| HS Code | 703925 |
| Material Type | Metallocene Linear Low Density Polyethylene (mLLDPE) |
| Grade | Film Grade |
| Density | 0.916 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Melting Point | 120 °C |
| Vicat Softening Point | 95 °C |
| Tensile Strength At Yield | 1400 psi |
| Tensile Strength At Break | 5000 psi |
| Elongation At Break | 600% |
| Dart Drop Impact | 300 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 5% |
| Gloss 45 | 80% |
| Coefficient Of Friction | 0.20 |
| Heat Seal Initiation Temperature | 100 °C |
As an accredited Bamberger Polymers Bapolene® 615FP LLDPE, Metallocene Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Bamberger Polymers Bapolene® 615FP LLDPE, Metallocene Film Grade, is packaged in 25 kg polyethylene bags on pallets for industrial use. |
| Container Loading (20′ FCL) | 20′ FCL loads approximately 17.5 MT of Bapolene 615FP LLDPE in 25 kg bags; palletized or floor-loaded, subject to carrier limits. |
| Shipping | Bamberger Polymers Bapolene® 615FP LLDPE, Metallocene Film Grade, is a non-hazardous polymer resin. It is typically shipped in 25 kg bags, stacked on pallets, stretch-wrapped, or in bulk trucks/railcars. Keep dry, cool, and away from direct sunlight, moisture, and contamination. No special hazardous-materials transport classification applies. |
| Storage | Store Bamberger Polymers Bapolene® 615FP LLDPE, Metallocene Film Grade, in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers/bags tightly closed, off damp floors, and protected from moisture, dust, and UV. Use first-in, first-out rotation; avoid damaging bags/pallets. Maintain good housekeeping. Consult the SDS for details. |
| Shelf Life | Shelf life is typically 24 months when stored in a cool, dry place in original unopened packaging, protected from direct sunlight and moisture. |
Bapolene® 615FP is a metallocene-catalysed linear low-density polyethylene film grade specified in downstream converting sectors where narrow molecular weight distribution, controlled seal initiation, and aggressive down-gauging determine line profitability. Lot release testing is conducted under ISO 1133-1:2022 for melt flow rate and ISO 1183-1:2022 for density; downstream processing windows described below are derived from standard industrial practice and must be revalidated against the certificate of analysis for each production lot. The application sections identify processing constraints, test standards, formulation boundaries, and finished product categories observed in industrial conversion.
On high-output cast film lines operating above 600 m/min, gauge uniformity in a 23 µm pallet wrap is controlled by the melt fracture threshold of the metallocene resin rather than by downstream haul-off alone. Bapolene® 615FP is processed on cast coextrusion equipment with 90 mm to 120 mm extruders having 30:1 L/D ratios and slot die gaps between 0.6 mm and 1.0 mm. Barrel set-points are maintained between 190 °C and 230 °C, while die-bolt temperature adjustments are limited to ±5 °C to avoid transverse gauge bands. The addition ratio in a monolayer hand-wrap recipe can be 100 wt% of the resin; in machine-wrap structures a 70–90 wt% letdown of Bapolene® 615FP with 10–30 wt% of an ethylene plastomer or LDPE is used to shift the stretch force plateau and reduce web snap-back at high pre-stretch levels. Cling force is not supplied by the base resin; polyisobutylene or an approved olefinic tackifier is metered at 0.5–3.0 wt% into the outer layer via masterbatch or liquid injection. Pre-stretch ratios above 250% are common, but local necking develops if the melt orientation is frozen with insufficient quench uniformity; cast roll temperatures below 20 °C and air-knife velocity above 25 m/s are used to maintain web flatness. Industry compliance is anchored to ASTM D4649 for stretch-wrap selection, ASTM D5458-95 for cling force, ASTM D5748-19 for puncture resistance, ASTM D882-18 for tensile properties, and ASTM D1922-15 for Elmendorf tear. Terminal products include machine stretch wrap rolls, hand stretch wrap rolls, pre-stretched pallet wrap, vented pallet wrap, and tinted or UV-marked load-containment films.
