Bamberger Polymers Bapolene 155fp Lldpe Hexene Extrusion Grade

Bamberger Polymers Bapolene® 155FP LLDPE, Hexene Extrusion Grade

    • Product Name: Bamberger Polymers Bapolene® 155FP LLDPE, Hexene Extrusion Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 964964
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene
    Grade 155FP
    Processing Method Extrusion
    Form Pellets
    Density 0.918 g/cm³
    Melt Index 1.0 g/10 min at 190°C/2.16 kg
    Melting Point 123 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 11.0 MPa
    Tensile Strength At Break 22.0 MPa
    Elongation At Break 800%
    Flexural Modulus 276 MPa
    Haze 10%
    Gloss 60
    Dart Drop Impact 120 g
    Elmendorf Tear Strength 300 g

    As an accredited Bamberger Polymers Bapolene® 155FP LLDPE, Hexene Extrusion Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 155FP LLDPE, Hexene Extrusion Grade comes in 25 kg (55 lb) polyethylene bags, 40 bags per pallet.
    Container Loading (20′ FCL) 20′ FCL loading: Bamberger Polymers Bapolene® 155FP LLDPE Hexene Extrusion Grade, 25 kg bags, palletized, stretch-wrapped, secured for ocean freight.
    Shipping Bamberger Polymers Bapolene® 155FP LLDPE, Hexene Extrusion Grade is a non-hazardous resin shipped as dry pellets in 25 kg polyethylene bags on stretch-wrapped pallets, or in bulk trucks/railcars. Store cool and dry; avoid moisture, heat, and UV. No special DOT placards required.
    Storage Store Bamberger Polymers Bapolene® 155FP LLDPE, Hexene Extrusion Grade in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original bags sealed, palletized, and off the floor to prevent moisture and contamination. Avoid prolonged UV exposure, excessive stacking, and dust generation. Maintain normal ambient temperatures and follow the manufacturer’s SDS and local regulations.
    Shelf Life Typically 12 months from manufacture when stored in original unopened packaging, cool, dry, and away from direct sunlight.
    Application of Bamberger Polymers Bapolene® 155FP LLDPE, Hexene Extrusion Grade

    On a 55 mm single-screw blown-film line fitted with a 30:1 L/D barrier screw and a dual-lip air ring, Bapolene 155FP is converted to heavy-duty industrial liners using a formulation of 96.8 wt% hexene LLDPE, 3.0 wt% slip/antiblock masterbatch, and 0.2 wt% fluoroelastomer processing aid. The processing aid is limited to 0.2 wt% because higher addition has been observed in production to plate the die lip and produce a continuous haze band on the film web. Melt temperature at the die is held between 190 °C and 225 °C, the die gap is opened to 2.0–2.4 mm, and the blow-up ratio is maintained at 2.2:1–3.2:1 with a frost line height of 8–12 die diameters. Output on this line typically ranges from 90 kg/h to 120 kg/h, and the gauge profile is measured by a capacitance gauge with a target variation of less than ±6%. Dart impact is tested according to ASTM D1709-16A method A, tensile properties according to ASTM D882-18, and Elmendorf tear according to ASTM D1922-15. The terminal product is a 100–200 μm FIBC inner liner for dry bulk chemicals; seal integrity is evaluated by heat-seal strength testing at 0.5 s dwell time and 120 °C jaw temperature, with a minimum seal strength of 0.5 N/15 mm required for sift-proof certification.

    Bubble stability in this application is the main process boundary. Hexene LLDPE exhibits lower melt strength than high-pressure LDPE, so a high-stalk configuration is operated rather than a low-stalk pocket bubble. If the frost line is lowered below 6 die diameters, secondary bubble oscillation appears and the machine-direction tear balance shifts by more than 15% when tested by ASTM D1922-15. Conversely, raising the frost line above 14 die diameters reduces transverse direction tear to a level that produces field failures during pallet handling. The air ring chiller is therefore set to deliver air at 10–18 °C, and the internal bubble cooling exhaust is throttled to keep the bubble neck stable during ambient temperature swings. Amine-based additive masterbatches are avoided in this formulation because amine moieties at die temperatures above 200 °C can accelerate thermo-oxidative chain scission at the lip exit. For dry food powder liners, the film must comply with FDA 21 CFR 177.1520 and EU Commission Regulation 10/2011; migration testing is conducted under EN 1186-1:2002 conditions, and the hexene copolymer structure typically gives lower hexane extractables than butene-modified LLDPE, although end users must verify lot-specific certificates because additive masterbatch composition influences the overall extractable profile.

