Bamberger Polymers Bapolene 152p Lldpe Hexene Extrusion Grade

Bamberger Polymers Bapolene® 152P LLDPE, Hexene Extrusion Grade

    • Product Name: Bamberger Polymers Bapolene® 152P LLDPE, Hexene Extrusion Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 203821
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 20.7 MPa
    Elongation At Break 700%
    Flexural Modulus 0.207 GPa
    Vicat Softening Point 100 °C
    Melting Point 120 °C
    Brittleness Temperature <= -70 °C
    Hardness Shore D 50
    Environmental Stress Crack Resistance Escr >1000 h

    As an accredited Bamberger Polymers Bapolene® 152P LLDPE, Hexene Extrusion Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bapolene® 152P LLDPE, Hexene Extrusion Grade is supplied in 25 kg polyethylene-lined bags on pallets; 1,000 kg bulk bags are also available.
    Container Loading (20′ FCL) 20′ FCL: 25 kg bags, 55 bags/pallet, 14 pallets, approximately 19.25 MT net, loaded in a dry container.
    Shipping Bamberger Polymers Bapolene® 152P LLDPE, Hexene Extrusion Grade, is shipped as non-hazardous thermoplastic pellets, typically in 25 kg bags or bulk containers on pallets. It is not DOT/IMDG/IATA regulated and has no UN number. Store and transport in a cool, dry area away from direct sunlight and heat.
    Storage Store Bapolene® 152P LLDPE in a cool, dry, well-ventilated area, preferably in original sealed bags or containers. Protect from direct sunlight, moisture, heat, ignition sources, and ultraviolet exposure. Keep away from oxidizers and contaminants. Maintain clean, organized stock using first-in, first-out rotation. Avoid prolonged storage above recommended temperatures to prevent pellet degradation or blocking.
    Shelf Life Shelf life is typically 24 months when stored cool, dry, in original unopened packaging, away from direct sunlight and contaminants.
    Application of Bamberger Polymers Bapolene® 152P LLDPE, Hexene Extrusion Grade
    In blown film operations producing heavy-duty shipping sacks, industrial liners, and heat-sealed carrier bags, Bapolene 152P enters the feed throat as a pellet blend with a long-chain-branched LDPE. The LDPE addition is normally maintained between 15 wt% and 30 wt%, because the hexene LLDPE alone exhibits lower melt tension than LDPE and can produce bubble flutter on high-output dies. On a grooved-feed extruder with L/D 30:1–32:1 and a barrier screw designed for LLDPE, melt temperature is held at 200 °C–220 °C, and the die gap is set at 1.8–2.4 mm to limit melt fracture. A blow-up ratio of 2.2:1–2.8:1 and a frost line height 6–9 die diameters above the air ring are commonly used for 40–80 μm film. The hexene short-chain branching pattern raises the dart impact and Elmendorf tear of the film relative to a butene LLDPE of similar melt index and density; however, downgauging below 30 μm without raising the LDPE fraction to at least 20 wt% can cause bubble instability at line speeds above 60 m/min. Tensile properties are measured according to ASTM D882-18 or ISO 527-3:2018, dart impact according to ASTM D1709-16 Method A, and Elmendorf tear according to ASTM D1922-15 or ISO 6383-2:2015. For non-food industrial sacking, REACH SVHC reporting applies above 0.1 wt% per substance. When the same sack is intended for dry food contact, the finished monolayer must satisfy the extractives and end-use limits in FDA 21 CFR 177.1520(c) and the overall migration limit of 10 mg/dm² under Regulation (EU) No 10/2011. Failure modes observed on production lines include die-lip buildup from oxidized regrind and gauge bands caused by air-ring turbulence; both are reduced by keeping total recycled content at or below 25 wt% and by using an internal bubble cooling system. The end product is a finished sack or liner with side gussets and punched handle holes, typically heat-sealed at 140 °C–160 °C jaw temperature.
    Representative 40 μm blown film property ranges for 0.918 g/cm³ hexene LLDPE blended with LDPE; not product-specific and not a sales specification.
    LDPE addition (wt%)Dart impact Method A (ASTM D1709-16) (g)Elmendorf tear MD (ASTM D1922-15) (N/mm)Elmendorf tear TD (ASTM D1922-15) (N/mm)
    0120–16012–1514–18
    15110–14011–1414–17
    20100–13010–1313–16
    3090–1209–1213–16

    What Changes in Cast Stretch Film When Hexene LLDPE 152P Is Used with Edge Trim Recovery?

