| HS Code | 772101 |
| Density | 0.922 g/cm³ |
| Melt Index | 2.0 g/10 min |
| Film Tensile Strength At Break Md | 3000 psi |
| Film Tensile Strength At Break Td | 2500 psi |
| Film Elongation At Break Md | 500% |
| Film Elongation At Break Td | 600% |
| 1 Secant Modulus Md | 26000 psi |
| 1 Secant Modulus Td | 30000 psi |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Haze | 8.0% |
| Gloss 60 | 60 |
| Coefficient Of Friction | 0.15 |
| Vicat Softening Point | 88°C |
As an accredited Bamberger Polymers Bapolene® 222F Polyethylene, Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Bamberger Polymers Bapolene® 222F Polyethylene, Film Grade is packaged in 25 kg (55 lb) polyethylene-lined bags on pallets. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Bamberger Polymers Bapolene® 222F Polyethylene Film Grade in 25 kg bags, palletized; approximately 18–20 metric tons. |
| Shipping | Typically, Bapolene® 222F polyethylene resin ships as a non-hazardous solid in 25 kg moisture-barrier bags, 1,000 kg bulk bags, or bulk truck/rail hopper cars. Keep dry, away from heat, UV, and contamination. Transport by standard truck or rail; no special ventilation required. Follow local regulations and supplier handling instructions. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Use proper grounding to prevent static discharge. Maintain good housekeeping; rotate stock first-in, first-out. Follow SDS and local regulations. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored unopened in original packaging in a cool, dry area. |
For monolayer blown film extrusion on a 65 mm single-screw line with 30:1 L/D barrier screw and 60/80/100 mesh screen pack, Bapolene® 222F is processed at melt temperatures between 165°C and 185°C using a die gap of 1.0 mm to 1.5 mm; the nominal melt index of 2.0 g/10 min (ASTM D1238, 190°C/2.16 kg) and nominal density of 0.922 g/cm³ (ASTM D1505) place the grade in the medium-flow LDPE film range, where industrial sack and liner gauges from 75 µm to 150 µm are drawn at a blow-up ratio of 2.0:1 to 2.8:1 and a frost line height of 8 to 10 die diameters. Under these settings, bubble oscillation is normally limited to ±2% of layflat width; larger movements at frost line heights above 12 die diameters are associated with gauge banding and a reduction in Elmendorf tear (ASTM D1922) of up to 15%, attributable to uneven orientation relaxation before nip collapse. Dart impact (ASTM D1709 Method A) for unfilled LDPE of this density class typically falls between 2.5 g/µm and 4.0 g/µm, with the lower boundary encountered in low-blow-up or high-frost-line operation; published data for Bapolene 222F across the complete gauge span is limited, and converter qualification trials are therefore required. Heat seal strength on such gauges, measured by ASTM F88 at 115°C to 130°C seal bar temperature with a 25 mm specimen, commonly exceeds 10 N/25 mm if dwell time is adequate, but the seal plateau narrows when antiblock addition exceeds 0.1 wt%, making seal initiation verification per ASTM F2029 necessary before high-speed sack conversion.
Collation shrink film for multi-pack beverage or can overwrap is controlled by draw-down ratio and blow-up ratio rather than by a separate tenter frame; an LDPE tube extruded at a blow-up ratio of 3.0:1 and a DDR of 8:1 will relax differently at 135°C than a tube extruded at 2.0:1 BUR with the same frost line height. Unrestrained linear shrink measured to ASTM D2732 at 135°C for 30 s often falls between 10% and 20% in MD and 5% and 10% in TD for monolayer LDPE, but the numerical range is sensitive to frost line position and internal bubble air volume. Shrink force, where measured by ISO 14616, in monolayer grades of 2.0 g/10 min melt index rarely exceeds 2.0 MPa; Bapolene 222F should therefore not be substituted for high-shrink LLDPE or coextruded shrink grades in applications demanding tight final package conformity at tunnel temperatures below 120°C. The processing envelope is narrow: melts below 165°C produce inadequate bubble cooling on high-output lines and may generate haze bands from unrelaxed orientation, while melts above 190°C reduce melt strength and lead to bubble instability, especially when side gussets are used. For 50 µm collation film, a die gap of 0.8 mm to 1.0 mm and frost line height of 6 to 8 die diameters represent a stable envelope; deviation beyond 8 die diameters elevates TD shrink but reduces dart impact (ASTM D1709A). Equipment-specific data for Bapolene 222F on ISO 14616 shrink force is limited, so end-use tunnel validation remains mandatory.
