Bamberger Polymers Bapolene 2292g Lldpe Compounding Grade

Bamberger Polymers Bapolene® 2292G LLDPE, Compounding Grade

    • Product Name: Bamberger Polymers Bapolene® 2292G LLDPE, Compounding Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 618303
    Product Name Bapolene 2292G
    Manufacturer Bamberger Polymers
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Grade Compounding Grade
    Form Pellets
    Color Natural
    Density 0.920 g/cm³
    Melt Index 20 g/10 min at 190°C/2.16 kg
    Tensile Strength At Yield 9.7 MPa
    Tensile Strength At Break 12.1 MPa
    Elongation At Break 800%
    Flexural Modulus 234 MPa
    Vicat Softening Point 93°C
    Melting Point 122°C
    Hardness Shore D 50
    Brittleness Temperature < -70°C
    Thermal Expansion Coefficient 1.8E-4 cm/cm/°C
    Specific Gravity 0.920

    As an accredited Bamberger Polymers Bapolene® 2292G LLDPE, Compounding Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bapolene® 2292G LLDPE, Compounding Grade is packaged in 55 lb (25 kg) polyethylene bags, 40 bags per pallet (2,200 lb).
    Container Loading (20′ FCL) Container Loading (20′ FCL): Bapolene 2292G LLDPE Compounding Grade, 25 kg bags, palletized, stretch-wrapped; approximate net weight 24–25 metric tons.
    Shipping Bamberger Polymers Bapolene® 2292G LLDPE, Compounding Grade, is a non-hazardous solid resin. It typically ships in 25 kg moisture-resistant bags, palletized and stretch-wrapped, or in bulk trucks/railcars. No DOT/IMDG/IATA hazardous designation applies; keep dry and avoid excessive heat. Refer to SDS and carrier requirements.
    Storage Store Bapolene® 2292G LLDPE in a cool, dry, well-ventilated area. Keep containers closed and off the floor to prevent moisture, dirt, or other contamination. Protect from direct sunlight and extreme heat. Separate from oxidizing agents and ignition sources. Avoid prolonged storage near strong odors or chemicals that may be absorbed. Maintain good housekeeping; minimize dust generation. Use appropriate secondary containment.
    Shelf Life No specific shelf life is established; store in a cool, dry, well-ventilated area, protected from sunlight. Material is stable under normal conditions.
    Application of Bamberger Polymers Bapolene® 2292G LLDPE, Compounding Grade

    In colorant masterbatches destined for thin-wall injection-molded food packaging, Bapolene® 2292G is introduced as a carrier resin at 45 wt% to 65 wt% within the masterbatch itself, with final let-down ratios commonly ranging from 2 wt% to 6 wt% in natural polyolefin. The carrier is compounded on a co-rotating twin-screw extruder with an L/D ratio of 40:1 to 48:1, using a pigment side-feeder positioned downstream of the primary melt seal; melt temperature at the die plate is maintained between 200 °C and 230 °C to preserve thermal stability of organic pigments while still achieving agglomerate breakdown. A strand pelletizer with cooling water at 40 °C to 55 °C produces cylindrical granules, and optical film gel counters after 100 µm screen-pack filtration are used to reject batches exceeding plant-specific speck criteria. Melt mass-flow rate of the diluted compound is checked according to ASTM D1238-20 at 190 °C/2.16 kg, and density is verified by ISO 1183-1. For indirect food-contact use, compliance is evaluated under FDA 21 CFR 177.1520, while EU-finished articles are assessed under Regulation (EU) No 10/2011 Annex I with an overall migration limit of 10 mg/dm². Finished goods include injection-molded cups, closures, cutlery, thin-wall containers, and extrusion blow-molded bottles in which color consistency and gel control are process-release requirements.

    What Limits Carbon Black Dispersibility in LLDPE-Carrier Concentrates Above 45 wt%?

