    HS Code 972501
    Product Name Bamberger Polymers Bapolene® 152FP LLDPE, Hexene Extrusion Grade
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene
    Density 0.918 g/cm³
    Melt Index 1.0 g/10 min
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 20.7 MPa
    Elongation At Break 700%
    Flexural Modulus 0.586 GPa
    Vicat Softening Point 93 °C
    Brittleness Temperature -76 °C
    Hardness Shore D 55
    Haze 10%
    Gloss 60
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 400 g
    Processing Method Extrusion

    As an accredited Bamberger Polymers Bapolene® 152FP LLDPE, Hexene Extrusion Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 152FP LLDPE, Hexene Extrusion Grade, is packaged in 25 kg polyethylene bags, 40 bags per stretch-wrapped pallet.
    Container Loading (20′ FCL) 20′ FCL: 20 MT (800 × 25 kg bags) of Bamberger Polymers Bapolene® 152FP LLDPE, Hexene Extrusion Grade.
    Shipping Bapolene® 152FP LLDPE ships as non-hazardous polyethylene pellets, typically in 25 kg moisture-resistant bags or 1,000 kg bulk sacks on pallets. Transport in clean, covered trucks/trailers at ambient temperature; avoid heat, sunlight, moisture, and contamination. No special DOT/IMDG placards required. Follow local regulations and keep containers sealed until use.
    Storage Store Bapolene® 152FP LLDPE in a cool, dry, well-ventilated warehouse. Keep in original unopened bags or containers, elevated on pallets, away from direct sunlight, heat, sparks, flames, moisture, and strong oxidizers. Avoid dust accumulation and contamination. Maintain ambient temperatures, protect from prolonged UV exposure, and follow first-in, first-out inventory practices. Ensure bags are sealed and stack safely to prevent damage.
    Shelf Life Shelf life is typically 24 months from manufacture when stored unopened in a cool, dry, ventilated area away from sunlight.
    Application of Bamberger Polymers Bapolene® 152FP LLDPE, Hexene Extrusion Grade
    Application matrix for Bapolene® 152FP hexene LLDPE extrusion grade
    Downstream scenarioTypical addition ratioProduction windowPrimary compliance and test standards
    Heavy-duty industrial shipping sacks and drum liners70–85 wt%Blown film, BUR 2.5:1–3.2:1, 190–230°C, L/D 24:1–30:1ASTM D1709, ISO 527-3, ASTM D1922, EU 94/62/EC
    Agricultural greenhouse, silage, and mulch film80–90 wt%3-layer blown film, BUR 2.0:1–2.8:1, 180–210°CEN 13206, ISO 4892-2, ISO 6383-2
    Cast stretch film60–85 wt%3-layer cast die, 0.5–0.8 mm gap, 15–25°C chill roll, 200–500 m/minASTM D5748, ASTM D5459, ASTM D1922
    Food-contact flexible packaging60–80 wt%3/5-layer blown or cast coextrusion, 190–230°CFDA 21 CFR 177.1520, EU 10/2011, EN 1186-1
    LLDPE geomembrane sheet88–94 wt%Flat-die sheet, 0.5–2.0 mm, 200–230°CGRI-GM17, ASTM D6693, ASTM D1004, ASTM D5397, ASTM D3895

    In blown film operations producing 80–200 µm heavy-duty industrial shipping sacks, Bapolene® 152FP is introduced at 70–85 wt% as the primary hexene-based LLDPE, with 15–25 wt% high-pressure LDPE at 0.2–0.8 g/10 min (ASTM D1238, 190°C, 2.16 kg) added to raise bubble stability. The extrusion line is specified with a 24:1–30:1 L/D barrier screw, die diameter 200–350 mm, die gap 1.8–2.4 mm, and dual-lip air ring; the operating condition is BUR 2.5:1–3.2:1 with frost line height 500–900 mm and melt temperature 190–230°C. Compliance is assessed under EU Directive 94/62/EC Annex II, where combined lead, cadmium, mercury, and hexavalent chromium are limited to ≤100 mg/kg, and under REACH Regulation (EC) No 1907/2006 for SVHC notification. Mechanical acceptance is measured by ASTM D1709 drop dart impact, ISO 527-3 tensile, and ASTM D1922 Elmendorf tear. Finished goods include heat-sealed heavy-duty shipping sacks for 25–50 kg dry bulk, industrial drum liners, and flexible intermediate bulk container inner liners.

