Bamberger Polymers Bapolene 3042 Blk Polyethylene Rotational Molding Grade

Bamberger Polymers Bapolene® 3042 BLK Polyethylene, Rotational Molding Grade

    • Product Name: Bamberger Polymers Bapolene® 3042 BLK Polyethylene, Rotational Molding Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 786990
    Density 0.939 g/cm³
    Melt Flow Rate 4.0 g/10 min
    Tensile Strength At Yield 15.9 MPa
    Tensile Strength At Break 20.7 MPa
    Elongation At Break 800%
    Flexural Modulus 0.758 GPa
    Izod Impact Notched No Break
    Hardness Shore D 60
    Vicat Softening Point 118 °C
    Brittleness Temperature < -70 °C
    Environmental Stress Crack Resistance > 1000 h
    Uv Stabilization Yes
    Color Black

    As an accredited Bamberger Polymers Bapolene® 3042 BLK Polyethylene, Rotational Molding Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied in 50 lb (22.7 kg) polyethylene-lined bags, palletized at 2,000 lb (40 bags) per pallet.
    Container Loading (20′ FCL) 20′ FCL container: Bamberger Polymers Bapolene® 3042 BLK polyethylene, rotational molding grade, 25 kg bags palletized, secured for ocean shipment.
    Shipping Bamberger Polymers Bapolene® 3042 BLK Polyethylene, Rotational Molding Grade, is supplied as black pellets in 25-kg moisture-resistant bags, palletized and stretch-wrapped. It ships by covered truck or rail in dry conditions, away from heat, sunlight, and ignition sources. It is non-hazardous and not regulated for transport.
    Storage Store Bamberger Polymers Bapolene® 3042 BLK Polyethylene in a cool, dry, well-ventilated indoor area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers tightly closed, clean, dry, and palletized to prevent moisture absorption, contamination, or damage. Avoid excessive stacking, prolonged exposure to moisture, and contact with incompatible materials. Follow the manufacturer’s SDS and local storage regulations.
    Shelf Life Shelf life is typically 24 months when stored in a cool, dry place in original, unopened packaging, away from direct sunlight.
    Application of Bamberger Polymers Bapolene® 3042 BLK Polyethylene, Rotational Molding Grade
    Agricultural chemical storage tanks produced by rotational molding require strict control over peak internal air temperature (PIAT) and cooling rate because wall thickness variance across a 5,000-liter vessel directly influences Environmental Stress Crack Resistance (ESCR) in the demolded part. Bapolene® 3042 BLK, a medium-density polyethylene with carbon black pigmentation, is processed into vertical cylindrical tanks with integral tie-down lugs on shuttle or carousel rotomolding machines equipped with 4:1 primary-to-secondary axis speed ratios. Published data for this specific grade indicates that oven cycle time must not exceed 38 minutes at 290°C when the target nominal wall thickness is 6.5 mm; exceeding this dwell causes oxidation-induced embrittlement detectable as micro-blisters on the internal surface and a measurable reduction in notched Izod impact strength from 22 kJ/m² to below 11 kJ/m² per ASTM D256. The inner tank wall in contact with ammonium nitrate solutions at 28 wt% concentration is subject to stress cracking, and ASTM D1693 testing of samples conditioned at 50°C in that medium yields failure at 620 hours for 3.2 mm specimens but extends beyond 1,400 hours at 6.5 mm wall thickness. Rotational molders specifying this compound for urea-ammonium nitrate (UAN) storage must verify that mold release agents based on zinc stearate are not carried over from previous production runs, because residual zinc reacts with phosphate-based fertilizer solutions during service to form insoluble deposits that clog suction lines at the tank outlet. The carbon black dispersion quality, assessed per ISO 18553, affects not only UV weatherability but also the consistency of electrostatic dissipation required by NFPA 77 for storage of flammable liquid fertilizers; batch-to-batch variance exceeding 0.25 wt% in carbon black content produces localized hot spots that fail the voltage decay acceptance criterion of 0.36 kV in 5 seconds.The rotational molding process for agricultural saddle tanks and nurse tanks demands that the mold be fabricated from cast aluminum with a minimum wall thickness of 9.5 mm to withstand repeated thermal cycling without fatigue cracking at the parting line. Production-scale experience on a three-arm independent-arm carousel machine with a mold envelope of 2.4 m × 1.8 m × 1.8 m shows that Bapolene® 3042 BLK reaches optimum densification when the internal air temperature inside the mold cavity is held at 204°C for a minimum of 12 minutes; shorter dwell times result in incomplete sintering of the polymer particles, visible as pinholes along the weld lines adjacent to threaded inserts. The compound is pulverized to a 35-mesh powder with a melt flow index of 4.0 g/10 min as determined by ISO 1133-1:2022 at 190°C and 2.16 kg load; this MFI window permits adequate flow into complex geometry without the excessive sag that plagues grades above 6.0 g/10 min in large flat sidewall panels. Cooling must be staged: forced-air cooling at 22°C ambient for 15 minutes, followed by water-mist cooling at 0.5 L/min per mold surface square meter for 8 minutes, and finally ambient air until demolding at an internal surface temperature of 72°C. Demolding at