Bamberger Polymers Bapolene 615p Lldpe Metallocene Film Grade

Bamberger Polymers Bapolene® 615P LLDPE, Metallocene Film Grade

    • Product Name: Bamberger Polymers Bapolene® 615P LLDPE, Metallocene Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 663114
    Product Name Bamberger Polymers Bapolene® 615P LLDPE, Metallocene Film Grade
    Manufacturer Bamberger Polymers
    Polymer Type Metallocene Linear Low Density Polyethylene (mLLDPE)
    Form Pellets
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 119 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 1,200 psi
    Tensile Strength At Break Md 5,000 psi
    Tensile Strength At Yield Td 1,200 psi
    Tensile Strength At Break Td 4,800 psi
    Elongation At Break Md 500%
    Elongation At Break Td 600%
    1 Secant Modulus Md 25,000 psi
    1 Secant Modulus Td 28,000 psi
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Dart Impact Strength 200 g
    Haze 5%
    Gloss 45 80%
    Coefficient Of Friction 0.20
    Heat Seal Initiation Temperature 105 °C
    Recommended Film Thickness 1.0–4.0 mil
    Processing Method Blown Film Extrusion

    As an accredited Bamberger Polymers Bapolene® 615P LLDPE, Metallocene Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 615P LLDPE, Metallocene Film Grade, packaged in 25 kg polyethylene bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL loading: Bamberger Bapolene® 615P LLDPE metallocene film grade in 25 kg bags, palletized; approximately 20–22 MT net.
    Shipping Bamberger Polymers Bapolene 615P LLDPE Metallocene Film Grade is shipped as non-hazardous resin pellets, typically in 25 kg polyethylene bags or bulk containers, palletized and stretch-wrapped. Store in cool, dry conditions, away from moisture, sunlight, and contaminants. Handle with standard equipment; no special transport regulations apply. Keep sealed until use.
    Storage Store Bamberger Polymers Bapolene® 615P LLDPE, Metallocene Film Grade in a cool, dry, well-ventilated warehouse. Keep sealed in original packaging, on pallets, away from direct sunlight, heat, moisture, and ignition sources. Avoid contamination with dust, oils, or chemicals. Maintain stable ambient conditions; use FIFO stock rotation. Handle with care to prevent package damage. Do not stack excessively. Protect from ultraviolet light.
    Shelf Life Shelf life is two years from date of manufacture when stored in unopened packaging in a cool, dry, well-ventilated area.
    Application of Bamberger Polymers Bapolene® 615P LLDPE, Metallocene Film Grade

    On high-output cast film lines equipped with 75–90 mm single-screw extruders and barrier screws, Bapolene 615P is introduced in the core layer of three-layer A-B-A machine stretch film at 60–75 wt% of total formulation. The outer skin layers are compounded with 2–4 wt% polyisobutylene cling additive and 5–10 wt% low-density polyethylene to control unwind force. Melt temperature at the die is held between 240 °C and 255 °C; die gap is maintained at 0.45–0.65 mm, and chill roll temperature is set at 18–22 °C to quench the film before the draw resonance threshold. At 23 µm gauge, machine-direction elongation at break is evaluated according to ASTM D882-18, with typical converter targets above 350% and ultimate puncture force above 12 N by ASTM D5748-95(2019). Cast film neck-in is monitored as width loss between die exit and the cast roll; industrial practice for metallocene LLDPE in the 0.5–1.0 g/10 min melt-index range commonly records 40–70 mm total neck-in. Pre-stretch performance on powered rollers is assessed after 200% elongation by ASTM D5459-18, with load retention values above 55% after one minute considered acceptable for pallet unitisation. Cling force between adjacent wraps is measured by ASTM D5458-17; anti-cling or differential-cling constructions shift the skin-layer formulation to 0.5–1.5 wt% cling additive in the low-slip outer face. Melt index and density of Bapolene 615P should be verified from the supplier certificate of analysis before converting; the described window assumes a metallocene LLDPE film grade in the 0.5–1.0 g/10 min melt-index range and 0.912–0.918 g/cm³ density range, measured by ISO 1133-1:2022 and ASTM D1505. Published data for Bapolene 615P specifically in sub-15 µm machine film is limited; validation at target gauge should include core-layer weight distribution and chill roll surface roughness mapping.

    How Does Metallocene LLDPE Modify Seal Initiation in Low-Temperature Packaging?

