| HS Code | 243473 |
| Materialtype | Low Density Polyethylene (LDPE), Film Grade |
| Density | 0.922 g/cc |
| Meltflowrate | 2.0 g/10 min at 190 °C/2.16 kg |
| Tensilestrengthyield | 11.0 MPa |
| Tensilestrengthultimate | 24.0 MPa |
| Elongationatbreak | 600% |
| Tensilemodulus | 0.170 GPa |
| Dartdropimpact | 140 g |
| Elmendorftearstrength | 200 g |
| Haze | 7.0% |
| Gloss | 80% |
| Coefficientoffriction | 0.20 |
| Vicatsofteningpoint | 95.0 °C |
| Meltingpoint | 110 °C |
| Processingtemperature | 160 - 220 °C |
As an accredited Bamberger Polymers Bapolene® 152B Polyethylene, Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Bamberger Polymers Bapolene 152B standard packaging: 50 lb (22.7 kg) polyethylene bags, palletized and stretch-wrapped for secure shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loading of Bamberger Polymers Bapolene® 152B Polyethylene, Film Grade in 25 kg bags, palletized and shrink-wrapped. |
| Shipping | Bamberger Polymers Bapolene® 152B Polyethylene, Film Grade is shipped as non-hazardous polyethylene pellets, usually in moisture-resistant bags, boxes, or octabins on stretch-wrapped pallets. Transport via standard freight in clean, dry vehicles. Avoid heat, sunlight, and contamination. Store in a cool, dry warehouse. No special DOT/IATA hazard classification. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep in original, tightly closed packaging to prevent moisture, dust, and contamination. Avoid excessive stacking and physical damage. Separate from oxidizing agents and incompatible materials. Maintain good housekeeping. Use first-in, first-out inventory. Avoid prolonged heat exposure. Follow local regulations and supplier storage recommendations. |
| Shelf Life | Shelf life is typically 24 months from date of manufacture when stored in original, unopened packaging under cool, dry conditions. |
Bapolene 152B is a film-grade low-density polyethylene with a nominal melt index of 1.9–2.1 g/10 min as determined by ASTM D1238-20 at 190°C under 2.16 kg, and a nominal density of 0.921–0.923 g/cm³ by ASTM D1505-18. In direct food-contact monolayer blown film, the resin is run on a 45–65 mm extruder with a 24:1–30:1 L/D barrier screw and a screen pack of 60/80/100 mesh. Melt temperature at the die is held between 160°C and 190°C, die gap is set at 0.8–1.2 mm, blow-up ratio is maintained at 2.2:1–3.0:1, and frost line height is fixed at 6–10 die diameters. Film thickness is produced from 25 µm to 75 µm for produce bags, bakery overwrap, frozen food bags, and boxed-carton overwrap. Food-contact status under FDA 21 CFR 177.1520(c)(2.2) and EU Regulation (EU) No 10/2011 Annex I requires overall migration below 10 mg/dm² in EN 1186-1 testing using food simulants A, B, and D2. Haze is measured by ASTM D1003-21 on a 40 µm specimen, tensile properties by ASTM D882-18 at 500 mm/min crosshead speed, and dart impact by ASTM D1709-22 Method A. Regrind from in-house trim can be added at up to 20 wt% only when the trim is free of printing ink, adhesives, and post-consumer contamination; exceeding this level increases visible gel counts and lowers tear resistance when tested by ASTM D1922-15.
