Bamberger Polymers Bapolene 142b Polyethylene Film Grade

Bamberger Polymers Bapolene® 142B Polyethylene Film Grade

    • Product Name: Bamberger Polymers Bapolene® 142B Polyethylene Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 609451
    Product Name Bamberger Polymers Bapolene® 142B Polyethylene Film Grade
    Manufacturer Bamberger Polymers
    Brand Bapolene
    Grade 142B
    Material Type Polyethylene Film Grade
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Density 0.920 g/cm³
    Melt Index 1.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Break Md 35 MPa
    Tensile Strength At Break Td 32 MPa
    Tensile Strength At Yield Md 12 MPa
    Tensile Strength At Yield Td 11 MPa
    Elongation At Break Md 500%
    Elongation At Break Td 700%
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Dart Drop Impact 120 g
    Haze 12%
    Gloss 60%

    As an accredited Bamberger Polymers Bapolene® 142B Polyethylene Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 142B Polyethylene Film Grade is packaged in moisture-resistant 25 kg bags, typically 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) Bamberger Polymers Bapolene® 142B Polyethylene Film Grade loaded in 20′ FCL, palletized bags, clean dry container, securely stowed for transport.
    Shipping Bamberger Polymers Bapolene® 142B Polyethylene Film Grade ships as non-hazardous polymer pellets in sealed 25-kg polyethylene bags, stacked on stretch-wrapped pallets. Transport in clean, dry, covered trucks or containers at ambient temperature. Protect from moisture, sunlight, punctures, and contamination; no special DOT, IMDG, or IATA hazard classification.
    Storage Store Bamberger Polymers Bapolene® 142B Polyethylene Film Grade in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers tightly closed and off the floor on pallets. Prevent moisture, dust, and odor contamination. Avoid excessive stacking and prolonged UV exposure to maintain resin quality.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in a cool, dry place in the original packaging.
    Application of Bamberger Polymers Bapolene® 142B Polyethylene Film Grade

    In monolayer blown film extrusion for direct food contact, the polyethylene is processed through a grooved-feed extruder with a barrier screw of 30:1 L/D ratio and a spiral mandrel die having a die gap between 1.0 mm and 2.4 mm. The melt temperature measured at the adapter is maintained between 180°C and 210°C, while the frost line height is positioned at 1.5 to 2.5 die diameters above the air ring to balance transverse direction orientation and dart drop impact. Internal bubble cooling (IBC) systems with ultrasonic sensors regulate bubble diameter to ±2 mm, reducing gauge variation to below ±5% on production lines converting at rates up to 120 m/min. Compliance with direct food contact requirements is evaluated under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011, with overall migration limits from 10 mg/dm² for fatty simulants tested per EN 1186-1:2002. Specific property values for Bapolene 142B must be confirmed against the grade datasheet, because published data for this specific configuration is limited. Typical class-based acceptance ranges for LDPE film grade include dart impact per ASTM D1709 Method A of 60 g to 150 g at 25 µm thickness, tensile strength at break per ASTM D882 of 12 MPa to 18 MPa in the machine direction, and tear strength per ASTM D1922 of 3 N to 8 N in the transverse direction. These values are not grade-specific but represent the processing envelope for low-density polyethylene resins of this class. Batch-to-batch variance in melt index affects bubble stability; a shift of 0.05 g/10 min as measured per ISO 1133-1:2022 at 190°C/2.16 kg can require an adjustment of screw speed by 3-5 RPM to maintain constant throughput. The addition of slip and antiblock masterbatches must be controlled to avoid plate-out on the die lip; typical addition is 2 wt% to 4 wt% of a 5% erucamide concentrate, which is verified by coefficient of friction testing per ASTM D1894 with a target of 0.2 to 0.4 for automated packaging lines. Pre-drying is not generally required for neat polyethylene, but color concentrates exposed to relative humidity above 60% should be dried at 80°C for 4 h to prevent splay. Incompatibilities include amine-based antistatic agents that can cause yellowing at processing temperatures above 220°C; therefore, non-amine antistats are specified for clear film structures.