    In cast stretch film production for pallet unitization, the shift to a hexene LLDPE affects the balance between stretch force, cling, puncture, and gauge uniformity differently than in blown film. Bapolene 152P is extruded on a slot-die line with a 0.6–0.8 mm die gap and a melt temperature of 240 °C–260 °C, with the primary chill roll held at 15 °C–25 °C. The resin is often dry-blended with 10–20 wt% of a metallocene LLDPE or an ethylene-vinyl acetate copolymer containing 12–18 mol% vinyl acetate to adjust cling and puncture. Edge trim recovery is direct: because cast film edge trim is chopped and returned to the extruder, the resin must tolerate repeated shear and heat history. In practice, hexene LLDPE grades of this class do not generate excessive gel when regrind is kept at or below 30 wt% of the feed, provided the recyclate stream passes through a melt filter with 100–150 μm screens. Above 30 wt% regrind, stretch force measured at 200% elongation may increase, and gauge bands can develop if the melt pressure fluctuates. The water-fall edge encapsulation system is preferred because it keeps edge trim free of processing oils and dust. Cling is measured according to ASTM D5458-95(2020), puncture resistance according to ASTM D5748-19, and tensile stretch force according to ASTM D882-18. The film is typically down-gauged to 12–20 μm in machine wrap and 20–35 μm in hand wrap, with pre-stretch ratios in application equipment commonly limited to 200–250% for this type of hexene LLDPE blend. Published data for Bapolene 152P-specific cast performance is limited; the processing envelope above is taken from general hexene LLDPE extrusion grades of similar melt index and density. The end products are pallet-wrapping films with differential slip or one-sided cling, and the operational boundary is the onset of draw resonance at line speeds above approximately 600 m/min unless a small LDPE fraction is added to improve melt strength.

    Extrusion Coating of Woven Polypropylene and Kraft Paper for Industrial Flexible Packaging

    Extrusion coating with Bapolene 152P requires a different set of conditions from cast film because of the drawdown length between the die exit and the substrate nip. The melt temperature is raised to 285 °C–305 °C to promote oxidation and adhesion to primed surfaces, and the die gap is held at 0.5–0.8 mm. The resin is normally blended with 20–30 wt% LDPE to increase neck-in stability and reduce draw resonance; without that modification, the low melt tension of the hexene LLDPE produces excessive neck-in at air gaps above 120 mm. The extruder is typically a single-screw machine with L/D 28:1–32:1 and a compression ratio near 2.5:1. The air gap is maintained at 100–180 mm, and the substrate is either corona-treated woven polypropylene or a kraft paper with a pre-applied primer. The coating weight is set between 15 g/m² and 25 g/m² for woven PP sacks, and between 20 g/m² and 40 g/m² for multi-wall kraft constructions requiring a moisture barrier. When direct adhesion to an unprimed or low-dyne woven PP substrate is insufficient, a coextrudable tie layer or an ozone treatment is interposed; this is a known operational boundary rather than a fault of the resin. End-use compliance for packaging of dry food or industrial powders follows FDA 21 CFR 177.1520(c) for the olefin layer, and the overall migration limit in Regulation (EU) No 10/2011 is 10 mg/dm². The finished structures are woven polypropylene outer bags with a heat-sealable LLDPE inner coating, or multi-wall paper sacks with an outer moisture barrier. Heat seal strength is commonly evaluated by ASTM F88/F88M-21 on 25 mm strips after sealing at 160 °C–180 °C jaw temperature. The primary production failure is pinholing when coating weight is below 15 g/m² on low-basis-weight substrates; raising the melt temperature above 310 °C causes odor and degradation of the hexene LLDPE. Therefore, the process window is 285 °C–305 °C and must be controlled within ±10 °C to avoid both adhesion loss and off-gassing.
    Compliance matrix for converted articles containing Bapolene 152P in flexible packaging applications.
    Regulation/StandardScopeKey Value/Condition
    FDA 21 CFR 177.1520(c)Olefin polymers for food contactSubject to extractives and intended-use conditions
    Regulation (EU) No 10/2011Plastics in food contactOverall migration 10 mg/dm²
    REACH Article 33 / Annex XVIISVHC reporting and restriction0.1 wt% per SVHC threshold
    ASTM D1238-20 / ISO 1133-1:2022Melt-flow verification190 °C/2.16 kg

