Bamberger Polymers Bapolene 142a Polyethylene Film Grade

Bamberger Polymers Bapolene® 142A Polyethylene Film Grade

    • Product Name: Bamberger Polymers Bapolene® 142A Polyethylene Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 201699
    Polymer Type Low Density Polyethylene (LDPE)
    Density 0.921 g/cm³
    Melt Index 2.0 g/10 min
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 22.1 MPa
    Elongation At Break 500%
    Flexural Modulus 207 MPa
    Vicat Softening Point 88°C
    Melting Point 110°C
    Haze 8%
    Gloss 60%
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Coefficient Of Friction 0.20

    As an accredited Bamberger Polymers Bapolene® 142A Polyethylene Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 142A Polyethylene Film Grade is packaged in 25 kg (55 lb) polyethylene-lined bags, palletized for industrial handling.
    Container Loading (20′ FCL) Bamberger Polymers Bapolene® 142A Polyethylene Film Grade: non-hazardous, typically palletized in 25 kg bags; 20 pallets (20 MT) per 20′ FCL.
    Shipping Bamberger Polymers Bapolene® 142A Polyethylene Film Grade is shipped as non-hazardous polyethylene resin pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Keep containers closed; store dry, cool, ventilated, away from heat, moisture, and direct sunlight. Standard freight applies; no special UN classification required.
    Storage Store Bamberger Polymers Bapolene® 142A Polyethylene Film Grade in its original, unopened packaging in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, moisture, heat, ignition sources, strong oxidizers, and contamination. Keep away from acids and excessive temperatures. Use first-in, first-out stock rotation. Avoid excessive stacking; maintain clean handling areas and follow the manufacturer’s SDS storage guidance.
    Shelf Life Bapolene® 142A has a shelf life of 12 months when stored in original unopened packaging under cool, dry conditions.
    Application of Bamberger Polymers Bapolene® 142A Polyethylene Film Grade

    Bapolene® 142A is a high-pressure low-density polyethylene film resin with a nominal melt flow rate of 2.0 g/10 min at 190 °C under 2.16 kg load per ASTM D1238-20 or ISO 1133-1:2022. The nominal density is 0.922 g/cm³ per ASTM D1505-18 or ISO 1183-1:2019. Heavy-duty industrial liners in the 80–150 μm range are converted on single-layer blown film lines equipped with a 60 mm grooved-feed extruder and a 30 L/D barrier screw. Feed throat temperature is kept at 35–45 °C to prevent pellet bridging in the grooved section. Zone temperatures from feed to die are set at 160 °C, 175 °C, 185 °C, 190 °C, and 195 °C. A 1.8 mm die gap is used for a final 100 μm liner. Screen pack configuration is 60/80/100 mesh. Head pressure is held below 350 bar. A pressure rise above 350 bar at constant screw speed indicates melt filtration blockage or pellet-size instability. Blow-up ratio is held between 1.8:1 and 2.2:1. Frost-line height is maintained at 5–8 die diameters. Above this range, the bubble oscillates and gauge bands form at the fold edges. Capacitance thickness profiling should be run continuously because LDPE melt strength can mask minor melt delivery instability until tear or puncture testing. Gauge variation is held to ±5% on a well-centred bubble. Above 8%, thin spots become failure zones in tear and puncture testing. Puncture resistance is evaluated by drop-dart impact per ASTM D1709-16A. Elmendorf tear resistance is measured by ASTM D1922-15. The end product is used for construction debris, industrial waste, and medical waste liners. No food-contact claim applies to this segment. REACH Regulation (EC) No 1907/2006 applies to the supplied resin. Downstream converters must perform SVHC screening for any added masterbatch.

    Coextruded Food-Contact Film at 30 μm Gauge with EVA Skin Layers

    Food packaging structures use 142A in the core or outer layer of three-layer blown film. The layer ratio is typically 20/60/20 or 10/80/10. Skin layers are EVA with 18 wt% vinyl acetate for low-temperature seal initiation. Melt temperature is maintained at 190–200 °C. At 200 °C, the melt strength of 142A stabilizes the bubble. Above 210 °C, the as-supplied stabilizer package can undergo oxidative depletion. The film is not intended for retort or hot-fill above 85 °C. Seal initiation occurs near 105 °C on a 30 μm film with EVA skins. Heat-seal strength is measured by ASTM F88/F88M-15. Hot tack is evaluated by ASTM F1921. The olefin base is covered under 21 CFR 177.1520. Finished articles must meet FDA conditions of use. In the European Union, the finished structure must meet the overall migration limit of 10 mg/dm² per EU 10/2011. Regrind is allowed only if generated from the same food-contact line and free of printing ink. Amide-based slip agents in EVA skins can raise seal initiation temperature. Compatibility must be tested before qualification. LDPE does not provide oxygen barrier. If oxygen or aroma barrier is required, the structure must include aluminium foil, EVOH, or PVDC. Terminal products include frozen vegetable pouches, bakery film, and cheese wrap.

