Bamberger Polymers Bapolene Ll075f Polyethylene Film Grade

Bamberger Polymers Bapolene® LL075F Polyethylene, Film Grade

    • Product Name: Bamberger Polymers Bapolene® LL075F Polyethylene, Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 705878
    Polymertype Linear Low Density Polyethylene (LLDPE), Film Grade
    Density 0.920 g/cm³
    Meltindex 0.75 g/10 min
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 24.1 MPa
    Elongationatbreak 700%
    Tensilemodulus 172 MPa
    Dartdropimpact 120 g
    Elmendorftearstrengthmd 250 g
    Elmendorftearstrengthtd 400 g
    Haze 12%
    Gloss 60%
    Vicatsofteningpoint 95°C
    Meltingpoint 122°C

    As an accredited Bamberger Polymers Bapolene® LL075F Polyethylene, Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-resistant multi-wall bags, Bamberger Polymers Bapolene® LL075F Polyethylene, Film Grade resin for industrial applications.
    Container Loading (20′ FCL) 20′ FCL container loading: Bapolene LL075F polyethylene film-grade resin, typically palletized in moisture-protected bags and securely stacked for ocean transport.
    Shipping Bamberger Polymers Bapolene® LL075F Polyethylene, Film Grade, is a non-hazardous thermoplastic resin and is not regulated for transport by DOT, IMDG, or IATA. It is typically shipped in 25 kg bags, 1,000 kg bulk bags, or bulk containers. Store dry, cool, and away from direct sunlight.
    Storage Store Bamberger Polymers Bapolene® LL075F Polyethylene, Film Grade in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers or bags closed, off the floor, and protected from moisture, dust, and contamination. Maintain moderate temperatures, avoid prolonged UV exposure, inspect for damage, and use FIFO stock rotation. Follow SDS and local regulations.
    Shelf Life Shelf life is 24 months when stored unopened in original packaging, in a cool, dry area away from direct sunlight.
    Application of Bamberger Polymers Bapolene® LL075F Polyethylene, Film Grade

    Cast stretch film for pallet stabilisation on high-speed wrappers places a simultaneous demand on edge pinning, melt curtain stability, and pre-stretch retention. On a 3.2 m wide cast line with a 30:1 L/D single-screw extruder, the melt curtain is quenched through a 210 mm air gap onto a chill roll held at 18 °C; the web is then edge-trimmed and wound. Bapolene® LL075F is incorporated at 70–80 wt% with 20–30 wt% of a 2.0 g/10 min LDPE to balance neck-in against puncture. Cling is obtained by dosing 0.5–1.2 wt% polyisobutylene masterbatch at the feed throat; insufficient PIB yields release at corner stress during conveyor accumulation, while excess PIB produces two-sided cling and unwind noise on pre-stretch carriages. Increasing the air gap from 210 mm to 250 mm narrows the web and lowers edge trim yield, whereas decreasing it below 150 mm triggers draw resonance and gauge variation. Edge pinning via electrostatic wire or vacuum box maintains web width tolerance within ±1 mm at haul-off speeds up to 800 m/min. The relevant film test set includes ASTM D5748-95(2019) for protrusion puncture resistance, ASTM D5458-95(2020) for peel cling, ASTM D882-18 for tensile properties, and ASTM D1238-23 for lot-to-lot melt index verification. Regulatory compliance for industrial stretch wrap requires REACH 1907/2006 for substances in the article and EU Directive 94/62/EC Annex II heavy metal limits below 100 mg/kg; food-contact grades must be validated separately under FDA 21 CFR 177.1520 if direct food wrapping is intended. Downstream wrapped articles include palletised consumer goods, appliance crates, logistics centre unit loads, and A-frame warehouse racks. On high-speed wrappers, pre-stretch is typically set between 200% and 250%, but operators must confirm that the film retains at least 80% of pre-stretch after 72 h at 23 °C; otherwise the drum tension profile must be adjusted or the PIB dosage shifted.

    What Limits Bubble Stability in 100 µm Heavy-Duty Sacks on Monolayer Blown Extruders?