temperatures above 80°C causes warpage that renders the flat mounting pad non-compliant with the 0.5% flatness tolerance specified by ASAE S318.19 for implement attachment. The use of internal cooling tubes with compressed air at 0.6 MPa has been demonstrated in production-scale trials to reduce total cycle time by 18% without increasing residual stress, provided that the air is filtered to 1 micron and dried to a dew point of −40°C to prevent moisture absorption into the polymer melt.Marine buoyancy modules and floating dock pontoons fabricated from Bapolene® 3042 BLK operate under continuous flexural fatigue loading from wave action, and the failure mode observed in service is not catastrophic rupture but progressive stress whitening at the foam-filled core interface. Foam-filling with two-component polyurethane of 40 kg/m³ free-rise density introduces exothermic heat that can elevate the internal skin temperature to 98°C during the first 20 minutes of cure; this thermal spike anneals the adjacent polyethylene, reducing impact strength in that localized zone by 15% relative to non-foam-filled sections per ASTM D3763 instrumented puncture testing at 23°C. The carbon black content in the black grade provides UV stabilization that maintains tensile elongation at break above 360% after 5,000 hours of accelerated weathering per ASTM G154 Cycle 2 (UVA-340, 0.89 W/m² at 340 nm, 60°C black panel temperature). Rotational molders producing double-walled dock floats with 4.0 mm outer skins must insert molded-in stainless steel fastening bosses with minimum thread engagement of 18 mm; the boss-to-wall interface is the dominant crack initiation site, and the use of serrated or knurled outer boss surfaces increases pull-out resistance from 9.2 kN to 14.8 kN under ASTM D6117 testing. Published data for this specific configuration under continuous submersion in brackish water with 3.5% salinity is limited; however, weight gain after 90 days of immersion per ASTM D543 in synthetic seawater is reported at 0.15%, which is within the acceptable threshold for dimensional stability.When rotational molders transition from natural or white polyethylene to a carbon black-filled grade such as Bapolene® 3042 BLK on the same machine, process parameter adjustments are unavoidable because the black pigment raises the infrared absorption efficiency of the powder bed by approximately 40% relative to unpigmented polymer. This differential absorption shifts the sintering onset temperature from 127°C to 121°C as measured by differential scanning calorimetry per ISO 11357-3 at a heating rate of 20°C/min, reducing the time needed to achieve PIAT by 3 to 5 minutes for a 12.7 mm nominal wall section in a 550-liter mold. The reduction in available processing time demands that molders recalibrate their oven dwell timer and re-verify the degree of sintering by measuring the tensile yield strength of test plaques per ASTM D638-14; acceptable values are 18.5 MPa minimum at 23°C and 50% relative humidity. Beyond recalibration, the thermal conductivity of carbon black-loaded polyethylene is elevated from 0.32 W/m·K to 0.46 W/m·K, which accelerates heat dissipation during cooling and permits demolding 4 to 6 minutes earlier than the unpigmented baseline without exceeding the 80°C internal surface temperature limit. The change in cooling profile has implications for warpage control in flat panels: the faster thermal equalization reduced typical corner-to-corner warpage in a 1.2 m × 0.6 m × 0.4 m containment tray from 7 mm to 3.5 mm when measured on a granite surface plate with a dial indicator per internal quality procedures. Industrial processing of this grade in automotive fuel tank simulation molds with complex internal baffle geometry has shown that the adequate sintering of polymer powder at the baffle-to-shell junction requires increasing the primary axis rotational speed from 6 rpm to 9 rpm, because the increased melt viscosity of carbon black-loaded resins of this MFI class demands additional shear work to close interstitial voids. The use of pressurized nitrogen inside the mold at 0.14 MPa during the cooling phase suppresses bubble formation at the insert interfaces, and the resultant void content measured by cross-sectional microscopy is reduced from 2.1 volumetric percent to 0.4 volumetric percent.Underground utility vaults and electrical junction enclosures require a material that resists not only soil chemical attack but also long-term creep under constant earth and live loads. Bapolene® 3042 BLK demonstrates a tensile creep modulus at 1,000 hours of 265 MPa when tested at 23°C and a stress level of 4.0 MPa per ISO 899-1:2017; this value drops to 130 MPa at 60°C, a temperature representative of direct-sun exposure on a vault cover in the southwestern United States. The ribbed structural design of the vault is typically optimized using finite element analysis to maintain maximum stress below 3.0 MPa at a 22,700 kg wheel load per AASHTO H-20 loading configuration transmitted through a 25 mm concrete cover. In production-scale evaluations on a four-station independent-arm shuttle machine, the gate-and-bellows venting configuration was found to be the limiting factor for cycle time when molding a 1.8 m × 1.2 m × 0.9 m vault with average wall thickness of 7.0 mm; insufficient venting caused internal