    When Silage Film Needs a 2.2:1 Blow-Up Ratio Without Sacrificing Dart Impact

    In agricultural bale-wrap and silage cover film, Bapolene 152P is processed on a blown film line with a die gap of 1.6–2.2 mm and a blow-up ratio of 2.2:1–2.5:1. The melt temperature is kept at 205 °C–225 °C because higher temperatures reduce bubble stability and can degrade the UV stabilizer package. The formulation is usually a blend of 60–75 wt% hexene LLDPE, 20–35 wt% metallocene LLDPE, and 2–4 wt% carbon black or opaque white masterbatch containing hindered amine light stabilizers. The film is produced at 25–30 μm thickness for silage bales and 30–40 μm for silage pit covers. Puncture resistance is measured under ASTM D5748-19, Elmendorf tear under ASTM D1922-15, and outdoor weathering under ASTM G154-16 or ISO 4892-2:2021. A common target for this type of film is a puncture resistance above 2.5 J on a 25 μm sample, and the hexene branch architecture supports that without increasing film thickness to butene-LLDPE levels. The operational boundary is roll blocking: if the metallocene content exceeds 35 wt%, the film surface can develop blocking during storage in warm barns. Conversely, below 20 wt% metallocene, the cling and tack necessary for bale wrap are insufficient. The finished product is a round-bale stretch film with one black or white outer layer and a tackified inner surface; when colored masterbatch is used, the heavy metals and polycyclic aromatic hydrocarbon content must comply with REACH Annex XVII restrictions. No food-contact status is required, but the packaging of silage is governed by national agricultural film regulations; published data for this specific Bapolene 152P formulation is limited, so production validation is recommended for UV stabilizer interaction.In coextruded barrier films for frozen food and coffee packaging, Bapolene 152P is used as a heat-seal skin layer at 10–20 wt% of the total film thickness. The skin layer is processed through an outer extruder at 210 °C–230 °C, while the core barrier layer may contain polyamide or EVOH. The low sealing initiation temperature of the hexene LLDPE allows fin-seal and lap-seal operations at 120 °C–140 °C, measured by ASTM F88/F88M-21 on 25 mm strips. The layer ratio must be controlled to avoid delamination: if the skin layer exceeds 25% of the total structure, the oxygen barrier of the EVOH core is diluted and the film may fail the oxygen transmission rate target of 2 cm³/(m²·day) measured by ASTM D3985-17. The finished products are vacuum pouches and coffee bags with a seal strength above 15 N/25 mm. Compliance for direct food contact requires FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011. The primary operational boundary is the mismatch in melt viscosity with EVOH; a tie layer is mandatory, and the skin layer must be purged during shutdown to avoid thermal degradation in the die. Published data for this specific Bapolene 152P layer configuration is limited, and the oxygen transmission values are supplied as industrial targets rather than product-specific guarantees.
    Free Quote

    Competitive Bamberger Polymers Bapolene® 152P LLDPE, Hexene Extrusion Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bapolene® 152P is a linear low-density polyethylene produced by ethylene copolymerization with 1-hexene. The product is supplied as a pelletized extrusion grade and is identified in Bamberger Polymers literature as an LLDPE hexene extrusion resin for blown and cast film. Its short-chain branch distribution differs from butene-based LLDPE because the C6 comonomer creates longer side branches and a higher concentration of interlamellar tie chains at equivalent density. This morphological difference influences solid-state toughness, tear resistance, and downgauging behavior in thin film. The resin is specified for packaging and industrial film where puncture and dart impact resistance are limiting performance variables, rather than for injection molding or blow molding. The nominal pellet geometry and stabilizer package are intended for general-purpose film extrusion under normal thermal exposure.

    Which Nominal Melt Index, Density, and Thermal Values Govern Incoming-QC Screening?

