Bamberger Polymers Bapolene 610fp Lldpe Metallocene Film Grade

Bamberger Polymers Bapolene® 610FP LLDPE, Metallocene Film Grade

    • Product Name: Bamberger Polymers Bapolene® 610FP LLDPE, Metallocene Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 275014
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Tensile Strength At Yield 9.65 MPa
    Tensile Strength At Break 31.0 MPa
    Elongation At Break 600%
    Tensile Modulus 0.172 GPa
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 6%
    Gloss At 45 70
    Coefficient Of Friction 0.20
    Melting Point 120 °C
    Vicat Softening Point 95 °C

    As an accredited Bamberger Polymers Bapolene® 610FP LLDPE, Metallocene Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 610FP LLDPE metallocene film grade is supplied in 25 kg polyethylene bags, 40 bags per pallet.
    Container Loading (20′ FCL) 1x20' FCL container loaded with Bamberger Polymers Bapolene 610FP LLDPE metallocene film-grade resin in 25 kg bags for export shipment.
    Shipping Bapolene® 610FP LLDPE, Metallocene Film Grade, is shipped as non-hazardous polymer pellets in moisture-barrier bags, octabins, bulk bags, or bulk trucks/railcars. Store cool, dry, ventilated, away from sunlight and heat. Not regulated by DOT, IATA, IMDG, or ADR.
    Storage Store Bapolene® 610FP indoors in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags/containers closed, palletized, and off the floor to prevent moisture pickup, dust, and contamination. Avoid prolonged UV exposure, excessive stacking, and temperature extremes. Use first-in, first-out stock rotation. Follow supplier SDS and local regulations.
    Shelf Life Two years from date of manufacture when stored in original, unopened packaging in a cool, dry area away from direct sunlight.
    Application of Bamberger Polymers Bapolene® 610FP LLDPE, Metallocene Film Grade

    In high-speed cast stretch film lines operating at haul-off speeds above 500 m/min, Bapolene 610FP is normally extruded through a single-screw machine with 30:1 L/D and a barrier-flighted mixing section. Melt temperature at the die lip is held between 245°C and 275°C, while the adapter and melt pipe are controlled within ±5°C of the die set point to prevent localized shear heating and gel formation. The slot die gap is set at 0.8 mm to 1.0 mm, and the extrudate is cast onto a chill roll maintained at 18°C to 28°C with an air knife or vacuum box used to stabilize edge pinning. In three-layer coextrusion, the core layer contains 70–80% of total thickness and is formulated entirely from Bapolene 610FP to provide draw elongation and puncture resistance. The cling layer at 10–15% of total thickness is compounded with polyisobutylene at 2–4 wt%; the release layer at 10–15% of total thickness contains erucamide at 500–2,000 ppm and synthetic silica antiblock at 2,000–5,000 ppm. Finished machine stretch film is produced at 10–23 µm thickness. Elongation at break and ultimate tensile strength are measured according to ASTM D882; cling is batch-released against ASTM D5748; coefficient of friction is checked after 24 h because tackifier migration changes the release surface value. A film aged for 24 h before ASTM D1894 testing produces more repeatable data than an immediate measurement on the winder. The grade does not require pre-drying under normal storage; if surface condensation occurs above 60% RH, dry-air purging at 50°C is applied before extrusion.

    Typical cast stretch coextrusion layer structure using Bapolene 610FP
    LayerThickness fractionResin/additive formulationFunctionTest method
    Cling10–15%Bapolene 610FP + polyisobutyleneTack to pallet and filmASTM D5748
    Core70–80%100% Bapolene 610FPElongation and puncture resistanceASTM D882
    Release10–15%Bapolene 610FP + erucamide 500–2,000 ppm + silica 2,000–5,000 ppmControlled unwind and blocking resistanceASTM D1894

    Dart impact retention after downgauging is assessed according to ASTM D1709, with punch and tensile failure modes recorded separately. On a 2,000 mm wide die, output above 400 kg/h can increase transverse thickness variation to more than ±3% if deckle position and air knife pressure are not adjusted during start-up. Edge neck-in is controlled by chill roll temperature and air gap, with a deviation of more than 5% from the target air gap producing visible edge bead defects. For export shipments, a REACH SVHC statement and RoHS Directive 2011/65/EU material declaration are normally supplied; the grade contains no intentionally added substances above the heavy metal limits of Packaging and Packaging Waste Directive 94/62/EC.

