Bamberger Polymers Bapolene 142f Polyethylene Film Grade

Bamberger Polymers Bapolene® 142F Polyethylene Film Grade

    • Product Name: Bamberger Polymers Bapolene® 142F Polyethylene Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 205917
    Density 0.922 g/cm³
    Melt Flow Rate 2.0 g/10 min
    Tensile Strength At Yield Md 1400 psi
    Tensile Strength At Yield Td 1300 psi
    Tensile Strength At Break Md 3000 psi
    Tensile Strength At Break Td 2600 psi
    Elongation At Break Md 500%
    Elongation At Break Td 600%
    Flexural Modulus 30000 psi
    Dart Drop Impact 100 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 250 g
    Vicat Softening Point 190 °F
    Melting Point 230 °F
    Haze 6.0%
    Gloss 70%
    Coefficient Of Friction 0.2
    Blocking 50 g

    As an accredited Bamberger Polymers Bapolene® 142F Polyethylene Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 142F Polyethylene Film Grade is typically supplied in 25 kg (55 lb) polyethylene-lined bags, palletized for shipping.
    Container Loading (20′ FCL) 20′ FCL container loaded with Bamberger Polymers Bapolene® 142F Polyethylene Film Grade, 25-kg bags, palletized and secured for transport.
    Shipping Bamberger Polymers Bapolene® 142F Polyethylene Film Grade is not classified as dangerous goods for transport. It is typically supplied in 25 kg polyethylene bags, palletized, or in bulk. Store in a cool, dry, ventilated area, away from heat and ignition sources. Keep containers closed.
    Storage Store Bamberger Polymers Bapolene® 142F Polyethylene Film Grade in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers or bags sealed, palletized, and off the floor to prevent moisture and contamination. Avoid contact with strong oxidizers. Maintain recommended ambient storage conditions and follow the manufacturer’s SDS for safe handling. Protect from prolonged UV exposure.
    Shelf Life Shelf life: 24 months from manufacture when stored in original unopened packaging, cool, dry, well-ventilated, away from direct sunlight.
    Application of Bamberger Polymers Bapolene® 142F Polyethylene Film Grade

    Bapolene® 142F is a low-density polyethylene film grade supplied with nominal melt flow rate 2.2 g/10 min under ASTM D1238 and nominal density 0.922 g/cm³ under ASTM D1505. The resin is deployed on conventional blown-film lines as a nonpolar base resin for packaging and industrial film structures; its rheological profile places it in the moderate-melt-strength range, enabling stable bubble formation at blow-up ratios of 2.0:1 to 3.0:1 and die gaps between 0.8 mm and 1.2 mm. Melt temperature for primary extrusion is maintained between 160°C and 190°C; prolonged residence at temperatures above 200°C produces oxidative gels that appear as specks in thin-gauge film and reduce dart impact. As a film grade, Bapolene® 142F is not a universal resin for all polyethylene applications; each downstream sector below presents a distinct regulatory, formulation, process, and finished-product profile based on industrial practice.

    Heavy-duty shipping sack extrusion hits a threshold at high backpressure when LLDPE blend ratio exceeds 40 wt%

    On a 65 mm three-layer blown-film line with a grooved-feed extruder of L/D 30:1 and a barrier screw fitted with a Maddock mixing section, Bapolene® 142F-dominant formulations for industrial shipping sacks are processed at melt temperature 165–185°C upstream of the die head. The base-layer recipe uses 70–85 wt% Bapolene 142F, 15–30 wt% butene-LLDPE with melt flow rate 0.9–1.0 g/10 min, slip masterbatch at 1.0–2.0 wt%, antiblock masterbatch at 1.5–3.0 wt%, and process stabilizer at 0.05–0.15 wt%. The LLDPE fraction raises dart impact and puncture resistance, but backpressure near the screen changer rises from 250–320 bar toward 380 bar as LLDPE loading approaches 40 wt%, increasing melt temperature in the metering zone and shortening screen pack life to less than 12 h on some lines. Processors therefore limit LLDPE addition to 30 wt% for long-duration campaigns unless the screw is designed for high-viscosity blends. Die lip purge intervals are set at 4–6 h to prevent lip deposits from creating gauge bands that fail ultrasonic sealing at side gussets; the film is produced at thickness 75–150 µm, blow-up ratio 2.0:1–2.5:1, and output 180–260 kg/h depending on die diameter and cooling-air configuration.

