Bamberger Polymers Bapolene 2272g Lldpe Compounding Grade

Bamberger Polymers Bapolene® 2272G LLDPE, Compounding Grade

    • Product Name: Bamberger Polymers Bapolene® 2272G LLDPE, Compounding Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 968569
    Density 0.920 g/cm³
    Meltindex 2.0 g/10 min
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 20.7 MPa
    Elongationatbreak 800%
    Flexuralmodulus 276 MPa
    Vicatsofteningpoint 100 °C
    Brittlenesstemperature -70 °C
    Hardnessshored 50
    Meltingpoint 122 °C
    Thermalconductivity 0.33 W/m·K
    Specificheat 1.9 J/g·°C
    Waterabsorption <0.01%
    Dielectricconstant 2.3
    Volumeresistivity 1e+16 ohm·cm
    Dielectricstrength 20 kV/mm

    As an accredited Bamberger Polymers Bapolene® 2272G LLDPE, Compounding Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing The product is typically supplied in 25 kg (55 lb) polyethylene-lined multiwall bags, palletized and stretch-wrapped for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL: Bapolene® 2272G LLDPE in 25 kg bags, approx. 20 MT, palletized or floor-loaded, securely stowed for transport.
    Shipping Bamberger Polymers Bapolene® 2272G LLDPE, Compounding Grade ships as non-regulated, non-hazardous polymer pellets in 25 kg bags, boxes, or bulk containers. No DOT, IMDG, or IATA hazardous shipping description is required. Use original packaging; keep containers closed. Store dry, cool, and away from ignition sources. Follow SDS and local regulations.
    Storage Store Bamberger Polymers Bapolene® 2272G LLDPE, Compounding Grade, in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep material in original, closed containers or bags, elevated on pallets, and protected from moisture, dust, and contaminants. Avoid excessive stacking, prolonged UV exposure, and incompatible materials. Follow the supplier’s SDS and local regulations.
    Shelf Life Stable for 24 months from manufacture when stored cool, dry, and sealed in original packaging; avoid direct sunlight and moisture.
    Application of Bamberger Polymers Bapolene® 2272G LLDPE, Compounding Grade

    Bapolene® 2272G enters a 40 mm co-rotating twin-screw extruder with an L/D ratio of 44:1 at the main feed throat when the downstream concentrate is a 40 wt% N550 carbon black masterbatch intended for dilution in 25 µm LLDPE cast film. The nominal melt flow rate of 2.7 g/10 min per ASTM D1238-20 at 190 °C/2.16 kg and the nominal density of 0.918 g/cm³ per ASTM D1505-18 place the carrier viscosity in a range that allows carbon black agglomerates to be infiltrated by polymer under the shear field generated in kneading block sections located in barrel zones 4 through 6. A barrel profile of 170 °C to 210 °C is maintained from feed throat to die, with the die zone held at 205 °C to keep melt discharge pressure between 30 bar and 55 bar. Specific mechanical energy for a 38–45 wt% carbon black loading typically settles between 0.18 kWh/kg and 0.24 kWh/kg, depending on the structure and volatile content of the selected N550 or N660 carbon black grade. On a production-scale line equipped with a 60/100/60 mesh screen pack, the first measurable symptom of incomplete dispersion is a pressure differential increase greater than 20 bar across the screen changer at 180–210 °C melt discharge. If that pressure rise occurs before 4 hours of continuous operation, the masterbatch lot is diverted for re-extrusion because the carbon black structure has not fully broken down in the kneading blocks; the failure is confirmed by ASTM D5596-03 microscopy, which counts undispersed agglomerates larger than 20 µm per 73 cm² of film specimen. Pellets are cut by underwater pelletizing with a die plate water temperature of 35–45 °C; soft or clumped pellets reduce dry-flow consistency and can bridge in the film processor’s vacuum loading system. The dilution step in cast film uses a let-down ratio of 10:1 to 20:1, delivering 2.0–4.0 wt% carbon black in the final film. Surface condensation on cold pellets moved from unheated warehousing into a warm, humid production hall can introduce enough moisture to generate microbubbles in cast film at draw speeds above 300 m/min, but resin drying is not required under controlled indoor storage conditions.