    When Bapolene 610FP is placed in the sealant layer of a three-layer blown film for frozen-food form-fill-seal pouches, the process window is narrower than for Ziegler-Natta LLDPE because the metallocene resin reaches stable bubble geometry at lower melt temperatures. Extruder barrel temperatures from 185°C to 215°C and a die gap of 1.8 mm to 2.2 mm with a blow-up ratio of 2.2:1 to 2.8:1 are used to maintain frost line height between 6 and 8 die diameters. The sealant layer constitutes 20–30% of total film thickness, and is run at 100% Bapolene 610FP or at 80 wt% Bapolene 610FP blended with 20 wt% LDPE for additional bubble stability. Hot tack strength is tested per ASTM F1921, heat seal strength per ASTM F88, and the observed seal initiation threshold on production lines is commonly reported in the range of 88–95°C for a 2.0 N/25 mm seal strength target; published data for this specific configuration is limited and should be confirmed on the converter’s sealing equipment. The film is used in vertical form-fill-seal formats for frozen vegetables, shredded cheese, fresh-cut produce, and frozen seafood, where low-temperature sealing reduces dwell time and protects heat-sensitive products. Organoleptic performance is evaluated by FDA 21 CFR 177.1520(c) 3.2a and EU Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² under aqueous, acidic, and alcoholic food simulants. If the converter stores film at temperatures below -25°C before use, the tensile impact measured by ASTM D1822 should be compared on conditioned specimens because cold embrittlement changes sealant layer rupture behavior. The use of polyisobutylene tackifier in this sealant layer is avoided unless a specific dual-use compliance statement covers the final packaging structure.

    Compliance checklist for food contact films containing Bapolene 610FP
    RegionRegulationTest/conditionLimit
    United StatesFDA 21 CFR 177.1520(c) 3.2aOlefin polymer compliance and end-use extractionFood contact suitable as defined by the regulation
    European UnionEU Regulation (EU) No 10/2011Overall migration in simulants A, B, D210 mg/dm²
    ChinaGB 9685-2016Positive list for additivesSpecific migration limits per additive
    Export non-food packagingREACHSVHC declarationAs currently listed by ECHA

    What Limits Puncture Propagation Resistance in Silage Bale Wrap Exposed to Field UV?

    Oxygen ingress through improperly stabilized silage film accelerates aerobic spoilage at the bale face, so converters specify a blown film structure at 20–25 µm thickness, with an extrusion die gap of 2.0–2.5 mm and a blow-up ratio of 2.5:1 to 3.0:1. Melt temperature is maintained at 195–225°C, and the film is wound with a controlled taper to preserve cling force at the outer roll layers. The compound includes a hindered amine light stabilizer at 0.2–0.6 wt%, a white or black color masterbatch at 4–6 wt%, and polyisobutylene-based cling additives at 2–3 wt%. Puncture resistance is tested according to ISO 7765-1, and field exposure is simulated under ASTM G154 cycle 1 or ISO 4892-2 cycle A. The terminal product is round bale silage wrap and forage bale wrap in widths of 500 mm, 750 mm, and 1,000 mm, applied by round bale wrappers at pre-stretch levels between 55% and 70%. Acid-containing crop preservatives should not be applied directly to the wrapped film surface; residual acid can plasticize the cling layer and reduce tack within 12 h, leading to unwinding in field storage. The same acid exposure issue appears when bales are wrapped with moisture content above 60%, because condensation between film layers modifies the additive distribution at the cling interface. Agricultural film waste is subject to national extended producer responsibility schemes; for EU export, compliance with REACH and Packaging and Packaging Waste Directive 94/62/EC should be documented.