    Does Draw Resonance in Cast Stretch Film Compromise Hexene LLDPE Puncture Resistance?

    Draw resonance in cast pallet stretch film becomes severe when the draw ratio between the 2,600 mm slot die exit and the chill roll exceeds 30:1, producing periodic thickness bands that reduce puncture energy under ASTM D5748-19. Bapolene 155FP is processed on a 150 mm extruder with 33:1 L/D, a melt temperature of 240–270 °C, and an air gap of 25–150 mm. The die lip gap is set at 0.4–0.6 mm, and the chill roll temperature is maintained at 18–28 °C to prevent blocking. At line speeds of 400–800 m/min, a resin with insufficient melt strength can neck in by 80–120 mm per edge and oscillate in thickness by more than ±8%; therefore, 10–15 wt% high-pressure LDPE is frequently added to increase melt strength and delay the draw resonance threshold. The addition also reduces the storage modulus ratio at 1 s⁻¹ and 100 s⁻¹, as determined by dynamic oscillatory shear at 190 °C according to ASTM D4440-08. The terminal product is a 12–23 μm machine stretch film, with cling force measured by ASTM D4649 and puncture resistance by ASTM D5748-19. Published data for draw resonance thresholds on this specific hexene grade at air gaps below 100 mm is limited; therefore, line trials are required before reducing the air gap.

    The cast film process requires strict control of the chill roll surface finish and the melt web contact point. If the quench onset moves beyond 150 mm from the die exit, blocking tendency increases and the film may develop transverse striations that are visible after stretching at 200% elongation. The chill roll is operated with a matte surface roughness of Ra 0.5–1.0 μm to prevent air entrapment and improve roll release. Compliance for this industrial packaging article is governed by EU Directive 94/62/EC on packaging waste, REACH Regulation (EC) No 1907/2006 Annex XVII for restricted substances, and RoHS Directive 2011/65/EU for heavy-metal limits.

    For liquid packaging board coated at 450 m/min on a tandem extrusion lamination line with a 120 mm single-screw extruder and a 2,200 mm slot die, Bapolene 155FP is used as a 20–40 g/m² coating layer. The melt temperature at the die exit is 285–320 °C, and the air gap is expanded to 150–300 mm to maximize melt oxidation and improve adhesion to clay-coated paperboard. A blend of 80 wt% 155FP and 20 wt% LDPE with a density of 0.918 g/cm³ is generally selected to lower shear viscosity and reduce neck-in; at a 150 mm air gap, the web width from a 2,000 mm die typically stabilizes at 1,920–1,950 mm depending on backpressure and lip geometry. Adhesion is monitored on the line by a tape peel test according to TAPPI T 494, and off-line by ASTM D903-98 with single-edge razor assistance. The coating must satisfy FDA 21 CFR 177.1520(c) when used as a food-contact layer, and migration compliance under EU 10/2011 is verified using EN 1186-1:2002 total immersion and EN 1186-3:2002 3% acetic acid simulation. The final board is converted into gable-top cartons and paper cup blanks.

    The principal process hazard is thermo-oxidative degradation during long residence at 320 °C. If the screw speed is not synchronized with the line speed, static melt pools can form in the feed section of the die at residence times above 4 min, producing crosslinked gels that appear as coating lumps. To prevent this, the extruder throughput is held at 25–35 kg/h per 100 mm die width, and the die lips are purged with high-density polyethylene during every splice. The packaging converter must also control the paperboard moisture content between 5% and 8%, because lower moisture causes fiber lift and higher moisture generates pinholes at the coating interface. This application has a narrow melt-temperature window because the low-viscosity LDPE modifier degrades before the hexene LLDPE reaches its maximum throughput.

