| HS Code | 885787 |
| Product Name | Bamberger Polymers Bapolene® 222B Polyethylene Film Grade |
| Polymer Type | Polyethylene |
| Density | 0.922 g/cm³ |
| Melt Index | 2.0 g/10 min |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 276 MPa |
| Vicat Softening Point | 95°C |
| Melting Point | 112°C |
| Haze | 6.0% |
| Gloss | 85% |
| Dart Drop Impact | 100 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 350 g |
As an accredited Bamberger Polymers Bapolene® 222B Polyethylene Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Bamberger Polymers Bapolene® 222B Polyethylene Film Grade is supplied in 25 kg (55 lb) moisture-resistant bags, palletized for shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loading for Bamberger Polymers Bapolene® 222B Polyethylene Film Grade: 25 kg bags, palletized, shrink-wrapped; approx. 18–20 MT net. |
| Shipping | Bamberger Polymers Bapolene® 222B Polyethylene Film Grade ships as non-hazardous polyethylene resin pellets. Standard packaging is 25 kg polyethylene bags, 40 bags per stretch-wrapped pallet (1,000 kg). Bulk trucks or railcars are available. Store dry, away from heat and direct sunlight; prevent contamination. |
| Storage | Store Bapolene® 222B indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Maintain stable stacking, avoid physical damage, protect from prolonged UV exposure, and follow the manufacturer’s SDS/local regulations. Use first-in, first-out. |
| Shelf Life | Stable under normal storage; indefinite shelf life if kept dry, cool, and away from UV. Consult supplier for specific recommendations. |
In blown-film extrusion of heavy-duty industrial liners, Bapolene® 222B is processed as a butene linear low-density polyethylene with nominal density 0.918 g/cm³ and nominal melt index 2.0 g/10 min when conditioned to ISO 1133-1:2022 at 190 °C and 2.16 kg. The extruder configuration best suited to this grade uses a barrier screw with L/D ratio of 25:1 to 30:1, a die gap of 1.8 mm to 2.5 mm, and a blow-up ratio from 2.0:1 to 3.0:1. Melt-temperature setpoints are normally held between 190 °C and 215 °C, with the lower end reducing oxidative gel and the upper end improving bubble stability in films above 80 µm. A twin-lip air ring with chilled air between 8 °C and 15 °C is used to stabilize the frost line; the frost-line height is maintained at 2 to 4 die diameters for gauge uniformity. Heavy-duty liners are converted at 100 µm to 200 µm, and edge-fold or bottom-seal configurations are tested to ASTM F88/F88M-23 for seal strength after impulse sealing at 180 °C to 210 °C jaw temperature. The specification for dart impact, measured to ASTM D1709-22 Method A, is commonly set at an F50 threshold above 800 g for 100 µm film, although final acceptance depends on the packaged product profile and fill cycle. Elmendorf tear in machine direction, tested to ASTM D1922-15(2021), can be expected to fall below transverse-direction values because of orientation effects; this directional imbalance is not a defect but must be accounted for by orienting the film such that the higher transverse tear resistance absorbs the primary stress path. Addition of a slip/antiblock masterbatch at 2 wt% to 4 wt% is typical to reduce blocking during long roll storage; the exact level is adjusted by coefficient-of-friction testing to ASTM D1894-14. If the liner is intended for direct food contact, the grade must meet FDA 21 CFR 177.1520(c) olefin polymer conditions of use and EU Commission Regulation 10/2011 overall migration limits under the intended food simulant. Published data for this specific configuration is limited, so converters should establish film-level acceptance thresholds through internal capability studies rather than relying on nominal resin properties alone.
