| HS Code | 891866 |
| Productname | BASF Ultradur® PBT+GF B 4300 G2 BLACK 15042 |
| Manufacturer | BASF |
| Polymertype | PBT |
| Glassfibercontent | 10% |
| Color | Black 15042 |
| Density | 1.37 g/cm³ |
| Tensilemodulus | 6000 MPa |
| Tensilestrength | 85 MPa |
| Elongationatbreak | 2.5% |
| Charpynotchedimpactstrength 23c | 4 kJ/m² |
| Charpyunnotchedimpactstrength 23c | 25 kJ/m² |
| Hdt A | 200 °C |
| Hdt B | 215 °C |
| Meltingtemperature | 220 °C |
| Vicatsofteningtemperature B | 175 °C |
| Moldingshrinkage | 0.4-0.8% |
| Waterabsorption Saturation | 0.4% |
| Mvr 250c 2 16kg | 20 cm³/10 min |
As an accredited BASF Ultradur® PBT+GF B 4300 G2 BLACK 15042 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg moisture-barrier polyethylene bags, palletized, clearly labeled with product identification and safety information for industrial use. |
| Container Loading (20′ FCL) | 20′ FCL loaded with BASF Ultradur® PBT+GF B 4300 G2 BLACK 15042, palletized 25 kg bags, shrink-wrapped and secured for shipment. |
| Shipping | BASF Ultradur® PBT+GF B 4300 G2 BLACK 15042 is a glass-fiber-reinforced PBT compound supplied in pellet form. Ship in sealed, moisture-proof bags or containers under dry, ambient conditions, away from sunlight and contamination. Generally non-hazardous and not transport-regulated; follow SDS and local rules. |
| Storage | Store in a cool, dry, well-ventilated area away from heat, ignition sources, and direct sunlight. Keep containers tightly closed to prevent moisture pickup and contamination. Avoid contact with strong oxidizers and incompatible materials. Use good dust control and hygiene practices. Protect from physical damage and follow local regulations and the manufacturer’s safety data sheet. |
| Shelf Life | BASF Ultradur® PBT+GF B 4300 G2 BLACK 15042 has a shelf life of 24 months when stored dry in original sealed packaging. |
Desiccant-bed drying of Ultradur® B 4300 G2 BLACK 15042 at 120 °C for 4 h with a supply-air dewpoint of -30 °C lowers residual moisture below 0.04 wt% before the material reaches the feed throat. At ambient relative humidity above 60%, opened containers are re-dried under the same conditions to prevent hydrolysis at melt temperature. A three-zone screw is typically run with a rear-zone set point of 230–250 °C, a compression-zone set point of 250–265 °C, a metering-zone set point of 250–270 °C, and a nozzle set point of 250–265 °C. Melt excursions above 280 °C accelerate chain scission in the PBT ester backbone, even when residual moisture is controlled. In automotive wheel-speed sensor housings, tool surfaces are held at 80–100 °C to regulate skin-core morphology and to suppress differential shrinkage around magnetic insert pins. The fixed glass-to-PBT ratio of the G2 designation reduces linear mould shrinkage relative to unfilled PBT, but fibre orientation along the flow front produces anisotropic post-mould warpage. The result must be corrected by gate placement on the thick boss and by holding pressure rather than by increasing melt temperature. Moulded test plaques are evaluated under ISO 527-2:2012 and ISO 294-1:2017; values from this black grade are taken from the BASF Ultradur datasheet and the UL Yellow Card, not substituted from natural unfilled PBT data. Connector contact retention is validated to USCAR-2 and OEM-specific vibration profiles, while material compliance is confirmed to RoHS Directive 2011/65/EU and REACH Article 33 declarations. The terminal part class covers engine-compartment sensor bodies, accelerator-pedal position-sensor frames, and transmission-mount speed-sensor carriers.
The primary risk in insert moulding is not melt temperature but the thermal gradient between the preheated brass and the solidifying PBT matrix. Brass inserts are preheated to 120 °C in a circulating-air station immediately before robot placement. Insert temperatures below 80 °C quench the melt and create a micro-gap at the metal-polymer interface. Insert temperatures above 150 °C can induce local oxidative discolouration of the black 15042 surface. The moulding machine’s holding-pressure profile is set at 40–60 MPa for the first 2 s and ramped to 20–30 MPa for the next 5 s to compensate for the higher heat extraction of the brass core. Wall stock around the busbar is maintained at a minimum ratio of 1.5:1 polymer thickness to insert thickness. Lower ratios cause the melt front to bifurcate and leave a weld line along the busbar edge. The terminal programme includes dish-washer timer bases, washing-machine rotary switch cams, and oven function-selector bodies. End-product safety is tested to IEC 60335-1:2020 and glow-wire flammability is assessed to IEC 60695-2-12 at the production wall thickness. Published glow-wire ignition temperature data for this specific black glass-filled configuration is limited. Final approval therefore requires end-product glow-wire testing at the exact wall thickness and insert geometry used in the tool.