    What Limits the Processing Window When 2272G Replaces EVA in ATH-Filled LSZH Jackets?

    When Bapolene® 2272G is used as a fractional co-resin in low-smoke zero-halogen cable sheathing compound, it displaces a portion of EVA copolymer containing 18–28 wt% vinyl acetate to improve tensile strength retention at elevated service temperature. The formulation typically contains 100 phr of a polymer blend comprising EVA, 2272G, and 3–5 wt% PE-g-MAH, with precipitated alumina trihydrate at 150–165 phr, zinc borate at 8–12 phr, and a hindered amine stabilizer package at 0.2–0.4 phr. The lower molecular weight tail of the butene LLDPE grade improves filler wetting in the first mixing zones of a L/D 40 co-rotating twin-screw extruder, but the processing window narrows because alumina trihydrate releases structural water above 180 °C. Barrel zones 1 through 3 are therefore limited to 150–175 °C; zones 4 through 7 are held at 175–185 °C; and the die is controlled below 170 °C to maintain melt pressure in the 18–28 MPa range. Screw speed is capped at 260 rpm because frictional heat at higher speeds raises localized melt film temperature beyond the alumina trihydrate decomposition threshold, producing surface voids and a sharp acrid odor. Pellets are strand-quenched in a two-stage water bath and dried to less than 0.05 wt% residual moisture by Karl Fischer titration before packaging. The final compound is evaluated by IEC 60754-1:2011 for halogen acid gas evolution, IEC 60332-1-2:2015 for vertical flame propagation on a single insulated conductor, and ASTM D2863-19 for limiting oxygen index; compounds using 2272G at 15–20 wt% of the polymer fraction commonly maintain an LOI of 34–36% and tensile elongation at break above 150% per ASTM D638-14. The operational boundary is abrupt: raising 2272G above 25 wt% of the polymer fraction without a corresponding increase in EVA content depresses char formation and increases melt viscosity at the die, which can push head pressure beyond the 30 MPa rating of a standard pelletizing die plate.

    PropertyTest MethodCondition or Requirement
    Halogen acid gas evolutionIEC 60754-1:2011pH ≥ 4.3; conductivity ≤ 10 µS/mm
    Single-cable vertical flameIEC 60332-1-2:2015Char height below 425 mm from lower clamp
    Limiting oxygen indexASTM D2863-1934–36% O₂ for 2272G-containing jacket
    Tensile elongation at breakASTM D638-14Greater than 150% on Type IV specimens

    Notched Izod Transfer Across a 10–30 wt% 2272G Addition Window in Recycled PP

    In recycled polypropylene compounding, Bapolene® 2272G is blended into post-consumer PP regrind with an incoming melt flow rate of 10–14 g/10 min at 230 °C/2.16 kg per ASTM D1238-20. The material is fed into a 75 mm co-rotating twin-screw extruder with L/D 36:1, while a secondary PP/PE mixed flake stream is side-fed at barrel zone 5, and the melt is discharged through a gear pump that stabilizes pressure at 6–8 MPa before the strand die. Addition of 2272G at 10 wt% raises notched Izod impact strength at 23 °C by 25–40% over the unmodified regrind while reducing flexural modulus by 12–18%, measured according to ISO 180:2023 and ASTM D790-17, respectively. At 20 wt%, the reduction in flexural modulus becomes more pronounced; at 30 wt%, values drop from approximately 1150 MPa to 780 MPa. That stiffness loss is tolerated in automotive wheel arch liners and non-structural drainage fittings but not in load-bearing appliance bases where tensile modulus is controlled by ASTM D638-14. The viscosity ratio between the recycled PP melt and the LLDPE carrier is the primary process variable limiting pellet homogeneity because the lower melting point of 2272G, 120–125 °C, creates a low-viscosity interfacial layer on the screw root at barrel temperatures above 200 °C and reduces torque transfer to the PP-rich fraction. Reversing the pellet feed order or adding 2272G as a pre-extruded 50:50 PP/LLDPE blend through the side feeder reduces the standard deviation of notched Izod values across a 10-batch run from ±0.7 kJ/m² to ±0.3 kJ/m². Published formula-specific data for 2272G in post-consumer PP is limited, but the response envelope is consistent with the low secant modulus and low yield stress of butene LLDPE grades at equivalent melt flow.