    Blown coextruded film for frozen spinach, seafood, and prepared meals places a dual demand on the sealant layer: early seal initiation at high packaging speeds and resistance to brittle fracture below −25 °C. Bapolene 615P is commonly assigned to the sealant layer at 20–30% of total thickness in a three-layer or five-layer structure, blended with LDPE at 70:30 to 80:20 mLLDPE:LDPE to reduce heat-seal initiation temperature while maintaining hot tack. Sealing is conducted on vertical or horizontal form-fill-seal equipment at jaw temperatures of 105–125 °C, dwell times of 0.3–0.6 s, and seal bar pressure from 0.2–0.4 MPa. Hot tack strength is measured per ASTM F1921-18, with industrial minimum values of 2.0 N/25 mm at 110 °C for a 50 µm sealant film. Seal strength after cooling to 23 °C is tested by ASTM F88/F88M-23, with target values often between 8 N/15 mm and 15 N/15 mm. Dart impact of the finished laminate or monolayer film is evaluated using ASTM D1709-22 Method A; at 75 µm total gauge, frozen-food converters frequently specify dart impact above 800 g and Elmendorf tear above 15 N/mm in the transverse direction per ASTM D1922-23. The narrow molecular weight distribution of metallocene LLDPE contributes to reduced plate-out on the seal jaw surfaces and lower seal-through-contamination failure at powder-filled pack lines. However, the low melt strength of mLLDPE relative to LDPE narrows the bubble stability window; processors using dual-lip air rings should maintain blow-up ratios between 2.2:1 and 2.8:1 and frost line heights between 3 and 5 die diameters to avoid fluctuation in sealant thickness.

    Food-contact status of the final article is regulated under FDA 21 CFR 177.1520 for olefin polymers and EU 10/2011, with overall migration below 10 mg/dm²; converters are responsible for verifying that slip and antiblock additives do not exceed specified migration limits.

    Selected test methods for frozen food sealant webs containing Bapolene 615P
    PropertyMethodReported unit
    Heat seal strengthASTM F88/F88M-23N/15 mm
    Hot tackASTM F1921-18N/25 mm
    Dart impactASTM D1709-22 Method Ag
    Elmendorf tearASTM D1922-23N/mm
    Overall migrationEU 10/2011 Annex IIImg/dm²

    Traditionally, greenhouse or silage film producers blend metallocene LLDPE into an LDPE-rich matrix to improve dart impact and tear balance without raising haze to unacceptable levels. For three-season greenhouse cladding, Bapolene 615P may be incorporated at 20–40 wt% with LDPE and a hindered amine light stabiliser package at 0.15–0.40 wt%; the film is processed on blown film lines with die diameter 250–350 mm, die gap 1.6–2.2 mm, blow-up ratio 2.5:1–3.2:1, and melt temperature 195–215 °C. Accelerated weathering is assessed by ISO 4892-2:2021 using 340 nm UVA lamps at 0.68 W/m², with industrial minimum tensile retention of 50% after 3,000 h for multi-season covers. Haze in the finished film is measured by ASTM D1003-21, with target clarity values below 12% for photosynthetically active radiation transmission in greenhouse applications; the narrow molecular weight distribution of Bapolene 615P limits gel-induced light scattering when the resin is melt-filtered through 60–80 µm screens.

    In silage stretch film, the grade is used at 70–85 wt% in the core of a three-layer cast or blown structure, with polyisobutylene tackifier distributed in surface layers at 1–3 wt%; puncture resistance by ASTM D5748-95(2019) is specified above 10 N at 25 µm and tear resistance by ASTM D1922-23 above 4 N in the machine direction. Oxygen transmission rate in the baled film is measured by ASTM D3985-17; because mLLDPE has higher gas permeability than EVOH, this grade is not suitable as an oxygen barrier in fermented silage where target oxygen transmission rate is below 100 cm³/(m²·day·atm). The reported processing window is derived from industrial lines running metallocene LLDPE in the 0.5–1.0 g/10 min melt-index range; published data specific to Bapolene 615P in agricultural film is limited and does not replace plant trials.

    When Pre-Stretch Ratios Exceed 250% on Powered Roller Lines

    Pallet-wrapping systems with powered pre-stretch can induce 250–320% elongation before film contact with the load. Under these conditions, film failure is dominated by localised necking and transverse tear propagation from small notches. Bapolene 615P at 20–25 µm gauge is evaluated for high-stretch applications by measuring load retention after 200% and 300% elongation per ASTM D5459-18; acceptable industrial load retention is typically between 55% and 70% after 30 s at 23 °C. Elastic recovery by ASTM D5459-18 after 200% elongation should exceed 85% to prevent load shifting during transport. In high-speed rotary wrappers operating above 35 wraps/min, film tension is controlled by dancer roll systems and load-cell feedback; total thickness tolerance should be maintained within ±3% to avoid banding and tiger striping. Cling force measured by ASTM D5458-17 is balanced against unwind noise; surface layers usually contain 1.0–2.5 wt% cling additive in the inside face and 0.5–1.0 wt% anti-cling or low-cling additive in the outside face.