    Test methodParameterTypical class range for LDPE film grade
    ASTM D1709 Method ADart drop impact, 25 µm film60 g to 150 g
    ASTM D882Tensile strength at break, machine direction12 MPa to 18 MPa
    ASTM D1922Elmendorf tear, transverse direction3 N to 8 N
    ISO 1133-1:2022Melt mass-flow rate, 190°C, 2.16 kg0.2 g/10 min to 0.5 g/10 min
    ASTM D1894Coefficient of friction, film-to-film0.2 to 0.4

    What Limits Seal Integrity in Multilayer Flexible Packaging?

    In vertical form-fill-seal operations requiring seal through contamination, the sealant layer formed from a blend of LDPE and metallocene LLDPE is tested for hot tack and ultimate seal strength per ASTM F1921 and ASTM F88/F88M. Sealing initiation temperature for this class typically falls between 90°C and 110°C, with plateau seal strength reached at 130°C to 150°C using jaw pressures of 0.4 MPa to 0.6 MPa and dwell times of 0.5 s to 1.0 s. Failure modes observed on production machines include seal peeling caused by contamination from product dust, and delamination at the interfacial layer when the sealant layer lacks sufficient thickness; a minimum sealant thickness of 15 µm is recommended to prevent channel leaks in gusseted pouches. Coextrusion is performed on a three-layer die with a die gap of 1.8 mm to 2.2 mm and a layer distribution of 15/70/15 by volume, where the LDPE-containing sealant forms the inner layer. The addition of slip additives such as erucamide above 1000 ppm in the sealant layer can reduce plateau seal strength by 10% to 25% because amide bloom acts as an interfacial contaminant. Batch-to-batch variance in melt index shifts the hot tack window by ±5°C, requiring real-time adjustment of sealing jaw temperature when the melt mass-flow rate changes by 0.1 g/10 min as determined by ISO 1133-1:2022. Web tension on VFFS equipment should be maintained between 0.5 N/mm and 1.5 N/mm to prevent elongation that causes registration drift and seal bar misalignment. Compliance for food contact multilayer structures follows FDA 21 CFR 177.1520 for the polyolefin components and EU Regulation (EU) No 10/2011 with testing per EN 1186-2:2002 for aqueous simulants.

    Silage Film Requires Specific Carbon Black Loading and UV Stabilizer Packages

    For agricultural silage wrap, the three-layer coextruded structure incorporates a carbon black-loaded core layer between two outer layers that may be white or black depending on solar reflectance requirements. The core layer typically contains 3 wt% to 5 wt% carbon black masterbatch and a hindered amine light stabilizer (HALS) at 0.2 wt% to 0.5 wt% to meet outdoor weathering resistance under ISO 4892-2 cycle 1 with a target of no surface cracking after 2000 h of accelerated exposure. An ethylene-vinyl acetate copolymer with 14% vinyl acetate is blended at 10 wt% to 20 wt% in the outer layers to impart cling force of 2 N/cm² to 5 N/cm² when tested per ASTM D638 film modification. Processing on three-layer blown film lines uses a die gap of 1.8 mm to 2.5 mm, a blow-up ratio of 2.5:1 to 4.0:1, and a high frost line positioned at 8 to 12 die diameters to increase machine direction tear resistance for wrapping high-density round bales. Failure on production lines frequently manifests as pinholing from carbon black agglomerates; therefore, melt filtration with 200 mesh screens is mandatory before the die. Carbon black masterbatch exposed to relative humidity above 60% must be pre-dried at 80°C for 4 h to eliminate moisture-induced splay. The finished film is evaluated under EN 13207 for silage film and must demonstrate a tensile break strength of at least 20 MPa in the machine direction and an elongation at break above 400% per ISO 527-3. UV stabilization packages should not be combined with amine-based processing aids because premature breakdown of HALS can occur at processing temperatures exceeding 220°C.