    In extrusion lamination lines where Bapolene 610FP serves as the heat-seal layer on printed PET or metallized OPP, the melt is applied at 280–305°C through a flat die with a nominal coating thickness of 12–20 µm, and the web is nipped against a chill roll held at 15–20°C. The air gap between die exit and nip is set at 100–150 mm to promote oxidative adhesion to primed film or aluminum foil; a shorter air gap can produce insufficient bond strength on foil-based structures. Line speeds are between 100 m/min and 250 m/min, depending on web width and edge bead formation. Bapolene 610FP is melt-compounded with 0–10 wt% LDPE to adjust neck-in and draw resonance; mineral oil or fluoropolymer processing aids at 200–500 ppm may be added to reduce die deposit formation. Terminal structures include snack food laminations, lidding films for dairy cups, and medical packaging where a lock-up seal is acceptable. The sealant layer is qualified by ASTM F88 and ASTM F2029 for heat seal strength and hot tack. Compliance for food contact is verified under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. Draw resonance appears as cyclic thickness banding in the machine direction; it is minimized by keeping the draw ratio below 15:1 and by maintaining melt temperature stability within ±5°C.

    When Collation Shrink Film Demands Low-Temperature Sealing on High-Speed Lines

    Double-bubble lines orient the film in machine and transverse directions after an initial blown film bubble is collapsed and reheated. Bapolene 610FP is blended with LDPE at 60–80 wt% to balance shrink forces and stiffness. The first bubble is extruded at melt temperatures of 190–210°C, then reheated in a secondary bubble at 95–110°C and expanded at a blow-up ratio of 3.0:1 to 4.0:1. Finished thickness is commonly 40–70 µm. Free shrink is tested after immersion at 100°C in a silicone oil bath according to ASTM D2732; converters typically require machine-direction and transverse-direction shrink values in the range of 60–75% for tight collation around beverage cans and bottles. Seal strength and seal initiation temperature are measured by ASTM F88 and ASTM F1921, with the low seal initiation of Bapolene 610FP allowing sealing at 90–100°C on high-speed overwrap lines. Terminal products include shrink-wrapped multipacks of bottles, cans, and cartons for warehouse club distribution. Film stored above 35°C may begin low-level relaxation, so warehouse temperature should be maintained below 30°C and stock rotation should follow first-in-first-out inventory control. If the film is corona-treated for print adhesion, the treatment level should be verified at 38–42 mN/m within 24 h of converting, because metallocene LLDPE surfaces decay more quickly than treated LDPE surfaces in humid storage above 60% RH. For EU packaging exports, the film is supplied under REACH and EU Directive 94/62/EC documentation.

    Heavy-Duty Industrial Liners: Dart Impact Retention after Calcium Carbonate Loading