    The process window on cast lines is critical: melt temperature above 260 °C can increase oxidative gel formation, while chill roll temperature above 25 °C slows quench and reduces transverse stretch uniformity. Extruder backpressure should be maintained below 35 MPa with 60–80 µm screen packs to avoid polymer degradation. Published data for Bapolene 615P at 300% pre-stretch is limited; field validation on specific turntable and rotary-arm machines is recommended because clamp force and roller durometer affect film performance more than resin type alone.

    When a laminate converter specifies a metallocene-rich sealant web for stand-up pouches holding dry powders, sauces, or frozen sauces, the sealant layer is coextruded rather than monolayer to balance hot tack and seal-through-contamination performance. Bapolene 615P may form the core of a 40–60 µm three-layer sealant web with LDPE skin layers; the web is then adhesive-laminated to polyester or biaxially oriented nylon films using solvent-free polyurethane adhesives at 2.5–3.5 g/m² coating weight. Heat seal initiation is characterised by ASTM F2029-16, with seal initiation below 95 °C considered suitable for high-speed pouch lines. Hot tack strength at 120 °C and 0.5 s dwell is measured by ASTM F1921-18; industrial expectations for retortable and hot-fill stand-up pouches range from 3.0 N/25 mm to 6.0 N/25 mm. Seal strength after 124 °C sealing is evaluated by ASTM F88/F88M-23, with hermetic seal failure identified by ASTM F2338-19 vacuum decay testing; converters often set rejection limits at 10 cm³/min pressure change. The low extractables associated with metallocene catalysis support compliance with EU 10/2011 overall migration limits below 10 mg/dm² for food simulants A, B, and D2, but final compliance depends on the complete laminate stack, printing inks, and lamination adhesives.

    Process instability in the sealant layer appears as gauge bands and gel streaks; blown film dies with 1.8–2.4 mm die gap and 2.0:1–2.5:1 blow-up ratio are used to reduce film blocking when the reel is stored at 35–40 °C warehouse temperatures. Processors often limit melt temperature to 220 °C in blown sealant webs because higher temperatures can reduce bubble stability and increase gauge variation.

    Heavy-Duty Sack Film and Tear Propagation Resistance

    Form-fill-seal heavy-duty sacks for granular fertiliser, resin pellets, and construction chemicals are extruded at 80–140 µm gauge with a stiffness-to-toughness balance that conventional LLDPE cannot provide at high output. Bapolene 615P is typically blended with high-density polyethylene in a 60:40 to 80:20 mLLDPE:HDPE ratio in the core layer to raise secant modulus while maintaining transverse tear resistance. The film is run on blown film lines with die diameter 300–400 mm, die gap 1.8–2.4 mm, blow-up ratio 1.8:1–2.4:1, and melt temperature 190–210 °C. Tensile properties are evaluated by ASTM D882-18, with industrial targets for heavy-duty sack film at 100 µm exceeding 25 MPa tensile strength at break in the machine direction and 22 MPa in the transverse direction. Elmendorf tear resistance is tested per ASTM D1922-23; a balanced sack film should retain above 5 N in both MD and TD at 100 µm, with the TD value typically lower due to orientation effects. Dart impact by ASTM D1709-22 Method B at 100 µm is specified above 1,500 g to survive drop tests from 1.2 m onto concrete.

    The low-branch structure of metallocene LLDPE improves stress-crack resistance in filled sacks exposed to surfactant-containing products, but blending ratios with HDPE above 40 wt% HDPE reduce the environmental stress-crack resistance benefit and should be avoided when the packaged material contains wetting agents. Processing on grooved-feed extruders requires barrel temperatures from 180 °C at the feed throat to 205 °C at the die; screw speed should be limited to maintain melt pressure below 30 MPa. Published data for Bapolene 615P in heavy-duty sack blends is limited, and the exact ratio must be revalidated on the target line because HDPE melt index and die gap affect tear balance more than resin selection alone.

