Bamberger Polymers Bapolene 133f Polyethylene Film Grade

Bamberger Polymers Bapolene® 133F Polyethylene, Film Grade

    • Product Name: Bamberger Polymers Bapolene® 133F Polyethylene, Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 880022
    Polyethylene Type Low Density Polyethylene (LDPE)
    Density 0.921 g/cm³
    Melt Flow Rate 0.70 g/10 min at 190°C/2.16 kg
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 500%
    Flexural Modulus 0.241 GPa
    Vicat Softening Point 95 °C
    Melting Point 110 °C
    Haze 8%
    Gloss 50%
    Dart Drop Impact 80 g
    Elmendorf Tear Strength 200 g
    Coefficient Of Friction 0.20

    As an accredited Bamberger Polymers Bapolene® 133F Polyethylene, Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 133F Polyethylene, Film Grade is supplied in 25 kg (55 lb) moisture-resistant bags, palletized for shipment.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Bamberger Polymers Bapolene® 133F Polyethylene Film Grade, 25 kg bags, palletized, stretch-wrapped; approximate 18–20 MT net payload.
    Shipping Bamberger Polymers Bapolene® 133F Polyethylene, Film Grade is shipped as non-hazardous resin pellets in moisture-barrier bags or boxes, palletized and stretch-wrapped. Transport in clean, dry vehicles at moderate temperatures. Avoid direct sunlight, excessive heat, moisture, and contamination. No special UN hazardous shipping classification typically applies. Follow SDS handling guidance.
    Storage Store Bamberger Polymers Bapolene® 133F Polyethylene, Film Grade indoors in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep in tightly closed original packaging, off the floor, to prevent moisture, dust, and contamination. Separate from strong oxidizers. Use first-in, first-out stock rotation. Follow local regulations and the manufacturer's SDS. Do not expose to ignition sources.
    Shelf Life Shelf life is typically 12 months from manufacture when stored unopened in original packaging under cool, dry conditions.
    Application of Bamberger Polymers Bapolene® 133F Polyethylene, Film Grade

    Typical lot-analysis values for melt flow rate are 1.3 g/10 min under ASTM D1238-20 at 190°C/2.16 kg, with density of 0.922 g/cm³ under ASTM D1505-18. In monolayer and coextruded blown-film lines producing food-contact packaging, Bapolene® 133F is processed as the primary sealing and body resin at melt temperatures of 160°C–200°C, with die gap settings of 1.5 mm–2.5 mm and blow-up ratios in the range 2.0:1–2.8:1. Frost line height is typically maintained at 5–8 die diameters on a single-lip air ring, and total film thicknesses are between 20 µm and 100 µm. On 60 mm–120 mm extruders with L/D ratios of 25:1–30:1, barrel temperature profiles are ramped from feed throat 140°C to adapter 180°C. The resin does not require pre-drying under normal internal warehouse conditions; however, condensation on cold pellets at ambient relative humidity above 60% can produce surface microgels and should be addressed through material warming or compressed-air drying. For monolayer produce and bread bag constructions, the resin is used at 100 wt%; for structures requiring higher dart impact and seal integrity on vertical form-fill-seal lines, 80 wt%–95 wt% Bapolene® 133F is dry-blended with 5 wt%–20 wt% butene-based LLDPE to increase machine-direction tear resistance and hot-tack force. Slip and antiblock masterbatches are introduced at 1 wt%–3 wt%, yielding typical erucamide concentrations of 0.05 wt%–0.15 wt% and synthetic silica concentrations of 0.1 wt%–0.3 wt% in the final film. Compliance is anchored to FDA 21 CFR 177.1520 for food-contact olefin polymers, Regulation (EU) No 10/2011 with overall migration limits of 10 mg/dm², and Regulation (EC) No 1935/2004 combined with Commission Regulation (EC) No 2023/2006 for good manufacturing practice. Copolymer and additive-specific migration limits are confirmed under the test conditions prescribed in EN 1186-1:2002. Terminal finished product types include produce bags, bakery bread bags, frozen-food liners, form-fill-seal pouches, and retail carrier bags. The grade is not suited to hot-fill applications above 90°C or to structures requiring oxygen barrier properties; such applications require coextrusion with EVOH and tie layers, which places Bapolene® 133F in the sealant and skin layers rather than as a functional barrier. Published migration data for high-throughput vertical form-fill-seal production at speeds above 60 cycles/min is limited.

    Can Bapolene® 133F Be Used as the Base Resin in UV-Stabilized Silage and Greenhouse Cover Films?

    Processing of agricultural silage bale wrap and greenhouse cover structures using Bapolene® 133F occurs on three-layer blown-film coextrusion lines with die diameters of 200 mm–400 mm, blow-up ratios of 2.5:1–3.2:1, and melt temperatures of 170°C–200°C. For silage wrap, film thickness is held between 20 µm and 30 µm; greenhouse covers are run at 100 µm–180 µm with widths of 8 m–14 m, requiring dual winders and bubble stabilizers. The base resin is incorporated at 92 wt%–96 wt%, with a UV-stabilizer masterbatch at 4 wt%–8 wt% delivering hindered amine light stabilizer levels of 0.3 wt%–0.8 wt% in the finished film; greenhouse grades additionally receive an anti-drip or anti-fog additive masterbatch at 1 wt%–2 wt%. Compliance for silage and horticultural films is based on EN 13206:2017 for cover films used in agriculture and horticulture, with tensile properties determined by ISO 527-3:2018, tear resistance by ISO 6383-1:2015, and light transmission/ageing performance under EN 13206 weathering protocols. Finished product types include round bale silage wrap, tube silage covers, greenhouse roofing and side sheets, and low tunnel covers. Outdoor service life is dependent on regional solar irradiance and stabilizer package; published data for this specific resin configuration under tropical UV ageing is limited, so site-specific weathering tests under ISO 877-1:2009 are required before warranty decisions. The grade is not formulated for long-term mulch film requiring three-season tensile retention; such configurations typically require LLDPE-dominant structures with higher stabilizer loadings and filler packages to control thermal radiation.