    Blown film lines with 50–75 mm grooved-feed extruders produce tubular film at 80–130 µm thickness for FIBC liners, chemical powder sacks, and e-commerce mailers. Bapolene 610FP is compounded with 10–20 wt% calcium carbonate masterbatch to increase stiffness, block resistance, and surface opacity; the compound is extruded at 200–240°C with a die gap of 2.5 mm and a blow-up ratio of 2.0:1 to 2.5:1. Dart impact is tested through ASTM D1709, and tensile properties through ASTM D882. Calcium carbonate loading above 20 wt% can produce a sharp decrease in dart impact and should be validated on the specific compounding line because published data for this filled configuration with Bapolene 610FP is limited. End-use liners are inserted into woven polypropylene FIBCs for moisture-barrier packaging of chemical powders, pigments, and construction additives, or converted into flat and gusseted sacks with heat-sealed bottoms. The film may be formulated with antistatic additive masterbatch at 1–3 wt% to reduce dust attraction and surface resistivity, with surface resistivity verified according to IEC 61340-2-3 or ASTM D257. If the liner is used for hazardous chemical packaging, the converter must certify the completed sack construction under the applicable dangerous goods transport regulation, because the film alone does not confer UN packaging certification. Multiple-layer liners with high filler loading can show delamination at the sack bottom seal if the seal bar temperature exceeds 160°C by more than 10°C, so hot-tack and seal-strength validation per ASTM F1921 and ASTM F88 should be carried out on production samples before filling trials.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 610FP LLDPE, Metallocene Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bapolene® 610FP is a metallocene-catalyzed linear low-density polyethylene film resin supplied by Bamberger Polymers under the grade designation Bapolene® 610FP LLDPE, Metallocene Film Grade. The grade is specified for blown film extrusion, particularly in monolayer and coextruded structures that require a controlled balance of dart impact resistance, tear propagation behavior, and low-temperature seal response. The metallocene architecture produces a narrower molecular weight distribution and more uniform comonomer placement than conventional Ziegler-Natta butene linear low-density polyethylene. Melt flow rate is reported under ASTM D1238 or ISO 1133-1:2022 at 190 °C and 2.16 kg; density is reported under ASTM D1505 or ISO 1183-1:2019. Lot-specific certificates of analysis supersede nominal grade descriptions because additive loadings and melt flow values vary within established release limits.

    Published nominal values for the 610FP grade are positioned around a melt index of 1.0 g/10 min and a density near 0.918 g/cm³. The current technical data sheet must be consulted for minimum and maximum specification limits. The melt flow-rate band places the grade in the general-purpose film extrusion range, where converters require sufficient draw for thin gauge without sacrificing bubble stability. The product is not a broad-molecular-weight fractional-melt resin, and processing parameters should not be copied from a 0.5 g/10 min or lower melt index LLDPE without rebalancing the film line.

    Film evaluation is commonly performed on specimens in the 25–50 µm gauge band after conditioning at 23 ± 2 °C and 50 ± 5 % relative humidity. Tensile yield, elongation at break, and energy-to-break values are generated under ASTM D882-18 or ISO 527-3:2018; dart impact is generated under ASTM D1709-16 Method A; Elmendorf tear propagation is generated under ASTM D1922-09; and optical haze is generated under ASTM D1003-13. Seal initiation temperature is not a single resin constant; it is measured on a heat sealer with controlled jaw pressure, dwell time, and temperature increments by ASTM F88/F88M-21 or by ASTM F1921-12 for hot tack.

    What limits stable bubble formation with 610FP on high-output blown film lines?

    Field behavior on single-screw blown-film lines is governed by melt strength, die geometry, and air-ring control. With die gaps of 1.4–2.8 mm and blow-up ratios from 2.0:1 to 3.0:1, melt temperatures are typically set between 190 °C and 220 °C. Screw configurations with L/D 24:1 to 30:1 and barrier sections with spiral or Maddock mixing elements provide sufficient melt homogeneity without excessive shear heating. At head pressures above 35 MPa, melt temperature can rise beyond the set point, leading to gel formation and film optical defects. Bubble stability decreases when the frost line height is set too low because the quenched melt has insufficient time to redistribute stress at the draw ratio; conversely, an excessively high frost line increases sag and gauge variation. Specific throughput on blown-film lines for this melt flow-rate class is generally in the range of 0.7–1.1 kg/h/cm of die circumference, but the actual limit is determined by screw design, die diameter, and air-ring pressure balance.

    Sharkskin melt fracture can appear when shear stress at the die lip exceeds the critical stress for a narrow molecular weight distribution melt. The onset shear stress for metallocene LLDPE is lower than for broad-MWD Ziegler-Natta LLDPE at equivalent melt index. Increasing die gap, raising melt temperature within the 220 °C limit, or reducing output can shift the transition to higher rates. Die-lip geometry and land length also affect the critical shear rate. No pre-drying is normally required for polyethylene, but pellets stored at temperatures below the plant dew point can acquire surface condensation that introduces moisture into the feed throat and produces voids or surface defects in the film. Such condensation must be eliminated before processing.