Machine stretch wrap produced by cast-film extrusion imposes a narrower thickness tolerance than blown film and shifts the critical control point from bubble stability to chill-roll quench uniformity. Bapolene® 222B can be extruded at 15 µm to 23 µm through a cast die with a die gap of 0.6 mm to 1.0 mm and an air-knife position within 2 mm of the roll contact point. The chill roll is maintained at 18 °C to 25 °C; lower roll temperatures increase line speed capability but may produce transverse gauge bands if roll surface temperature varies by more than ±1 °C. Pre-stretch on the conversion line is typically set between 200 % and 300 %, and the film must retain puncture resistance after elongation; puncture resistance is assessed to ASTM D5748-19, with acceptance often expressed as a minimum break force per unit thickness. Cling performance is obtained by compounding with polyisobutylene or a specialty cling additive at 1 wt% to 3 wt%, but the additive has a direct negative effect on unwind force and can increase roll blocking above 35 °C warehouse conditions. Slip migration from a competing slip additive must not be introduced at the same time; the resulting coefficient-of-friction balance is verified to ASTM D1894-14 in both machine and transverse directions. Because cast film has lower machine-direction orientation than blown film, tensile elongation at break to ISO 527-3:2018 generally exceeds 400 %, but published data for this specific configuration is limited and startup trials should establish the lower statistical control limit. The roll core must be dimensionally stable; a 76 mm paper core with a 3 mm wall is common for machine-film lengths above 1500 m. For industrial pallet wrap, EU Regulation 10/2011 may apply if the film contacts food packaging under dry or fatty conditions, while REACH SVHC screening is required for the cling additive system.
Agricultural silage wrap and cover films derived from Bapolene® 222B are exposed to a process conflict between required UV protection and the mechanical losses caused by high additive loadings. A hindered amine light stabiliser package is typically introduced at 1.5 wt% to 3.0 wt% through a compounded masterbatch, while a carbon black or titanium dioxide opacifier may be added at 2 wt% to 6 wt% to block UV and reduce heat build-up. In blown-film processing, the presence of the opacifier changes bubble emissivity and can move the frost line upward by 10 % to 20 %; operators compensate by reducing melt temperature by 5 °C to 10 °C or increasing cooling-air pressure. The trade-off appears in Elmendorf tear resistance to ASTM D1922-15(2021) and dart impact to ASTM D1709-22: high inorganic filler loadings can reduce transverse tear strength by as much as 15 % to 25 % relative to unfilled film at the same gauge, though this range varies with dispersion quality and masterbatch carrier resin. A twin-screw compounding step with distributive mixing elements is preferred over simple tumble blending because agglomerates above 50 µm create pinholes during bale wrap stretching. The terminal silage film is commonly produced at 25 µm to 45 µm, with puncture resistance tested to ISO 7765-1:2021 or ASTM D5748-19. For silage stretch wrap, adhesion must be low on the exterior but sufficient to hold film layers together; a cling layer is applied only on one side by coextrusion with a very low-density polyolefin or by selective coating, because uniform incorporation of cling additive into Bapolene® 222B would cause telescoping on pre-stretch. Compliance in the EU is checked against Regulation 10/2011 when silage film is sold for indirect food storage; EN 13206:2017 covering thermoplastic films for agricultural use provides durability classifications that converters use to set warranty periods. The film is not a replacement for UV-barrier laminates beyond one or two seasons; published data for this specific configuration is limited and annual reapplication or replacement should be specified by the agronomic service provider.
