| HS Code | 742189 |
| Density | 0.939 g/cm3 |
| Melt Flow Rate | 3.5 g/10 min |
| Tensile Strength At Yield | 24.1 MPa |
| Tensile Strength At Break | 20.0 MPa |
| Elongation At Break | 800 % |
| Flexural Modulus | 758 MPa |
| Tensile Modulus | 724 MPa |
| Vicat Softening Point | 116 °C |
| Brittleness Temperature | -70 °C |
| Hardness Shore D | 55 |
| Environmental Stress Crack Resistance | >1000 hr |
| Thermal Expansion Coefficient | 1.3E-4 1/°C |
As an accredited Bamberger Polymers Bapolene® 3039U Polyethylene, Rotational Molding Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Bamberger Polymers Bapolene® 3039U is typically supplied in 50 lb (22.7 kg) multiwall bags, palletized for shipping. |
| Container Loading (20′ FCL) | 20′ FCL: approximately 20 metric tons (800 × 25 kg bags) of Bapolene 3039U polyethylene, palletized or floor-loaded. |
| Shipping | Bapolene® 3039U polyethylene rotational molding grade is a non-hazardous, pelletized resin. It typically ships in 25 kg bags, bulk bags, or bulk trucks/railcars. Transport in clean, dry, covered equipment; avoid moisture, contamination, and excessive heat. Not regulated for transport under DOT/IMDG/IATA; follow SDS and local rules. |
| Storage | Store Bamberger Polymers Bapolene® 3039U Polyethylene, Rotational Molding Grade, in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers or bags tightly closed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizing agents. Protect from ultraviolet light and physical damage. Palletize off the floor, use first-in-first-out rotation, and follow local regulations. |
| Shelf Life | Shelf Life: Bamberger Polymers Bapolene® 3039U has no specific shelf life; store in cool, dry area away from direct sunlight and moisture. |
Potable water contact service imposes a different compliance architecture than industrial chemical containment because the rotomolded article is evaluated for contaminant extraction rather than only structural and environmental stress crack resistance performance. Under NSF/ANSI 61, the tank is subjected to extraction waters at pH 5 and pH 10 at 23°C for cold-water service; the specific exposure protocol depends on the ratio of surface area to water volume and the intended use temperature. The rotomolding powder must be free of lead-based colorants and cadmium-based pigments; only 0.25–0.75 wt% of a compliant pigment masterbatch should be used, and the masterbatch carrier resin must also comply with FDA 21 CFR 177.1520. External mold release is limited to zinc stearate applied at 0.1–0.3 g/m²; higher loadings can create a hydrophobic surface layer that increases organic carbon extraction in the first draw. Processing on a shuttle-type rotational molding machine with 4:1 biaxial rotation uses an oven temperature between 275°C and 290°C and a peak internal air temperature between 185°C and 195°C. The cooling segment is staged: forced air for 10–15 min, followed by water mist for 5–8 min, with demolding at or below 70°C to avoid thermal shock and surface microcracking. Potable water tanks produced from Bapolene® 3039U generally require compliance with ASTM D1998-21 for upright storage tank wall thickness and hydrostatic design. The following matrix summarizes the principal regulatory boundaries for this application.
| Standard | Test requirement | Application boundary |
|---|---|---|
| NSF/ANSI 61 | Extraction at pH 5 and pH 10 at 23°C | Potable water contact surfaces |
| FDA 21 CFR 177.1520 | Olefin polymer classification and migration limits | Food contact and potable water components |
| ASTM D1998-21 | Minimum wall thickness and hydrostatic design basis | Upright polyethylene storage tanks |
| EU 10/2011 | Overall migration limit 10 mg/dm² | EU food contact applications |
Published extraction data for Bapolene® 3039U under NSF/ANSI 61 is limited; pre-production extraction testing is required because slight changes in pigment grade, mold release concentration, or cooling rate can shift the extractables profile. The inner skin of a rotomolded potable water tank is formed under low shear and prolonged heat, which can concentrate low-molecular-weight oxidation byproducts at the surface if the peak internal air temperature exceeds 200°C. Therefore, the processor should avoid over-soaking the part and should verify that the antioxidant package does not contribute above the allowable total organic carbon threshold in the first extraction draw.