| Failure mode | Standard designation | Apparatus | Production variable controlled |
|---|---|---|---|
| Puncture | ASTM D5748-19 | Universal test machine with probe fixture | Core layer gauge and tackifier distribution |
| Cling | ASTM D5458-95 | Peel test fixture with 180° separation | Tackifier concentration and outer layer melt temperature |
| Elmendorf tear | ASTM D1922-15 | Elmendorf tearing tester | MD/CD orientation balance and die gap |
| Tensile yield | ASTM D882-18 | Constant-rate-of-extension tensile tester | Pre-stretch ratio and roll temperature |
The seal integrity of a three-layer blown-film food-contact structure is governed by the sealant skin resin’s crystallization rate and hot-tack plateau, not solely by film thickness. In a typical A/B/C structure, Bapolene® 615FP is placed in the sealant layer at a thickness fraction of 15–30% of total film, formulated neat or blended with 10–20 wt% LDPE to modify seal bar release and hot-tack viscosity. Slip and antiblock masterbatches are incorporated at 1–3 wt% in the skin layer; print-web layers are typically HDPE, LDPE, or PP. The lower seal initiation temperature versus conventional Ziegler-Natta LLDPE permits a 5–10 °C reduction in seal bar set-point on horizontal form-fill-seal machines, but published hot-tack curves for this specific grade should be generated per ASTM F1921-12 because converter heat-seal jaw geometry and dwell time alter the plateau. Published hot-tack curves for this specific configuration are limited, and converter trials must be conducted before production sealing speeds are locked. The blown-film process uses a 2.2:1 to 2.8:1 blow-up ratio, a die gap of 1.6–2.4 mm, and internal bubble cooling to control frost-line height. Compliance for food contact is evaluated under FDA 21 CFR § 177.1520 for olefin polymers and EU Regulation (EC) No 10/2011 with an overall migration limit of 10 mg/dm²; REACH obligations are maintained under Regulation (EC) No 1907/2006. Terminal finished product types include frozen-food bags, cereal liner films, fresh-cut produce bags, bakery film, and sealant webs in stand-up pouches.
| Regulatory domain | Standard designation | Clause or limit | Verification parameter |
|---|---|---|---|
| United States | 21 CFR § 177.1520 | Olefin polymers | Density and extractives; finished-food-contact testing |
| European Union | (EU) No 10/2011 | Article 12; 10 mg/dm² overall migration | Overall migration in simulant D1, D2, or E |
| European Union packaging | 94/62/EC | Sum of Pb, Cd, Hg, Cr(VI) 100 ppm | Packaging heavy metal concentration |
| REACH | Regulation (EC) No 1907/2006 | Candidate list | SVHC declarations |
Heavy-duty form-fill-seal (FFS) conversion of metallocene LLDPE into 60–80 µm shipping sacks subjects the melt to a different stress history than thin-gauge stretch film, specifically through oscillating vertical sealing jaws and high-temperature impulse seal bars. In this segment Bapolene® 615FP is added at 70–90 wt% in blown-film formulations, with 10–30 wt% HDPE or high-molecular-weight HDPE added to raise modulus and reduce elongation under stacking load. The downstream production process consists of a high-output blown-film coextrusion line with die gaps from 2.0 mm to 2.8 mm, frost-line control, and corona treatment to 40–44 mN/m surface energy before flexographic printing. On FFS equipment, seal jaw temperatures between 150 °C and 180 °C are typical; the metallocene resin’s lower seal initiation reduces seal bar dwell time, but the presence of filler or high-print ink coverage can depress seal strength if the sealant layer is diluted below 70 wt%. Drop resistance is verified by ISO 7965-1 or ASTM D5276-19 for filled sacks, tear propagation by ASTM D1922, and tensile properties by ISO 527-3. Terminal finished product types include polyethylene resin shipping sacks, pet food bags, mineral filler sacks, fertilizer bags, and heavy-duty industrial liners.
Down-gauging agricultural silage film to 25 µm while maintaining resistance to tear propagation requires a balance between film yield stress and machine-direction orientation that is measurable under ISO 527-3 and ASTM D1922. In silage wrap, Bapolene® 615FP is used at 80–95 wt% with a UV-stabilizer masterbatch at 5–12 wt% and a cling additive at 2–6 wt% in the surface layer. The conversion process is blown-film coextrusion with blow-up ratios of 2.5:1 to 3.0:1, die gaps of 1.8–2.6 mm, and internal bubble cooling; the high tack layer requires a lower melt temperature at the outer extruder to avoid additive degradation. For low-tunnel covers and greenhouse films, the base resin is blended with 10–20 wt% LDPE and a UV/HALS package, with thicknesses ranging from 25 µm to 150 µm. Compliance with EN 13206:2017 for agricultural thermoplastic films applies to weathering and mechanical performance. Published long-term weathering data for this specific resin under field exposure is limited to supplier technical literature; outdoor service life must be verified by the film producer because the base resin does not contain an inherent UV-stabilizer package. Terminal finished product types include bale wrap, silage cover film, low-tunnel cloche film, greenhouse sidewall film, and silage bag liners.