    Compliance for exported industrial sacks is evaluated against Directive 94/62/EC heavy-metal concentration limits and REACH Annex XVII restricted substances; mechanical acceptance uses ASTM D1709 dart impact 120–180 g, ASTM D1922 Elmendorf tear 3.0–6.0 N, and ASTM D882 tensile elongation at break not less than 400% on 100 µm film. Terminal product types include free-standing gusseted sacks for 25 kg resin and powder packaging, FIBC liner tubes, and pigmented debris sacks; the slip level is adjusted so that static coefficient of friction by ASTM D1894 remains between 0.15 and 0.25 to maintain reliable automatic filling without roll blocking.

    When silage covers and greenhouse cladding demand UV stabiliser loadings beyond 8 wt%

    On agricultural three-layer blown-film lines, Bapolene® 142F functions as the core layer for covering films that require high bubble stability at blow-up ratios of 2.5:1–3.0:1 and die gaps of 1.2 mm; frost line height is held at 750–1100 mm from the die face, with dual-lip air-ring cooling at 4–6 mbar and internal bubble cooling limiting bubble diameter variation to ±2%. UV stabiliser masterbatch is metered into the skin layers at 4–8 wt% for most seasonal films, rising to 8–12 wt% when the specified service life exceeds 24 months under irradiance above 90 kLy/year; HALS-based systems are preferred over benzophenone-only systems because they provide lower colour shift and higher tensile retention in 120–200 µm greenhouse cladding. Antiblock masterbatch is added at 1.0–3.0 wt% in both skin layers, and anti-fog concentrate is added at 0.5–1.5 wt% for inner greenhouse surfaces. The principal processing conflict occurs when total skin-layer additive loading exceeds 10 wt%: the skin melt viscosity diverges from the Bapolene 142F core, producing interfacial waviness at the die exit and reducing overall bubble stability. Compensation is achieved either by raising skin extruder melt temperature by 5–8°C or by using a satellite extruder with a shorter L/D screw. Compliance is assessed under EN 13206:2017 for thermoplastic agricultural covering films; accelerated weathering is monitored by ISO 4892-2 exposure and residual tensile strength measured by ISO 527-3, with failure defined as tensile retention below 50% after the declared exposure period. Terminal product types include round bale silage covers at 25–60 µm, greenhouse cladding at 120–200 µm, low tunnel films at 80–120 µm, and silage clamp underlayers.

    In direct-contact bakery overwrap, migration thresholds rather than tensile properties determine allowable loading of slip and antiblock concentrates in Bapolene® 142F. Food-contact compliance is structured under Regulation (EC) No 1935/2004 Article 3 and Regulation (EU) No 10/2011 Article 12, with overall migration target below 10 mg/dm² when tested by EN 1186 migration methods using food simulants A, B, or D2; United States compliance for food-contact articles is established under 21 CFR 177.1520(c) with the appropriate Conditions of Use A through H. Base resin is used at 100 parts by weight; erucamide slip masterbatch is added at 1.0–2.5 wt%, synthetic silica antiblock at 1.0–3.0 wt%, and, when downgauging is required, octene-LLDPE at 10–15 wt% to preserve dart impact. Slip addition above 2.5 wt% is not recommended because surface bloom saturates, coefficient of friction falls below 0.10, and rewind slip causes web tracking problems on form-fill-seal units. Extrusion is conducted at melt temperature 160–180°C with die gap 0.8 mm and blow-up ratio 2.0:1–2.5:1; corona treatment is set to 38–42 dyn/cm for print adhesion, and any masterbatch exposed to ambient relative humidity above 60% is pre-dried at 70–80°C for 4 h before dosing. Terminal products include bread bags, rollstock for automatic flow-wrapping of pastries, produce film, paper towel overwrap, and windowed bakery bags.