Converting 25 µm to 30 µm monolayer film for retail garment bags requires consistent web stiffness and stable slip; the 0.922 g/cm³ density provides secant modulus per ASTM D882 that prevents web flutter on rotary sealing machines while retaining soft hand on finished bags. If the selected lot does not contain a migratory slip additive, coefficient of friction per ASTM D1894 can exceed 0.6 and wicket bundling becomes unreliable, while blocking force per ASTM D3354 must be verified before order acceptance. Pre-drying is ordinarily unnecessary unless pellets are stored under condensation cycling; surface moisture then has been observed to generate melt fracture at the die lip.
For black mulch film extruded at 25 µm gauge, addition of 6 wt% to 8 wt% of a 40% carbon black masterbatch produces a final carbon black loading of 2.4 wt% to 3.2 wt%, and dispersion quality is assessed by microscopic count of undispersed agglomerates per ASTM D5596-21 on a 0.01 mm² scan area. UV durability in non-black agricultural film is provided by a combination of ultraviolet absorber and hindered amine light stabilizer at combined additions of 0.2 wt% to 0.4 wt%; for black film, carbon black dominates shielding, but a lower HALS addition of 0.1 wt% to 0.2 wt% is still used to suppress photo-oxidation at the film surface between pigment particles. Accelerated weathering per ISO 4892-2, method A, with 340 nm UVA lamps and 0.76 W/(m²·nm) irradiance is used to compare lot-to-lot retention of elongation at break; film containing no UV stabilization typically embrittles below 50% retention within 1,500 h, while well-dispersed black formulations may retain 70% after 4,000 h, although published data for Bapolene 222F under this protocol is limited. The base resin carries only minimum heat stabilizer and no functional UV package, so outdoor service life is entirely masterbatch-dependent. Sulfur-containing pesticides and halogenated soil fumigants have been associated with accelerated oxidative degradation and loss of tear strength exceeding 50% within two contact seasons in agricultural film field reports; film destined for fumigated soil must be re-stabilized for that chemical environment. Melt temperature is held between 170°C and 190°C; temperatures above 200°C degrade carbon black dispersion and can create pinholes as agglomerates deposit on the mandrel.
| Application | Standard designation | Parameter | Requirement or limit |
|---|---|---|---|
| Industrial sacks and liners | ASTM D1238 (ISO 1133-1) | Melt mass-flow rate | 2.0 g/10 min nominal at 190°C/2.16 kg |
| All film applications | ASTM D1505 (ISO 1183) | Density | 0.922 g/cm³ nominal |
| Mechanical evaluation | ASTM D882 / ISO 527-3 | Tensile properties at break | Report MD/TD against end-use specification |
| Heavy-gauge sacks | ASTM D1709 Method A | Dart impact | 2.5–4.0 g/µm typical; customer minimum applies |
| All film applications | ASTM D1922 / ISO 6383-2 | Elmendorf tear | Report MD/TD; packaging spec may define minimum |
| Frozen food packaging | ASTM F2029 / ASTM F88 | Seal initiation and seal strength | Initiation 95°C–110°C typical; seal strength ≥ 2 N/25 mm per customer |
| Food contact — US | FDA 21 CFR 177.1520(c) | Olefin polymers | End-test compliance for food type and use condition |
| Food contact — EU | Regulation (EU) No 10/2011 | Overall migration | ≤ 10 mg/dm² |
| EU market access | REACH 1907/2006 | SVHC communication | No SVHC above 0.1 wt% per Article 33 |
| Agricultural film | ISO 4892-2 | Accelerated weathering | Retention benchmark per customer; no universal limit |
| Construction vapor retarder | ASTM E1745 Class A | Water vapor permeance | ≤ 0.1 perm |
| Construction vapor retarder | ASTM E96/E96M | Water vapor transmission | Report at 23°C/50% RH |
Kraft, board, and aluminum foil lamination with Bapolene 222F requires a differentiated thermal regime compared with dedicated coating grades of 4.0 g/10 min to 8.0 g/10 min; barrel temperatures are commonly raised to 280°C to 320°C to reduce melt viscosity for curtain formation through a 0.5 mm to 0.7 mm slot die, though the lower melt index still generates higher die pressure and greater screw amperage on a 90 mm, 30:1 L/D extruder. At 25 µm coating thickness, neck-in measured from die edge to coating edge on a 600 mm slot die is typically 20 mm to 30 mm per side; increasing the air gap from 100 mm to 180 mm raises neck-in further but improves adhesion to paper by increasing melt surface oxidation, a mechanism documented in extrusion coating literature. Draw resonance becomes visible as periodic thickness variation in the machine direction when draw ratio exceeds 10:1; the limiting draw ratio for film-grade 2.0 MI may be lower than for dedicated coating grades, but published data for Bapolene 222F as a coating resin is limited. Where the lamination enters food contact service, the structure must comply with FDA 21 CFR 177.1520(c) and, for EU trade, with Regulation (EU) No 10/2011 including overall migration limits of 10 mg/dm² under the food simulant conditions specified in Annex III. Corona treatment to 42 mN/m to 46 mN/m wetting tension is standard for coating adhesion; re-treated wetting tension should be re-checked after 72 h because LDPE surface polarity decays with storage time.