A protective surface film laminated to stainless steel or anodised aluminium relies on a polyolefin core that must survive slitting without edge fibrillation. Bapolene® 615FP is added at 60–85 wt% in the core layer of a cast three-layer protective film, with an adhesive layer based on a modified polyolefin at 10–25 wt% and a release-consistent skin layer at 5–15 wt%. The downstream process is cast coextrusion with a slot die gap of 0.5–0.8 mm, corona treatment to 42–48 mN/m, and in-line slitting; line tension must remain below 2.5 N/cm of web width to prevent permanent core orientation that causes film chatter during automated application. Tensile properties are measured per ASTM D638-14 or ISO 527-3, and peel adhesion is verified by ASTM D3330 after a controlled dwell time. Compliance for electronic-sector surface protection is assessed under RoHS Directive 2011/65/EU, and general chemical registration is maintained under REACH Regulation (EC) No 1907/2006. Terminal finished product types include coil protection film, glass protection film, stainless steel sheet masking, and furniture-surface protective film.
Competitive Bamberger Polymers Bapolene® 615FP LLDPE, Metallocene Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Bapolene® 615FP is a metallocene-catalyzed linear low-density polyethylene (mLLDPE) film extrusion resin supplied by Bamberger Polymers in pellet form. The grade is polymerized with single-site metallocene chemistry, which distributes hexene comonomer along the polymer backbone more uniformly than conventional Ziegler-Natta catalysts and shifts chain architecture toward a narrow molecular weight distribution. Published trade data list a nominal melt index of 0.5 g/10 min at 190 °C under 2.16 kg load per ASTM D1238 and a solid density of 0.918 g/cm³ per ASTM D1505. The resin is intended for monolayer and coextruded blown film as well as cast film processes where improved toughness, optics, and seal performance are required. Pellet bulk density is typically reported between 0.50 g/cm³ and 0.55 g/cm³; the resin is supplied with a phenolic/phosphite stabilization package and does not contain slip or antiblock additives in the base polymer. Certificate-of-analysis values should be checked against the production lot before screw speed and die geometry are finalized.
The narrow molecular weight distribution of 0.5 g/10 min mLLDPE produces less shear thinning than a Ziegler-Natta LLDPE of the same melt index. On a 90 mm 30:1 L/D grooved-feed extruder with barrier screw and Maddock mixer, the melt pressure at 1.8 kg/h/mm die circumference can be 350–450 bar, and motor load is typically 10–15% higher than for a butene-based LLDPE of equivalent density. Melt temperature should be maintained at 190–220 °C, with the die zone set at 200–230 °C and die gap between 1.2 mm and 2.0 mm. Blow-up ratio is usually controlled at 2.0:1–2.5:1; frost line height should not exceed 3.5 die diameters when output exceeds 2.5 kg/h/mm circumference because the low melt strength of the narrow molecular-weight resin permits low-frequency oscillation before bubble tear. On high-output lines above 2.0 kg/h/mm, the die gap should be raised to 1.8–2.0 mm to keep die pressure from exceeding 500 bar. Dual-lip air rings with internal bubble cooling are preferred because the resin cannot tolerate impingement velocity above 20 m/s without surface distortion. On cast film lines, die gap is typically 0.5–1.0 mm, air gap 100–150 mm, and chill-roll temperature 20–30 °C to preserve low haze. Die-lip buildup from oxidized low-molecular-weight species is managed by adding fluoropolymer process aid at 200–400 ppm; preheating hopper air to 40 °C prevents condensation on pellets stored below 15 °C.
