with contrast, but the marking quality depends on the specific pigment formulation; dark carbon black can reduce contrast for certain laser wavelengths. Where enhanced ultraviolet stability is required, additional stabilizer packages or protective coatings may be necessary because PBT without UV stabilization loses surface gloss and mechanical properties after prolonged outdoor exposure. The product is not flame-retarded and should not be substituted for V-0 grades in open-arc electrical applications unless the end-use product meets the relevant IEC 60695 or UL 94 end-product test. Compared with natural or non-black variants of B4040G6, the BK Q29 15075 colorant package may shift comparative tracking index and electrical surface resistance; black pigments can alter surface conductivity modestly and change laser-marking contrast. Therefore homologation on a natural lot is not sufficient for production lots. The product also differs from glass/mineral hybrid PBT grades in warpage behavior: all-glass grades have higher shrinkage anisotropy, so long flow or flat parts may warp more than a glass/mineral hybrid. Mold-flow simulation with fiber-orientation tensors is required for warpage-critical geometries.

    Top