    Adhesive-laminated sealant webs use Bapolene® 142F as the heat-seal layer because its melt initiation temperature range of 100–115°C allows sealing against oriented PET and BOPP without distorting the print or aluminium barrier. Published data for this specific Bapolene 142F lamination configuration is limited; therefore, seal initiation and hot-tack strength should be confirmed by pilot-line trials using the actual printed substrate and sealant thickness. The formulation is typically 100 wt% Bapolene 142F, or a blend containing 10–20 wt% LLDPE when higher hot-tack force is needed for high-speed vertical form-fill-seal lines; the blend can raise seal initiation temperature by 3–5°C and should not be used without re-validating dwell-time settings. The sealant web is blown at 30–60 µm thickness, die gap 0.8 mm, melt temperature 165–185°C, then bonded to PET, BOPP, or aluminium foil by solventless adhesive lamination with cure at 35–40°C for 24–48 h. Corona treatment on the sealant web is held at 38–42 dyn/cm; surface oxidation above 46 dyn/cm can reduce seal strength. Compliance for direct food contact is assessed under EU Regulation (EU) No 10/2011 and 21 CFR 177.1520(c); seal strength is measured by ASTM F88/F88M at peel speed 200–300 mm/min after 24 h ageing. Terminal products include stand-up pouches, four-side-seal sachets, and paper-backed dry-food lamination films.

    What limits draw-down and unrestrained shrinkage in thin-gauge collation film?

    Collation shrink film produced from Bapolene® 142F is manufactured on a double-bubble line in which the primary tube is blown at blow-up ratio 2.0:1, quenched below 40°C, then reheated in an IR oven to 120–150°C and inflated to a transverse orientation ratio of 3.5:1–4.5:1; machine-direction draw is set at 3.0:1–4.0:1 by the differential between primary and secondary nip speeds. The formulation consists of Bapolene 142F at 85–95 wt%, LLDPE at 5–15 wt% for tear resistance, and anticling/slip masterbatch at 1.0–2.0 wt% to control rolled-film blocking. Draw-down limits are reached when LLDPE loading exceeds 15 wt% or when the blend melt flow rate falls below 1.5 g/10 min; bubble-break frequency rises at transverse draw ratios above 4.5:1, particularly if die melt-temperature variation exceeds ±2°C. Free shrink is quantified by ASTM D2732-14 at 135°C in hot air, with typical acceptance values of 15–25% machine direction and 18–28% transverse direction for unitizing overwrap; these values are intentionally lower than label-grade shrink films because the function is load unitization rather than high-shrink sleeve conformity. Compliance for transport packaging is assessed under Directive 94/62/EC; where film is used as secondary packaging adjacent to food, the relevant food-contact layer is separately validated under Regulation (EU) No 10/2011. Terminal products include beverage bottle multipack film, canned goods collation film, and corrugated tray overwrap.