    The practical ceiling for carbon black loading in a low-density carrier arises from the balance between agglomerate attrition and melt viscosity: once carbon black exceeds 45 wt% in the masterbatch, the viscosity rise under shear begins to limit droplet elongation, and side-fed carbon black must be added in two stages to prevent agglomerate survival. Bapolene® 2292G is formulated at 50 wt% to 60 wt% as the carrier, with carbon black at 40 wt% to 50 wt% and processing aid at 0.2 wt% to 0.8 wt%; final dilution in blown film and injection molding typically ranges from 3 wt% to 8 wt%. Production-scale dispersion uses a co-rotating twin-screw extruder with high-shear kneading blocks in the first 8 D of mixing and a downstream forced side-feeder; vacuum devolatilization at −0.08 MPa to −0.095 MPa removes moisture and entrained air from the carbon black structure. The strand die is held below 240 °C to avoid thermal degradation of the polyolefin carrier and to preserve carbon black primary particle structure. Compliance for colorants used in indirect food-contact polymers is anchored to FDA 21 CFR 178.3297, while EU industrial applications must meet Regulation (EC) No 1907/2006 (REACH) and Directive 2011/65/EU (RoHS) restrictions on heavy-metal impurities. Terminal products include UV-stabilized greenhouse films, silage films, geosynthetic materials, conductive packaging, and industrial refuse sacks requiring carbon-black-mediated opacity and outdoor weathering performance.

    Reprocessing post-consumer HDPE bottle recyclate with an MFI below 0.4 g/10 min at 190 °C/2.16 kg produces torque instability on single-screw equipment when the fraction contains residual PP and label contamination; adding Bapolene® 2292G at 15 wt% to 30 wt% widens the processing window and raises the blend MFI into the 0.6 g/10 min to 1.1 g/10 min range, depending on contamination level. The recycling line is built around a single-screw vented compounding extruder with L/D 36:1, a continuous screen changer with 80 µm to 150 µm melt filtration, and water-ring pelletizing; melt temperature is maintained below 220 °C to reduce gel generation from residual adhesives and to limit odour development. The MFI of the recompounded material is verified under ISO 1133-1 at 190 °C/2.16 kg, and density is checked by ISO 1183-1. Traceability and conformity verification follow EN 15343:2007, which specifies recycled-content calculation and assessment of conformity for recycled plastics; REACH and RoHS restrictions apply to hazardous substances carried into the recyclate from upstream packaging inks and labels. The resulting recompounded material is used for non-pressure drainage pipe, corrugated culvert liners, industrial pallets, wheel-bin bodies, and rigid material-handling components where higher impact toughness and processability outweigh a modest reduction in stiffness. Batch-to-batch variance in the waste input requires torque-control rather than fixed screw speed, and the LLDPE addition is adjusted in 2 wt% increments when melt-filter pressure deviates by more than 10% from baseline.

    When Aluminium Trihydroxide Exceeds 60 wt% in Low-Smoke Sheathing

    Halogen-free flame-retardant cable sheathing formulations operate near the decomposition threshold of aluminium trihydroxide: as filler loading rises to 60 wt% to 70 wt%, the polyolefin continuous phase represented by Bapolene® 2292G is reduced to 30 wt% to 40 wt%, with a coupling or dispersing agent at 1 wt% to 3 wt%. Because aluminium trihydroxide begins endothermic dehydration near 180 °C to 220 °C, the compounding extruder must operate with a descending temperature profile from feed throat to die, with the melt seal not exceeding 170 °C and the die zone maintained between 170 °C and 190 °C; external oil cooling of barrel zones is used to remove shear heat. On a co-rotating twin-screw extruder with L/D 44:1, flame-retardant filler is introduced through a side stuffer after the polymer is melted, and vacuum venting at −0.09 MPa removes surface moisture; filler moisture content above 0.15 wt% requires pre-drying before side feeding to prevent voiding and pellet porosity. Compliance for the finished compound includes IEC 60332-1-2 vertical flame propagation testing for single insulated wire, IEC 60754-2 for acidity and conductivity of gases evolved during combustion, and Directive 2011/65/EU (RoHS) for restricted substances. Terminal products include halogen-free flame-retardant sheathing for building installation cables, control cables, and railway signalling cables. Published data for this specific configuration is limited, so compounding trials should bracket filler loading and screw speed before commercial production.