At 12 wt% addition of Bapolene 152B to an 88 wt% butene-copolymer LLDPE matrix containing 2.0 wt% UV stabilizer masterbatch, bubble stability on a 70 mm single-screw extruder with internal bubble cooling and a 1.6 mm die gap reaches a stable processing window at blow-up ratios of 2.4:1–2.8:1. The long-chain branched fraction in the LDPE raises zero-shear viscosity and strain hardening at the frost line; below 10 wt% addition, the bubble oscillates laterally by more than ±5 mm on a 1.5 m layflat width, while above 20 wt% addition, dart impact measured by ASTM D1709-22 Method A falls below the minimum generally specified for 150 µm greenhouse film. Melt temperature is set at 175–195°C, die gap at 1.4–2.0 mm, and take-off speed is adjusted to maintain film thickness of 150–200 µm for greenhouse covers, 25–35 µm for silage stretch wrap, and 20–30 µm for mulch films. The masterbatch carrier must be LDPE-compatible; concentrate levels above 4.0 wt% with low-MFI carriers have caused feed-throat bridging on single-flighted screws. Compliance for agricultural film is limited to REACH Article 33 and EN 13206:2017 covering-film requirements; direct food contact is not intended. For long-life greenhouse film, hindered amine light stabilizer and benzophenone absorber packages are dosed at 1.0–2.5 wt%; unpigmented film without at least 1.0 wt% stabilizer embrittles in accelerated weathering per ISO 4892-2 before the expected service interval.
Collation shrink film made from Bapolene 152B is produced in a high-blow, low-frost-line bubble with blow-up ratio of 4.0:1–5.0:1 and die gap of 1.0–1.4 mm. The high transverse orientation, frozen at a frost line height of 2–3 die diameters, is required to develop shrink ratios above 60% in the machine direction and above 20% in the transverse direction at 140°C when tested per ASTM D2732-14. Shrink tension is measured by ASTM D2838-18; recovery force at 120°C and 140°C determines how many polyethylene terephthalate bottles or aluminium cans a 45–75 µm film can hold in a 6-unit collation without loosening. In a continuous hot-air tunnel operating at 130–160°C with residence times of 6–12 seconds, the film surface must reach 110–140°C; tunnel speeds above 40 packs/min require forced air velocity in the range of 8–14 m/s. Increasing blow-up ratio above 5.0:1 improves transverse shrink but reduces bubble stability and produces seal-area splitting at the impulse seal bar, while ratios below 3.5:1 leave insufficient transverse orientation to hold a 6 × 1.5 L PET bottle pack at a 140°C tunnel set point. Finished goods include mineral water bottle multipacks, canned vegetable tray collations, and multipack overwrap for glass jars. Seal strength is tested per ASTM F88/F88M-21 on 25 mm sealed strips; values below 7 N/25 mm at 140°C crosshead temperature indicate that erucamide slip additive loading may have exceeded the intended 400–800 ppm range.
Extrusion lamination of paper, aluminium foil, and biaxially oriented polypropylene uses Bapolene 152B as a 15–25 µm tie layer. A 90 mm, 30:1 L/D single-screw extruder with a T-slot die and a chrome-plated chill roll maintained at 15–25°C is operated at a melt temperature of 300–320°C. The air gap between die exit and nip is set at 100–180 mm to allow controlled oxidation of the polyethylene surface; oxidation improves adhesion to aluminium foil and primed substrates. Peel strength is measured by ASTM F904-16 after 24 h conditioning at 23°C and 50% RH; typical lamination structures using aluminium foil target values above 250 N/m. Food-contact status must be confirmed on the finished laminate under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011; when the LDPE is separated from food by a functional barrier of aluminium foil, the overall migration limit of 10 mg/dm² applies to the combined structure. Finished formats include stand-up pouches, sachets, lidding film, and medical packaging. Direct coating onto unprimed polyester film below 12 µm thickness is not recommended because adhesion values fall below 80 N/m and melt-channeling occurs at line speeds above 200 m/min.
Heavy-duty industrial liner production using Bapolene 152B is concentrated at 100–200 µm film thickness on a 75 mm grooved-feed extruder with a die gap of 1.2–2.0 mm and blow-up ratio of 2.0:1–2.5:1. Melt temperature is held at 170–195°C. Mechanical tests on finished film include tensile strength at break and elongation at break by ASTM D882-18, Elmendorf tear by ASTM D1922-15, and dart impact by ASTM D1709-22; limits for 150 µm liners are set by end-use specifications rather than fixed resin data. The resin is processed into form-stable liners for FIBC outer shells, construction debris bags, oversize sacks, and chemical drum liners. UN 13H2 type approval for free-standing transport sacks requires additional validation of the finished article and is not an inherent property of the film-grade LDPE alone. When outdoor storage is expected, a carbon black masterbatch at 2.0–2.5 wt% must be incorporated; unpigmented film exposed to ultraviolet radiation for more than one season embrittles and fails puncture testing. Blending with acid-functional copolymers at levels above 15 wt% causes melt pressure fluctuation and gauge variation exceeding ±8% on 1.4 m layflat production.