    A separate additive masterbatch route uses Bapolene® 2272G as the carrier for process stabilizers, slip agents, and antiblock concentrates at let-down ratios between 20:1 and 50:1 in polyethylene film extrusion. The carrier melt flow rate of 2.7 g/10 min per ASTM D1238-20 is sufficiently low to wet additive powder and sufficiently high in molecular weight to maintain pellet hardness during bulk railcar unloading. Additives are tumble-mixed with 2272G pellet feed at 20–30 wt% active loading in a 300 L heated ribbon blender at 60 rpm for 20 min, then compound-extruded on a 30 mm single-screw compounding line with L/D 30:1 and a sleeve heater profile from 150 °C to 190 °C. The low melt temperature avoids erucamide slip agent volatilization, which accelerates above 200 °C, and prevents silica antiblock agglomeration into hard particles larger than 40 µm that would score die lips in cast film. Pelletized masterbatch is checked by ASTM D1895-17 apparent density and purge film inspection per ISO 18553:2002; re-extrusion at 5 wt% in a 25 µm blown film line should produce fewer than 5 visible particles per 1 m². Carrier moisture is not a primary limitation at processing temperatures below 190 °C, but amine-based antistatic agents in the same masterbatch should not be used with this LLDPE carrier when downstream food-contact film must comply with 21 CFR 177.1520, because amine-sourced nitrogen can extract into fatty food simulants and complicate migration review.

    When 2272G Pellets Are Ground to 35 Mesh for Rotational Molding Service

    Rotational molding compounds built on 2272G require dry grinding to a powder with 95 wt% passing a 35-mesh screen at 500 µm and a median particle size between 250 µm and 300 µm, as determined by sieve analysis using ASTM D1921-18. The pellet feed is ground under nitrogen on a high-speed attrition mill with a 76 cm rotor diameter and a 3000 rpm tip speed, then passed through a cyclonic classifier to remove fines below 100 µm that reduce bulk density and promote pinholing. The powder is charged into an aluminum mold at 35–45 g/cm² of projected wall area, and the mold is rotated biaxially at a 4:1 minor-to-major axis ratio inside an oven set at 280–300 °C. Inside-mold air temperature reaches 210–220 °C by 12–14 min, after which the mold is cooled under forced air. The butene comonomer distribution in 2272G widens the sintering window enough to produce a continuous melt skin on a 3 mm wall section in 18–22 min, whereas narrow-molecular-weight LLDPE grades frequently leave longitudinal cold-flow lines in the same mold geometry. Drop impact of molded tanks is tested at −20 °C using Association of Rotational Molders drop-impact methodology, and tensile yield is verified per ASTM D638-14. Low-temperature impact performance remains density-dependent; 2272G at 0.918 g/cm³ per ASTM D1505-18 is rarely selected for freezer-service tanks below −30 °C because the butene branch architecture delivers lower crack-arrest energy than hexene LLDPE alternatives. Pre-drying of the powder is required when bulk storage humidity exceeds 70% RH because surface moisture on LLDPE powder increases cycle time by 4–6% and can generate steam bubbles at the mold surface.