    Impact Modification of Homopolymer Polypropylene for Low-Temperature Ductility

    With homopolymer polypropylene as the continuous phase, blends containing 10 wt% to 25 wt% Bapolene® 2292G are compounded on a co-rotating twin-screw extruder with L/D 40:1 and two high-shear mixing zones; barrel-zone setpoints follow a rising profile from 180 °C at the feed to 230 °C at the die, with vacuum venting and strand pelletizing. Gravimetric dosing of PP and LLDPE into the main feed is used, and the melt temperature is held below 240 °C to prevent chain scission of the LLDPE fraction. Notched Charpy impact is determined according to ISO 179-1/1eA at −20 °C, Izod impact by ASTM D256, and tensile properties by ISO 527-2; the LLDPE phase improves low-temperature ductility relative to unmodified homopolymer, while flexural modulus measured by ISO 178 declines as the softer ethylene-rich fraction increases. Baseline material compliance is verified under Regulation (EC) No 1907/2006 (REACH) and Directive 2011/65/EU (RoHS) for restricted substances. The resulting thermoplastic polyolefin-like compound is used in injection-molded appliance housings, automotive interior trim panels, power-tool bodies, and material-handling containers where low-temperature ductility is specified by ISO 179-1/1eA at −20 °C.

    Greenhouse films in high-UV geographies demand a carrier resin that does not exude into the film surface over multi-season service; Bapolene® 2292G is used as the carrier at 80 wt% to 90 wt% within a stabilizer masterbatch, with hindered amine light stabilizers, UV absorbers, and anti-dust agents at total additive concentrations of 10 wt% to 20 wt%. The masterbatch is produced on a low-temperature co-rotating twin-screw extruder with a screw profile that limits melt temperature to 190 °C at the die, protecting temperature-sensitive light stabilizers from decomposition; downstream blown-film extrusion adds this masterbatch at 5 wt% to 10 wt% to the natural LLDPE film resin. Compliance under Regulation (EC) No 1907/2006 (REACH) is required for stabilizer substances and their degradation products, while EU waste and recycling directives apply at the film end of life; in non-food-contact greenhouse service, no separate Regulation (EU) No 10/2011 migration assessment is triggered, but the masterbatch supplier must provide REACH safety data sheets. Accelerated weathering is verified under ISO 4892-2, and retained light transmission is measured by ASTM D1003; batch release criteria include filterability through a 100 µm screen pack and pellet moisture below 0.08% to prevent feed throat bridging in film lines. Terminal products include multi-season greenhouse covers, low-tunnel films, banana bunch covers, and silage wrap outer layers in which additive distribution and bloom resistance are verified by accelerated weathering and optical inspection.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 2292G LLDPE, Compounding Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bamberger Polymers Bapolene® 2292G LLDPE, Compounding Grade, is a linear low-density polyethylene resin intended for masterbatch, filled-compound, and custom concentrate production. The nominal melt flow index is 20 g/10 min at 190 °C/2.16 kg when tested per ASTM D1238, and the nominal density is 0.924 g/cm³ when tested per ASTM D1505. These values distinguish the grade from fractional-melt film resins and place it in the low-viscosity carrier class for high-filler dispersion. The resin is supplied as pellets for gravimetric or volumetric feeding; pellet geometry and stabilization are intended to reduce dusting and feed-throat bridging during continuous extrusion. The product is not intended as a direct food-contact article resin unless the complete compound and finished article are evaluated under the applicable end-use standard.

    PropertyTest MethodNominal ValueUnit
    Melt flow indexASTM D123820g/10 min at 190 °C/2.16 kg
    DensityASTM D15050.924g/cm³
    Physical formVisualPelletized—

    In typical letdown operations, Bapolene® 2292G is diluted into polyolefin base resins at 10 wt% to 70 wt%, depending on concentrate formulation and final part mechanical requirements. Calcium carbonate masterbatches based on the grade can be produced at filler loadings approaching 75 wt%; however, published data for this specific configuration is limited, and the maximum loading depends on filler particle size distribution, coating chemistry, and screw configuration. The low melt viscosity promotes pigment and filler dispersion by maintaining shear stress within the compounding screw, but it also reduces melt strength. That reduction is seldom limiting in compounded articles because the letdown resin contributes the main mechanical and optical properties; it does, however, restrict the use of Bapolene® 2292G as a blown-film resin except at high dilution ratios.