    Regulatory checks for 142A-based food films are summarized in the matrix below.

    US food contact21 CFR 177.1520Olefin polymersBase resin may be used subject to finished-article extraction testing
    EU food contactEU 10/2011Overall migration limit 10 mg/dm²Select simulants under Annex III
    REACHRegulation (EC) No 1907/2006Article 33 SVHC communicationApplies above 0.1 wt% SVHC in article
    Packaging wasteDirective 94/62/ECLead, cadmium, mercury, chromium VI sumMaximum 100 ppm by weight in packaging

    Silage wrap at 25 μm gauge is made using 142A as the base resin. The as-supplied pellet is not marketed as a cling-containing grade. Polyisobutylene or a metallocene polyolefin plastomer tackifier is added at 2–6 wt%. HALS-based UV stabilizer is added at 0.3–0.6 wt% for one-season weathering. The film is extruded on a 70 mm high-output blown film line with internal bubble cooling. Melt temperature is held at 185–195 °C. Blow-up ratio is set at 2.5:1 to balance machine-direction and transverse-direction stretch. During wrapping, the film is pre-stretched 60–70%. The film must not be corona treated. Corona treatment increases surface energy and can cause overly aggressive cling, resulting in difficult roll unwind. Tensile strain at break is measured by ASTM D882-18. UV retention of tensile elongation is assessed by ASTM G154-16 with UVA-340 lamps for 500 h. Finished rolls stored above 30 °C can undergo cling migration. This produces layer blocking and uneven unwind tension on the wrapper. Field failures usually appear at the overlap seam where cling force is lowest. The terminal product is round bale wrap for haylage and corn silage.

    Can 142A Serve as a 15 wt% LDPE Component in LLDPE-Rich Collation Shrink Film?

    Shrink bundling lines for bottles and cartons demand stable bubble geometry and low melt fracture. 142A is dry-blended with metallocene LLDPE at 15–25 wt% LDPE fraction. The dry blend is fed to a 50 mm smooth-bore extruder with a barrier screw. Melt temperatures are maintained at 200–210 °C. A dual-lip air ring is used. Blow-up ratio is set at 2.0:1 to 2.5:1. Frost-line height is kept at 9–12 die diameters to increase machine-direction orientation. The LDPE fraction raises bubble stability and reduces neck-in. The LLDPE fraction retains dart impact strength. Silica antiblock is added at 0.5–1.0 wt% to prevent blocking on the reel. Haze is measured by ASTM D1003-13. Free shrink is measured by ASTM D2732-14 after 10 s immersion in a 120 °C bath. On a 50 μm film, the LDPE fraction can raise shrink tension. At addition levels above 25 wt%, dart impact can decline sharply. Published dart impact data for this exact dry blend is limited. Converter trials are required before commercial settings are fixed. The terminal application is bundling of canned goods and multipack cartons.

    When 142A is Used as the Sealant Layer in Adhesive-Laminated Structures

    Single-serve sachets and barrier pouches use a blown 142A-based sealant web laminated with adhesive to oriented polyester or biaxially oriented polypropylene. The construction is often printed film, adhesive, aluminium foil, adhesive, and a 30–50 μm sealant web. The sealant web is produced in a separate blown film step. Melt temperature is kept at 185–195 °C. Gels are the primary rejection criterion. Gel particles from degraded resin produce pinholes in thin foil laminates and reduce seal integrity. Seal strength is measured by ASTM F88/F88M-15. Seal initiation occurs near 105–115 °C depending on gauge and dwell time. For food use, the olefin base is covered by 21 CFR 177.1520 or EU 10/2011. The structure is not intended for high-fat foods above 60 °C. LDPE can swell with fatty simulants, increasing overall migration test results. For pharmaceutical packaging, the converter must verify pharmacopoeial requirements separately. Terminal structures are sachets, lid stock, and barrier pouches.

    Surface protection film for powder-coated aluminium profiles uses a 40 μm coextruded web with a 142A backing layer and an EVA-based adhesion layer. The backing is produced on a cast film line at 220–240 °C melt temperature. Cast film is preferred for low gel counts and uniform thickness. The outer surface may be corona-treated to 40–42 dyn/cm wetting tension per ASTM D2578 for printing or coating. The adhesion layer is not corona-treated. Adhesion is tested per ASTM D3330/D3330M-02(2017) at 180° peel angle. Controlled peel strength is necessary to avoid adhesive transfer to the profile after 3 months of outdoor storage. The base resin has limited UV resistance. It must be UV-stabilized for extended exterior exposure. Contamination with dust or silicone from the extrusion floor can reduce peel uniformity. Peel force drift of more than 0.2 N/25 mm across a coil is used as a rejection limit. The terminal product is temporary protection for window frames and aluminium extrusions.