    Geomembrane Sheet Flat-Die Extrusion and Field Seaming Requirements

    Flat-die sheet extrusion of Bapolene 155FP for LLDPE geomembrane liner applications requires the addition of 2.0–3.0 wt% carbon black masterbatch with a particle size below 25 nm to provide ultraviolet stabilization. The compound is processed on a 150 mm vented single-screw extruder with a 33:1 L/D ratio and a 4,000 mm flat die; sheet thickness is controlled between 0.75 mm and 2.5 mm. The three-roll polishing stack operates at 60–90 °C, and the line speed is set to 5–15 m/min. Edge trim from neck-in typically amounts to 60–100 mm per side and is reground into the feed stream at no more than 10 wt% to avoid reducing stress crack resistance. Tensile yield and break properties are evaluated according to ASTM D6693, puncture resistance according to ASTM D4833, and tear resistance according to ASTM D1004. Oxidative induction time is measured by ASTM D3895-19; for LLDPE geomembrane applications, the specification basis should follow GRI-GM17, not GRI-GM13 HDPE thresholds. Published data for this specific 155FP configuration under GRI-GM17 is limited, so suppliers must provide third-party test reports for each production lot.

    Field seaming imposes a separate operational boundary. Hot-wedge fusion welding of LLDPE geomembrane panels is conducted at wedge temperatures of 350–450 °C, with seam peel and shear tested according to ASTM D6392-12. If the sheet contains carbon black dispersion defects from inadequate masterbatch let-down, the weld track may show localized cold spots and seam strength retention below the required 80% of parent sheet tensile value. The operator must therefore verify carbon black dispersion by ASTM D5596-03 microscopy or equivalent, and monitor the melt temperature at the die lip within ±5 °C, because a temperature drift greater than that can alter the quiescent crystallinity gradient across the sheet width and produce warped panels that are difficult to weld on grade. The terminal product is a landfill or pond liner with a nominal 1.5 mm thickness, double wedge seams, and factory-fabricated panels that are deployed under environmental conditions of −40 °C to 60 °C.

    When Irrigation Tubing Wall Thickness Drops Below 1.0 mm

    When 155FP is extruded into thin-wall drip irrigation laterals with an outside diameter of 16 mm and a wall thickness of 0.9–1.1 mm, the critical process risk is draw-down instability in the vacuum sizing tank leading to out-of-roundness above 0.3 mm and wall-thickness variation greater than ±8%. The line uses a 45 mm twin-screw extruder with 28:1 L/D, a spiral mandrel die head, barrel temperatures from 150 °C to 210 °C, and melt temperature at 210–230 °C. Vacuum calibrator pressure is held at 0.3–0.5 bar, and line speed is kept between 15 m/min and 30 m/min. The compound contains 2.0–2.5 wt% carbon black UV masterbatch and 0.2–0.4 wt% high-molecular-weight HALS stabilizer; the carbon black grade is selected with a primary particle size below 25 nm because larger aggregates can initiate environmental stress cracking around inserted emitter barbs. Hydrostatic design basis for long-term internal pressure is evaluated under ISO 9080:2012 at 20 °C for a 50-year service life, and rapid crack propagation resistance is assessed by ISO 13479:1997 for PE pressure pipes.

    In-line wall-thickness control uses ultrasonic gauges fitted around the circumference of the tube. If the wall thickness falls below 0.85 mm, the tube becomes vulnerable to kinking during coiling, and the insertion force for button emitters increases by more than 25%, which can tear the wall. The operator therefore maintains a minimum wall-thickness setpoint of 0.90 mm and compensates for shrinkage by increasing the calibrator vacuum to 0.45 bar when ambient humidity exceeds 60%. The resulting pipe is cut into 500 m coils and is intended for low-pressure agricultural drip irrigation networks operating below 1.0 bar. Because the final product is not rated for potable water, compliance focuses on REACH Regulation (EC) No 1907/2006 Article 33 and RoHS Directive 2011/65/EU for heavy-metal restrictions rather than drinking water approvals.