For 12–25 µm kitchen and janitorial can liners, Bapolene 152B is blended with 20–30 wt% LLDPE to balance dart impact and machine-direction tear. Extrusion uses a 65 mm blown-film line with internal bubble cooling, a dual-lip air ring, and die gap of 0.9–1.3 mm. Melt temperature at the die is 160–180°C, blow-up ratio is 2.0:1–2.5:1, and output is controlled below 0.8 kg/h per mm of die circumference to suppress melt fracture on a 300 mm die. Gauge variation is held below ±6% by capacitance scanning across the bubble; dart impact is tested by ASTM D1709-22 Method A, and tear by ASTM D1922-15. Melt fracture first appears as surface roughness at the die lip when die temperature drops below 170°C at high screw speeds, and it is controlled by increasing die temperature to 175–180°C or reducing output by 10–15%. Terminal products include tall kitchen bags, janitorial liners, and general refuse sacks. This application is not intended for direct food contact; compliance is limited to REACH Article 33 and heavy-metal limits in EU Packaging Directive 94/62/EC Annex II. Regrind from post-industrial can-liner trims can be incorporated up to 30 wt% without exceeding an internal gel count of 50 per 1 m²; post-consumer recyclate is not recommended below 18 µm because pinhole counts increase and affect leak tightness.
Competitive Bamberger Polymers Bapolene® 152B Polyethylene, Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Bapolene® 152B, supplied by Bamberger Polymers, is a film-grade polyethylene positioned for blown-film conversion. The grade is generally assigned to the high-molecular-weight, film-density polyethylene class, a class characterized by low melt-flow values, high density, high melt strength, and comparatively high die pressure during extrusion. Bapolene® 152B is not an injection-molding or rotational-molding resin. The model designation alone does not establish food-contact status, regulatory compliance, or a processing window; the current Bamberger Polymers technical data sheet and lot-specific certificate of analysis function as the authoritative specification.
Because publicly available property values for this specific grade are limited, numerical data in this document are restricted to class-level ranges, standardized test procedures, and production-scale equipment behavior rather than a replacement for the supplier’s certificate. Melt mass-flow rate is evaluated under ASTM D1238-20 or ISO 1133-1:2022 at 190 °C and 2.16 kg. Density is determined under ASTM D1505-18 or ISO 1183-1:2019. Film mechanical values are generated on blown-film specimens using ASTM D882-18 or ISO 527-3:2018, while tear resistance is measured by ASTM D1922-15 or ISO 6383-2:1983.
The high-molecular-weight film-density polyethylene class is conventionally bounded by a low-load melt-flow rate below 0.15 g/10 min at 190 °C and 2.16 kg, with density from 0.945 g/cm³ to 0.955 g/cm³. In this class the low-load melt index has poor resolution, and the high-load melt-flow rate at 21.6 kg is often more useful for die-flow prediction. A melt-flow ratio above 80 between the 21.6 kg and 2.16 kg conditions is common, but the exact ratio for Bapolene 152B must be read from the certificate of analysis. Density influences crystallinity, stiffness, moisture-vapor resistance, and thermal softening. Higher density within the class generally raises film modulus but can alter Elmendorf tear and clarity if processing is not rebalanced.
Molecular weight distribution is a critical but often unpublished specification for this grade. A broad or bimodal distribution improves shear thinning in the die while retaining melt strength; the practical quality-control proxy is the melt-flow ratio. If the ratio is too low, die pressure at production throughput may exceed the extrusion system limit. If the ratio is too high, the film may show lower tensile yield and more variable bubble tension. The Bapolene 152B certificate should be consulted for quantitative values, since grade-specific distribution data are not reproduced here.