Where 150 µm LDPE sheeting is specified as a sub-slab vapor retarder under ASTM E1745, Class A performance requires water vapor permeance not exceeding 0.1 perm as measured by ASTM E96/E96M desiccant method; LDPE at this thickness normally meets that threshold unless the film contains excessive low-molecular-weight extractables or is heavily filled. Tensile properties per ASTM D882 and puncture resistance per ASTM D1709A are reported against project specifications, but no universal minimum exists across all construction applications. Unprotected LDPE exposed to solar UV for more than 60 days may lose elongation markedly; black sheeting containing carbon black is used when extended outdoor exposure is expected. Radon mitigation and methane barrier installations typically require seam laps of at least 300 mm and tape sealing per project specification; hot-air welding is generally not recommended for thin LDPE because the narrow melt-temperature window makes pinhole formation likely.
In vertical form-fill-seal packaging of frozen vegetables, the seal bar set point is constrained by dwell time and package edge geometry; LDPE of nominal 2.0 g/10 min melt index and 0.922 g/cm³ density typically falls in a seal initiation band of 95°C to 110°C when measured by ASTM F2029, but the actual grade must be qualified against the converter’s jaw configuration because seal surface temperature can lag the set point by 5°C to 15°C on short dwell times. At -20°C, LDPE retains flexibility, and cold brittleness temperature by ASTM D1790 for this density class is generally below -50°C, though published data for Bapolene 222F is limited. Seal strength per ASTM F88 on 25 mm specimens cut from a 40 µm film commonly ranges from 2.0 N to 4.0 N at failure when the seal bar temperature is 105°C and dwell time is 0.4 s; lower dwell or contamination from filling dust reduces that value, so on-line burst testing of finished pouches is required. The package is not an oxygen barrier, with oxygen transmission rate at 25°C, 0% RH for 25 µm LDPE typically above 3,000 cm³/(m²·day·atm) per ASTM D3985, meaning frozen food use is appropriate only where freezing itself suppresses quality loss and no extended shell-life moisture barrier is demanded. If a converter requires seal initiation temperature below 95°C, a blend with EVA or metallocene ethylene copolymer is normally required; Bapolene 222F alone may not satisfy that requirement.
Competitive Bamberger Polymers Bapolene® 222F Polyethylene, Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
For blown film converters requiring a general-purpose low-density polyethylene with a nominal melt flow rate of 2.2 g/10 min and a nominal density of 0.922 g/cm³, Bamberger Polymers Bapolene® 222F Polyethylene, Film Grade occupies the mid-melt-index LDPE film segment. The grade is a low-density polyethylene homopolymer; the film designation F indicates intended use in blown or cast film, while the numeric portion 222 corresponds to the 2.2 g/10 min melt flow rate target in the supplier’s nomenclature. Melt flow rate is quantified under 190 °C and 2.16 kg load using ASTM D1238-20 or ISO 1133-1:2022. Density is measured by ASTM D1505 or ISO 1183-1 and published at 0.922 g/cm³. These two values establish the material’s basic classification under ASTM D4976 and indicate that the resin is designed for flow in film extrusion while retaining sufficient melt strength for bubble formation. The material is typically supplied as pellets; standard polyethylene handling and storage precautions apply. No predrying is normally required for sealed, dry-stored resin, but bags exposed to high humidity or surface condensation should be dried with warm air at 60 °C to 70 °C for 2 h to 4 h before extrusion. A lot-specific certificate of analysis should be consulted because additive packages for slip, antiblock, or processing aid are not universal across all film grades.