| Property | Method | Unit | Typical value |
|---|---|---|---|
| Melt index | ASTM D1238 | g/10 min | 0.5 |
| Density | ASTM D1505 | g/cm³ | 0.918 |
| Tensile strength at yield MD | ASTM D882 | MPa | 10.5 |
| Tensile strength at break MD | ASTM D882 | MPa | 58 |
| Elongation at break MD | ASTM D882 | % | 620 |
| Dart drop impact Type A | ASTM D1709 | g | 850 |
| Elmendorf tear MD/TD | ASTM D1922 | g | 12/18 |
| Haze | ASTM D1003 | % | 7 |
| Gloss at 45° | ASTM D2457 | % | 75 |
Where the film enters vertical form-fill-seal and flow-wrap operations, the seal initiation temperature of Bapolene 615FP is lower than that of a conventional butene LLDPE of the same density. Heat-seal testing on 50 µm blown film with a 0.5 N/mm² jaw pressure and 0.5 s dwell typically records seal initiation at 95–105 °C, while hot-tack measured according to ASTM F1921 reaches its plateau between 110 °C and 130 °C. The lower seal initiation reduces dwell time on high-speed packaging lines but requires accurate jaw temperature control below ±3 °C to avoid burn-through at sealable coating thicknesses. For lamination film, the resin is processed as a sealant web against PET or BOPP; the metallocene architecture improves interlayer seal integrity under flex-crack testing but increases the coefficient of friction if no slip additive is incorporated. Converters add 500–1500 ppm silica antiblock and 300–800 ppm erucamide or oleamide slip to achieve a kinetic coefficient of friction below 0.30 per ASTM D1894.
In blown films used for collation shrink, the substitution of 0.5 g/10 min, 0.918 g/cm³ mLLDPE for a butene-based LLDPE of the same nominal density typically increases dart impact by 20–40% and puncture resistance by 15–30% because the uniform comonomer distribution increases the concentration of load-bearing tie molecules. The same change lowers film haze and improves gloss, but the machine-direction Elmendorf tear may be reduced unless the frost line is raised or the blow-up ratio is increased to 2.5:1. On high-stalk bubble configurations with stalk height above 8 die diameters, the polymer’s narrow molecular weight distribution can produce a less stable neck and draw resonance; adding 10–20 wt% of high-pressure LDPE with melt index 0.25–0.5 g/10 min is often used to restore melt strength, though this will raise haze and may lift seal initiation temperature by 3–6 °C. For heavy-duty sack applications, the film gauge is typically 100–200 µm, and the low shear thinning of the mLLDPE requires tighter barrel-temperature profiling from 160 °C feed to 220 °C metering. Compared with a Ziegler-Natta butene LLDPE of equal density and melt index, the metallocene grade generally shows lower hexane extractables, lower seal initiation temperature, higher dart impact, and lower melt strength; the lower melt strength is the primary processing limitation in high-stalk and deep-draw converting equipment.
Mechanical performance of Bapolene 615FP is controlled primarily by orientation and gauge, not by density alone. In 25 µm monolayer film blown at 2.5:1 blow-up ratio and 3 die-diameter frost line, the typical dart drop impact measured by ASTM D1709 Type A is 850 g, while Elmendorf tear in the machine direction is typically 12 g and in the transverse direction 18 g. The tear anisotropy is a direct consequence of the narrow molecular-weight distribution: tie-molecule orientation in the machine direction increases puncture and impact strength but lowers resistance to tear propagation along the same axis. Increasing blow-up ratio to 3.0:1 and raising frost line to 5 die diameters reduces the MD/TD tear differential but may reduce output because bubble cooling becomes less efficient. In cast film at 20–30 µm, the orientation is less balanced and tear values shift; published data for this specific configuration are limited, but cast film generally shows lower dart impact than blown film at equal gauge. For applications such as freezer film and poultry bags, the film is often coextruded with a lower-melt-index mLLDPE or an HDPE skin to recover tear resistance without sacrificing seal performance.
Under direct food-contact use, Bapolene 615FP is represented as a polyolefin within FDA 21 CFR § 177.1520 provided the finished film meets extraction limits for the intended food type. European migration compliance is not automatic; the converter must evaluate the final multilayer structure under EU Regulation 10/2011 for overall migration and specific migration limits. The base resin contains no intentionally added slip or antiblock, so optical and frictional properties are additive-dependent. Storage below 50 °C and protection from UV exposure are required to prevent stabilizer depletion; regrind additions above 20 wt% may raise gel counts and reduce dart impact because the antioxidant package is partially consumed during prior extrusion. Drying is not required under normal closed-hopper handling, but pellets stored below 15 °C in RH > 60% should be equilibrated to ambient temperature before entering the extruder throat to avoid condensation-induced feed slip. The material is not recommended for use with amine-based flame-retardant masterbatches that accelerate oxidative degradation of unstabilized polyethylene at elevated processing temperatures.