When laminated frozen-food pouches must survive handling at −20 °C to −30 °C, Bapolene® 222B is evaluated as a sealant web and not as a barrier layer. The blown sealant film is typically extruded at 30 µm to 50 µm, printed or laminated to polyester or oriented polyamide, and then run on pouch machines with impulse or constant-heat seal jaws. Low-temperature toughness is characterized by dart impact on the laminate to ASTM D1709-22 using Method A or B depending on thickness, and by tensile elongation at break to ISO 527-3:2018 after conditioning at −20 °C for 24 h. The butene LLDPE backbone retains sufficient chain mobility at frozen conditions, but the coefficient of friction rises as surface filming agents crystallize; therefore a high-purity erucamide slip agent at 500 ppm to 1200 ppm is used to stabilize the coefficient of friction to ASTM D1894-14. The seal initiation temperature of the sealant web is typically in the range of 105 °C to 125 °C, measured to ASTM F1921-18 as hot-tack force; the operating seal window should remain above the lower limit to avoid leakers but below the upper limit to avoid film distortion at 160 °C. For direct food contact, the sealant layer must comply with FDA 21 CFR 177.1520(c) conditions of use A through H depending on food type and temperature, and with EU Regulation 10/2011 overall migration below 10 mg/dm². The absence of an EVOH or metallisation layer means the laminate will have oxygen transmission above 2000 cm³/(m²·day·atm) at 23 °C and 0 % RH; this is acceptable only for products without oxidative rancidity risk or where a separate barrier web is used. Corona treatment of the sealant surface to 38 mN/m to 42 mN/m is required for lamination, but treatment must be applied immediately before the laminator because discharge above 48 mN/m can create low-molecular-weight oxidation products that interfere with seal strength.
Stretch-hood conversion requires a high degree of transverse orientation to resist tearing when the hood is pulled over a pallet. Bapolene® 222B is extruded at 50 µm to 100 µm with a blow-up ratio of 3.0:1 to 4.5:1 and a die gap of 1.4 mm to 2.0 mm. At upper blow-up ratio, bubble stability is more sensitive to air-ring turbulence; gel defects above 300 µm can propagate into transverse tears during the stretch cycle. The film is often dry-blended with 20 wt% to 30 wt% of an LDPE melt-strength resin to improve bubble stability, but the addition reduces puncture resistance to ASTM D5748-19 by an amount that must be tracked against the minimum load-retention requirement. Elastic recovery is tested to ASTM D5459-22; acceptable permanent deformation is typically below 15 % after 200 % elongation. Slip/antiblock additive level is kept at 1 wt% to 3 wt% because higher levels reduce the film-to-film friction needed to hold the hood on the pallet, leading to load shift. For industrial non-food use, REACH SVHC screening applies to the additive system, but FDA 21 CFR is not required unless the film contacts packaged food directly. The terminal stretch hood is applied at 50 % to 100 % pre-stretch on automatic stretch-hood equipment, and film must not fail at the gusset fold or weld line. Published data for this specific configuration is limited; converters usually run high-speed camera trials at the pallet wrap station to detect transient stress concentrations that standard roll-based film tests do not capture.
Vertical form-fill-seal of powdered detergent runs at line speeds from 60 pouches/min to 100 pouches/min, with dwell times as low as 0.3 s. Bapolene® 222B is converted at 40 µm to 75 µm, often with 20 wt% to 30 wt% HDPE to increase stiffness and reduce forming-collar drag. The HDPE raises seal initiation temperature by 5 °C to 10 °C; hot-tack force to ASTM F1921-18 must be evaluated over the entire jaw temperature range to avoid seal opening when product dust contaminates the seal area. Serrated or cross-hatch jaw profiles are used because they displace fine powder from the seal interface more effectively than flat jaws. The film coefficient of friction to ASTM D1894-14 is maintained below 0.25 by a slip package; higher values create erratic film advance on the forming tube. Seal strength after 24 h conditioning is tested to ASTM F88/F88M-23 with a minimum often set at 10 N/25 mm for a 50 µm film, though fill weight and product release gas may require higher values. Drop testing to ASTM D5276-19 from 1.2 m on filled pouches is used to quantify cold-climate leakers during distribution in unheated warehouses at −10 °C to 5 °C. For detergent packaging, EU Regulation 10/2011 does not apply unless the pouch is used for food; REACH and packaging waste regulations cover the concentrate and the film structure. The main processing boundary is dust-induced seal contamination, not resin melt strength; if hot-tack force declines below the qualified lower control limit after 30 min of continuous dusty sealing, the jaw profile must be cleaned or the blend ratio revised.