Film mechanical values are not resin constants; they are generated on blown film lines at controlled blow-up ratios, frost line heights, and thicknesses. Properties such as dart impact, Elmendorf tear, and tensile elongation change with film thickness, orientation, and cooling rate. Evaluations should therefore be performed on film specimens using ASTM D1709 for dart drop, ASTM D1922 for Elmendorf tear, and ASTM D882 for tensile properties of thin sheeting. The nominal density of 0.922 g/cm³ is commonly specified for overwrap, liners, and general packaging, but end-use performance cannot be assigned solely from density and melt flow rate.
The core published reference values for Bapolene 222F are the melt flow rate and density. The matrix below consolidates the standard test designations that should appear on the certificate of analysis or technical data sheet. Additional mechanical, optical, and thermal values are film-dependent and require conversion on the target line.
| Property | Reference method | Published nominal value | Condition or note |
|---|---|---|---|
| Melt flow rate | ASTM D1238-20 / ISO 1133-1:2022 | 2.2 g/10 min | 190 °C, 2.16 kg |
| Density | ASTM D1505 / ISO 1183-1 | 0.922 g/cm³ | 23 °C, after conditioning |
| Food-contact status | FDA 21 CFR 177.1520 | Supplier certification required | Condition-of-use dependent |
| EU food-contact framework | Commission Regulation (EU) No 10/2011 | Use-specific | Not a resin-only declaration |
Density testing by ASTM D1505 uses a density-gradient column; ISO 1183-1 uses an immersion method. The two methods can differ by 0.0005 g/cm³ or less under proper calibration, but the reported nominal value should be accepted only with the stated method. Melt flow rate values obtained under ASTM D1238-20 and ISO 1133-1:2022 may also differ due to die and temperature tolerances; certificates of analysis should therefore state the exact method used.
In comparative terms, a resin with a higher melt flow rate than 2.2 g/10 min would reduce viscosity further but may lower melt strength and bubble stability. A lower-melt-index LDPE, such as a 0.7 g/10 min film grade, increases melt strength and head pressure, which may be advantageous for thick-gauge heavy-duty films but may require higher melt temperatures or more powerful drives. The shift between flow categories measured by ASTM D1238-20 is not linear with molecular weight; it is an inverse viscosity indicator that correlates with extruder motor load only when screw geometry and temperature profile are fixed. Published data for this specific grade at varied melt flow rates are limited, so extrusion trials remain necessary.
Compared with a medium-density polyethylene at 0.930 g/cm³, Bapolene 222F has lower stiffness and a lower Vicat softening range, but improved clarity and typically lower heat seal initiation temperature. Actual values should be quantified by ASTM D1525 for Vicat softening and ASTM F2029 for heat seal. Compared with HDPE at 0.950 g/cm³ and above, the LDPE has a lower tensile modulus but often exhibits greater environmental stress crack resistance in flexible film geometries, although published data for this specific grade are limited.
Blown film processing of Bapolene 222F is typically run on single-screw extruders with screw diameters from 45 mm to 90 mm and 24:1 to 30:1 L/D. The barrel profile for a 60 mm extruder with a 24:1 L/D barrier screw may be set at 150 °C in zone 1, 165 °C in zone 2, 175 °C in zone 3, and 180 °C in the adapter. Actual setpoints must be adjusted for screw speed and backpressure. Melt temperature measured at the adapter should be maintained between 160 °C and 190 °C. Operation below 160 °C can create unmelted resin particles and increase screw amperage; operation above 190 °C can promote oxidative gel formation. Oxidative stability can be monitored by ASTM D3895.
For conventional single-lip air ring lines, the die gap is typically set from 0.8 mm to 1.5 mm, and the blow-up ratio is maintained between 2.0:1 and 3.0:1. At a die diameter of 100 mm, a frost line height of 6 to 10 die diameters normally stabilizes the bubble. A frost line located too low creates excessive quench and may reduce transverse direction tear strength; a frost line positioned too high promotes bubble breathing, film gauge variation, and loss of tubular stability, especially when blow-up ratio exceeds 3.0:1.