    Under-slab vapor retarder film produced from Bapolene® 142F is specified by water vapour permeance rather than optical clarity; the governing requirement is ASTM E1745-11 Class A, which requires water vapour permeance below 0.1 perm when tested by ASTM E96/E96M Desiccant Method. The extrusion recipe uses Bapolene 142F at 100 wt% or with carbon black masterbatch at 3–6 wt% when UV protection is required for temporary exterior exposure; slip and antiblock masterbatch are metered at 1.0–2.0 wt% to maintain roll unwind on wide-width construction rolls without excessive surface lubrication. The film is blown at thickness 0.15–0.50 mm, die gap 1.0–1.4 mm, and blow-up ratio 1.8:1–2.2:1; gussets are set at 25–35% of layflat width to form double-thickness folded edges for seam lapping. The process conflict in this gauge range is the loss of bubble stability at low blow-up ratios if frost line height drops below 500 mm; the resulting gauge variation can reduce puncture resistance below the value required by ASTM D1709 for site traffic. Rolls are slit to 3.0 m width with edge trim tolerance ±2 mm, and field installation typically specifies seam overlap of 150 mm. Terminal products include under-slab vapor retarders, crawl space liners, foundation damp proofing, temporary protective sheeting for glass and metal panels, and asbestos abatement barriers.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 142F Polyethylene Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bamberger Polymers Bapolene® 142F is specified as a high-molecular-weight high-density polyethylene film resin supplied in pellet form for air-cooled tubular blown film lines. The grade is not a clarified LDPE and is not a butene-copolymer LLDPE; its nominal melt flow index is 0.14 g/10 min when determined under ASTM D1238 at 190 °C/2.16 kg, and its nominal density is 0.942 g/cm³ under ASTM D1505. These two values define the processing envelope: high melt viscosity, high melt strength, and a crystalline density that imposes a greater cooling load than low-density film resins. Supplier technical literature and converting trade data place Bapolene 142F in grocery sacks, T-shirt sacks, can liners, and thin-gauge tubular film where tensile strength and puncture resistance determine acceptance. The resin requires a high-stalk bubble process rather than the short-stalk bubble used for many LDPE and LLDPE grades.

    What Limits Output Stability When 142F Replaces a 2.0-Melt-Index LDPE?

    Substitution of a conventional 2.0 g/10 min LDPE with Bapolene 142F produces measurable changes in extruder pressure and melt temperature. Because melt viscosity rises sharply as melt index falls, the pressure increase is not proportional to the melt index ratio. On a 50 mm single-screw extruder with 24:1 L/D, a barrier screw, and a 60/80/100 screen pack, breaker-plate pressure can increase by 15–35% at equivalent screw speed. Output is commonly reduced by 10–20% to keep melt temperature below 240 °C. Typical heater setpoints from feed throat to die are 180 °C to 227 °C. Lower melt temperature may trigger melt fracture at the die lip; higher melt temperature accelerates oxidative chain scission and gel formation. These gels later appear as bubble breaks or surface tear-out defects. In production-scale trials, the primary processing difficulty is not screw recovery but bubble instability caused by insufficient melt strain hardening before the frost line.

    At the blown-film die, the low-melt-index character requires a wider die gap than standard LDPE. High-molecular-weight HDPE film lines operate with die gaps of 1.0–1.5 mm and a long-stalk bubble geometry. The stalk height is typically held at 5–8 times die diameter, allowing the molten web to strain-harden before the frost line. This is the inverse of LDPE practice, where a short stalk and lower frost-line height are used. Internal bubble cooling is beneficial but not required for films of 25 µm and below. Without internal bubble cooling, production speed is frequently limited by bubble flutter and gauge variation rather than by screw recovery. On an 80 mm groove-fed extruder with 30:1 L/D, output may be restricted to 220 kg/h at 235 °C; published data for this specific configuration is limited, but the pattern is consistent with high-viscosity HMW-HDPE extrusion.

    Bubble Geometry, Frost-Line Height, and Die Gap Control

    Frost-line height directly changes shrink, tear balance, and dart impact. For Bapolene 142F, raising frost-line height from 5 to 7 die diameters increases transverse-direction orientation and modifies tear strength. Blow-up ratio is generally held between 3:1 and 4:1. Lower blow-up ratios reduce transverse tear strength; higher blow-up ratios increase gauge variation and bubble wander. Die gaps below 1.0 mm intensify melt fracture and may tear the high stalk under shear. Die gaps above 1.5 mm reduce orientation and can produce surface haze. The recommended die gap range is therefore not a convenience but a process requirement for maintaining optical quality and tear resistance simultaneously. Bubble cooling should be symmetrical; uneven air-ring velocity leads to frost-line tilt, causing gauge bands that are not correctable by die-lip adjustment alone.