    Cast film converters should not transfer blown-film die and temperature settings directly to a flat-die process. Cast film lines typically operate with shorter melt residence times and higher melt temperatures, but the absence of bubble stability constraints allows higher draw and thinner gauge. The grade’s melt index and narrow composition distribution support rapid quench and low gel counts, provided the extruder barrier screw is not overfed and the chill-roll temperature is maintained within 20–40 °C for polyolefin film. Incompatibility with excessive backpressure is a known operational boundary; a shallow-flight screw with insufficient melting capacity can produce unmelted resin particles in the cast web.

    Film Property Certification and ASTM/ISO Method Alignment

    Certification of Bapolene® 610FP film property balances requires alignment between resin release testing and fabricated film testing. The resin certificate of analysis typically records melt mass-flow rate and density, while film tensile, impact, tear, and optics are determined on film produced under defined laboratory conditions. Because film properties are not intrinsic constants, comparisons between resins require identical equipment, die gap, blow-up ratio, gauge, frost line height, and conditioning history. A shift of 0.002 g/cm³ in density or 0.2 g/10 min in melt index within the specification band can alter seal initiation, dart impact, and extrusion head pressure more than a resin name change alone.

    Principal test methods used for Bapolene 610FP film certification
    PropertyStandard designationSpecimen or condition
    Melt flow rateISO 1133-1:2022 / ASTM D1238190 °C / 2.16 kg
    DensityISO 1183-1:2019 / ASTM D1505Compression-molded plaque
    Tensile propertiesASTM D882-18 / ISO 527-3:2018Film strip, 25–50 µm
    Dart drop impactASTM D1709-16 Method AFalling weight, 25 µm film
    Elmendorf tearASTM D1922-09Machined notch, MD and TD
    HazeASTM D1003-13Film specimen, integrating sphere
    Seal initiationASTM F88/F88M-21Heat-sealed strip, controlled jaw conditions

    Puncture and slow-rate penetration resistance, where relevant for industrial liners and heavy-duty packaging, may be characterized under ASTM D5748 or ASTM F1306. These methods are not substitutes for end-use abuse testing on a packaging line, but they provide a reproducible basis for comparing Bapolene® 610FP against alternative resins or formulations. The narrow molecular weight distribution of metallocene LLDPE can produce a different tear-puncture balance than broad-MWD resins even when tensile yield values appear similar.

    When 610FP replaces a conventional Ziegler-Natta butene LLDPE in a blown film formulation

    Direct substitution without adjustment of die gap, output rate, or blow-up ratio can result in bubble instability and lower machine-direction tear. Comparative characterization by high-temperature gel permeation chromatography under ASTM D6474 typically shows lower polydispersity for metallocene LLDPE than for conventional butene LLDPE. Published values for metallocene grades commonly fall in the 2.0–3.5 Mw/Mn range, while conventional Ziegler-Natta grades often fall between 3.5 and 6.0. The resulting film may exhibit higher dart impact and lower haze under ASTM D1003-13, but the narrower distribution reduces melt strength and may require a lower frost line height or a higher blow-up ratio to maintain bubble geometry.

    Seal initiation behavior also differs. Metallocene LLDPE with uniform comonomer placement can seal at a lower temperature than broad-MWD butene LLDPE at equivalent density; published comparative studies report reductions in seal initiation temperature on the order of 3–7 °C. This difference is measurable by ASTM F88/F88M-21 only when heat-seal jaw temperature is incremented in small steps and seal strength is plotted against temperature. The practical result is that film structures using 610FP may allow a lower heat-seal jaw setpoint or shorter dwell on packaging lines, provided sufficient hot-tack strength is available for the fill-and-seal sequence.