    When Stretch Hood Film Is Converted at High Draw Ratios

    At draw ratios between 4:1 and 7:1, stretch hood film conversion places high molecular orientation on the bubble and requires a narrow processing window to avoid gauge bands and bubble breathing. Heavy-duty pallet wrapping from this class of polyethylene is produced at thicknesses from 50 µm to 150 µm on high-stalk blown film lines with a blow-up ratio of 3.0:1 to 4.5:1 and frost line heights controlled to 8 to 12 die diameters. Puncture resistance measured by ASTM D5748 typically ranges from 30 N to 60 N for a 100 µm film, while dart drop impact per ASTM D1709 Method A exceeds 200 g in class-based LDPE/LLDPE blends formulated for high toughness. Tensile properties under ASTM D882 show machine direction elongation at break between 400% and 600%, and tensile strength at break from 20 MPa to 30 MPa, which support stretch ratios required during pallet load containment. Bubble instability on production equipment is observed when melt pressure oscillation exceeds ±2 bar at the extruder head, leading to periodic gauge variation and reducing puncture resistance by up to 20% in the thin band. Automatic pallet wrappers operating at 20 to 40 pallets per hour require consistent film unwind force; the coefficient of friction against steel and the internal cling of the film must remain in a tight window to avoid film breaks during the stretch cycle. Batch-to-batch variance in dart drop impact of 15% or more can be traced to minor changes in LLDPE comonomer distribution, which alters tie chains and is detectable only through full notched tensile testing per ISO 8256.

    Test methodParameterTypical class range for stretch hood film
    ASTM D5748Protrusion puncture resistance, 100 µm film30 N to 60 N
    ASTM D1709 Method ADart drop impact200 g to 500 g
    ASTM D882Tensile strength at break, machine direction20 MPa to 30 MPa
    ASTM D882Elongation at break, machine direction400% to 600%

    When cast film is used as a hygiene backsheet lamination web, the chill roll temperature is set between 12°C and 20°C and the air gap is maintained at 20 mm to 40 mm. Thin gauges from 12 µm to 25 µm are extruded through a coathanger die onto a polished chill roll with water at 8°C to 16°C. A blown film grade such as Bapolene 142B may exhibit limited drawability in this configuration if the melt mass-flow rate is below 0.5 g/10 min because draw resonance and edge neck-in become uncontrollable at line speeds above 150 m/min. Blending with a higher melt index LDPE or metallocene LLDPE at 20 wt% to 30 wt% is a common corrective action, though published data for this specific configuration is limited. The resulting cast web is tested for tensile modulus per ISO 527-3 and for thickness uniformity with a beta gauge; variation above ±3% causes lamination defects in downstream adhesive coating. Regulatory compliance for hygiene backsheet applications focuses on REACH Regulation (EC) No 1907/2006 Annex XVII restrictions and absence of substances on the candidate list; direct food contact standards do not apply.

    Industrial Drum Liners and Chemical Barrier Structures

    Because industrial drum liners must withstand stress cracking, the blown film bubble is operated at a low frost line and a blow-up ratio of 2.0:1 to 3.0:1 to maximize impact strength. Liner thickness ranges from 100 µm to 250 µm, with gauge variation allowed up to ±10% across the layflat width, controlled by a dual-lip air ring and automatic bubble cage. Environmental stress crack resistance is evaluated per ASTM D1693, condition A, with typical failure time exceeding 1000 h in 10% Igepal solution for homopolymer LDPE film grades of adequate molecular weight. Weld integrity at the bottom seal is tested per ASTM F88/F88M and must survive a 2 m drop test with a filled drum liner at 50% capacity to meet industrial packaging practice. Chemical compatibility follows ASTM D543 practice A; the polyethylene liner is not recommended for concentrated nitric acid above 20% or aromatic hydrocarbons above 50°C because oxidative attack leads to rapid stress cracking and seal failure. For these aggressive media, a fluoropolymer or EVOH barrier layer must be added in coextrusion, and the operational boundary is documented in the end-user compatibility matrix.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 142B Polyethylene Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bapolene® 142B is a low-density polyethylene homopolymer supplied by Bamberger Polymers as a film extrusion grade. The resin is specified for blown film conversion on conventional single-screw equipment and is not intended for injection molding or profile extrusion. Melt flow index under ASTM D1238 / ISO 1133-1 at 190 °C/2.16 kg is 2.0 g/10 min; density under ASTM D1505 / ISO 1183-1 is 0.922 g/cm³. This places the grade in the general-purpose LDPE film range, balanced between bubble stability and thin-gauge drawdown. The product is used for industrial liners, garment bags, general packaging, and monolayer films where optical clarity is not the sole critical variable. Because the resin is supplied in pellet form, it is metered directly into the extruder hopper; the only required preparation is protection from gross moisture and fines contamination. The 142B designation is commonly positioned with an additive system that addresses film-to-film blocking and surface friction during winding and high-speed converting; converters requiring a specific coefficient of friction or slip level should confirm the additive package on the certificate of analysis.