For agricultural chemical containment, the failure mode differs fundamentally from potable water service because dilute fertilizer solutions and pesticide emulsifiable concentrates can accelerate environmental stress cracking at the inner wall. The selection of Bapolene® 3039U for sprayer tanks and nurse tanks is therefore governed by ASTM D1693-21 ESCR and ASTM D543-21 chemical resistance immersion tests in 30% urea-ammonium nitrate and 5% glyphosate solutions at 50°C for 30 days. A critical processing constraint is the post-mold cooling rate: rapid forced-air cooling above 15°C/min through the 120–90°C window increases crystallinity gradients between the inner and outer surfaces, producing residual stress that reduces ESCR by up to 40% in aggressive surface-active solutions. The mold exit temperature should not exceed 70°C before demolding to avoid warpage of wide flat side panels. For outdoor exposure, carbon black masterbatch is incorporated at 2.0–2.5 wt% or a hindered amine light stabilizer package at 0.35–0.50 wt%; dispersion must exceed 95% uniformity as checked on a 25 mm press-out film under transmitted light. In production, a spider-type rotary blender operating at 45–60 rpm for 20 min is used to compound the powder before charging. Peak internal air temperature is maintained between 190°C and 200°C to achieve full fusion without degrading the agricultural chemical resistance package. Published comparative field data for Bapolene® 3039U in pesticide contact is limited; compatibility with the specific formulation should be validated by immersion testing rather than assumed from generic polyethylene data.When material handling hoppers require combined abrasion resistance and impact strength, the wall thickness and rotational parameters shift away from thin-wall tank work. Material handling bins, hoppers, and tote boxes molded from Bapolene® 3039U are used in food processing, pharmaceutical intermediate transfer, and general dry-bulk logistics. The design must satisfy FDA 21 CFR 177.1520 for food contact, ASTM D638-22 tensile yield, ASTM D790-17 flexural modulus, and ASTM D256-23 Izod impact at -40°C for refrigerated warehouse use. For abrasive granular product handling, a wall thickness of 4.0–6.0 mm is generally specified; the bottom wear surface is thickened to 8.0–10.0 mm by adjusting the powder charge and using a drop box or molded-in rib pattern. Rotational molding parameters differ from thin-wall tank work because the thicker bottom requires a peak internal air temperature closer to 204–210°C and a longer soak time of 12–18 min to eliminate bubbles at the inner skin. The rotational ratio may be shifted to 2:1 for rectangular bins with narrow end walls to increase powder dwell time in the corners. Molded-in metallic or polymer inserts for hinge points and forklift pockets must be preheated to 60–80°C before charging to prevent local cold spots and sink marks. Impact failures on production lines often occur at the intersection of the sidewall and floor because powder bridging during early rotation leaves a low-density seam; this is mitigated by reducing powder flow agent content below 0.05 wt% and by increasing the primary-axis speed to 6 rpm during the first 3 min of heating. Published data for Bapolene® 3039U in large hopper configurations is limited; therefore, a full-scale mold trial with wall-thickness mapping via an ultrasonic transducer is advised before release.
For marine dock float and buoyancy components, cyclic compression loading is the governing service condition alongside ultraviolet radiation and water absorption. Rotationally molded marine floats and dock modules require long-term resistance to ultraviolet radiation, wave-induced cyclic compression, and water absorption under sustained hydrostatic pressure. Bapolene® 3039U is assessed for this service under ASTM D4329-21 QUV exposure in the UVA-340 cycle, ASTM D570-22 water absorption at 23°C, and ASTM D638-22 tensile property retention after 2,000 h weathering. The outer wall thickness is typically 4.5–6.0 mm for a nominal 450 mm float module; the internal cavity is either hollow with sealed inserts or filled with expanded polystyrene to maintain buoyancy after puncture. Foam filling requires that the EPS density be 10–15 kg/m³ and that no more than 85% of the cavity volume be filled, leaving thermal expansion headspace. Rotational molding of foamed floats demands peak internal air temperature between 190°C and 200°C; exceeding 205°C accelerates antioxidant depletion at the inner skin and risks EPS collapse. The cooling cycle uses forced air for 15–20 min, followed by water mist for 8–12 min, with demolding at 65°C or below. A UV stabilizer package of 0.5–0.75 wt% hindered amine light stabilizer and 0.05–0.15 wt% benzotriazole UV absorber is dry-blended into the powder; outdoor exposure above 50 kLy/year accelerates gloss loss and surface crazing if the additive loading falls below 0.35 wt%. Published accelerated aging data for Bapolene® 3039U in marine environments is limited; the above ranges are typical for medium-density rotomolding polyethylene and require confirmation against the grade’s datasheet.