    Comparative processing and property profile for 610FP versus conventional butene LLDPE
    Parameter610FP metallocene LLDPEConventional Ziegler-Natta butene LLDPE
    Molecular weight distribution by ASTM D6474Narrower, typically 2.0–3.5 Mw/MnBroader, typically 3.5–6.0 Mw/Mn
    Short-chain branching distributionUniform along chainsHeterogeneous, lower molecular weight fractions more branched
    Melt strength at equivalent melt indexLowerHigher
    Dart impact at 25 µm under ASTM D1709-16Higher at equivalent densityLower baseline
    Haze under ASTM D1003-13Lower at equal gaugeHigher
    Seal initiation by ASTM F88/F88M-21Lower by approximately 3–7 °CHigher
    Machine-direction tear resistanceMay require orientation or formulation adjustmentOften higher at same draw

    The choice between Bapolene® 610FP and a conventional butene LLDPE should be made on the basis of film property priorities and machine capability. A converter running an older air-cooled line with limited air-ring adjustment may prefer a broader-MWD resin because its higher melt strength provides a wider bubble-stability window. Conversely, a coextrusion line with automated die and air-ring control can exploit the impact and optics advantages of 610FP. These operational distinctions are more decisive than small differences in melt index or density within the same product family.

    Compared with high-pressure low-density polyethylene, 610FP requires different draw-down and bubble handling. LDPE possesses long-chain branching and higher melt strength; 610FP does not contain the same long-chain branching architecture. Blending LDPE into 610FP may improve processability but will alter film tensile balance and optical response. The mixed formulation must be evaluated under the same film test methods; published data for this specific configuration is limited and should not be extrapolated from single-resin data sheets.

    Applications for Bapolene® 610FP are those where the film must survive abuse during packaging, distribution, and end use. In food packaging, the grade can be employed in bag-in-box liners and frozen-food films where low-temperature seal strength and puncture resistance are measured under ASTM D5748 or ASTM F1306. In industrial liners and heavy-duty sacks, the resin may be blended with a fractional-melt LLDPE or an HDPE component to raise stiffness and tear propagation resistance. In stretch film, the drawn film performance is evaluated under ASTM D5459 or proprietary load-retention methods; the narrow molecular weight distribution can support higher ultimate stretch under controlled cast-film conditions, but the specific grade may require tackifier and cling additive adjustments. Published data for this specific configuration is limited beyond producer technical bulletins, so pilot-line trials are required.

    Verification protocols remain mandatory across food-contact and industrial end uses

    Before specifying Bapolene® 610FP in food-contact packaging, processors should obtain a current food-contact statement from Bamberger Polymers. Olefin polymers used in the United States may be evaluated for contact with food under FDA 21 CFR 177.1520, but the specific conditions of use, additive package, and multilayer structure determine compliance. For European Union food-contact applications, migration testing under Regulation (EU) No 10/2011 must account for the final package composition and simulant conditions. Industrial applications may be assessed under REACH and, when incorporated into electrical or electronic equipment, under RoHS Directive 2011/65/EU. The resin producer’s annual regulatory certificate documents whether the product is compliant with specific threshold limits, but it does not replace end-product testing by the converter or brand owner.

    Operational boundaries include avoiding prolonged melt residence times above 220 °C and preventing abrasive contamination in the feed system. A purge with a broad-MWD LLDPE or LDPE can be used when transitioning from a high-temperature polymer or a highly filled resin. The hopper, feed throat, and screw flights should be inspected for polymer fines accumulation that can produce black specks or gel particles. If film is produced for high-clarity applications, contaminated regrind should not exceed the concentration recommended by the manufacturer; the technical data sheet for 610FP should be consulted for regrind ratios. Published data for this specific configuration is limited where end-use performance is defined by the packaging line rather than by resin properties alone.

    Top