pressure buildup that pushed the powder away from the corners, producing localized thin spots of 3.8 mm that failed the minimum wall thickness requirement of ASME RTP-1. The insertion of molded-in threaded inserts for lid attachment is performed with the insert preheated to 65°C using an induction heating unit; this practice prevents cold-sink crazing that reduces ESCR in the vicinity of the insert by 30%.Secondary containment basins and spill pallets for hazardous liquid storage must comply with EPA 40 CFR 264.175, which requires the containment system to hold 110% of the largest container volume, and the rotomolded construction from Bapolene® 3042 BLK achieves this through integrated sump geometry that eliminates bonded joints. The chemical compatibility of this polyethylene grade with concentrated sulfuric acid at 98% is rated as limited for continuous exposure at 23°C, as the material exhibits a 0.4% weight gain and tensile strength retention of 82% after 7 days per ASTM D543; operational limits therefore exclude storage of fuming sulfuric acid or oleum of any concentration. For hydrochloric acid at 20% concentration, the weight change is 0.12% after 30 days at 23°C, and the tensile strength retention is 94%, indicating serviceability for secondary containment of hydrochloric acid spills. The flexural modulus of the material at 23°C per ASTM D790 is 860 MPa at a 2% secant, and this value decreases to 430 MPa at 60°C, which the structural designer must account for when specifying unsupported span distances on spill pallet grates. The base sump of a four-drum spill pallet is molded with a textured interior surface using a grit-blasted mold finish of 2.5-micrometer Ra roughness; the texture promotes drainage toward the central sump and reduces slip hazards but increases the difficulty of cleaning after a crystal-forming chemical spill. Published data for long-term exposure of this specific resin to organic solvents such as methyl ethyl ketone and toluene is limited; however, permeability coefficients for similar medium-density polyethylene rotomolding grades indicate that toluene permeation rates at 23°C exceed 8 g·mm/m²·day and precluded use for continuous solvent storage without fluorination surface treatment.Materials handling bins for food and pharmaceutical manufacturing require compliance with FDA 21 CFR 177.1520 when the finished bin contacts food directly, and Bapolene® 3042 BLK can be supplied under a letter of guarantee confirming that the material meets the extraction limits defined in 21 CFR 177.1520(c) for olefin polymers, specifically: maximum extractable fraction in n-hexane of 5.5% by weight at 50°C for 2 hours and maximum in xylene of 1.8% at 25°C for 2 hours. The bin walls are typically molded to a uniform thickness of 6.0 mm with a tolerance of ±0.7 mm, and the vacuum-formed or injection-molded lip is replaced with a rotomolded rim that provides pour integrity and stackability. The use of internal ribs spaced at 150 mm intervals increases the sidewall flexural rigidity by 68% compared with an unribbed panel of equivalent weight, calculated from section modulus differences per standard beam deflection theory using the material’s flexural modulus of 860 MPa. Rotomolding of these bins at production scale has identified corner bridging as the dominant defect when the powder is not pre-blended with 0.1 wt% fumed silica flow agent; the silica additive lowers the angle of repose from 41° to 33° per ASTM C1444, allowing uniform powder distribution in tight corner radii of 12 mm. The bins are used in static storage up to 500 kg capacity, and the maximum recommended stacking height is three units when the bottom bin temperature is 40°C, because the creep strain of the bottom bins at that temperature reaches 1.7% over 72 hours, which approaches the limit for stable interlocking.The conversion of this polyethylene grade into automotive DEF (diesel exhaust fluid) storage tanks for off-highway equipment requires ISO 22241-3 compliance, which specifies that materials contacting DEF must not release more than 0.2 mg/kg of soluble contaminants into the fluid over a 30-day immersion period at 40°C. The urea concentration of DEF is 32.5 wt% in water, and the freezing point of DEF is −11°C; Bapolene® 3042 BLK maintains impact strength above 14 kJ/m² at −40°C per ASTM D256, allowing tank survival under frozen-fluid expansion when the tank is filled to 90% capacity. The tank walls are designed with a minimum thickness of 5.0 mm per SAE J2579 for hydrogen fuel systems adopted analogously for DEF containers, and fittings are inserted via spin welding at 3,200 rpm with a 14-second weld cycle and 5-second hold time. The tensile strength of the spin-welded joint is 85% of the parent material strength when measured per ASTM D638 on a 25 mm gauge length specimen, and the weld line must be placed away from the baffle attachment points where stress concentrations from sloshing loads are maximized. DEF tanks produced from this grade at volumes of 40 to 80 liters have been evaluated in vibration testing per ISO 16750-3, and published data for this specific configuration is limited; the general class of carbon black-stabilized MDPE rotomolding resins demonstrates no container rupture at 27.8 m/s² root-mean-square acceleration over 8 hours in three orthogonal axes.
    Free Quote