    Greenhouse and silage cover films formulated at 80–90 wt% hexene LLDPE shift failure toward UV-embrittlement thresholds.

    Three-layer blown film lines running this grade for agricultural covers dose 80–90 wt% Bapolene® 152FP, 8–15 wt% UV/HALS masterbatch, and 2–6 wt% tackifier or cling masterbatch for silage structures. The stabilizer package is selected to meet EN 13206 weathering requirements, with laboratory exposure under ISO 4892-2; mechanical tracking uses ISO 527-3 tensile and ISO 6383-2 trouser tear. Extrusion equipment is configured with die diameter 250–400 mm, die gap 1.6–2.2 mm, BUR 2.0:1–2.8:1, melt temperature 180–210°C, and frost line height 400–800 mm. Gravimetric dosing is used rather than tumble mixing because HALS concentration variation greater than ±15% across the web can create localized early cracking under ISO 4892-2. Finished product types include 100–200 µm silage bags, 150–200 µm greenhouse covering film, 80–150 µm low tunnel film, and 15–30 µm short-cycle mulch film.

    What limits machine-direction tear in 15–25 µm cast stretch film when 152FP is blended with metallocene LLDPE?

    Cast stretch film lines running 15–25 µm webs use 60–85 wt% Bapolene® 152FP, 15–40 wt% metallocene LLDPE or VLDPE with density 0.902–0.912 g/cm³ (ASTM D1505), and 1–3 wt% tackifier masterbatch. The cast line is set with a three-layer die gap of 0.5–0.8 mm, melt temperature 220–250°C, chill roll temperature 15–25°C, and line speed 200–500 m/min. Cling and stretch force are measured under ASTM D5748 and ASTM D5459; tensile properties are tested under ISO 527-3, and tear resistance under ASTM D1922. The target pre-stretch ratio at winding is 150–250%; edge trim recycled at 5–15 wt% is accepted only when melt filtration below 250 µm is installed to prevent edge fold breakage. Finished product types include hand stretch film, machine stretch film, and agricultural baling stretch film.

    For dry-food and frozen-food flexible packaging, the sealant layer incorporating Bapolene® 152FP is formulated at 60–80 wt% with 20–40 wt% LDPE or metallocene LLDPE to adjust seal initiation, plus 2–4 wt% slip/antiblock masterbatch and 0.2–0.5 wt% polymer processing aid. Food-contact suitability is evaluated under FDA 21 CFR 177.1520 for olefin polymers and under Commission Regulation (EU) No 10/2011; overall migration is controlled to 10 mg/dm² or 60 mg/kg using the simulant assignments in Annex III, with testing according to EN 1186-1. The structure is produced as a 3-layer or 5-layer coextruded blown film on dies of 200–400 mm diameter, die gap 1.4–2.0 mm, BUR 2.0:1–2.8:1, and melt temperature 190–230°C; cast coextrusion variants use chill roll temperatures of 10–20°C. Finished goods include 40–100 µm frozen fruit and vegetable bags, bakery film, cereal pouch liners, and salt or sugar pouch webs.

    When flat-die geomembrane extrusion exceeds 1.5 mm, edge tear and oxidative induction time govern field acceptance.