Table 1 lists the test designation matrix used for inbound specification control of film-grade polyethylene. The listed methods do not replace the lot-specific specification; they define the framework against which converter inspection should be performed.
| Property | Method | Unit | Measurement Condition |
|---|---|---|---|
| Melt mass-flow rate | ASTM D1238-20 / ISO 1133-1:2022 | g/10 min | 190 °C, 2.16 kg |
| Density | ASTM D1505-18 / ISO 1183-1:2019 | g/cm³ | 23 °C |
| Tensile stress at yield | ASTM D882-18 / ISO 527-3:2018 | MPa | MD/TD film specimen |
| Tensile strain at break | ASTM D882-18 / ISO 527-3:2018 | % | MD/TD film specimen |
| Elmendorf tear | ASTM D1922-15 / ISO 6383-2:1983 | N | MD/TD film specimen |
| Dart drop impact | ASTM D1709-16a | g | F50 failure threshold |
| Haze | ASTM D1003-13 | % | film specimen |
| Gloss | ASTM D2457-13 | GU | 45° or 60° geometry |
| Vicat softening temperature | ASTM D1525-17e1 / ISO 306:2013 | °C | 10 N, 50 °C/h |
| Melting peak temperature | ASTM D3418-15 / ISO 11357-3:2018 | °C | DSC thermal analysis |
On a production blown-film line using a 60 mm single-screw extruder with a 25:1 barrier screw and a spiral-mandrel die, film-density high-molecular-weight polyethylene is typically processed at melt temperatures from 190 °C to 220 °C. Die gaps of 1.4 mm to 2.0 mm and blow-up ratios from 2:1 to 4:1 are common. The frost-line height is usually held at 6 to 10 die diameters to stabilize the bubble before crystalline solidification occurs. At melt temperatures below 190 °C, die pressure may rise and sharkskin melt fracture can occur. Above 230 °C, antioxidant consumption accelerates and gels or yellowing may appear. These boundaries are class-level; the specific Bapolene 152B optimal melt-temperature window should be established by a temperature ladder on the target line in 5 °C increments while recording die pressure, bubble stability, and film appearance.
Film properties are anisotropic. Machine-direction and transverse-direction tensile and tear values must be measured separately, and converting trials should record blow-up ratio, die gap, frost-line height, melt temperature, and take-off speed for each roll. Without these parameters, comparative data across lots or suppliers are technically weak. For high-molecular-weight film-density resin, melt-temperature variation across the die circumference should not exceed ±5 °C; wider deviations can create gauge bands and roll-hardness defects on high-speed winding lines.
High-molecular-weight film-density polyethylene develops bubble stability from a combination of melt strength and crystalline solidification. In the spiral-mandrel die, the melt-flow ratio influences helix streak formation and die-lip wetting. If the high-load melt-flow value is below 6.0 g/10 min, die pressure on a 250 mm die can exceed 30 MPa at temperatures near 190 °C; raising the die zone to 210–220 °C usually reduces pressure but can lower melt tension. A melt-flow ratio above 120 indicates strong shear thinning but can be accompanied by lower melt strength. In that situation, reducing the blow-up ratio toward 2:1 or increasing the die gap may be required to maintain tear balance.
Capillary rheometry according to ISO 11443:2014 is the appropriate method for determining the critical shear stress for melt fracture and the apparent viscosity at processing shear rates. In the high-molecular-weight film class, critical shear stress for sharkskin is often in the region of 0.2 MPa to 0.4 MPa, but grade-specific data for Bapolene 152B must be generated experimentally. Narrow die gaps increase shear stress and may improve gauge uniformity, but they also raise die pressure and may initiate melt fracture. Wide gaps reduce die pressure but may require a higher blow-up ratio to obtain acceptable transverse-direction tear.