    On monolayer blown lines producing heavy-duty sacks from LL075F-rich formulations, the primary process limit is bubble instability caused by high melt elasticity at low frost-line heights. A starting formulation of 70 wt% LL075F and 30 wt% LDPE is used to reduce melt tension while preserving dart impact. Extrusion through a die gap of 1.6–2.2 mm at a blow-up ratio of 2.5:1 and melt temperature of 199–216 °C produces film in the 75–125 µm thickness range. Die rotation or oscillating haul-off is required beyond 400 kg/h to prevent gauge banding and subsequent weak points in sack seams. The four compliance layers are EN ISO 21898:2004 for drop test performance of filled sacks, ASTM D1709-22 for dart impact, ASTM D1922-23 for Elmendorf tear, and EU Directive 94/62/EC Annex II heavy metal limits summing Pb, Cd, Hg, and Cr(VI) below 100 mg/kg. Finished articles include fertiliser sacks, polymer export sacks, mineral filler bags, and construction rubble sacks. A blown film line with internal bubble cooling can run 100% LL075F at 100 µm if the air ring is positioned below the frost line, but operators must monitor frost line fluctuation because a shift of more than 5% of die diameter produces film birefringence variation and sack leak path formation during impact.

    In greenhouse cover and silage clamp film compounding, hindered amine light stabilisers and mineral fillers are used to survive 24-month UV exposure; LL075F is let down at 50–65 wt% with 20–30 wt% LDPE and 10–20 wt% EVA (18% VA). The film is produced on a three-layer blown line with die gap 1.8 mm, blow-up ratio 2.8:1, and internal bubble cooling; thickness falls between 120 µm and 200 µm for greenhouse covers and 80–120 µm for silage underlay. UV stabiliser masterbatch addition is 0.6–1.0 wt% HALS plus 0.3–0.5 wt% benzophenone-type absorber; anti-fog additive is dosed at 0.5–1.0 wt% only when condensation control is specified. Compliance is assessed under EN 13206:2017 for agricultural/horticultural covering films and ISO 4892-2:2013 for accelerated UV ageing; tensile screening follows ASTM D882-18. Finished article types include multi-season greenhouse covers, low tunnels for horticulture, silage clamp covers, and stack covers for ensiled feedstock. The operational boundary is antioxidant package exhaustion: at European solar irradiance, films stabilised with the minimum antioxidant concentration may embrittle before the intended service life; converters must therefore select an additive masterbatch whose UV endurance is matched to the target cultivation period rather than relying on the base resin alone.

    Sealant Web Formulation for Form-Fill-Seal Laminates

    For form-fill-seal laminate sealant webs, a low seal initiation temperature is required to maintain cycle intervals below 0.5 s per seal station. LL075F is used as the primary sealant web component at 70–80 wt%, blended with 20–30 wt% of metallocene plastomer or low-density sealant resin to shift seal initiation downward without losing interlayer adhesion. The sealant web is produced by cast coextrusion at 20–40 µm thickness and then adhesive-laminated to a barrier substrate of polyester or aluminium foil. Seal strength is measured in accordance with ASTM F88/F88M-23 after 1.0 s dwell and 0.35 MPa jaw pressure; coefficient of friction is controlled with 0.1–0.3 wt% slip/antiblock masterbatch to maintain bag-forming track performance. The food-contact compliance matrix includes the following entries:

    Standard/RegulationRequirementCritical Limit
    FDA 21 CFR 177.1520Olefin polymers for food contactExtractives limits under Conditions B–H
    EU 10/2011Overall migration into food simulants10 mg/dm²
    REACH 1907/2006SVHC concentration in article0.1 wt%
    EU 94/62/ECSum of Pb, Cd, Hg, Cr(VI) in packaging100 mg/kg

    Finished article types include frozen food pouches, dry mix pouches, portion-control sachets, and bag-in-box liners where sealant layers incorporate LL075F. The operational limitation is that pure LL075F sealant layers can exhibit an elevated seal initiation temperature compared with metallocene grades; converter trials should establish the optimal plastomer loading and seal dwell settings before full production, because under-seal failures on FFS lines generate food spoilage returns that are traceable to the sealant rather than the barrier layer.

    When collation shrink film is converted for beverage multi-packs and bottle bundle trays, the primary process requirement is a balance between free shrink in the transverse direction and resistance to corner puncture during tunnel shrink. LL075F is introduced at 20–40 wt% into a shrink-grade LDPE blown film matrix to raise dart impact without suppressing free shrink below 40% at 150 °C. The film is extruded on a single-screw blown line with die gap 1.0 mm and a high-stalk bubble configuration; free shrink is measured under ASTM D2732-14, and corner puncture is screened under ASTM D5748-95(2019) for protrusion puncture resistance. Articles produced from this configuration include beverage multi-packs, bottle bundle trays, canned goods overwrap, and insulation batt compression wrap. Compliance for non-food wrap falls under EU 94/62/EC heavy metal limits and REACH 1907/2006; direct food overwrap requires FDA 21 CFR 177.1520 clearance. Published data for this specific configuration is limited; line trials should verify free shrink and shrink force values before tunnel settings are locked.