    Flat-die geomembrane lines producing 0.5–2.0 mm sheet from this hexene LLDPE grade are operated with 88–94 wt% Bapolene® 152FP, 6–10 wt% carbon black masterbatch to achieve 2–3 wt% carbon black, and 0.5–1.5 wt% antioxidant/processing stabilizer package. The flat-die gap is 1.5–2.5 mm, melt temperature 200–230°C, and the polishing roll stack is temperature-controlled. Sheet thickness at 1.5–2.0 mm is the main production control because GRI-GM17 tensile and tear specimens require full-thickness coupons; thickness below 1.0 mm is reserved for temporary cover applications. Geomembrane acceptance follows GRI-GM17, with tensile properties per ASTM D6693, tear resistance per ASTM D1004, notched constant tensile load per ASTM D5397, oxidative induction time per ASTM D3895, and seam peel adhesion per ASTM D6392. Because published long-term oxidative performance data for this specific grade in geomembrane service is limited, lot-specific OIT and notched constant tensile load testing are used as acceptance controls. Finished product types include landfill caps, decorative pond liners, aquaculture containment, and secondary containment liners.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 152FP LLDPE, Hexene Extrusion Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bamberger Polymers supplies Bapolene® 152FP as a linear low-density polyethylene resin with a hexene comonomer, produced for cast and blown film extrusion. The grade carries a nominal density of 0.920 g/cm³ when measured under ASTM D1505 and a nominal melt flow rate of 1.0 g/10 min under ASTM D1238 at 190°C/2.16 kg. The hexene branch distribution, relative to butene-based LLDPE, raises the concentration of load-bearing tie molecules across adjacent lamellae; this shift is observed in higher dart impact values under ASTM D1709 and improved low-temperature ductility under ASTM D746. As a pelletized extrusion grade, it is typically processed on single-screw lines with L/D ratios between 24:1 and 30:1, and it is suited to blown film structures with gauges from 25 µm to 150 µm where puncture resistance and tear balance are specified. Release limits, slip and antiblock additive loadings, and lot-specific melt flow rates should be confirmed against the producer’s certificate of analysis before line qualification.

    Material Identity, Specification Limits, and Regulatory Baseline

    Material identity is defined by the combination of density, melt flow rate, comonomer type, and molecular architecture. The nominal 0.920 g/cm³ density places the resin in the lower-density region of the LLDPE range, which limits crystalline fraction and improves clarity relative to 0.935 g/cm³ grades. The melt flow rate of 1.0 g/10 min is low enough to maintain melt strength in high-stalk bubbles, but high enough to avoid excessive head pressure on 24:1 to 30:1 L/D extruders at 200°C to 220°C melt temperature. In the United States, the base resin may fall within olefin polymers listed in 21 CFR 177.1520(c), but final food-contact articles require extraction or end-testing against the specific condition of use. In the European Union, compliance is assessed under Regulation (EU) No 10/2011 and its amendments, with overall migration limits of 10 mg/dm² for plastic materials intended for food contact; migration testing must be conducted on the finished structure, not the pellet alone. Grade-specific data concerning heavy metal content, slip additive, or antiblock type should be obtained from the applicable safety data sheet and product data sheet because customer-specific letdowns may alter regulatory status.

    How Does Hexene Comonomer Distribution Shift Tear and Puncture Mechanics?

    In LLDPE, short-chain branches act as defects that limit lamellar thickness and reduce density. A hexene-derived branch contains six carbon atoms, compared with the two-carbon branch from butene; the longer branch is more effective at excluding comonomer from the crystal lattice and promoting tie-molecule formation. Under ASTM D1709 dart impact testing at 38 µm gauge, the result is generally a higher failure energy before film puncture than an equivalent butene copolymer of 0.920 g/cm³ density and 1.0 g/10 min melt flow rate. Elmendorf tear resistance measured by ASTM D1922 often shows lower machine-direction tear for highly oriented films, but improved transverse-direction tear and slower crack growth due to the tie-molecule network. The low-temperature brittleness value under ASTM D746 is commonly targeted below -40°C for liners and agricultural film exposed to freezing environments; however, the user should verify the exact value on the certificate of analysis because comonomer distribution can vary between production campaigns.