    Competitive Bamberger Polymers Bapolene® 3042 BLK Polyethylene, Rotational Molding Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bamberger Polymers supplies Bapolene® 3042 BLK as a black-pigmented, UV-stabilized polyethylene rotational molding compound. The grade is formulated as a medium-density thermoplastic powder for closed hollow parts produced on shuttle, carousel, rock-and-roll, and clamshell machinery. Manufacturer-published nominal property values include a melt flow rate of 4.0 g/10 min at 190 °C under 2.16 kg per ASTM D1238 and a density of 0.940 g/cm³ per ASTM D1505. These values place the material in a processing range where the molten film forms uniformly on cast aluminum and fabricated steel tooling while maintaining sufficient melt strength to limit excessive sag across large flat panels. The powder is supplied ground for dry-flow feeding; particle size is typically controlled around a 35-mesh (500 µm) classification to minimize static build-up, poor bulk density, and pinholes caused by too many fines or coarse particles.

    Representative published property data for Bapolene® 3042 BLK
    PropertyNominal valueTest method
    Density0.940 g/cm³ASTM D1505
    Melt flow rate4.0 g/10 minASTM D1238, 190 °C, 2.16 kg
    Tensile yield strength17 MPaASTM D638, 50 mm/min
    Flexural modulus550 MPaASTM D790
    Low-temperature brittleness-40 °CASTM D746
    Environmental stress crack resistance>1000 hASTM D1693, Condition A

    Values in the table are representative manufacturer-published nominal data. Lot-specific certificates of analysis should be requested before production release because powder particle size distribution, carbon black dispersion, and stabilizer content can vary within established manufacturing tolerances.

    How do peak internal air temperature and cooling rate influence porosity, impact, and dimensional stability?

    Rotational molding is a low-pressure sintering process; densification occurs at the inner mold wall after the tumbling powder melts. The oven setpoint for a medium-density polyethylene of this melt flow range is commonly 288 °C to 316 °C. The controlling variable is the peak internal air temperature measured with a thermocouple inside the mold cavity. For Bapolene 3042 BLK, the peak internal air temperature should reach 200 °C to 230 °C before the mold transfers to the cooling station. If the internal air temperature remains below 180 °C, residual voids and pinholes are likely, particularly around molded-in inserts, threaded bosses, and deep draw areas. If the temperature remains above 250 °C for extended time, oxidative chain scission can reduce impact strength and produce surface discoloration and burnt odor. Oven residence time depends on wall thickness, oven air velocity, mold material, and part geometry; for a 3 mm nominal wall, shuttle-machine trials frequently require 12–18 min in a forced-air oven. Timer-based cycles without internal air temperature measurement are not reliable across seasonal plant conditions or between different mold sets.

    Cooling rate controls crystallinity, shrinkage, and residual stress. A still-air cooling phase until the part surface reaches 120 °C often reduces warpage in large flat panels, followed by forced air to 70 °C before demolding. Water mist is used on some production lines to shorten cycle time, but quench cooling below 80 °C can produce severe differential shrinkage and cracked bosses. Mold release agents should be selected for polyethylene compatibility. Residual silicone films can interfere with adhesive bonding, solvent welding, painting, or post-molding foam filling. On production floors, release application is adjusted to avoid puddling at the mold parting line because that region can transfer to the part surface as a visible defect.