    What Melt-Pressure and Torque Signatures Appear in High-Filler Compounding?

    On a co-rotating twin-screw extruder with an L/D ratio of 40:1, Bapolene® 2292G-based filler masterbatches are commonly processed with barrel temperatures from 180 °C in the rear zones to 230 °C at the die, yielding melt temperatures of 200 °C to 240 °C. The 20 g/10 min melt flow index lowers specific mechanical energy input relative to a 1.0 g/10 min film-grade LLDPE because viscous dissipation is reduced and motor torque remains below the drive limit at screw speeds of 400 rpm to 600 rpm. Die plate pressure remains lower than an equivalent-density 4.0 g/10 min LLDPE under identical throughput and screw profile, although the exact reduction depends on orifice diameter, land length, filler content, and melt temperature. The lower pressure headroom allows higher filler loadings before extruder drive or die-pressure alarms are reached. However, devolatilization must be reviewed because low melt viscosity can increase the entrainment of filler dust into vent ports when vacuum levels exceed 0.08 MPa.

    Formulators using Bapolene® 2292G as a carrier typically add 0.05 wt% to 0.20 wt% of a primary phenolic antioxidant and a secondary phosphite stabilizer when high-temperature processing or multiple passes are expected, although the base resin is supplied with a stabilization package sufficient for single-pass compounding under normal conditions. If peroxide-initiated grafting or crosslinking is used, the peroxide-to-polymer ratio must be adjusted to the carrier’s unsaturation content, which is not specified in the standard technical data sheet; pilot-scale grafting studies are required before production. Amine-based additives should be evaluated for discoloration because some hindered amine light stabilizers can yellow olefin carriers at elevated processing temperatures. The density of 0.924 g/cm³ provides a balance between filler wetting and final compound stiffness; however, talc and barium sulfate formulations may require a higher-melt-flow carrier if total filler content exceeds 80 wt%.

    Carrier Resin Selection Against Fractional-Melt LLDPE and High-Pressure LDPE

    Compared with fractional-melt linear-low-density polyethylene grades having melt flow indices below 2.0 g/10 min, Bapolene® 2292G exhibits lower extensional viscosity and lower bubble stability, which make it unsuitable for monolayer blown-film production at high letdown ratios. In compounding service the carrier is dispersed into a host resin, and the final article properties are dominated by the letdown resin, filler, and additive package rather than by the carrier itself. Relative to a high-pressure low-density polyethylene carrier of similar melt flow, Bapolene® 2292G typically provides higher tensile yield stress and improved environmental stress-crack resistance when tested per ASTM D638 and ASTM D1693, respectively, because the linear backbone and short-chain branches limit large-scale chain entanglement under load. The corresponding limitation is reduced melt extensibility; a branched LDPE carrier may be preferred in cast film or extrusion coating where high melt strength must be maintained at high draw rates. The exact comonomer type and catalyst system for Bapolene® 2292G are not disclosed in the standard technical data sheet, so comparisons against metallocene grades should rely on melt rheology, extractables, and finished article haze measurements rather than nominal density or melt flow index alone.

    Mechanical property retention in letdown compounds is influenced more by carrier density and dosage than by carrier melt flow alone. Because Bapolene® 2292G has a density of 0.924 g/cm³, a 10 wt% addition to a 0.918 g/cm³ film resin shifts compound density by approximately 0.0006 g/cm³, assuming no filler or additive; this shift is negligible in most extrusion and injection-molding operations. Tensile yield stress in the final compound is governed mainly by the host resin, while the filler content and carrier fraction control flow. For example, a 20 wt% masterbatch containing 60 wt% calcium carbonate in Bapolene® 2292G reduces the base resin tensile yield stress in proportion to filler concentration rather than carrier viscosity. Complete rheological characterization of the carrier can be performed by parallel-plate oscillatory shear according to ISO 6721-10; however, the standard data sheet does not provide a full viscosity curve, so filled-compound viscosity should be measured on the actual production compound.