For terminal-block bodies that must survive 85 °C continuous service under IEC 60947-7-1, the material’s tracking resistance and dimensional stability under clamping pressure are evaluated before tensile strength is considered. The 15042 black colour package contains carbon black, which lowers surface resistivity relative to natural PBT but does not guarantee static dissipative performance. If an application requires a surface resistivity below 10^6 Ω/sq measured to IEC 62631-3-2, a dedicated conductive grade must be selected instead. Moulding uses a two-plate tool with a central sprue and fan gates into the terminal-barrel region. Barrel temperatures are held at 250–270 °C, while the tool surface is held at 70–90 °C to reduce post-mould shrinkage below the threshold needed for 0.8 mm-pitch terminal retention. Melt residence time is limited to 5 min from plastication start to gate seal. Longer residence times reduce un-notched Charpy impact measured to ISO 179-1/1eU and create brittle fracture at the wire-clamp insertion point. Terminal products include plug-in relay bases, panel-mount terminal strips, and PLC I/O connector blocks used in machinery control cabinets. Tracking resistance is verified under IEC 60112, and flame class is taken from the UL Yellow Card under UL 94 HB at the tested thickness. The assembled end product may require a higher glow-wire classification than the raw material because metal parts act as heat sinks during ignition testing.
| Standard | Measured property or condition | Application context |
|---|---|---|
| ISO 527-2:2012 | Tensile modulus, 1 mm/min | Connector shell stiffness |
| ISO 179-1/1eU | Un-notched Charpy impact, 23 °C | Terminal-block insertion |
| IEC 60112 | Comparative tracking index | Brush-holder creepage path |
| UL 94 HB | UL Yellow Card minimum thickness | Flame class verification |
| IEC 60695-2-12 | Glow-wire end-product test | Appliance timer base |
Regrind reuse in glass-filled PBT is limited by glass-fibre length attrition in the screw and by hydrolysis at the gate. BASF processing recommendations for Ultradur grades permit up to 30% regrind blended with virgin pellets for non-safety interior applications when the regrind is dry, free of dust, and passed through a magnet and a screen pack before the hopper. Higher regrind fractions reduce notched Izod impact measured to ASTM D256-10 because the mean fibre length after a single extrusion pass is shorter than the original pellet fibre length. The practical consequence appears in automotive relay bases when the terminal busbar insertion force rises above the specification limit. The lower fracture resistance of the regrind-rich matrix promotes micro-cracks at the terminal slots. For relay bases moulded in 24-cavity family tools, the shot volume should not exceed 60–70% of barrel capacity so that material residence time remains below 6 min at 250 °C. The tool is run with valve gates sequenced in three groups to balance cavity pressure within 5%. Cavity pressure sensors in the first and last cavities provide the control signal for holding-pressure switchover at 45 MPa. Compliance for relay bases is verified to IEC 61810-1:2015 and, where used in engine compartments, to USCAR-2 Class 3. Published data for the effect of multiple regrind passes on this exact black 15042 grade is limited. A production validation of impact strength and dimensional stability at 0%, 10%, 20%, and 30% regrind fractions is required before final approval.
Shot-to-shot consistency in 16-cavity hot-runner moulds for electric motor brush holder bodies is governed by manifold balance rather than by the material’s melt volume-flow rate alone. The grade is processed with a hot-runner manifold set at 250–260 °C. Valve-gate tips open sequentially with a delay of 0.5 s between the centre and outer cavities to prevent premature freeze-off at the small gate land of 0.5 mm. Back pressure is maintained at 0.5–0.8 MPa hydraulic to homogenise the glass-fibre distribution. Screw speed is limited to 80–120 rpm to avoid fibre breakage in the plastication zone. The brush-holder body is moulded around a copper commutator ring insert that is preheated to 100 °C. The resultant part cannot be judged by visual inspection alone. Ultrasonic C-scan imaging is used to detect interfacial voids smaller than 0.3 mm. Terminal components include fractional-horsepower motor brush holders, armature support plates, and trigger-switch housings in hand-held power tools. Compliance for tool motors is tested to IEC 62841-1:2014, and the material is checked for comparative tracking index under IEC 60112 because brush dust can create conductive tracks across the holder surface during service. Carbon black in the 15042 black colour package masks some surface degradation. Thermal ageing is therefore tracked by tensile elongation at break following ISO 527-2:2012 after 1,000 h at 120 °C. Published long-term ageing data for this specific black configuration is limited and should be generated on production-representative plaques.