    Vented Extrusion and Residual Moisture Tolerance in Wood-Flour-Filled 2272G Composites

    Wood-plastic composite decking compound that uses 2272G as a secondary matrix component is commonly mixed at 50–60 wt% hardwood flour with a moisture content of 0.8–1.4 wt%, 2272G at 20–30 wt%, HDPE at 10–20 wt%, maleated polyethylene coupling agent at 3–5 wt%, and zinc stearate lubricant at 1.5–2.5 wt%. The mixture is processed on a 58 mm co-rotating twin-screw extruder with L/D 40:1, with atmospheric venting at barrel zone 4 and vacuum venting at −0.08 MPa at barrel zone 7 to strip water released from the wood flour. Without the vacuum vent, residual steam increases melt pressure at the die by 25–35% and produces melt fracture on the profile surface. Barrel temperatures are limited to 155–175 °C in the first three zones to prevent thermal degradation of hemicellulose, and the die is held at 155 °C. Main-drive torque is the key process variable, with a normal band of 70–85% of motor capacity at 120 rpm for the 58 mm extruder. The compounded pellets are subsequently extruded through a 50 mm single-screw profile line with a 2 m vacuum calibration tank, and the board is evaluated by ASTM D7031-11 for flexural performance and ASTM D7032-17 for outdoor decking compliance. The lower density of 2272G relative to HDPE lowers final board weight by 1.5–2.5%, but its use above 30 wt% of the polymer fraction can reduce surface hardness below the value required for high-traffic decking. The operational boundary is clear: wood flour entering the compounder above 1.5 wt% moisture cannot be fully removed by a single vacuum vent, and the resulting pellets exhibit a bulk density drop of 8–12% that affects feeding stability on the downstream single-screw profile extruder.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 2272G LLDPE, Compounding Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bamberger Polymers Bapolene® 2272G is a linear low-density polyethylene compounding-grade resin. It is specified for melt-compounded products in which filler uptake, melt-flow stability, strand pelletizing behavior, and batch-to-batch viscosity control are more important than thin-film optics or low gel counts. The resin is an ethylene/α-olefin copolymer with a nominal density of 0.918 g/cm³ measured according to ASTM D1505 or ISO 1183-1. The nominal melt mass-flow rate is 2.7 g/10 min at 190°C under 2.16 kg load, tested according to ASTM D1238 or ISO 1133-1. This mid-flow index places the resin in the range used for mineral-filled compounds, carbon black and additive masterbatches, flame-retardant olefin formulations, and recycled polyolefin upgrading. The grade is supplied in high-bulk-density granular/pellet form suitable for gravimetric feeding; the exact particle size distribution should be confirmed from the supplier certificate of analysis. The product is not a film-extrusion grade and is not optimized for dart impact, haze, or bubble stability in blown-film dies. In a compounding matrix, it provides a stable low-viscosity melt phase that can accept high loadings of dispersed solids while retaining sufficient melt strength for strand pelletizing. Published data for this specific configuration is limited in peer-reviewed form; therefore, incoming melt-index and density verification should be combined with process trials on the target compounding line.

    Does Incoming-Quality Verification Require More Than Melt Index and Density?

    Yes. Melt index and density establish the rheological and crystallinity class, but incoming-quality verification on a compounding line should also include volatiles, pellet size, metal contamination, and lot-to-lot melt-index shift. Volatiles should be below 0.05 wt% when measured by ASTM D6869; higher surface moisture alters filler dispersion in the first mixing zones. Melt index variation is normally held to ±0.3 g/10 min from the nominal 2.7 g/10 min. A shift larger than 0.5 g/10 min is meaningful because it changes specific energy input and filler dispersion at constant screw speed. The table below lists typical property values used for specification screening. These are not batch-release values; the certificate of analysis for each lot should be used for formal lot acceptance.

    Table 1. Typical screening values for Bapolene 2272G
    PropertyTypical valueTest method
    Melt mass-flow rate2.7 g/10 minASTM D1238 / ISO 1133-1
    Density0.918 g/cm³ASTM D1505 / ISO 1183-1
    Tensile strength at yield10.5 MPaASTM D638 / ISO 527-2
    Elongation at break750%ASTM D638 / ISO 527-2
    Flexural modulus, 1% secant260 MPaASTM D790 / ISO 178
    Vicat softening temperature95°CASTM D1525 / ISO 306
    Peak melting temperature122°CASTM D3418 / ISO 11357-3

    Tensile and flexural values are generated on compression-molded specimens according to the cited methods; injection-molded values may differ due to orientation and cooling rate. The Vicat softening temperature and peak melting temperature are used to set maximum barrel and melt temperatures during compounding. When the resin is blended with high-density polyethylene or polypropylene, the final compound properties shift away from these LLDPE baseline values, and the blend ratio rather than the neat resin data controls finished-part specifications.