    On high-stalk blown film lines equipped with 24:1 to 30:1 L/D barrier screws, the principal process conflict lies between bubble stability and gauge uniformity below 25 µm. When melt temperature falls below 199°C, the resin may exhibit increased head pressure and reduced homogeneity at high screw speeds; when melt temperature exceeds 232°C, oxidation gel formation and gel counts rise. A die gap of 1.8 mm to 2.5 mm and a blow-up ratio of 2.0:1 to 3.0:1 provide a practical starting point. On dual-lip air ring and internal bubble cooling systems, a stalk height of 400 mm to 700 mm generates sufficient orientation for physical property development, but stalk heights above 800 mm can lead to machine-direction tear loss under ASTM D1922. Frost line height should be controlled as a secondary variable rather than the primary setpoint because ambient air temperature and line speed shift the apparent solidification point. Extruder barrel profiles from 180°C in the feed throat to 210°C in the metering zone are typical when processing at output rates up to the screw manufacturer’s torque limit. If gauge variation exceeds ±5%, the first corrective action is to verify die centering and air ring pressure distribution, not to increase melt temperature.

    When Cast Film Lines Demand Low Neck-In and Rapid Quench

    In cast film, the molten web is quenched against a chill roll rather than oriented in a bubble. The low melt flow rate of 1.0 g/10 min generates higher neck-in and potential draw resonance at high draw ratios. On a cast line with 30:1 L/D extruder and 0.6 mm to 0.8 mm die gap, melt temperatures of 232°C to 260°C are used to reduce shear stress and stabilize the web. The die-to-chill-roll gap should be minimized, typically to 10 mm to 20 mm, while a venturi or air knife positioned at 45° to 60° relative to the web assists edge pinning. Chill roll temperatures of 21°C to 32°C increase clarity, but condensation must be avoided when ambient humidity exceeds 60% due to surface frost formation. Draw resonance appears as periodic gauge bands in the machine direction; it is suppressed by reducing line speed, lowering melt temperature, increasing die gap, or moving the air knife closer to the die. Neck-in below 50 mm per edge is achievable on narrow laboratory lines, but production lines may show higher values depending on die width and draw distance. The grade is not specifically formulated for extrusion coating onto porous substrates, and adhesion to paper or board should not be assumed without a separate adhesion-promoting layer or oxidized surface treatment.

    Regulatory Assessment Matrix for Extruded Film Structures

    Regulation or standard Designation / clause Assessment basis
    US FDA olefin polymers 21 CFR 177.1520(c) Base resin within olefin polymer listing; final article extraction testing required
    EU food contact plastics Regulation (EU) No 10/2011 Overall migration limit 10 mg/dm²; specific migration limits depend on additives
    Melt flow rate ASTM D1238 190°C/2.16 kg; nominal 1.0 g/10 min; certificate of analysis controls release limits
    Density ASTM D1505 Nominal 0.920 g/cm³; lot-specific variation confirmed
    Tensile properties ASTM D882 Film property testing after fabrication, not pellet property
    Dart impact ASTM D1709 Gauge-dependent; report method A/B and film gauge

    Comparative performance against a butene-based LLDPE is material at the same density and melt flow rate because butene grades often show lower incipient dart impact and lower transverse-direction tear. However, hexene grades typically exhibit a wider processing window for thin-gauge films due to better melt strength, though they may require slightly higher extruder torque. The choice between a hexene grade and an octene-based solution metallocene polyethylene depends on the required seal initiation temperature, hot tack strength, and optics; those properties are controlled by molecular weight distribution and comonomer distribution as well as by comonomer length. For Bapolene® 152FP, the absence of very high clarity claims is significant: blow-up ratio, frost line height, and die gap must be controlled to prevent haze caused by surface roughness and melt flow instabilities. When optical clarity below 10% haze under ASTM D1003 is required, the film should be fabricated on cast equipment with chilled rolls rather than blown film towers.

    The resin is supplied as pellets and should be kept in sealed containers away from direct sunlight and moisture. When ambient relative humidity exceeds 60%, drying at 80°C for 2 hours to 4 hours is a common precaution, though LLDPE is not hygroscopic and drying is usually not required unless surface moisture is present. Excessive drying temperatures above 100°C may lead to pellet agglomeration. Avoid blending with amine-based antifog or certain slip concentrates without verification, because additive interactions can shift coefficient of friction and plate-out on downstream equipment. For long-term storage exceeding 6 months, a melt flow rate check under ASTM D1238 is recommended to detect any molecular degradation during storage.

    Top