    Specification Boundaries under ASTM D1238 and ASTM D1505

    The two invariant resin properties supplied for Bapolene 142B are melt flow index and density. The melt flow index of 2.0 g/10 min is measured at 190 °C under a 2.16 kg load; this is the standard condition for low-density polyethylene. A resin with this melt index permits lower extrusion head pressure than fractional-melt LDPE grades with melt indexes of 0.20 to 0.50 g/10 min, but it still retains sufficient melt strength for blown film bubble stability at blow-up ratios of 2:1 to 3:1. The density of 0.922 g/cm³ corresponds to a low-crystallinity LDPE solid-state structure, which contributes to flexibility and optical properties but reduces tensile modulus compared with HDPE in the 0.945 to 0.965 g/cm³ range. Film tensile properties are measured under ASTM D882 / ISO 527-3; dart impact under ASTM D1709 / ISO 7765-1; haze under ASTM D1003; and gloss under ASTM D2457. Because film properties vary with thickness, blow-up ratio, frost-line height, and additive migration, lot-specific values should be taken from the certificate of analysis.

    Specification parameter Test method Value basis
    Melt flow index ASTM D1238 / ISO 1133-1 2.0 g/10 min nominal
    Density ASTM D1505 / ISO 1183-1 0.922 g/cm³ nominal
    Tensile strength at break ASTM D882 / ISO 527-3 Certificate of analysis; gauge-dependent
    Elongation at break ASTM D882 / ISO 527-3 Certificate of analysis; gauge-dependent
    Dart drop impact ASTM D1709 / ISO 7765-1 Certificate of analysis; method A/B dependent
    Haze ASTM D1003 Certificate of analysis; thickness-dependent
    Coefficient of friction ASTM D1894 / ISO 8295 Certificate of analysis; migration-time dependent

    Because the ASTM D1238 melt flow index is a single-point low-shear measurement, it does not predict high-shear viscosity through the die lip. Converters operating at high outputs should measure capillary viscosity under ASTM D3835 if die-lip melt fracture or excessive head pressure occurs. The grade’s melt index of 2.0 g/10 min corresponds to a moderate molecular weight distribution for LDPE; this distribution influences shear thinning behavior and the onset of sharkskin. At die lip shear rates above the critical value for the resin, film surfaces exhibit periodic roughness. The countermeasures are raising die and adaptor temperatures by 5 to 10 °C, widening the die gap from 1.0 to 1.6 mm, or reducing output until the melt pressure stabilizes. Processing aids can extend the stable output window but require laboratory evaluation because they alter surface tension and may increase coefficient of friction.

    Blown film conversion of Bapolene 142B is typically conducted on a 40 to 80 mm single-screw extruder with 24:1 to 30:1 L/D and a barrier screw. Barrel set temperatures from 160 °C to 190 °C and die zones from 175 °C to 195 °C are typical for LDPE of this melt index; melt temperature measured at the die should remain below 200 °C to limit oxidation. Die gaps of 1.0 to 2.0 mm with blow-up ratios of 2:1 to 3:1 and frost line heights of 8 to 12 die diameters provide a stable bubble envelope for film thicknesses from 25 µm to 150 µm. The primary processing conflict is bubble instability at high throughput or high blow-up ratio; if the melt temperature is too low, film gauge variation increases near the frost line, and if the frost line is set too high, blocking may occur before winding. Screen packs of 80 to 120 mesh are used to remove gel particles; pressure buildup across the screen pack should be monitored, and excessive screen pressure can indicate melt temperature below the recommended set point or contamination from regrind. The resin is not hygroscopic; desiccant drying is not routinely required. Surface moisture from high-humidity storage can produce bubble defects; if condensation is observed, pellets should be air-purged or dried at 60 °C to 70 °C for 2 to 4 h before use.

    How Does the Controlled Additive Package Affect Friction and Blocking?