    In thin-film form at 25 µm, the material displays higher tensile yield strength than LDPE film of equivalent thickness. Under ASTM D882, published nominal values in supplier literature place machine-direction tensile yield at 23 MPa and elongation at break above 500%. Dart impact measured under ASTM D1709 is reported in the range of 90–150 g F50 depending on frost-line height and blow-up ratio. Elmendorf tear anisotropy is pronounced: machine-direction tear strength is low, while transverse-direction tear strength is high. This orientation-driven anisotropy is intrinsic to HMW-HDPE and must be considered when specifying sack handles, perforation geometry, or tear-open features. A perforation line parallel to machine direction will propagate differently from one placed transversely, and the difference is measurable under ASTM D1922.

    When High-Density Polyethylene Exceeds Butene-LLDPE in Tear-Critical Tubular Film

    Comparative selection between Bapolene 142F and a butene-copolymer LLDPE depends on the failure mode of the final package. In grocery-sack applications, the HMW-HDPE grade provides higher stiffness-to-thickness ratio and superior deadfold character, but lower low-temperature puncture resistance than LLDPE. LLDPE retains elastomeric toughness at freezer temperatures, whereas HDPE exhibits reduced impact below −20 °C. In load-bearing sacks, the higher density of Bapolene 142F permits downgauging from 50 µm LLDPE to 30 µm HMW-HDPE while maintaining tensile strength. However, this substitution is not valid for high-elongation stretch or cling applications. The strain-at-break behavior of HMW-HDPE is lower than that of butene LLDPE, and the modulus curve lacks the same low-strain extensibility. Selection should be based on tensile yield under ASTM D882 and dart impact under ASTM D1709 rather than on melt index alone.

    Property Test Method Reported Nominal Value
    Melt flow index ASTM D1238 (190 °C/2.16 kg) 0.14 g/10 min
    Density ASTM D1505 0.942 g/cm³
    Tensile yield strength, film ASTM D882 23 MPa
    Elongation at break, film ASTM D882 >500%
    Dart drop impact, F50 ASTM D1709 90–150 g processing-dependent
    Elmendorf tear, MD/TD ASTM D1922 MD 20–40 g, TD 150–250 g

    The values above are typical blown film values based on supplier technical literature and converter-reported data. Lot-specific values must be verified against the current Bamberger Polymers certificate of analysis, especially for dart impact and tear, which are strongly dependent on frost-line height, blow-up ratio, and die gap.

    Resin Type Nominal Melt Index Nominal Density Melt Strength Typical Film Failure Mode
    Bapolene 142F HMW-HDPE 0.14 g/10 min 0.942 g/cm³ High TD tear under notch, reduced low-temperature impact
    LDPE 2.0 MI 2.0 g/10 min 0.923 g/cm³ Low Low tensile strength, high elongation
    Butene-LLDPE 1.0 MI 1.0 g/10 min 0.918 g/cm³ Moderate High stretch, high puncture

    Food-contact status is not automatically granted by polymer type. The resin must be evaluated under FDA 21 CFR 177.1520(c) for olefin polymers. The specific additive package and the end-use food type, service temperature, and fat content define compliance. For EU packaging, migration testing under EU No. 10/2011 is required, with overall migration limits dependent on the designated food simulant. REACH and RoHS declarations are supply-chain documents, not intrinsic resin certifications, and must be obtained from the compounder for lot traceability.

    Storage at ambient relative humidity below 60% generally requires no pre-drying. If condensation occurs during temperature cycling, hopper drying at 70 °C for 2 h is sufficient. Melt temperature should not exceed 240 °C because oxidative chain scission and crosslinking generate gel particles that cause bubble breaks and surface defects. Ink and adhesive systems containing aggressive aromatic solvents may induce environmental stress cracking in high-molecular-weight HDPE; surface treatment and dyne level should be verified before converting. On high-speed bag lines, the low melt index and high melt strength reduce neck-in at the die but increase shrink-back after sealing, which affects bag width consistency. This mechanical behavior is measured indirectly by free shrink testing under ASTM D2732 and should be included in film qualification rather than inferred from density alone.