Continuous exposure to under-hood air above 120 °C shifts the limiting failure mode from fibre-matrix debonding to thermo-oxidative embrittlement of the PBT ester. The black pigmentation in 15042 absorbs infrared energy and can increase surface temperature by 5–10 K under direct lamp exposure. Dark-colour parts therefore require a service-temperature margin. Moulded parts for charge-air cooler end caps or exhaust-gas sensor brackets are not recommended unless the end-user validates thermal endurance because published data for this specific black glass-filled configuration is limited. The recommended screening test is tensile elongation at break measured to ISO 527-2:2012 after 1,000 h oven exposure at 120 °C, with a retention threshold of 50% of initial elongation. Processing for thick-section covers uses a melt temperature of 250 °C and a tool temperature of 80 °C. The shot is compressed at 50 MPa until gate freeze. Terminal products include relay-box covers, fuse-box lids, and sensor brackets where maximum continuous surface temperature does not exceed 120 °C. Compliance for under-hood plastic parts is checked against ISO 75-2:2013 heat deflection temperature and the OEM’s long-term heat-ageing specification. The black grade’s UL Yellow Card gives the thickness-dependent flame class, and end-use flame performance must be verified on the finished assembly. Avoid purging with PVC compounds because residual chlorine degrades PBT at melt temperatures above 250 °C.
Competitive BASF Ultradur® PBT+GF B 4300 G2 BLACK 15042 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
BASF Ultradur® PBT+GF B 4300 G2 BLACK 15042 is a 10% glass-fibre-reinforced polybutylene terephthalate compound supplied as black pellets in the 15042 colour code. The grade belongs to the B 4300 family, where the suffix G2 denotes a nominal glass-fibre loading of 10% by weight; G4, G6 and G10 grades contain 20%, 30% and 50% glass respectively. The base polymer is semicrystalline, melting at approximately 223 °C, with a density reported under ISO 1183-1 of 1.31–1.33 g/cm³. Under ISO 1133-1:2022 at 250 °C and 2.16 kg, the melt volume-flow rate is commonly reported in the range 18–24 cm³/10 min. This flow range permits injection pressures of 60–90 MPa for parts with flow length/wall thickness ratios up to 150:1 in properly gated tools; higher glass loadings require higher injection pressure and may exhibit flow hesitation in sections below 0.8 mm. Typical applications include thin-wall connector housings, relay bases, sensor bodies, coil formers and switch components where resistance to fuels, greases and dilute aqueous cleaning solutions at ambient to moderate temperatures is required. The nominal glass loading lowers mould shrinkage and raises tensile modulus relative to unfilled PBT while retaining a lower melt viscosity than 20% and 30% glass-reinforced grades.
Hydrolytic degradation is the dominant process risk for PBT. Prior to plastication, pellet moisture must be reduced to less than 0.04% by weight using a closed-loop desiccant dryer with an air temperature of 80–100 °C and a dew point of −30 °C or lower. For surface-moisture pickup after saturation storage or intermittent hopper charging, 4 h at 80 °C is the minimum; at ambient conditions above 60% relative humidity, manual conveying lines should be purged with dry air and hopper residence times kept below 1 h. Melt temperature zones from the feed throat to the nozzle are typically set between 240 °C and 270 °C. The maximum measured melt temperature should remain below 280 °C because hydrolytic chain scission and thermal oxidation reduce molecular weight and weld-line strength.
Screw configuration on a production injection-moulding machine affects dispersion. A 20:1 to 25:1 L/D three-zone screw with a compression ratio of 2.5:1 and a shallow metering section is sufficient for glass-fibre distribution. The non-return valve should have hardened steel surfaces because 10% glass fibre is mildly abrasive; flame-hardened or bimetallic barrels are recommended where annual throughput exceeds 300 t. Barrel residence time at melt temperature should not exceed 5 min; longer residence causes yellowing and a loss of notched impact strength that may exceed 10% compared with minimum residence time. Hot-runner manifolds require externally heated channels with no dead spots; internal radius bends below 3 mm produce black specks and fibre accumulation.