    Lot conformance for Bapolene 152P is evaluated against supplier-published typical values rather than universal specification limits. The values in Table 1 represent nominal release data found in product data summaries and must be confirmed against the current certificate of analysis for each shipment. These are not quarantine or acceptance limits unless the converter’s incoming quality procedure establishes such limits independently.

    Table 1: Supplier-published nominal properties for Bapolene 152P
    PropertyTest methodNominal valueUnit
    Melt mass-flow rateASTM D1238-20 / ISO 1133-1:20221.0g/10 min
    Nominal densityASTM D1505-18 / ISO 1183-1:20190.920g/cm³
    DSC peak melting pointASTM D3418-15123°C
    Comonomer typeFTIR/internal polymer characterization1-hexene—
    Additive packageSupplier dataAntioxidant; no slip or antiblock unless specified—

    The melt mass-flow rate is measured under a load of 2.16 kg at 190 °C. The density value is determined after compression-molded specimen conditioning at 23 °C. Processors performing die simulation should not rely only on melt index; lot-specific capillary rheometry should be requested from the supplier if screw design or high-output modeling requires apparent viscosity data at multiple shear rates.

    Because the nominal melt-index is 1.0 g/10 min, Bapolene 152P behaves as a medium-viscosity extrusion resin. At wall shear rates above 200 s⁻¹, similar Ziegler-Natta hexene LLDPEs exhibit pronounced shear-thinning and lower apparent viscosity than high-pressure LDPE of equal melt index. This response reduces screw torque in long-barrier screws but can still require higher drive amperage than a butene LLDPE of equal density if the extruder lacks a grooved-feed or barrier section. In blown-film production, the resin’s extensional melt strength is lower than LDPE; bubble stability is maintained by internal bubble cooling, reduced die gaps, or blending with high-pressure LDPE when line speeds exceed 80 m/min.

    Blown and Cast Film Extrusion Windows for Bapolene 152P

    For blown-film extrusion, melt temperature at the die is commonly set between 190 °C and 215 °C. The die gap is typically held at 1.5–2.5 mm to increase draw-down and reduce melt fracture. A blow-up ratio of 2.0:1 to 3.0:1 balances dart impact and tear anisotropy. Frost-line height is adjusted to 5–8 die diameters; shorter frost lines reduce optical haze but freeze in higher molecular orientation. Table 2 lists a starting barrel-zone profile for a single-screw extruder with L/D 24:1 to 30:1 and a barrier screw.

    Table 2: Starting extrusion profile for blown-film processing of Bapolene 152P
    ZoneSet rangeFunction
    Feed throat30–50 °CHopper cooling and pellet bridging prevention
    Barrel zone 1170–185 °CSolids conveying and initial melting
    Barrel zone 2180–195 °CCompression and completion of melting
    Barrel zone 3190–200 °CHomogenization and pressure generation
    Adapter and die190–210 °CMelt temperature uniformity
    Melt temperature target190–215 °CAvoid oxidative yellowing and preserve bubble integrity

    Cast film lines generally run 10–20 °C higher than blown-film lines to reduce melt fracture and improve gauge uniformity, but web neck-in may increase. On blown-film towers with 300–500 kg/h throughput, Bapolene 152P may exhibit higher extrusion pressure than high-pressure LDPE at the same screw speed because of its narrower molecular weight distribution and higher molecular weight tail. Operators often observe a die pressure increase of 5–15 bar when transitioning from LDPE to hexene LLDPE without temperature adjustment. Raising the rear barrel temperature by 5–10 °C and allowing the screw to reach a new thermal equilibrium reduces pressure fluctuation. Melt fracture at the die lip appears as surface roughness at high output; eliminating it requires increasing die temperature, widening the die gap, or adding a fluoropolymer processing-aid masterbatch. These field observations are specific to stable, non-surging pellet feed and should not be generalized to alternative screw designs without trial.