| Application segment | Applicable standard / regulation | Measured property or limiting condition |
|---|---|---|
| Heavy-duty industrial liners | FDA 21 CFR 177.1520(c); EU 10/2011 | Olefin polymer direct food-contact conditions |
| Machine stretch wrap | ASTM D5748-19; ASTM D1894-14 | Puncture resistance and cling/slip balance |
| Agricultural silage film | EN 13206:2017; ISO 7765-1:2021 | Durability classification and puncture resistance |
| Frozen-food sealant web | FDA 21 CFR 177.1520(c); EU 10/2011 | Overall migration below 10 mg/dm² |
| Stretch hood | ASTM D5459-22; ASTM D5748-19 | Elastic recovery and puncture after pre-stretch |
| VFFS powdered detergent | ASTM F1921-18; ASTM F88/F88M-23 | Hot tack and seal strength with dusty seal area |
Competitive Bamberger Polymers Bapolene® 222B Polyethylene Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Bamberger Polymers Bapolene® 222B is a high-molecular-weight, high-density polyethylene film resin supplied in pellet form. The grade is specified for blown film extrusion of thin-gauge packaging structures where elevated dart impact strength and environmental stress crack resistance are required, including T-shirt sacks, can liners, industrial liners, and carry-out bags. The base resin is a polyethylene copolymer with a typical density of 0.954 g/cm³ measured by ASTM D1505 / ISO 1183-1 and a melt flow rate of 0.22 g/10 min determined at 190 °C under a 2.16 kg load by ASTM D1238 / ISO 1133-1. These two values place the grade in the high-molecular-weight HDPE film category rather than in general-purpose injection or sheet extrusion classifications.
The melt flow rate of 0.22 g/10 min functions as an inverse indicator of weight-average molecular weight in this HDPE family. As molecular weight increases, the concentration of tie-chain segments traversing the crystalline lamellae increases. Under the tensile impact conditions of ASTM D1709, those tie chains distribute stress across lamellar boundaries and raise the F50 dart-impact value of a 25 µm blown film to approximately 350 g. Simultaneously, slow crack growth resistance measured by ASTM D1693 remains above 500 h in Condition B with 100% Igepal because long-chain molecules bridge microvoids ahead of the crack front. The typical property set is shown in Table 1; the values are nominal manufacturer data and are not lot-to-lot guaranteed limits.
| Property | Test method | Typical value |
|---|---|---|
| Melt flow rate, 190 °C, 2.16 kg | ASTM D1238 / ISO 1133-1 | 0.22 g/10 min |
| Density | ASTM D1505 / ISO 1183-1 | 0.954 g/cm³ |
| Tensile yield strength | ASTM D638 / ISO 527-2 | 28 MPa |
| Tensile elongation at break | ASTM D638 / ISO 527-2 | >600% |
| Flexural modulus, 1% secant | ASTM D790 / ISO 178 | 1,300 MPa |
| Dart impact F50, 25 µm film | ASTM D1709 / ISO 7765-1 | 350 g |
| Environmental stress crack resistance, F50 | ASTM D1693, Condition B, 100% Igepal | >500 h |
| Vicat softening point | ASTM D1525 / ISO 306 | 126 °C |
| Low-temperature brittleness | ASTM D746 | <-76 °C |
The density of 0.954 g/cm³ contributes to stiffness and moisture-barrier performance but does not place the product in the ultra-high-modulus HDPE range above 0.960 g/cm³. This intermediate density allows a measurable balance between yield strength and film tear resistance. Dart impact values must always be interpreted with gauge, blow-up ratio, frost-line height, and die temperature because the F50 result is a film-property measurement, not an intrinsic resin constant. The same limitation applies to ESCR: molded plaques for ASTM D1693 are not directly predictive of failure times in stressed bag handles or liner seams.