Mould temperature is a second control point. At 40 °C, cycle times are shortest but moulded-in stress is higher; at 80 °C, polymer crystallinity and part dimensions are more stable. A temperature differential greater than 30 °C across cavity inserts causes differential shrinkage and warpage. Thickness transitions should be radiused to no less than 0.5 mm and wall thickness variation should remain within 0.8–1.0 mm of nominal to avoid sink marks and hot spots. For thin-wall sections, filling speed should be high enough to prevent freeze-off but not so high that shear heating exceeds the 280 °C limit at the gate. Regrind addition up to 30% by weight is acceptable when the material is dry and free of contamination, but glass-fibre length is shortened by repeated extrusion and notched impact strength may fall by 10–20% at 30% regrind.
Dry-as-moulded test specimens conditioned under ISO 291 are used to generate comparative data. The values are not specification limits. The dry tensile modulus of B 4300 G2 is 4,200–4,800 MPa according to ISO 527-2. The tensile stress at break is 80–95 MPa, and flexural strength according to ISO 178 is 130–150 MPa. Moisture conditioning at 23 °C/50% RH lowers these values by less than 10%, but hot-water ageing above 80 °C produces progressive losses due to ester hydrolysis. Glass transition temperature is near 55 °C by DSC per ISO 11357-2; heat deflection temperature under 0.45 MPa is in the range 210–220 °C and under 1.80 MPa in the range 150–165 °C per ISO 75-2/B. Flammability is normally graded as HB under UL 94 for typical wall thicknesses; the current yellow card for the exact colour and wall thickness must be consulted before design release.
| Property | Standard | Unit | Representative range |
|---|---|---|---|
| Density | ISO 1183-1 | g/cm³ | 1.31–1.33 |
| Melt volume-flow rate at 250 °C/2.16 kg | ISO 1133-1:2022 | cm³/10 min | 18–24 |
| Tensile modulus | ISO 527-2 | MPa | 4200–4800 |
| Tensile stress at break | ISO 527-2 | MPa | 80–95 |
| Flexural strength | ISO 178 | MPa | 130–150 |
| Charpy notched impact strength, 23 °C | ISO 179-1/1eA | kJ/m² | 4.0–6.0 |
| Heat deflection temperature, 0.45 MPa | ISO 75-2/B | °C | 210–220 |
| Heat deflection temperature, 1.80 MPa | ISO 75-2/B | °C | 150–165 |
| Vicat softening temperature B50 | ISO 306/B50 | °C | 210–220 |
Longitudinal coefficient of linear thermal expansion is 30–50 × 10⁻⁶ K⁻¹ and transverse is 90–120 × 10⁻⁶ K⁻¹ measured per ISO 11359-2. This anisotropy is smaller than 30% glass-fibre PBT, but still sufficient to cause out-of-plane movement in long thin parts when cooling is uneven. Mould shrinkage measured after 24 h on a 60 mm × 60 mm × 2 mm plaque is approximately 0.9–1.2% in flow direction and 1.2–1.6% transverse; gate type and mould temperature move these values. Warpage in rectangular housings with side gating can be reduced by using multiple end gates or by lowering the glass content from GF20 to GF10, which is one reason this grade is selected for dimensions above 100 mm.
Selection of B 4300 G2 is typically made after an unfilled PBT part fails in creep or dimensional stability but a 20% or 30% glass-filled grade creates over-stiffness, warpage, or tool wear. The tensile modulus of unfilled PBT is typically 2,500–2,800 MPa; substituting B 4300 G2 raises modulus by approximately 60–80%, but the 30% glass variant reaches 9,000–10,000 MPa. The lower fibre loading of G2 preserves better flow and a smoother surface; the presence of 10% glass produces a surface roughness lower than GF30 but with visible glass-fibre orientation. Impact behaviour is intermediate: Charpy notched impact at 23 °C is 4.0–6.0 kJ/m² for G2, while GF30 is often 7–9 kJ/m². However, in cold environments below −30 °C, all PBT glass-filled grades become significantly more brittle; impact requirements must be tested under ISO 179-1/1eA at the lowest use temperature.