    When Drum Liners Require Puncture Resistance Without Sacrificing Extruder Throughput

    In the conversion of industrial drum liners and refuse sacks in the 50–100 µm thickness range, LL075F is used as the dominant component at 80–100 wt%, with 0–20 wt% recycled LLDPE post-industrial reclaim where the converter’s feedstock certificate permits. The blown film line uses a die gap of 1.2 mm, a blow-up ratio of 3.0:1, and an internal bubble cooling system; die temperatures are held between 200 °C and 230 °C to prevent melt fracture on high-output screw designs with 30:1 L/D. Puncture resistance is screened according to ISO 7765-1:2004 and ASTM D1709-22 for dart impact, while elongation at break is measured under ASTM D882-18. Regulatory compliance for non-food industrial packaging falls under EU 94/62/EC heavy metal limits and REACH 1907/2006; if the liner is used for UN-certified dangerous goods, the packaging must be tested under the relevant UN performance certification programme and marked accordingly. Product types include open-top drum liners, UN-certified fibre drum liners, refuse sacks, and construction debris bags. The operational boundary is recycled post-industrial reclaim quality: if the reclaimed LLDPE melt index varies by more than 0.5 g/10 min from the nominal value, the blown bubble becomes asymmetric and tear propagation increases in the finished liner.

    Free Quote

    Competitive Bamberger Polymers Bapolene® LL075F Polyethylene, Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bapolene LL075F from Bamberger Polymers is a butene-comonomer linear low-density polyethylene supplied as pelletized feedstock for blown-film and cast-film conversion. The grade is classified by the manufacturer as a film-grade material and is specified by nominal melt mass-flow rate and density. The melt mass-flow rate is published as 0.75 g/10 min when determined at 190 °C under 2.16 kg load according to ISO 1133-1:2022, with equivalent reporting under ASTM D1238. Density is published as 0.918 g/cm³ when tested by ISO 1183-1:2019 or ASTM D1505. The 0.918 g/cm³ density reflects a short-chain branching level typical of butene-based LLDPE film resins, yielding a balance between tear resistance and stiffness in blown film below 100 µm gauge.

    Because the additive package can vary between production campaigns, slip and antiblock loadings must be verified from the lot-specific certificate of analysis before setting coefficient-of-friction targets on packaging lines. The pellet form is compatible with gravimetric blending, and drying is not normally required unless condensation is present from outdoor storage at relative humidity above 60%.

    PropertyValueTest method
    Melt mass-flow rate0.75 g/10 minISO 1133-1:2022 / ASTM D1238
    Density0.918 g/cm³ISO 1183-1:2019 / ASTM D1505

    Values are manufacturer-published typical resin properties. Film-level tensile, tear, and impact data are not fixed resin constants; they depend on die gap, blow-up ratio, frost line height, and draw ratio. Published data for this specific configuration is limited in the public domain, and converters should rely on supplier data sheets and internal trials.

    The butene comonomer introduces ethyl branches along the ethylene backbone. The resulting short-chain branching distribution broadens the crystal thickness distribution and produces lower stiffness and lower Vicat softening temperature than an HDPE of equivalent density. In blown film, orientation balance is controlled by blow-up ratio and draw ratio; at a 2.5:1 BUR and 2.0:1 take-up ratio, transverse direction tear is generally higher than machine direction tear because machine direction orientation dominates under those conditions. This anisotropy can be quantified with ASTM D1922 tear specimens cut in both directions.

    What separates Bapolene LL075F from other film-grade polyethylenes?

    Relative to high-pressure LDPE of comparable melt index, the butene-LLDPE architecture of LL075F increases dart impact strength and Elmendorf tear resistance at equal gauge; however, the melt tension is lower, narrowing bubble stability on air-cooled lines. The 0.75 g/10 min MFR is in the medium-low region for LLDPE blown film. This favors melt strength and drawn-down stability over a 0.918 g/cm³ density film, but it lowers torque-limited throughput on single-screw extruders compared with 1.0 or 2.0 g/10 min MFR grades. Against a hexene-comonomer LLDPE of the same density and MFR, LL075F typically exhibits lower puncture toughness and lower hot-tack strength, but remains adequate for general-purpose bags and liners. Compared with an HDPE film grade at 0.952 g/cm³ density, LL075F shows reduced tensile yield strength and modulus, with improved dart impact and lower flex-crack resistance in thick sections. These differences are quantifiable using ASTM D1709 for dart drop, ASTM D1922 for Elmendorf tear, and ASTM D882 for film tensile.