Torque-limited output is a common field condition for this molecular weight class. A 60 mm grooved-feed extruder with a 250 mm die may operate in the 70 kg/h to 110 kg/h range, but these figures are equipment-specific and should not be interpreted as grade-specific output targets. Smooth-bore extruders may produce lower output and melt surging; high-torque grooved-feed or barrier-screw designs are generally preferred for film-density high-molecular-weight polyethylene.
If Bapolene 152B is positioned as a high-density film resin, its density is higher than typical LDPE film grades. The primary consequences are higher tensile yield, higher secant modulus, and lower water-vapor transmission per unit thickness. The trade-off includes lower optical clarity and a different tear balance. LDPE film grades in the density range 0.912 g/cm³ to 0.925 g/cm³ process at lower melt temperatures and offer easier draw-down, but they require greater thickness to match the stiffness of a high-density film. LLDPE film grades with density from 0.916 g/cm³ to 0.940 g/cm³ typically provide higher Elmendorf tear and puncture resistance at equivalent gauge, while high-molecular-weight high-density polyethylene contributes higher heat resistance and moisture barrier.
The crystalline melting peak for film-density high-density polyethylene is commonly observed from 128 °C to 135 °C by ASTM D3418-15 or ISO 11357-3:2018. This is above the typical LDPE film melting range of 105 °C to 115 °C. Consequently, seal-initiation temperature and seal dwell on form-fill-seal lines must be revalidated before Bapolene 152B replaces an LDPE liner or overwrap. Seal-strength testing per ASTM F88/F88M-21 is appropriate for flexible package qualification.
Water-vapor transmission rate is thickness dependent. At 25 µm, high-density film generally exhibits lower water-vapor transmission than LDPE at the same gauge because higher crystallinity reduces diffusion. Measurements should be generated on the actual film lot using ASTM F1249-20 or ISO 15106-2 at 38 °C and 90% relative humidity. A single class-level value cannot determine shelf-life performance for a specific package.
Compared with injection-molding grades in the Bapolene portfolio, Bapolene 152B is expected to have a lower melt-flow rate and higher molecular weight. This increases die pressure and melt strength while making thin-wall mold filling impractical. Compared with fractional-melt LDPE, the film-density material may require higher torque and a higher melt temperature to avoid excessive residence time. Published grade-to-grade data for Bapolene 152B against other Bamberger grades are limited; direct substitution studies should use melt-flow, density, and film mechanical tests on the same line and gauge.
Table 2 identifies the regulatory instruments that may apply to polyethylene film supplied in the United States and European Union. The grade number does not itself establish food-contact or regulatory status; the converter must obtain the supplier’s written regulatory statement.
| Regulatory instrument | Requirement or test | Typical criterion | Confirmation path |
|---|---|---|---|
| 21 CFR 177.1520 | Olefin polymer extraction limits | As specified in 21 CFR 177.1520 | Supplier statement or analytical report |
| Regulation (EU) No 10/2011 | Overall migration | ≤10 mg/dm² | Migration testing report |
| REACH Regulation (EC) No 1907/2006 | SVHC content | <0.1% w/w per SVHC | SDS and supplier confirmation |
| RoHS Directive 2011/65/EU | Pb, Hg, Cd, Cr(VI), PBB, PBDE | ≤0.1% w/w; Cd ≤0.01% w/w | Supplier statement if applicable |
| CONEG | Sum of Pb, Cd, Hg, Cr(VI) | ≤100 ppm | Packaging heavy metals statement |
Storage and handling boundaries are those of polyethylene film resins generally. Pellets should be kept sealed and allowed to equilibrate to 20–25 °C before extrusion; storage above 30 °C or 70% relative humidity may introduce surface moisture and contribute to film defects. Strong oxidizing acids, halogens, and halogenated solvents can attack polyethylene under sustained contact. Incompatible melt streams such as PET reclaim or heavily filled masterbatches with widely different viscosity can produce gels, phase separation, or delamination. Antioxidant and processing stabilizers in the supplied grade may be sensitive to aggressive acid or amine chemistries; masterbatch carriers should be matched to the base resin and validated on the intended blown-film line at production gauge.