    In stretch-hood logistics, Bapolene 155FP is extruded as a heavy-gauge tubular film on a high-blow-ratio blown line with 4.0:1–4.8:1 blow-up ratio and internal bubble cooling. The melt temperature is held at 190–215 °C, the die gap at 1.8–2.0 mm, and the frost line at 12–16 die diameters. Because the bubble is close to the stability limit, 10–20 wt% LDPE is added to raise melt strength and prevent helical upset, and 0.1–0.2 wt% fluoroelastomer processing aid is used to delay melt fracture at high screw speeds. Film thickness is typically 100–200 μm, and the tube is wound as gusseted layflat of 1,200–2,000 mm width. Elastic recovery after 50% elongation is measured according to ASTM D5459-95, puncture resistance by ASTM D5748-19, and tensile impact by ASTM D1822-13. The terminal hood film covers palletized loads and must survive outdoor storage; UV stabilization is therefore provided by 0.3–0.6 wt% HALS plus 0.1–0.2 wt% UV absorber, and compliance with REACH Regulation (EC) No 1907/2006 Annex XVII for restricted additives and Directive 94/62/EC packaging waste is required. The main failure mode in this application is bubble collapse caused by ambient air turbulence below 15 °C, so the tower is enclosed and the air ring supply is conditioned to 12–18 °C dew point to avoid condensation on the bubble.

    Table 1. End-use regulatory and test matrix for Bapolene 155FP hexene LLDPE extrusion applications
    Downstream articleRegulation or standardTest method or verification basisCritical control point
    Heavy-duty food-contact linerFDA 21 CFR 177.1520EN 1186-1:2002Extractables from masterbatch system
    Pallet stretch filmRoHS Directive 2011/65/EUASTM D5748-19Puncture energy after pre-stretch
    Liquid packaging board coatingEU 10/2011EN 1186-3:2002Overall migration into acetic acid simulant
    LLDPE geomembraneGRI-GM17ASTM D3895-19Oxidative induction time at 200 °C
    Irrigation tubingISO 9080:2012ISO 13479:1997Long-term hydrostatic strength and slow crack growth
    Stretch hood filmREACH Regulation (EC) No 1907/2006ASTM D5459-95Elastic recovery hysteresis at 50% elongation
    Free Quote

    Competitive Bamberger Polymers Bapolene® 155FP LLDPE, Hexene Extrusion Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bamberger Polymers Bapolene® 155FP is classified as a linear low-density polyethylene extrusion grade produced with 1-hexene as the alpha-olefin comonomer. The resin is positioned for blown-film extrusion where hexene-derived short-chain branching contributes to higher tie-molecule formation than shorter 1-butene branches at equivalent density. Melt flow index is placed in the 0.9–1.2 g/10 min range under ASTM D1238-20 at 190°C/2.16 kg, and density is placed in the 0.916–0.920 g/cm³ band under ASTM D1505-18. The controlling Certificate of Analysis remains the required document for lot-specific values. The product is not a high-pressure low-density polyethylene: the linear backbone and short-chain branching distribution differ from the long-chain-branched architecture of autoclave or tubular LDPE. In cast film, extrusion coating, or coextrusion structures, the selection criteria differ because melt strength, draw resonance, and neck-in are governed by long-chain branching and molecular weight distribution rather than by comonomer type alone. All processing data below are stated as equipment-dependent ranges and are not a substitute for line-specific qualification.

    What Distinguishes Hexene-Mediated Short-Chain Branching from Butene Grades?

    The difference between 1-hexene and 1-butene comonomers is expressed in the length of the pendant branch and the probability that the branch participates in tie-molecule formation across adjacent lamellae. A C6 branch extends beyond the crystalline lamella fold surface more effectively than a C4 branch, which reduces the number of mechanically ineffective loose loops and increases the density of load-bearing interlamellar tie chains. Comparative blown-film evaluations on 25 µm monolayer structures tested under ASTM D1922-15 and ASTM D1709-16a commonly show Elmendorf tear improvements of 20–35% and dart impact improvements of 25–50% for hexene-based LLDPE relative to butene-based LLDPE at similar melt index and density. Puncture resistance measured under ASTM D5748-19 can shift from 40–60 N to 55–85 N depending on bubble cooling rate and film gauge. Published data for Bapolene® 155FP in every end-use configuration is limited, so pilot-line trials remain mandatory when replacing a butene grade in a running production specification.