On conventional high-stalk blown film extruders with a 24:1 to 30:1 L/D grooved-feed barrel, barrel zone temperatures are typically profiled from 160 °C in the feed section to 210 °C at the adapter. Die and head zones are maintained between 210 °C and 225 °C. A spiral mandrel die with a die gap of 1.2 mm is a common starting condition for 15 µm to 25 µm film. Narrowing the die gap below 1.0 mm increases the probability of melt fracture at the die lip unless head temperature is raised, and it also raises die pressure. Blow-up ratios of 3.5:1 to 4.5:1 are normally required to achieve balanced tear strength, while frost-line heights from 600 mm to 900 mm are used to generate the long-stalk orientation typical of high-molecular-weight HDPE film. Internal bubble cooling is required on most production lines because the heat removal rate from the long stalk alone limits output. Without internal bubble cooling, achievable line speed falls significantly and bubble instability near the frost line becomes the controlling constraint.
Head pressure at the screen changer typically ranges from 250 bar to 450 bar depending on die diameter, output rate, and melt temperature. On a 150 mm spiral mandrel die running approximately 200 kg/h, the pressure drop may approach 400 bar. Screen-pack sequences of 20/40/80 mesh or equivalent are used to protect the die lip and to raise residence time for melt homogenization, but finer screens increase back pressure and can force the extruder into its motor-load limit before the barrel temperature limit is reached. Extruder drives on HMW-HDPE film lines must therefore be sized for the torque requirement of a low-MFR resin; a machine rated for LDPE film throughput will not automatically deliver the same output with Bapolene 222B. Published data for this specific resin on a given extruder configuration is limited, so start-up should be validated by pressure, motor-amperage, and melt-temperature measurements rather than by fixed rpm settings.
Surface moisture is normally not a processing problem when pellet storage remains below 60% RH and the hopper is not exposed to condensation. If sacks are opened in an unheated warehouse and stored at high humidity, surface water can create film defects through steam volatilization in the feed zone. No predrying is required under standard closed-hopper conditions, but a hopper dryer set to 70 °C for 1 h may be used when condensation is visible or when regrind content exceeds 20% of the total feed. Regrind from edge trim and start-up scrap should be kept clean and dry; the high molecular weight of the resin increases the sensitivity of the melt to contamination-derived gels, which appear as fisheyes in thin film.
The manufacturer’s published compliance statements for Bapolene 222B are limited to the base resin and do not automatically extend to finished articles containing color concentrates, slip agents, antiblock additives, printing inks, or recycled content. Under U.S. law, the resin may be used in contact with food only when the finished article meets the extractive and compositional requirements of 21 CFR §177.1520. For European food-contact applications, compliance with EU No 10/2011 must be established on the final packaging article, including verification of overall migration below the applicable limit and confirmation that any additives present are listed in the positive list. The grade is not supplied with a medical-grade or pharmaceutical-grade certification unless separately negotiated and documented by the manufacturer. RoHS Directive 2011/65/EU restrictions on lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE are not normally relevant to unmodified polyethylene packaging, but downstream converters must verify that added colorants or processing aids do not introduce restricted substances.
Compared with higher-melt-index HDPE film grades with MFR values above 0.7 g/10 min, Bapolene 222B penalizes extrusion throughput per screw revolution and raises specific energy consumption per kilogram of film. The higher melt strength permits a taller, more stable stalk and thinner achievable gauge on internal-bubble-cooling lines, but drawdown to gauges below 10 µm may require elevated die temperatures and reduced stalk height. Relative to injection-molding HDPE grades with MFR values from 6 g/10 min to 12 g/10 min, this film grade is not a direct substitute in ram or screw injection machines because the low MFR increases fill pressure, reduces flow length, and can produce visible flow lines at low clamp force. Compared with medium-molecular-weight HDPE film resins of the same nominal density, the product’s higher molecular weight results in measurably higher dart impact by ASTM D1709 and longer ESCR by ASTM D1693, but the processing window is narrower and the melt-pressure requirement is higher. The grade is also not formulated as a cast-film resin; its rheology and crystallization rate are compatible with the long-stalk blown film process rather than the rapid quench and high line speeds characteristic of cast HDPE film.