    Surface protection films for appliance and architectural sheet stock are cast or blown in three-layer structures where the core layer carries the tensile load and the skin layer controls peel adhesion. Bapolene 615P is used as the core layer at 60–80 wt% of the total structure, with ethylene-vinyl acetate or polyolefin elastomer skins at 10–20 wt% each to achieve peel adhesion from 0.5–2.5 N/25 mm on stainless steel. Peel adhesion is measured by ASTM D3330/D3330M-04(2015) under 180° peel angle at 300 mm/min; industrial targets vary by substrate, with high-gloss ABS requiring 0.8–1.5 N/25 mm and brushed stainless steel requiring 1.5–2.5 N/25 mm. Core layer melt temperature is held at 220–240 °C on cast lines with 0.5–0.8 mm die gap, and chill roll temperature is set at 15–20 °C to minimise surface roughness and prevent gel transfer. Film clarity is assessed by ASTM D1003-21, with haze below 5% required for optical surface inspection; gel count is measured by inline camera or laboratory film inspection against ASTM D7310-21, with critical gels above 200 µm rejected. The low gel level of metallocene LLDPE supports this application, but surface morphology is strongly influenced by chill roll finish and die lip cleanliness rather than resin alone. Published data for Bapolene 615P in surface protection configurations is limited; initial qualification should include peel adhesion retention after 72 h at 60 °C and UV exposure per ISO 4892-3:2021 to evaluate residue on gloss acrylic surfaces.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 615P LLDPE, Metallocene Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bamberger Polymers Bapolene® 615P is classified as a metallocene linear low-density polyethylene blown film grade. The base resin is supplied with a melt index of 1.0 g/10 min when tested under ASTM D1238 at 190°C and 2.16 kg, and a density of 0.918 g/cm³ under ASTM D792. The metallocene catalyst system produces a narrower molecular weight distribution and more uniform comonomer placement than conventional Ziegler-Natta LLDPE of equivalent density. As a result, Bapolene® 615P is directed toward monolayer and coextruded packaging film, heavy-duty liners, agricultural film, and protective packaging where downgauging, dart impact resistance, puncture resistance, and optical uniformity are conversion objectives. The resin is not intended for rotational molding, injection molding, or extrusion coating.

    Because the density is 0.918 g/cm³, the crystalline fraction is lower than that of a 0.924 g/cm³ or 0.934 g/cm³ LLDPE. The lower density reduces film stiffness while shifting performance toward energy absorption and tear resistance. The melt index of 1.0 g/10 min places the material in the medium-viscosity blown film range, compatible with single-screw extruders from 45 mm to 90 mm screw diameter and 24:1 to 30:1 L/D. High-shear dispersive mixing is not required for the neat polymer, but when slip or antiblock masterbatches are introduced, a barrier screw with a Maddock mixing section or an equivalent distributive mixing element is advisable. Pellets should be stored in dry indoor conditions away from direct sunlight and ultraviolet exposure. Prolonged storage above 40°C can increase additive migration and pellet blocking. When ambient relative humidity exceeds 60%, surface moisture on pellets can destabilize the bubble, and drying at 60°C to 80°C for two to four hours in a desiccant dryer is commonly applied before extrusion.

    What melt temperature and die gap are required to avoid melt fracture?

    On air-cooled blown film lines, a starting profile from 150°C to 160°C in the feed zone, rising to 210°C to 225°C at the adapter and die, is typical for metallocene LLDPE. Narrow die gaps below 1.0 mm increase wall shear stress and can trigger sharkskin melt fracture at moderate output rates. Die gaps of 1.5 mm to 2.5 mm are therefore standard. Blow-up ratios of 2.2:1 to 2.8:1 and frost line heights from 200 mm to 400 mm are common, although internal bubble cooling lines may operate at higher output with shorter frost line height. The narrow molecular weight distribution of Bapolene® 615P reduces low-shear melt strength and can lower bubble stability relative to LDPE. Air ring, bubble cage, and collapsing frame alignment must be maintained to prevent fluttering, particularly during gauge changes or ambient temperature swings.

    Melt pressure at the die is often higher than that of a fractional-melt LDPE at the same throughput because metallocene LLDPE exhibits a different shear-thinning curve. If excessive backpressure is observed, widening the die gap from 1.5 mm to 2.0 mm is preferable to raising melt temperature beyond 230°C, which can initiate oxidative degradation, gel formation, and off-taste in sensitive food packaging. Screws designed for LLDPE should use a compression ratio of 2.5:1 to 3.5:1 and a barrier flight beginning in the feed section. Before shutdown, purging with a fractional-melt LDPE is generally recommended to remove metallocene LLDPE from the barrel and die. During idle periods, screw speed and barrel temperatures should be reduced to prevent stagnant material from oxidizing.