    In pallet stretch-hood conversion, 142A is used as a melt-strength modifier in a metallocene LLDPE-rich film at 60–80 μm. The LDPE fraction is typically 10–20 wt%. The film is blown on a 1200 mm die with internal bubble cooling. Melt temperature is set at 190–205 °C. Blow-up ratio is kept at 2.0:1–2.4:1. Frost-line height is lowered to 7–9 die diameters to improve impact resistance. The film must maintain yield stress high enough to secure pallet loads during transport. Tensile yield is measured by ASTM D882-18. Puncture resistance is measured by ASTM D5748-95. Gauge variation is monitored by capacitance thickness measurement. Gauge variation above ±5% produces uneven stretch force around the pallet. The terminal application is pallet unitization for construction materials and industrial bags.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 142A Polyethylene Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bapolene 142A, supplied by Bamberger Polymers, is classified as a low-density polyethylene film extrusion grade. The resin carries a nominal density of 0.922 g/cm³ when measured under ASTM D1505 and a melt index of 2.0 g/10 min when determined at 190°C under a 2.16 kg load according to ASTM D1238. These values place the material in the general-purpose LDPE film segment used for industrial sheeting, garment bags, overwrap, and thin-gauge protective packaging. On conventional blown-film lines, Bapolene 142A is processed at die temperatures of 190–200°C and blow-up ratios of 2.0:1 to 3.0:1. Because the melt index is intermediate, the resin operates with a measurable balance between extruder backpressure and melt strength; production-scale runs on a 60 mm extruder with 30:1 L/D and a barrier screw are commonly held at 40–80 rpm, with die head pressure maintained below 35 MPa.

    What processing envelope governs stable bubble formation for this LDPE film grade?

    Blown-film bubble stability for LDPE with a melt index of 2.0 g/10 min is controlled by extensional strain hardening associated with long-chain branching. The branched architecture produces a shear viscosity of approximately 800 Pa·s at 100 s⁻¹ and 190°C, with a power-law index of approximately 0.4 across the 50–500 s⁻¹ shear-rate range. The extensional viscosity departure from the linear-viscoelastic envelope at 190°C and an extensional strain rate of 1 s⁻¹ is typically a factor of 2–5 for branched LDPE film resins. This strain hardening suppresses draw resonance and stabilises the bubble; linear LLDPE grades do not show the same magnitude of departure from the linear-viscoelastic envelope. Published data for Bapolene 142A in this specific extensional configuration is limited, but the material is processed within the stable branched-LDPE window when blow-up ratio and frost line height are controlled.

    The die lip gap is set between 0.8 mm and 1.5 mm. Thin-gauge film below 50 µm is run through the narrower gap, while thicker film from 100 µm to 250 µm uses the wider gap to limit melt fracture. Blow-up ratio is maintained from 2.0:1 to 3.0:1. Operation below 2.0:1 produces insufficient transverse orientation and increases machine-direction tear propagation, while operation above 3.0:1 makes the bubble more sensitive to air turbulence and can increase gauge variability. Frost line height is set at 6–8 die diameters. A lower frost line increases optical clarity and machine-direction tensile strength, whereas a higher frost line improves bubble stability and dart impact at the expense of haze. At 6 die diameters frost line height, haze is approximately 7% under ASTM D1003; extending the frost line to 10 die diameters can increase haze above 10% because of larger spherulitic texture.

    On a 60 mm single-screw extruder with 30:1 L/D and a barrier screw, a barrel profile of 150/165/180/190/195°C from feed throat to die is used for Bapolene 142A. The screen changer is held at 190°C, the adapter at 195°C, and the die at 195°C. A screen pack of 40/60/80 mesh is used to raise melt pressure to 20–30 MPa and to trap gel particles. Sustained pressure above 35 MPa is not recommended because shear heating increases local melt temperature and can form oxidised gel defects. External bubble cooling uses a dual-lip air ring with chilled air at 7–15°C; internal bubble air is held at 25–35°C to control bubble expansion. Chilled air volume is set at 0.5–1.5 m³/min per 100 mm of die diameter. Bubble diameter is regulated by internal air pressure; a pressure variation of ±10 Pa can alter bubble diameter by 5–10 mm on a 200 mm die. For a die diameter of 200–400 mm and film gauge of 25–75 µm, typical specific output is 0.5–1.0 kg/h/mm of die circumference. Non-contact gauge scanners with capacitive or beta sensors measure film thickness to ±0.5 µm and feed back to segmented die bolts. These values are drawn from equipment manufacturer technical bulletins for LDPE film extrusion; published production data specific to Bapolene 142A on wider dies is limited.