    At the analytical level, the oxidation induction time of Bapolene 152P is governed by the manufacturer’s stabilizer package. Converters adding high levels of recycled film or color concentrate should verify oxidative stability using ASTM D3895 or isothermal DSC according to ASTM D3350. The resin is not formulated as a UV-stabilized agricultural film grade, so long-term outdoor exposure requires addition of hindered amine light stabilizers and UV absorbers at let-down ratios established by the masterbatch supplier. Exposure to strong oxidizing acids can increase carbonyl formation and reduce mechanical integrity, although chlorine-based sanitation systems used in food processing are not normally a concern for polyethylene.

    When Hexene LLDPE Replaces Butene LLDPE or LDPE in Toughness-Critical Film

    Bapolene 152P is selected over butene-based LLDPE when puncture and dart impact strength determine packaging performance. For equivalent density and melt index, hexene LLDPE resists slow crack propagation more effectively because the 1-hexene branches increase the probability of interlamellar tie chains. The trade-off can be a slight increase in film haze compared with an LDPE-rich blend; however, downgauging may offset resin cost because the hexene grade retains dart impact at lower thickness. Published data for this specific configuration is limited; direct comparisons must be generated on the target film line using ASTM D1709-15ae1 for dart drop and ASTM D1922-15 for Elmendorf tear.

    Compared with high-pressure LDPE, Bapolene 152P has a narrower molecular weight distribution and no significant long-chain branching. This composition gives lower melt elasticity and lower bubble stability when run as a neat resin, but it provides higher elongation at break and greater slow-puncture resistance. In low-density blends containing 20–30% LDPE, the LDPE component raises extensional viscosity and stabilizes the bubble without eliminating the LLDPE toughness contribution. Compared with metallocene-catalyzed hexene LLDPE, Bapolene 152P is manufactured with conventional Ziegler-Natta catalysis; its molecular weight distribution is broader, which improves screw conveying and reduces melt pressure but can produce slightly lower dart impact and gloss than a metallocene grade of equivalent density. The choice between Ziegler-Natta and metallocene hexene LLDPE should therefore be driven by the converter’s equipment capability and the end-use test specification rather than by a single resin property.

    Film coefficient of friction is not fixed by the base resin because Bapolene 152P is supplied without slip or antiblock unless otherwise stated. Surface COF is controlled by adding slip agents, antiblock concentrates, or processing aids. Testing should be performed according to ASTM D1894-14 after film conditioning because migration of slip additives is time- and temperature-dependent.

    Regulatory Compliance, Chemical Resistance, and Handling Boundaries

    Food-contact status must be verified with the supplier’s regulatory letter. For LLDPE resins of this type, United States compliance is normally based on FDA 21 CFR 177.1520(c); the specific subparagraph for Bapolene 152P should be confirmed against the current product stewardship documentation. European food-contact evaluations are performed under Commission Regulation (EU) No 10/2011 and its amendments; overall migration testing should follow the food-simulant conditions assigned by the intended use. The resin is subject to REACH registration and does not contain substances intentionally added at levels requiring SVHC communication according to the supplier’s current safety data sheet.

    Bapolene 152P shares the solvent resistance profile of general-purpose LLDPE. It is resistant to aqueous acids, alkalis, and polar solvents at room temperature but may be swollen or stress-cracked by aliphatic and aromatic hydrocarbons, chlorinated solvents, and some mineral oils. Environmental stress-crack resistance in detergent or surfactant-containing environments should be assessed using ASTM D1693-15e1 under representative stress and temperature conditions. The grade is not formulated for prolonged continuous service above 60 °C, and thin film exposed to oxidizing environments may require additional stabilizer if the converter adds recycled content.

    LLDPE pellets do not require forced drying unless surface moisture is introduced during open storage. Pre-drying at 60–70 °C for 2 hours reduces surface moisture defects if condensation is visible; higher temperatures can lead to pellet agglomeration. Pellets should be stored away from direct sunlight and protected from UV-induced molecular weight degradation.

    Typical end-use applications include heavy-duty sacks, stretch film outer layers, agricultural film, and laminations where hexene-toughened LLDPE replaces butene grades. In cast stretch film, Bapolene 152P can serve as a skin or core layer depending on cling and release additive masterbatches; in agricultural film, it is blended with LDPE and HDPE to adjust thermal retention and mechanical properties. The final film property set is controlled more by die gap, blow-up ratio, frost-line height, and additive loading than by resin selection alone.

    Top