Output rate is not fixed by the resin alone; it depends on screw geometry, die diameter, internal bubble cooling, and air-ring performance. Field observations on blown film lines indicate that this 2.2 g/10 min LDPE generates lower head pressure than a 0.5 g/10 min fractional-melt LDPE at constant screw speed, which can permit lower melt temperatures or longer filtration intervals. However, the lower melt viscosity also reduces high-stalk bubble stability; the practical upper blow-up ratio for stable operation is usually 3.5:1 unless internal bubble stabilization is used. Lines processing the resin at very high frost line heights or very high haul-off speeds should monitor film thickness variability with an on-line capacitance gauge.
Blending Bapolene 222F with LLDPE or color masterbatch is performed on the production line. For precompounded color concentrates, a letdown ratio of 2 wt% to 4 wt% is common; the concentrate carrier should be LDPE-based to maintain compatibility. High-shear mixing is not required for uniform pellet blends, but the blending system should avoid segregation at silo discharge. Published data for this specific grade in high-letdown liquid color systems are limited, so screw mixing sections and screen pack condition should be evaluated during trial.
Purging and shutdown practice should follow the supplier’s recommended sequence. A lower-melt-index purge compound or commercial polyolefin purge is typically introduced at 190 °C to 200 °C to displace degraded resin before shutdown. Extended hold times above 190 °C should be avoided because they can cause gel formation in the next startup.
In thin-gauge retail packaging, liners, and overwrap, Bapolene 222F is selected where an LDPE is preferred over LLDPE for bubble stability, seal initiation, or surface gloss. Relative to a butene LLDPE of similar 0.918 g/cm³ density, the LDPE long-chain branching improves melt strength and reduces bubble instability in air-ring-controlled processes, but the film typically shows lower dart impact strength under ASTM D1709 and lower Elmendorf tear under ASTM D1922. The 2.2 g/10 min melt flow rate supports increased throughput compared with a 0.7 g/10 min LDPE, but the grade may not provide adequate melt strength for very large heavy-duty sacks or high-stalk extrusion. In those cases, a lower-melt-index LDPE or a bimodal polyethylene is normally required.
Grade substitution within the Bapolene LDPE film series is not a drop-in process. A lower-melt-index film grade will generally show higher head pressure and higher melt strength; a higher-melt-index grade will show easier flow but may reduce mechanical properties in oriented or thin film. Substitution of Bapolene 222F for another film resin requires re-qualification of seal initiation temperature, hot tack, and seal strength under ASTM F1921 or ASTM F2029. Additive packages also shift coefficient of friction and blocking tendency; film-to-film slip should be measured with ASTM D1894.
Published shrink-performance data for this specific grade at defined MD/TD shrink percentages are limited. For shrink bundling and collation shrink, film produced from this resin can be oriented via bubble expansion and haul-off speed, but shrink percentage, shrink force, and residual stress should be measured under ASTM D2838 or equivalent. This grade should not be assumed to replace a formulated shrink-film resin without line-specific trial data.
Food-contact compliance is use-specific and is not established by the resin data sheet alone. In the United States, the base olefin polymer may be listed under 21 CFR 177.1520, but the final film must be tested or certified for the intended food types, temperatures, and contact times. A supplier-issued food-contact statement is required for each lot or family. In the European Union, compliance is assessed under Commission Regulation (EU) No 10/2011, including its Annex I authorized substances and Annex II restrictions. Overall migration and specific migration limits must be evaluated under the intended simulant and time/temperature conditions; no universal food-contact approval exists. Laboratory methods for such testing include EN 1186-1 and EN 13130-1. Converters should retain migration test reports for each packaging article because compliance is article-specific.
Industrial REACH obligations under EC No 1907/2006 require the downstream user to review Section 3 of the safety data sheet and confirm the absence of substances of very high concern above the stated thresholds. RoHS compliance under 2011/65/EU applies only when the film is incorporated into an electrical or electronic equipment component; converters must verify the finished article against the directive’s material restrictions. Published data for this specific configuration in regulatory databases is limited because the resin is supplied as a polymeric raw material, not as a finished article.
Additive selection imposes processing boundaries. If the film requires printing or laminating, the converter should specify a no-slip or low-slip variant and confirm the absence of migratory amide additives such as erucamide or oleamide by infrared analysis. Excessive slip agent concentration can exude to the film surface and reduce print adhesion or lamination bond strength. Store the resin away from direct sunlight at ambient temperatures below 40 °C to minimize additive migration and pellet caking.