    Coefficient of friction in LDPE film is tested according to ASTM D1894 or ISO 8295. When a migratory slip additive is present, the measured kinetic coefficient of friction will decrease during the first 24 to 72 h after extrusion as the additive migrates to the film surface. This time dependence creates a converting conflict: film wound immediately after extrusion may exhibit blocking on the roll, while film tested too early may show higher coefficient-of-friction values than the final product. Blocking resistance is measured by ASTM D3354; the controlled antiblock component in 142B is intended to prevent film layers from adhering under roll pressure and storage temperatures below 50 °C. In applications where coefficient of friction must remain below 0.20, converters may need to confirm additive concentration with the certificate of analysis or blend with a high-slip masterbatch, because published data for the exact additive package in 142B is limited.

    On conventional blown film lines, the mechanical properties of film produced from 142B are anisotropic because of the transverse direction orientation imposed by the blow-up ratio and the machine direction draw from nip speed. Tensile strength and elongation are measured in both machine direction and transverse direction according to ASTM D882 / ISO 527-3. At blow-up ratios above 2.5:1, transverse direction elongation increases while machine direction elongation may decrease; the effect becomes more pronounced below 50 µm. Dart impact measured by ASTM D1709 method A or B is also gauge-dependent and is not controlled by melt flow index alone; film crystallinity, orientation, and additive dispersion contribute. When the film is drawn down below 25 µm, gauge variation is influenced more by die temperature uniformity and air-ring stability than by the resin specification. Heat-sealing behavior is similarly converter-dependent. Seal initiation temperature should be determined using ASTM F2029 or seal strength using ASTM F88; values are not typically supplied in the base resin technical data because seal performance depends on film gauge, dwell time, jaw pressure, and additive bloom. For critical seal-strength applications, the film should be evaluated after additive migration and not immediately after extrusion.

    When 142B Replaces Fractional-Melt LDPE or Butene LLDPE

    The choice between 142B and a fractional-melt LDPE depends on bubble stability and drawdown. Fractional-melt LDPE with a melt index of 0.20 to 0.50 g/10 min has higher melt strength and is preferred for thick-gauge heavy-duty film, but it generates higher extruder pressure and requires more motor torque. At 2.0 g/10 min, 142B reduces backpressure and allows thinner gauges, but it is less resistant to bubble sag on high-stalk or large-die configurations. In comparison with butene LLDPE at 0.918 g/cm³, 142B typically produces lower dart impact and puncture resistance as measured by ASTM D1709 and ASTM D5748; the trade-off is lower haze, higher gloss, and a broader melt processing window on standard LDPE screws. In form-fill-seal packaging, the coefficient-of-friction and blocking package of 142B is intended to provide predictable film transport without external lubricants, whereas LLDPE may require additional slip or antiblock masterbatch to avoid blocking.

    Parameter Bapolene 142B LDPE Fractional-melt LDPE Butene LLDPE
    Melt flow index 2.0 g/10 min 0.20 to 0.50 g/10 min Typically 0.8 to 2.0 g/10 min
    Density 0.922 g/cm³ 0.922 to 0.925 g/cm³ 0.916 to 0.920 g/cm³
    Bubble stability Moderate High Lower; may require internal bubble cooling
    Dart impact Lower than LLDPE Similar to 142B Higher
    Optical haze Lower Similar Higher
    Friction control Controlled package Grade-dependent Additive-dependent

    The Regulatory Status Is Defined by Food-Contact and Electrical/Electronic Directives

    Neat low-density polyethylene homopolymer is listed under FDA 21 CFR 177.1520(c) as an olefin polymer acceptable for food-contact use subject to the end-use conditions and extractives limitations in the regulation. The converter must verify that all additives in 142B, including slip and antiblock agents, are also cleared under 21 CFR 177.1520, an applicable food additive regulation, or an effective food contact notification. European food-contact compliance is assessed under Regulation (EU) No 10/2011 on plastic materials and articles intended to come into contact with food; overall migration limits and specific migration limits must be verified on the finished article. RoHS recast 2011/65/EU and its delegated directives restrict lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE; unfilled LDPE typically meets these heavy-metal restrictions, but flame-retardant or colorant additions require separate verification. REACH registration status must be confirmed through the supplier’s safety data sheet; the resin is not intended for medical device implantation or long-term implant applications. Continuous service temperature is bounded by the Vicat softening point; applications should not exceed 60 to 70 °C under sustained load without heat-stabilization. The grade does not contain UV stabilizers by default, so outdoor exposure requires additional stabilization or coextruded UV barrier layers.

    Top