    On conventional blown-film extruders with screw diameters of 45–75 mm and L/D ratios of 24:1 to 30:1, the melt temperature for hexene LLDPE extrusion grades is typically maintained between 190°C and 230°C. Barrel temperature profiles from the feed throat to the metering zone commonly follow 170–190°C, 190–210°C, and 205–225°C; die zones are held at 210–225°C. Melt temperatures above 240°C can reduce bubble stability through lowered melt strength and may increase oxidative gel formation if residence time exceeds 4–6 minutes at screw speeds below 20 rpm. Melt pressure before the screen changer is typically in the 20–35 MPa range, depending on die tooling, output rate, and melt filter condition. The processing window is narrow; a die-temperature shift of ±5°C can measurably alter frost line height, film gauge uniformity, and the onset of sharkskin. Grooved-feed throat sections improve solids conveying at lower feed-zone temperatures but may raise motor load and require higher screw torque capacity on older extruders.

    Film Mechanical Performance, Gauge Uniformity, and Bubble Stability Limits

    Tensile properties for hexene LLDPE blown film are measured under ASTM D882-18. Typical yield strengths fall near 10–12 MPa in the machine direction and 9–11 MPa in the transverse direction; ultimate tensile strengths commonly range from 30–40 MPa depending on draw ratio and frost line height. Elongation at break generally exceeds 600% in both directions when gauge control is maintained within ±5% of target. The 1% secant modulus under ASTM D882-18 is typically 160–200 MPa in the machine direction, which is lower than high-density polyethylene but sufficient for heavy-duty industrial liners, agricultural films, and collation shrink overwrap structures requiring puncture and tear resistance. Bubble stability is most affected by gauge uniformity, die gap, and the ratio of melt temperature to die lip temperature. Large rapid fluctuation in melt pressure of more than 2 MPa across a 30-second interval indicates feedblock or screw metering instability and should be corrected before collecting mechanical property data.

    Table 1: Representative comparative film property ranges for butene-based and hexene-based LLDPE at 0.918 g/cm³ density and 1.0 g/10 min melt index, 25 µm blown film
    PropertyTest methodButene LLDPEHexene LLDPE
    DensityASTM D1505-180.917–0.919 g/cm³0.917–0.919 g/cm³
    Melt indexASTM D1238-200.9–1.1 g/10 min0.9–1.1 g/10 min
    Dart impactASTM D1709-16a90–130 g140–210 g
    Elmendorf tear MDASTM D1922-15200–350 g300–500 g
    Elmendorf tear TDASTM D1922-15350–500 g450–650 g
    Puncture resistanceASTM D5748-1940–60 N55–85 N
    1% secant modulus MDASTM D882-18180–220 MPa160–200 MPa
    HazeASTM D1003-1310–15%8–13%

    Heat seal initiation and hot tack are not primary specifications for all extrusion grades, but they constrain downgauging and package conversion speed. Hexene LLDPE blown films typically show seal initiation temperatures near 95–105°C and plateau seal strengths of 15–25 N/25 mm under ASTM F88/F88M-21, depending on seal bar geometry, dwell time, and film gauge. Hot tack strength under ASTM F1921-18 may be 4–7 N/25 mm at 110–120°C. These ranges are not product release limits for Bapolene® 155FP; they represent the expected performance envelope for conventional hexene LLDPE extrusion grades and must be verified with the manufacturer’s current data sheet.

    Blown Film Die Configurations, Bubble Geometry, and Output Rate Constraints

    Die gap selection for hexene LLDPE extrusion grades is commonly set at 1.5–2.5 mm, with wide die gaps used to lower shear stress and delay melt fracture. Blow-up ratios are typically 2.0:1 to 3.0:1, and frost line height is maintained at 6–10 die diameters for balanced tear performance. Output rates on single-screw lines without internal bubble cooling commonly fall between 0.5 kg/h/mm and 1.2 kg/h/mm of die circumference, while internal bubble cooling can extend output to 1.5 kg/h/mm or higher if the air ring and die are matched for the resin viscosity. Sharkskin or melt fracture onset is associated with wall shear stress above approximately 0.14 MPa; processing aid masterbatches based on fluoroelastomers can extend stable output by 10–30% at the same die gap. The specific influence of Bapolene® 155FP on output limits depends on lot melt flow index, die lip condition, and the use of polymer processing aid.