Component designs for outdoor recreation and furniture rely on low-temperature impact resistance, vibrational fatigue strength, and color retention under intermittent load. Playground step units, bench slats, and cooler body panels are molded with wall thicknesses between 3.5 mm and 5.5 mm; the design must meet ASTM F1487-21 for public playground equipment and ASTM D256-23 for impact at -20°C. Because these parts are often two-tone or complex-shape, the powder is dry-colored with 0.5–2.0 wt% pigmented polyethylene masterbatch; the pigment system must not contain heavy metals regulated under ASTM F963-23 where the component is accessible to children. Processing on a rock-and-roll machine with single-axis oscillation is used for flat panels, whereas complex three-dimensional parts require a shuttle machine with 4:1 biaxial rotation and an oven temperature of 275–290°C. Mold release is minimized to 0.1–0.2 g/m² to maintain paint and adhesive bonding on post-molded surfaces. The demolded part is allowed to cool to 45°C before any mechanical trimming; trimming above this temperature creates burrs and microcracks at gate and vent locations because the semicrystalline matrix is still above its secondary relaxation region. Field failure modes include stress whitening at screw bosses when torque exceeds 4 N·m in un-reinforced polyethylene and UV chalking on unstabilized light colors after 1,500 h of QUV-A exposure.Competitive Bamberger Polymers Bapolene® 3039U Polyethylene, Rotational Molding Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Bamberger Polymers Bapolene® 3039U is a UV-stabilized high-density polyethylene copolymer powder supplied for rotational molding of hollow parts that require outdoor weathering resistance, low-temperature impact resistance, and environmental stress-crack resistance. The product designation places the nominal density at 0.939 g/cm³ under ASTM D1505; this intermediate-density HDPE range is used to balance flexural stiffness with ductility in thick-walled parts. Unlike general-purpose rotomolding grades that are supplied without light stabilizers, the 3039U variant is formulated with a hindered-amine light stabilizer package and is typically ground to a 35-mesh powder for dry-flow charging. The material is specified for agricultural sprayer tanks, outdoor water storage tanks, marine buoys, playground components, utility cabinets, and kayak hull sections where nominal wall thickness generally ranges from 3 mm to 20 mm. Published property values are typical lot averages, not documented minimum specifications, and should be verified against the supplier’s certificate of analysis before tooling is cut.
Table 1 compiles the typical physical property profile for Bapolene® 3039U under standard test conditions. The values are extracted from manufacturer technical literature and are used for material selection rather than design allowables. Melt flow rate at 190 °C with 2.16 kg weight is reported near 3.0 g/10 min under ASTM D1238, a low-to-medium flow range for rotational molding that supports adequate wall thickness distribution without excessive sintering time. The density of 0.939 g/cm³ provides higher stiffness than linear low-density polyethylene rotomolding grades but marginally lower rigidity than 0.945 g/cm³ HDPE grades. Tensile yield strength is reported near 19 MPa under ASTM D638, and elongation at break exceeds 600%, indicating ductile failure under slow strain. Flexural modulus near 800 MPa under ASTM D790 places the grade at the lower-to-intermediate stiffness end for HDPE, which reduces shrinkage-induced warpage in large flat panels. Environmental stress-crack resistance under ASTM D1693, Condition B, is reported at greater than 1000 h without 50% failure, a value that supports long-term contact with aqueous surfactant solutions. Low-temperature ARM impact at -40 °C is typically above 30 ft-lb, a practical threshold for outdoor service in cold climates.
| Property | Test Method | Reported Value |
|---|---|---|
| Nominal density | ASTM D1505 | 0.939 g/cm³ |
| Melt flow rate, 190 °C/2.16 kg | ASTM D1238 | 3.0 g/10 min |
| Tensile yield strength | ASTM D638 | 19 MPa |
| Elongation at break | ASTM D638 | >600% |
| Flexural modulus | ASTM D790 | 800 MPa |
| ESCR, 100% Igepal, Condition B | ASTM D1693 | >1000 h |
| Low-temperature impact, ARM, -40 °C | ARM | >30 ft-lb |
| Hardness, Shore D | ASTM D2240 | 63 |
| Vicat softening temperature | ASTM D1525 | 122 °C |
The reported tensile and flexural values are generated on compression-molded plaques, not on rotomolded parts. Rotomolded walls frequently display a slight skin-to-core morphology difference because the outer skin cools faster against the tool surface. Consequently, design calculations for large tanks should apply a safety factor to the published modulus. The Vicat softening temperature of 122 °C under ASTM D1525 defines a short-term thermal deflection threshold, not a continuous service temperature. Continuous outdoor service above 60 °C ambient is not recommended without prototype testing because creep in flat vertical walls can produce dimensional change under hydrostatic load. The ESCR result is most relevant for detergent and wetting-agent exposure; it does not replace chemical immersion testing for aggressive agricultural formulations.