    Because the density is 0.918 g/cm³, the resin introduces less crystalline rigidity than higher-density polyethylene grades. In process terms, this can produce a softer bubble and a more pronounced tendency to sag at high die temperatures. Stable operation is improved by controlling the melt temperature profile tightly and avoiding rapid frost line movement. For converters running broad-distribution LLDPE with minimal thermal control, barrel zone control to ±5°C may be required to prevent melt instability and film gauge variation. Trim re-introduction in-house can be practiced at 10% to 20% by weight, but repeated heat histories may increase gel content and reduce optical quality.

    Optical, tear, and seal-performance response at 25 µm

    Film mechanical properties are thickness-dependent and orientation-dependent. For 100% Bapolene® 615P at 25 µm, tensile properties are tested under ASTM D882, Elmendorf tear under ASTM D1922, dart impact under ASTM D1709 Method A, and puncture resistance under ASTM D5748. In comparative class data for metallocene LLDPE film near 0.918 g/cm³, machine-direction tensile strength can exceed 35 MPa, while transverse-direction elongation can exceed 500%. However, film values shift with die gap, blow-up ratio, frost line height, cooling rate, and additive package. Bapolene® 615P-specific film data should be taken from converter qualification trials rather than from class averages. Haze under ASTM D1003 and gloss under ASTM D2457 improve relative to butene LLDPE when the narrower comonomer distribution reduces surface irregularity after quenching, but additive selection can reverse this trend.

    Heat-seal initiation is evaluated by ASTM F1921 for hot tack and ASTM F88 for seal strength. Metallocene LLDPE is reported to initiate sealing at temperatures 10°C to 20°C lower than a conventional LLDPE of equivalent density, which can reduce dwell time on high-speed vertical form-fill-seal equipment. Actual seal initiation temperature for Bapolene® 615P must be confirmed on the target packaging line because seal jaw configuration, film gauge, dwell time, and slip/antiblock additives affect heat transfer. Compared with butene Ziegler-Natta LLDPE of the same nominal density and melt index, Bapolene® 615P generally yields lower film haze, reduced extractable content, and improved dart impact at equal thickness. The metallocene distribution also narrows the melting range, which supports faster sealing but reduces tolerance to temperature fluctuations during extrusion.

    When LDPE blending is required for bubble stability

    Because Bapolene® 615P does not contain long-chain branching, its melt strength is lower than LDPE. In downgauging trials below 20 µm, or on lines with limited cooling air, 5% to 20% LDPE is commonly added to stabilize the bubble, increase melt strength, and reduce neck-in. The exact blend ratio depends on die gap, output, frost line height, and bubble geometry. Additions beyond 20% generally reduce dart impact and tear resistance relative to 100% metallocene LLDPE. In coextruded film, Bapolene® 615P may be placed in a core or outer layer while a high-melt-strength LDPE or HDPE skin provides bubble rigidity. The resin should not be melt-blended with polypropylene or polyamide without a tie layer; these polymers form incompatible interfaces that lower interlayer adhesion and can delaminate during flexing or drop testing. If a barrier layer is required, a separate extruder and appropriate tie resin are necessary.

    For food-contact packaging, the converter must obtain a raw-material compliance statement from Bamberger Polymers or its distributor. Polyethylene homopolymers and copolymers are generally covered for food contact under FDA 21 CFR 177.1520, but final film must comply with the end-use and extractive conditions of the regulation. In the European Union, plastic food-contact materials are evaluated under Commission Regulation (EU) No 10/2011; overall migration testing is conducted according to EN 1186. The product must be included in the converter’s hazard analysis and process control system if food contact is intended. REACH compliance is handled through Regulation (EC) No 1907/2006, and converters should request an SVHC declaration for the purchased grade. The RoHS Directive 2011/65/EU applies to finished electrical and electronic equipment rather than raw polymer resin; nevertheless, film used in wrapping electrical articles may be influenced by the customer’s restricted substance list. Additives used by converters, such as slip or antiblock masterbatches, are separate compliance obligations.

    In heavy-duty shipping sack applications, the resin is typically run at 75 µm to 125 µm thickness to provide puncture and drop resistance. For agricultural film, ultraviolet stabilizer masterbatch must be added because the base resin does not provide long-term outdoor weatherability. Collation shrink film can be produced from Bapolene® 615P, although high-shrink structures often require LDPE blending to adjust shrink force and prevent premature bubble collapse. In laminated structures, the resin may be used as an outer sealing layer where a metallocene surface improves seal integrity and optics. Applications requiring higher tensile modulus or greater stiffness should incorporate a higher-density LLDPE or HDPE layer, because the 0.918 g/cm³ density of Bapolene® 615P limits the modulus available from the neat resin.

    Top