    Additive selection for Bapolene® 155FP is governed by the end-use requirement and by the potential for plate-out on the die lip. Slip and antiblock masterbatches are added at controlled levels, typically not exceeding 5 wt% total for monolayer food-contact films, because excessive antiblock reduces gloss and increases haze. Fluoroelastomer processing aids are used at 400–800 ppm when melt fracture limits output or when die gap reduction is required for gauge control. The resin should not be combined with unsaturated or highly acidic additive packages without testing, because acidic residues can interfere with stabilizer performance and contribute to corrosion on chrome-plated die surfaces. Food-contact applications require confirmation that the final formulation meets FDA 21 CFR 177.1520 and applicable regional migration limits, including EU Regulation 10/2011, with compliance demonstrated on the finished package rather than on the neat resin alone.

    When Metallocene LLDPE Replaces Conventional Ziegler-Natta Hexene Grades in Coextruded Films

    Substitution of a metallocene-catalysed LLDPE for a conventional hexene extrusion grade such as Bapolene® 155FP is not a drop-in change. Metallocene resins typically exhibit narrow molecular weight distribution and lower melt strength, which can require a reduction in blow-up ratio from 3.0:1 to 2.0:1 and a lower frost line height to maintain bubble stability. Seal initiation temperature may drop by 5–15°C under ASTM F88/F88M-21, but equipment torque and motor load may also decline because of reduced shear viscosity at comparable melt index. In coextruded structures, the higher melt strength of a conventional hexene grade can provide wider processing latitude in the skin layer, especially when the core layer is high-density polyethylene or regrind-rich material. Published data for Bapolene® 155FP in tri-layer machine-direction-oriented film configurations is limited; line trials are required when changing catalyst families.

    Regrind utilization on high-output blown-film lines is commonly limited to 10–30% of the total feedstock. Higher regrind fractions can reduce dart impact and increase gel count, particularly when the regrind contains print ink, paper fibre, or oxidized film edge trim. Screen packs of 100–200 mesh are recommended to capture gel and foreign material without creating excessive melt temperature rise. The material should be stored below 40°C, away from direct ultraviolet exposure, and should be kept dry. Although LLDPE does not require predrying at ambient relative humidity below 60%, condensation on cold pellet surfaces can introduce surface moisture that contributes to bubble pinholes or melt pressure variation. Silo or gaylord unloading systems should be purged with dry air when ambient dew point exceeds 15°C.

    Which Compliance Standards Govern Food Contact and Transportation Packaging?

    Table 2: Compliance standards and regulatory frameworks applicable to LLDPE hexene extrusion grades in packaging
    Standard or regulationDesignationScope and applicability to Bapolene® 155FP
    U.S. food contactFDA 21 CFR 177.1520Olefin polymers for food contact; final package compliance must be confirmed by the converter.
    European food contactEU Regulation 10/2011Plastics intended for food contact; migration testing applies to the finished package.
    Melt flow indexASTM D1238-20Melt flow rate at 190°C/2.16 kg for lot verification.
    DensityASTM D1505-18Solid-state density for grade identification and lot acceptance.
    Film tensile propertiesASTM D882-18Tensile strength, elongation, and modulus for blown film.
    Elmendorf tearASTM D1922-15Machine-direction and transverse-direction tear resistance.
    Dart impactASTM D1709-16aFree-falling dart impact for film toughness.
    REACHRegulation (EC) 1907/2006Registration and SVHC reporting obligations for monomers and additives.

    The material designation does not by itself establish compliance for a finished package. A converter must verify that the specific lot, additive package, and processing history meet the conditions of use required under FDA 21 CFR 177.1520 or EU Regulation 10/2011. For transportation packaging outside food contact, the principal specification is mechanical toughness under ASTM D1709-16a and ASTM D1922-15, while environmental compliance may require REACH and RoHS declarations only when the package is placed into electrical or electronic equipment supply chains.

    Top