    Compounding usage on segmented twin-screw extruders with 40:1 to 44:1 L/D ratios is the primary industrial route. The resin is metered into the main feed throat; filler is side-fed after the polymer melt seal. Barrel set temperatures are typically 180°C to 230°C, with a die temperature of 210°C to 225°C. This thermal window maintains melt temperature below the oxidative degradation threshold while preventing excessive viscosity. At filler loadings of 10–20 wt% calcium carbonate, dispersion can be achieved with two mixing zones and a screw speed of 400–500 rpm on a 50-mm machine. At 30–40 wt% talc or other platy mineral loadings, a side-stuffer with forced metering is required to suppress feed-throat bridging. Screw configuration should include neutral and reverse kneading blocks to generate elongational shear. Pre-drying is generally not required when the resin is stored below 60% relative humidity. Drying at 70°C for 2 h is sufficient when surface moisture is suspected. The resin can be pelletized by strand or underwater pelletizer; melt pressure and die-hole fill must be balanced to prevent tailing and agglomerate formation. Temperature profile design is more critical than absolute screw speed. In practice, a barrel profile of 180°C/190°C/200°C/205°C/210°C/215°C from feed to die on a 40:1 line provides stable melting without excessive melt-index shift. If melt temperature exceeds 235°C, screw speed is reduced before barrel temperatures are lowered, because barrel changes act slowly and can destabilize filler feeding. When the compound is heavily filled, water-cooled barrels in the feed and metering zones are used to limit residence-time-induced degradation. The specific mechanical energy input for unfilled 2272G is lower than for fractional-melt LLDPE, allowing higher throughput at equivalent torque; however, lower melt strength can lead to strand breaks during pelletizing if die temperatures are too high.

    Melt Rheology, Screw Design, and Dispersion Limits

    Shear viscosity of LLDPE of this melt-index and density class at 190°C is markedly non-Newtonian. Literature capillary rheometry values for similar ethylene/α-olefin copolymers fall near 850–950 Pa·s at 100 s⁻¹ and 180–220 Pa·s at 1,000 s⁻¹, with a power-law exponent near 0.45–0.55. These values are not lot-specific and should be checked by ISO 11443 before final screw design. The lower shear-thinning exponent compared with high-pressure LDPE means that raising screw speed does not reduce melt viscosity as sharply; therefore, filler dispersion must be generated by mixing-zone geometry rather than shear rate alone. Dispersion of platy talc at loadings above 30 wt% requires two or three kneading blocks arranged in a 30/60/90° progression. A 44:1 L/D machine with 12 barrel zones is typical for such formulations. Vacuum venting at approximately -0.08 MPa is used to remove moisture and volatiles; inadequate venting causes porosity in the pelletized compound. The melt filtration section should use screen packs of 60/80/100 mesh or a continuous belt screen to protect the die plate from agglomerates. If a gear pump is installed, suction pressure should remain above 0.3 MPa to prevent cavitation. At high filler loading, specific energy input can exceed 0.25 kWh/kg; the extruder must have adequate drive capacity and cooling-bore control to avoid melt temperature excursions above 230°C. Melt temperatures above 250°C for more than a short residence time are undesirable because oxidative chain scission can increase the melt index by 0.3–0.6 g/10 min and reduce compound toughness.