    At shear rates typical of blown-film extrusion, viscosity is shear-thinning. Capillary rheometry according to ISO 11443 should be used to establish pressure drop and extensional viscosity for new die tooling. Users should not infer film toughness from MFR and density alone because comonomer type and additive package influence solid-state draw and tear behavior.

    When blown-film lines switch from high-pressure LDPE to LL075F

    Typical process settings for a 60 mm single-screw extruder with 24:1 L/D and 2.5:1 compression ratio include a barrel profile from 160 °C at the feed throat to 210 °C at the die, with melt temperature measured at the adapter between 195 and 220 °C. The low melt strength of LL075F relative to LDPE requires either a narrower die gap of 1.5–2.0 mm or an internal bubble cooling system when blow-up ratio exceeds 2.5:1. Frost line height is typically maintained at 6–8 die diameters; if frost line height is raised beyond 10 die diameters, bubble flapping can occur and gauge variation around the bubble circumference increases.

    Melt temperature should not exceed 240 °C during extended runs to limit oxidation-induced gel formation. On grooved-feed extruders, batch-to-batch MFR variation within the supplier’s specification can shift torque by 5–10% at constant screw speed; operators record melt pump inlet pressure and die pressure to maintain gauge. Purging after extended runs should use a low-MFR LDPE or a dedicated purging compound because LL075F retains a narrow residence-time distribution when the die has no dead spots.

    For cast-film lines, melt temperature at the die is commonly set between 220 and 250 °C, with chill-roll temperature held at 20–30 °C. Edge trim generated at 10–15% of web width is reintroduced through a proportional regrind feeder; added regrind above 20% may reduce film clarity and increase gel counts. The product is also used in multilayer structures as a toughness layer between outer HDPE skins and tie layers, where the layer distribution should be optimized by coextrusion rheology models.

    In five-layer coextrusion, LL075F can be used as a bulk layer between skins of HDPE and tie layers. Die temperature uniformity across the layers should be maintained within ±2 °C to avoid interfacial flow instabilities. The melt pump controlling the LLDPE layer should be operated at 80–90% of capacity to maintain consistent layer ratio.

    Regulatory status and additive-package documentation

    The base olefin polymer is generally covered by 21 CFR 177.1520(c) for food-contact articles, provided conditions of use and migration limits in 21 CFR 176.170(c) are met. For European Union applications, compliance with EU Regulation 10/2011 as amended must be verified against the supplier’s Declaration of Compliance, which states overall migration limits and specific migration limits for the additives present. Under REACH, the supplier’s safety data sheet identifies whether the product contains substances of very high concern above 0.1 wt%. For non-food packaging, conformance to CONEG heavy-metal limits is typically declared by the supplier, but users must confirm the specific additive package.

    Regulatory areaReferenceVerification requirement
    U.S. food contact21 CFR 177.1520(c)Conditions of use and migration limits per 21 CFR 176.170(c)
    EU food contactEU Regulation 10/2011Declaration of Compliance with overall and specific migration limits
    REACHEC 1907/2006SDS check for SVHC above 0.1 wt%

    Published application literature lists general-purpose liners, garment bags, carrier bags, and thin packaging film as suitable uses. In form-fill-seal operations, seal initiation temperature should be determined by the converter using ASTM F88 and ASTM F1921 because hot-tack performance of butene LLDPE is lower than that of metallocene LLDPE. Gauge control should be verified with ASTM D5199 and may help maintain dart impact consistency when the film is converted at thicknesses between 20 and 80 µm.

    Incoming resin should be tested for MFR and density on each bulk truck or railcar before silo discharge. A rotating riffler or pellet splitter conforming to ASTM D1898 provides representative samples. If MFR falls outside the supplier’s agreed range, the lot should be quarantined because a 0.05 g/10 min MFR shift can alter extrusion backpressure and film gauge profile on lines without automatic die control.

    Regrind levels up to 15% typically do not cause measurable loss of dart impact in monolayer film when the regrind is sized consistently and free of fines. Above 15%, gel count and film appearance should be monitored with ASTM D7310 or camera-based gel counting.

    This resin is not intended for continuous service above 80 °C or for aggressive oxidative environments unless stabilized by the converter with suitable antioxidant masterbatches. It is incompatible with strong oxidizing agents and should not be blended with high levels of polar polymers without compatibilization. Published data for outdoor weathering of this specific grade is limited; applications requiring extended UV resistance should incorporate a carbon black or hindered amine stabilizer masterbatch at the supplier’s recommended let-down ratio.