The lower fibre content also affects fibre orientation and shrinkage anisotropy. In a centre-gated flat plate, GF20 and GF30 grades show greater difference between flow and transverse shrinkage than GF10; the flow-to-transverse shrinkage ratio in B 4300 G2 is often 0.7–0.9, whereas GF30 can fall to 0.2–0.4 in the direction of fibre orientation. The smaller orientation effect is used in parts with multiple side walls and snap-fit features that would otherwise distort. The creep behaviour of unfilled PBT at 60 °C is often insufficient for snap-fit retaining forces; the 10% glass reinforcement raises the short-term creep modulus but does not alter the base polymer time-dependent response. For long-term loads, tensile creep tests under ISO 899-1 are required because available datasheet modulus values do not substitute for creep data.
| Property | Unfilled PBT reference | B 4300 G2 | B 4300 G6 |
|---|---|---|---|
| Density | 1.30–1.31 g/cm³ | 1.31–1.33 g/cm³ | 1.51–1.53 g/cm³ |
| Tensile modulus | 2500–2800 MPa | 4200–4800 MPa | 9000–10000 MPa |
| Charpy notched impact strength, 23 °C | 2.5–3.5 kJ/m² | 4.0–6.0 kJ/m² | 7.0–9.0 kJ/m² |
| Heat deflection temperature, 1.80 MPa | 50–60 °C | 150–165 °C | 200–205 °C |
| Mould shrinkage, flow direction | 1.8–2.0% | 0.9–1.2% | 0.2–0.4% |
These are representative data from dry-as-moulded specimens; they do not form part of a specification release. Published data for each coloured grade and specific lot is available in the producer's product datasheet and UL yellow card.
Electrical connector housings, relay bases, coil formers and sensor bodies are the main part geometries for this black 15042 grade. Comparative tracking index measured under IEC 60112 is commonly reported above 400 V for unreinforced PBT; the glass fibre and black pigment can reduce the value by 100–200 V depending on board-level contamination. A 1.0 mm moulded plaque typically shows dielectric strength of 25–35 kV/mm under IEC 60243-1. These electrical values are not design guarantees: weld lines, moisture uptake and surface contamination in end-use environments reduce them. Creepage and clearance dimensions should be based on worst-case conditioned values from the final moulded component, and the material should be re-qualified if the customer changes moulding parameters.
Fuel, engine oil, transmission fluid and cleaning solvent resistance are often required in the target applications. PBT has broad resistance to aliphatic hydrocarbons, engine oil, diesel fuel and dilute aqueous salt solutions at temperatures up to 80 °C. It is not resistant to hot water, steam, strong mineral acids, strong bases or long-chain aromatic alcohols above ambient temperature. Hydrolysis proceeds by ester backbone scission; glass fibre creates extra interfacial area, so this grade is not a hydrolysis-stabilized product. For coolant or hot-water contact above 80 °C, hydrolysis-stabilized PBT or PBT/polyester blends are required. Exposure to ethanol blends above 50% or aggressive brake fluids should be tested according to ISO 62 immersion methods because swelling can change dimensional measurements by more than 0.5%. Water absorption after 24 h at 23 °C per ISO 62 is below 0.1%, which makes the grade dimensionally stable in short-term humidity. Saturation moisture is below 0.4%; nylon alternatives absorb several percent by weight, producing greater dimensional change. However, continuous exposure to 50 °C/95% RH can cause hydrolysis after several weeks if the part is under mechanical load.
The black 15042 colour and the non-flame-retardant base resin are generally outside food-contact and medical certifications; compliance with RoHS 2011/65/EU and REACH SVHC restrictions is supplier-confirmed. If an application requires V-0 flammability under UL 94, a flame-retarded BASF Ultradur PBT grade is required instead of this standard glass-reinforced grade.
Black 15042 contains short glass fibres with a typical number-average fibre length after plastication of 200–400 μm; the exact distribution depends on screw speed, back pressure and residence time. Gates should have a minimum wall thickness of 0.8–1.0 mm for wall sections of 1.5 mm; for wall sections below 1.0 mm, a film or flash gate is preferred to reduce fibre breakage. Land lengths should remain below 1.5 mm to avoid premature freeze-off. Vent depths for PBT-glass compounds are typically 0.015–0.025 mm; depths above 0.03 mm produce flash because of the low melt viscosity. Tool steel should be hardened to at least 48 HRC for inserts, runners and hot-tip seats; 10% glass fibre is mildly abrasive, and annual shot counts above 250,000 may require bimetallic barrel liners and hardened reciprocating screws. Direct valve-gated cold-runner systems with heated sprue bushings provide lower pressure drop than hot runners with narrow drops below 2.5 mm. Hot-runner drops below 2.0 mm can shear the melt, causing local temperatures above 300 °C and black speck formation. Polished mould surfaces produce high-gloss black parts; textured surfaces require draft angles increased by 1° per 0.025 mm texture depth to prevent drag marks. The glass-fibre content is low enough to produce a uniform surface in black 15042, but fibre-rich weld lines remain visible.