    When Feed-Throat Bridging and Pellet Fines Constrain Throughput

    Feed-throat bridging is a production-scale failure mode that appears when pellets soften in the feed passage and form an arch above the screw. With a melt flow index of 20 g/10 min, Bapolene® 2292G is not inherently tacky at ambient temperature, but the feed throat should be maintained below 40 °C; if cooling water is insufficient, localized pellet softening can occur and throughput becomes erratic. Gravimetric feeders should be equipped with agitated hoppers when pellet regrind or fine fillers are added, because fines can segregate and compact into layers that reduce feed uniformity. Pre-drying is generally unnecessary at ambient relative humidity below 60% RH. However, cold pellets transferred from an outdoor silo into a warm compounding building may develop surface condensation, producing steam pockets in the melt and strand surface roughness. The corrective action is conditioned storage at 20 °C to 25 °C for 24 h before processing rather than hot-air drying. If a dryer is used for hygroscopic additives, the base resin should not be co-dried above 60 °C because pellet surface softening can increase fines and cause dryer bridging.

    Processing ParameterTypical Starting RangeUnit
    Barrel temperature, rear to die180–230°C
    Melt temperature200–240°C
    Screw speed200–600rpm
    Feed throat temperaturebelow 40°C
    Pre-drying requirementNot required below 60% RH—

    Prolonged exposure of Bapolene® 2292G to melt temperatures above 260 °C should be avoided; degradation is detected as a decrease in melt viscosity, an increase in gel particles, and yellowing in unpigmented compounds. The standard stabilizer package is intended for single-pass compounding at 180 °C to 240 °C. If the material is reprocessed multiple times, additional phenolic and phosphite stabilizers are required to maintain oxidation resistance. Chlorinated flame retardants and strong Lewis acid catalysts can accelerate polyolefin degradation and should be evaluated before large-scale production. The low melt strength of the grade also limits performance in underwater pelletizing; strand pelletizing is generally more tolerant of high-melt-flow carriers, while underwater pelletizing requires die plate temperatures above the crystallization range and rapid water quenching to avoid pellet agglomeration.

    Batch-to-batch variability of melt flow index should be confirmed for high-speed compounding lines where viscosity limits are narrow. Polyethylene production tolerances for a 20 g/10 min grade are often in the range of ± 1.5 g/10 min, but published lot-to-lot data for Bapolene® 2292G should be requested from the supplier. Incoming inspection should include melt flow index per ASTM D1238 and density per ASTM D1505, because these properties are sensitive to comonomer content and molecular weight changes. If the material is stored for extended periods, a 0.05 wt% antioxidant top-up may be considered before high-temperature processing, but oxidative degradation in ambient polyethylene storage is slow and is rarely the controlling shelf-life factor.

    Target applications for compounds based on Bapolene® 2292G include indoor extruded profiles, injection-molded crates, industrial films at high dilution, and rigid packaging where the final carrier fraction is low. In foam masterbatches, the high carrier flow can distribute chemical blowing agents uniformly, but gas retention is controlled by the letdown resin’s melt strength rather than by the carrier. Conductivity compounds require a separate selection of carbon black grade and dosage; Bapolene® 2292G is not formulated as a conductive or semiconductive matrix and should not be used as such without formulation studies. The grade is also not recommended for sustained outdoor exposure without added UV stabilization, because polyethylene without sufficient light stabilizers undergoes ultraviolet degradation.

    Regulatory documentation should be verified with Bamberger Polymers for each production lot. Polyethylene resins of this type generally fall within U.S. FDA 21 CFR 177.1520 as olefin polymers, provided the finished article meets applicable extractables and end-use limitations; the presence of additives, pigments, or non-olefin polymers requires a separate assessment. In the European Union, plastic food-contact materials are regulated under EU Regulation 10/2011; overall migration testing per EN 1186 and specific migration testing per EN 13130 must be performed on the finished article, not on the resin alone. The resin is not classified as hazardous under typical industrial hygiene standards, but pellet regrind dust should be controlled under applicable particulate exposure limits. REACH registration and RoHS compliance are substance-and-article-level issues, and no product technical sheet statement replaces an end-user’s obligation to assess the complete compound.

    Top