Melt rheology controls the sintering window more directly than the melt flow value alone. At rotational molding shear rates, which are low relative to injection molding, the zero-shear viscosity of Bapolene® 3039U is high enough to prevent rapid melt sag in deep-draw tools but low enough to allow particle coalescence at peak internal air temperatures above 200 °C. Comparative molding trials on shuttle-type machines have shown that a peak internal air temperature plateau of 205 °C to 215 °C for 2 min to 4 min produces fully densified walls without the surface oxidation that appears as yellowing at temperatures above 220 °C. Sintering rate is governed by melt viscosity, surface tension, and powder particle contact area. The 35-mesh particle size of 3039U provides a finer contact network than 20-mesh rotomolding powders, which accelerates void removal in thin ribs. In thick sections above 12 mm, the limiting factor shifts to heat transfer through the polymer melt, and cycle time increases nonlinearly with wall thickness.
Rotational molding trials with internal air temperature probes indicate that the time to reach 180 °C is a useful predictor of densification in complex tooling. If the tool reaches 180 °C internal air before 12 min, the outer skin may densify before deep pockets have filled. If the ramp is slower than 20 min for a 6 mm wall, the melt may begin to degrade in thin regions while thick bosses remain porous. Production-scale rotomolders have observed that the optimum oven air temperature for 3039U is lower than that used for 0.945 g/cm³ HDPE grades because the intermediate density reduces the thermodynamic barrier to particle fusion. Oven air set points between 285 °C and 315 °C are typical; set points above 330 °C are associated with surface oxidation and release-agent breakdown.
Bapolene® 3039U is processed on carousel, shuttle, and rock-and-roll rotational molding machines with clamped aluminum or steel tools. The powder is charged at ambient temperature, and the tool rotates simultaneously on two axes. A representative oven air temperature range is 285 °C to 315 °C; peak internal air temperature is held between 205 °C and 215 °C to complete sintering without oxidative degradation. The mold rotation ratio is typically 4:1 for uniform wall thickness, with arm speed adjusted to 5 rpm to 8 rpm for large tanks and 10 rpm to 12 rpm for small parts. Cycle time depends on wall thickness: parts with 6 mm nominal wall may require 18 min to 22 min oven residence, while 12 mm walls may require 28 min to 35 min. After the oven cycle, forced-air or water-mist cooling is applied until the internal air temperature falls below 85 °C before demolding. Excessive cooling rates should be avoided because they can induce warpage and residual stress in flat panels. Production-scale experience indicates that warpage in large storage tank halves is reduced when cooling air is directed first to the mold frame, not to the part surface, and when mold release is delayed until internal air is below 75 °C.
Tool rotation ratios outside the 3:1 to 5:1 range may produce wall thickness variation in tank corners. On carousel machines with multiple arms, the powder should be weighed to within ±1 wt% of the target shot weight because overcharging increases wall thickness and cycle time, while undercharging creates edge thinning. Aluminum tools with 8 mm to 10 mm wall thickness provide faster heat transfer than steel tools and reduce cycle time, but they are more susceptible to warpage in large flat panels. Steel tools are preferred for long production runs because of dimensional stability, despite longer oven residence. Mold release agents should be applied at the minimum effective thickness; excessive release agent volatilizes during the oven cycle and can generate pinholes in the outer skin.
Powder particle-size distribution controls dry-flow and mold fill in complex tools. Bapolene® 3039U is typically supplied with a 35-mesh top cut, corresponding to a maximum particle size of 500 µm, and a bulk density near 0.48 g/cm³. In multi-cavity tools with deep ribs, fine fractions promote sintering but can reduce dry-flow due to electrostatic agglomeration. Rotomolders in the field have observed bridging at sharp corners when the cavity depth-to-width ratio exceeds 1.5:1 and when the powder is stored at relative humidity above 60%. Moisture pick-up in the powder may produce pinholes after densification. Dry-air storage or hopper drying at 40 °C to 50 °C for 4 h is used on production lines where ambient humidity exceeds that threshold. The use of external dry-flow additives is not required for 3039U, and compounding with metallic stearates is not recommended because it may alter the UV stabilization package.