    Mechanical property verification and optical test standards

    Manufacturer-published typical values for Bapolene 142A are summarised in Table 1. The values are not release limits and vary with gauge, blow-up ratio, frost line height, and extrusion temperature. Film property testing follows the cited ASTM designations.

    PropertyTest methodTypical valueUnit
    Melt indexASTM D12382.0g/10 min
    DensityASTM D15050.922g/cm³
    Tensile strength at break, MDASTM D88221MPa
    Tensile strength at break, TDASTM D88217MPa
    Elongation at break, MDASTM D882300%
    Elongation at break, TDASTM D882500%
    Dart drop impact, F50ASTM D1709 Method A90g
    HazeASTM D10037%
    Gloss, 45°ASTM D245760—
    Vicat softening pointASTM D152591°C

    Dart drop impact of 90 g under ASTM D1709 Method A is typical for a 50 µm film. Reducing gauge to 25 µm lowers dart impact to approximately 40–50 g, while increasing gauge to 75 µm raises dart impact to 120–140 g. Heat-seal strength for 50 µm film sealed at 115°C and 0.3 MPa for 1 s is typically 8–12 N/25 mm under ASTM F88. The material is supplied without intentionally added high-slip or antiblock surface modifiers. As a result, film-to-film blocking is higher than for formulated film grades unless a slip/antiblock masterbatch is added at 1–3% by mass. Converters running high-speed form-fill-seal equipment commonly target a coefficient of friction of 0.2–0.4 under ASTM D1894; that range is achieved through masterbatch addition rather than by selecting the neat resin. The absence of migratory surface additives permits heat-seal initiation temperatures of 105–115°C, which is lower than typical octene-LLDPE film initiation at 110–125°C, and reduces seal-jaw contamination in thermal lamination.

    Compared with HDPE film of density 0.952 g/cm³ and melt index 0.5 g/10 min, Bapolene 142A exhibits lower tensile yield strength and lower moisture-barrier performance. Water vapour transmission for LDPE at 25 µm is approximately 18 g/m²·day under ASTM E96, whereas HDPE of equivalent gauge transmits around 8 g/m²·day. Optical haze is lower for Bapolene 142A than for HDPE film, which typically exceeds 25% haze under ASTM D1003. For food-contact applications, compliance with 21 CFR 177.1520 and EU Regulation (EU) No 10/2011 is possible when the converter verifies overall migration limits under the intended use conditions.

    When Bapolene 142A replaces linear low-density polyethylene in high-stretch film lines

    Three measurable process changes occur when Bapolene 142A is substituted for octene-LLDPE on a blown-film line. First, melt pressure at constant screw speed decreases because branched LDPE exhibits stronger shear thinning than LLDPE at equivalent melt index. Second, bubble stability improves because extensional strain hardening suppresses strain rate localisation; the frost line height can often be reduced by 1–2 die diameters without loss of bubble integrity. Third, ultimate tensile elongation and dart impact decrease. At the same gauge, an octene-LLDPE film with dart drop impact of 150 g under ASTM D1709 Method A may be replaced by an LDPE film with dart drop impact of 90 g; to match puncture resistance, film thickness must be increased by 20–30%. The heat-seal initiation temperature is lower for LDPE, typically 105–115°C versus 110–125°C for octene-LLDPE, which reduces seal-bar energy consumption but narrows the hot-tack operating window.

    ParameterBapolene 142AOctene-LLDPE filmHDPE film
    Density0.922 g/cm³0.918 g/cm³0.952 g/cm³
    Melt index2.0 g/10 min1.0 g/10 min0.5 g/10 min
    Dart drop impact, F5090 g150 g50 g
    MD tensile at break21 MPa35 MPa40 MPa
    Haze7%12%25%
    Heat-seal initiation105–115°C110–125°C130–140°C

    Operational boundaries include a recommended melt temperature ceiling of 220°C. Residence time above 210°C should not exceed 2 min to limit oxidative gel formation. The Vicat softening point of 91°C under ASTM D1525 means the resin is not intended for sustained load-bearing service above 60°C. Bapolene 142A is incompatible with strong oxidising acids, aromatic hydrocarbons, and chlorinated solvents under tensile stress. Environmental stress-cracking resistance under ASTM D1693 is lower for LDPE than for HDPE; the branched LDPE grade should not be used in direct contact with polar surfactants under continuous stress. Outdoor film requires 2–3% UV stabiliser masterbatch and 1–2% carbon black in exposed layers unless the application specification permits shorter service life. For high-speed packaging where coefficient of friction must remain below 0.3, slip/antiblock masterbatch addition is required.

    Top