    For carbon black masterbatches, 2272G is used as the carrier at 50–60 wt% with furnace black loadings of 35–45 wt%; the remaining mass is wax and metal stearate dispersant. This carrier level balances pigment wetting and final let-down performance. In additive concentrates, such as slip/antiblock or UV masterbatch, let-down ratios of 20:1 to 40:1 are typical in film or pipe extrusion. The higher melt index of 2272G relative to film-grade LLDPE improves incorporation into polyethylene at low addition rates, but it may lower extrudate melt strength when very high let-down ratios are used in large-diameter pipe. For recycled polyolefin upgrading, additions of 10–30 wt% 2272G to post-industrial polyethylene or polypropylene regrind can improve strand pelletizing and homogenization; the final melt index should be controlled by blend ratio rather than by excessive melt temperature. If the regrind contains high-melt-flow polypropylene, phase compatibility is limited, and a compatibilizer may be required to maintain tensile yield. Dispersion quality in mineral-filled compounds is often evaluated by ash content per ISO 3451-1 and by tensile elongation retained after filler addition. A compound based on 2272G with 20 wt% talc typically retains ductility for non-structural backing applications; with 40 wt% talc, elongation decreases and the material becomes stiff, requiring flexural modulus testing per ASTM D790 or ISO 178 as the primary specification.

    When 2272G Is Compared with Film-Grade and High-Flow LLDPE

    Film-grade LLDPE of density 0.918 g/cm³ and melt index 1.0 g/10 min is selected for blown-film bubble stability, optical haze, and dart impact resistance. In contrast, 2272G is specified for compounding and is not released against the same film appearance criteria; its higher melt index improves filler wetting and permits higher filler loadings, but reduces melt strength for large-diameter bubble stability. High-flow injection LLDPE with melt index of 18–22 g/10 min is selected for injection-molding spiral-flow length and mold release; 2272G is unsuitable for thin-wall injection molding without viscosity reduction. The following comparative matrix summarizes these distinctions.

    Table 2. Comparative positioning of 2272G against adjacent LLDPE classes
    ParameterBapolene 2272GFilm-grade LLDPEHigh-flow injection LLDPE
    Nominal MFR2.7 g/10 min0.9–1.1 g/10 min18–22 g/10 min
    Nominal density0.918 g/cm³0.918–0.920 g/cm³0.924–0.926 g/cm³
    Primary processing routeTwin-screw compoundingBlown/cast filmInjection molding
    Release focusFiller dispersion, melt stabilityHaze, gel count, dart impactSpiral flow, mold release
    Limiting property in compoundingMelt strength at high filler loadingMelt flow for filler wettingMelt strength for film

    The substitution is not symmetrical. A mineral-filled compound designed around a film-grade resin may require a reduction in filler content when moving to 2272G because the higher melt index can lower melt strength and increase filler segregation if screw mixing zones are not adjusted. Conversely, a high-flow injection grade cannot replace 2272G in a mineral-filled compound without accepting lower filler dispersion or adding more mixing elements. In direct substitution trials, replacing a 1.0 g/10 min film-grade resin with 2272G reduces extrusion head pressure at constant screw speed and improves filler wetting, but lowers blow-up ratio stability in film. Blending 2272G with high-flow injection LLDPE at 70:30 or 60:40 produces an intermediate melt index suitable for injection-molded olefin compounds with moderate flow and acceptable melt strength.

    Operational boundaries and incompatibilities should be defined before compounding. Sustained melt temperature above 260°C can cause oxidative degradation and crosslinked gel formation. Peroxide grafting, when used, should begin at 0.05–0.10 wt% peroxide and be monitored by torque; higher levels can create rapid chain extension and equipment overload. The resin should not be exposed to high-shear mixing with pro-oxidant additives unless the oxidative degradation profile is validated by ASTM D6954. For flame-retardant compounds containing halogenated additives, acid scavengers are required; contact of the melt with halogen acids at high temperature can corrode screw and die metallurgy. Food-contact uses should be confirmed by the converter under 21 CFR 177.1520(c) for olefin polymers in the United States or EU Regulation 10/2011 in Europe; final article migration testing is required because the additive package determines compliance. For outdoor service, unmodified LLDPE has limited weather resistance; added hindered amine light stabilizers and UV absorbers are required, and accelerated weathering should be performed under ASTM G155 or ISO 4892-2. Published data for long-term UV performance of this specific grade is limited; field validation remains necessary. The product should not be blended with polyethylene grades containing high levels of catalyst residues or oxidized regrind without pilot evaluation; gel formation may increase under high-temperature compounding.

    Top