For outdoor tanks, kayaks, and marine components, the selection of Bapolene® 3039U is justified by the UV stabilizer package. The base polyethylene is not inherently UV-stable; unstabilized HDPE undergoes chain scission under UV-B exposure, leading to surface crazing, loss of impact, and eventual cracking. Bapolene® 3039U is produced with a hindered-amine light stabilizer system. Accelerated weathering is typically evaluated under ASTM D2565 or ISO 4892-2 xenon-arc conditions, but published data for this specific configuration is limited to lot-specific test programs. Rotomolders specifying this grade for potable water tanks should confirm the exact additive package status under 21 CFR 177.1520; UV-stabilizer compliance may vary by supplier formulation and should not be assumed from base resin compliance alone. For chemical storage, the grade has stress-crack resistance above 1000 h under ASTM D1693, but solvent compatibility must be tested with the intended chemical at the service temperature, particularly for organic solvents and strong oxidizing agents.
Outdoor color retention is additive-dependent, not base-resin dependent. Natural 3039U is supplied in an uncolored form; black, green, or tan concentrates are added by the processor at typical letdown ratios of 1 wt% to 5 wt%. Carbon black concentrates improve UV endurance more than non-black organic pigments, but carbon black also absorbs heat and can raise part surface temperature in direct sunlight, increasing creep in unsupported tank walls. The use of white or light pigments reduces surface temperature but may leave the material more dependent on the hindered-amine stabilizer package. Electrical enclosure applications requiring RoHS compliance should be assessed under 2011/65/EU; heavy-metal content is not expected, but a supplier declaration is required for lot-specific enforcement.
Bapolene® 3039U occupies an intermediate position among unfilled rotational molding polyethylene families. General-purpose HDPE rotomolding grades with density near 0.945 g/cm³ provide higher flexural modulus, often above 900 MPa, but lower ESCR and lower low-temperature impact than intermediate-density grades. Linear low-density polyethylene rotomolding grades with density near 0.925 g/cm³ provide higher impact and better flex fatigue, but flexural modulus is typically below 500 MPa, which is insufficient for large vertical tank walls. Crosslinked polyethylene rotomolding grades offer higher service-temperature capability, but they require longer cure cycles and cannot be ground back into the process because of thermoset network formation. Table 2 provides the class-level comparison.
| Material Class | Nominal Density Range | Melt Flow / Process Indicator | Flexural Modulus Range | Low-Temperature Impact | UV Stabilization |
|---|---|---|---|---|---|
| Bapolene® 3039U HDPE | 0.939 g/cm³ | 3.0 g/10 min | 800 MPa | High | Yes |
| General-purpose HDPE rotomolding | 0.940–0.950 g/cm³ | 2–6 g/10 min | 850–1100 MPa | Moderate | Optional |
| LLDPE rotomolding | 0.920–0.935 g/cm³ | 3–7 g/10 min | 300–500 MPa | Very high | Optional |
| Crosslinked HDPE rotomolding | 0.930–0.945 g/cm³ | Crosslinked, no melt flow | 500–800 MPa | Very high at elevated temperature | Optional |
The primary separating variables are density, melt flow, UV stabilization, and the presence or absence of crosslinking. Bapolene® 3039U is distinguished from general-purpose HDPE by the U modifier, which indicates the UV-stabilized package; the base resin density and melt flow are otherwise in the same working range as intermediate-HDPE rotomolding grades. Against LLDPE grades, 3039U provides higher stiffness and lower flexural creep, but lower ultimate elongation and lower low-temperature impact. Against crosslinked HDPE, 3039U provides easier reprocessing of post-industrial regrind and a shorter cycle because no cure time is required. The crosslinked alternative is favored when continuous service above 70 °C or aggressive solvent exposure is required, but it is less suited to closed-loop regrind programs.
Pinholing, warpage, and incomplete densification are the principal process limits observed on production-scale rotomolding lines running Bapolene® 3039U. Pinholing is concentrated in high-surface-area zones where powder particles fail to coalesce, most often when peak internal air temperature remains below 200 °C for less than 2 min. Incomplete densification also appears as porosity in the outer skin when mold release agents are applied at excessive thickness, because volatilized release agents become entrapped in the melt. Warpage in large flat panels is managed by reducing cooling rate after demolding temperature and by using tooling with uniform heat-transfer coefficients. The grade should not be blended with fractional-melt-index blow-molding HDPE for rotational molding because the resulting melt-flow mismatch produces visible flow lines and uneven wall thickness in deep-draw tools. The operational boundary for reprocessed powder is generally limited to 20 wt% of clean post-industrial regrind; above that level, low-temperature impact may decline and dry-flow variability may increase in multi-cavity tooling. Chemical compatibility should be confirmed with the intended contents at the upper service temperature, because HDPE resists many aqueous acids, alkalis, and salt solutions but is not suitable for strong oxidizing acids, chlorinated solvents, or high-aromatic hydrocarbon streams.