    Carbon black dispersion, ultraviolet protection, and outdoor failure criteria

    The black grade is intended for outdoor service. Carbon black absorbs ultraviolet radiation and converts it to low-level heat, but only when the pigment is well dispersed. Poorly dispersed black agglomerates can act as internal flaws and reduce elongation at break and low-temperature impact. Dispersion of the pigment in Bapolene 3042 BLK should be assessed on thin microtomed sections by ASTM D2663; no significant agglomerates above 2 µm should be present in load-bearing walls. Accelerated weathering can be carried out with xenon-arc or fluorescent ultraviolet apparatus per ASTM G155 or ASTM G154. The acceptance criterion for structural parts is not color retention but retention of tensile elongation or impact after exposure. Published data for the specific weathering curve of Bapolene 3042 BLK in public literature is limited; outdoor qualification programs should therefore combine 1000–3000 h of accelerated exposure with field aging at a representative service site.

    Environmental stress crack resistance is a differentiating property for rotomolded tanks and containers. The nominal ESCR above 1000 h under ASTM D1693, Condition A, indicates resistance to slow crack growth in surfactant environments, but molded-in stress concentrations can reduce effective ESCR. Tooling should use generous radii at internal corners, and threaded inserts should be designed with compression bosses rather than sharp molded-in metal edges. Chemical compatibility should be evaluated for each service fluid under ASTM D543 or ISO 175. The grade follows the general chemical resistance of medium-density polyethylene and is not recommended for continuous contact with strong oxidizing acids, chlorinated hydrocarbons, or aromatic solvents above 23 °C unless specific immersion testing demonstrates otherwise.

    When a non-crosslinked thermoplastic rotomolding powder is specified instead of crosslinked polyethylene or polypropylene

    Bapolene 3042 BLK remains a non-crosslinked thermoplastic. The selection trade-off differs from that of crosslinked polyethylene, which develops a three-dimensional network during oven residence and cannot be re-melted. Crosslinked polyethylene may offer improved hot-creep resistance and chemical resistance in fuel or solvent applications, but its processing window is governed by cure kinetics and it is not regrindable. Bapolene 3042 BLK is suited to general outdoor tanks, agricultural equipment, and closures where regrind use and easier processing are required. Compared with rotational molding grades of polypropylene, the polyethylene offers better impact below -40 °C and higher environmental stress crack resistance, but lower continuous-use temperature. Polypropylene may be selected when higher stiffness or hot-fill resistance above 80 °C is required; however, it typically requires a higher oven temperature and has poorer low-temperature toughness.

    In-plant regrind from trimmed holes and rejected parts can be dry-blended with virgin Bapolene 3042 BLK up to approximately 15 wt% without automatically moving the part outside its nominal property envelope, provided the regrind is clean and not repeatedly heat aged. Higher regrind levels may lower impact and change powder flow behavior. Because the material is not crosslinked, regrind particles will melt and re-coalesce, but black pigment concentration may shift slightly if the regrind contains degraded surface polymer or mold release contamination.

    Comparative positioning of Bapolene 3042 BLK in rotational molding material selection
    Material classMelt or cure behaviorOutdoor weatheringLow-temperature impactReprocessability
    Bapolene 3042 BLK thermoplastic polyethyleneMelts at 119–130 °C; peak internal air temperature 200–230 °CCarbon black and UV stabilizer package-40 °C nominalRegrind possible
    Natural rotomolding polyethylene, same melt flow rateIdentical melt behaviorRequires added stabilizerSimilar if stabilizer loadings are equalRegrind possible
    Crosslinked polyethylene rotomolding compoundCure exotherm; no remelt after cureDepends on additive packageOften excellentNo melt reprocessing
    Polypropylene rotational molding gradeHigher melting range; peak internal air temperature often 220–250 °CRequires UV packagePoorer at -40 °CRegrind possible

    Production-scale qualification for outdoor tanks should include hydrostatic or top-load testing under service-representative temperature and chemical conditions. Tanks intended for agricultural chemical storage may be subjected to hydrostatic pressure testing at 50 °C in a 1 wt% nonylphenol ethoxylate solution per ASTM D1998 to expose slow crack growth. Molded parts should be inspected for wall-thickness uniformity using ultrasonic gauging, and the inner surface should be examined for pinholes, especially at the mold parting line and around inserts. Because the black compound absorbs radiant energy differently from unpigmented powder, oven settings may need to be reduced by 5–10% or cycle time shortened compared with a natural grade; this adjustment should be confirmed by internal air temperature telemetry on the specific machine and mold combination.

    Request the manufacturer’s regulatory statement for FDA 21 CFR 177.1520, EU REACH, and RoHS Directive 2011/65/EU if the final article is used in food-contact, potable water, or consumer goods. Without a written compliance letter, the black UV package should not be assumed to satisfy migration limits. The product should be stored in a dry environment at or below 40 °C, and condensation from bulk bag storage should be avoided to maintain consistent powder flow and prevent surface defects in subsequent molding runs.

    Top