    Where construction vapor retarders and heavy-duty industrial liners must withstand creasing, rebar contact, and site-abrasion during concrete placement, Bapolene® 133F is specified at 150 µm–250 µm thickness and run on high-stalk blown-film lines with die diameters of 250 mm–400 mm, output rates of 350 kg/h–600 kg/h, and blow-up ratios of 2.0:1–2.6:1. The extruder barrel lengths are typically 30:1–33:1 L/D, and internal bubble cooling is used to limit film blocking at maximum throughput. Formulations combine 60 wt%–80 wt% Bapolene® 133F with 20 wt%–40 wt% post-industrial recycled LDPE or LLDPE; carbon black masterbatch is added at 2.5 wt%–3.5 wt% when UV exposure is anticipated, and anti-static or slip masterbatch may be added at 1 wt%–2 wt% for waste-handling liners. Compliance for construction sheeting is based on ASTM D4397-16 for polyethylene sheeting in construction, ASTM D882-18 for tensile properties, ASTM D1922-15 for tear resistance, and ASTM D1709-16a for dart impact. Terminal finished products include dumpster liners, demolition debris bags, under-slab vapor retarders, asbestos-abatement containment, temporary weather shielding for framed structures, and equipment covers. The material is not appropriate for primary geomembrane containment of hydrocarbon or solvent streams; such service requires HDPE or f-PVC geomembrane formulations with welded seam testing under ASTM D6392-12.

    Formulation gradient and blown-film process window matrix for food-contact, agricultural, and industrial liner applications
    Application fieldBapolene® 133F loadingCo-resin or additive loadingDie gapMelt temperatureBlow-up ratioFilm thickness
    Food-contact monolayer/coextruded packaging80–100 wt%0–20 wt% LLDPE + 1–3 wt% slip/antiblock masterbatch1.5–2.5 mm160–200°C2.0:1–2.8:120–100 µm
    Agricultural silage and greenhouse cover films92–96 wt%4–8 wt% UV masterbatch + 1–2 wt% anti-drip masterbatch1.8–2.2 mm170–200°C2.5:1–3.2:120–180 µm
    Heavy-duty industrial liners and construction vapor barriers60–80 wt%20–40 wt% recycled LDPE/LLDPE + 2.5–3.5 wt% carbon black masterbatch2.0–2.8 mm165–200°C2.0:1–2.6:1150–250 µm

    When Collation Shrink Film Demands Burn-Through Resistance Along the Seal Edge

    Collation shrink and display overwrap films incorporating Bapolene® 133F are produced as coextruded tubes using die gaps of 1.2 mm–1.8 mm, then oriented in the machine direction and transverse direction in a double-bubble process at orientation ratios of 3:1–5:1. In the formulation, Bapolene® 133F is used at 70 wt%–85 wt% with 10 wt%–25 wt% EVA containing vinyl acetate content of 12%–18%, or with LLDPE for higher puncture resistance in bottle bundling. The EVA modification lowers seal initiation temperature to 85°C–100°C and widens the heat-seal window on transverse seal-jaw lines, reducing burn-through at gauges of 35 µm–60 µm. Thermal shrinkage is assessed according to ASTM D2732-14 in oil or air, and shrink force is measured by ISO 14616:1997; typical free shrink values for collation films are 60%–80% in the transverse direction and 20%–40% in the machine direction. Regulatory compliance for general packaging is anchored to REACH Article 33 and RoHS Directive 2011/65/EU where the overwrap enters electronics-related packaging streams. Terminal finished products include can multipack overwrap, bottle bundling film, boxed-product display overwrap, and printed shrink sleeves for promotional trays. The grade is not formulated for high-shrink polyolefin food-contact use requiring oxygen barrier; such applications require multilayer structures with EVOH or PVDC, and published data for high-speed bundling at speeds above 45 cycles/min is limited.

    Sterile Barrier Pouch Sealing Layers and Ethylene Oxide Compatibility

    Bapolene® 133F is processed into the plastic web of sterile barrier pouch systems at 40 µm–80 µm thickness on blown-film lines with contaminant-controlled cooling air and inline thickness profiling. The film is treated by corona discharge to a surface energy of 38 dyn/cm–42 dyn/cm before lamination or extrusion coating with a sealant adhesive; the LDPE layer provides the heat-seal surface against paper or Tyvek® in chevron pouch and header bag constructions. In formulation, the resin is used at 100 wt% or blended with 5 wt%–15 wt% ethylene-vinyl acetate or LDPE-based sealant tie resins to broaden seal latitude on rotary band sealers running at 115°C–140°C. Compliance is defined by ISO 11607-1:2019 for sterile barrier systems, EN 868-5:2018 for sealable pouches and reels of porous materials and plastic film construction, FDA 21 CFR 177.1520 for the olefin polymer, and biocompatibility evaluation under ISO 10993-5:2009 for cytotoxicity and ISO 10993-12:2021 for sample preparation. Terminal finished product types include chevron pouches for ethylene oxide sterilization, header bags, and reel stock for form-fill-seal packaging of gowns, drapes, syringes, and procedure kits. The material is not appropriate for steam autoclave cycles at 121°C or higher because dimensional distortion and seal creep may occur; ethylene oxide processing at 50°C–60°C and gamma sterilization up to 25 kGy are the operational boundaries typically accepted for LDPE-based sterile barrier webs.

    Compliance standard matrix by application field
    Application fieldPrimary standardTest method or clauseRequirement or limit
    Food-contact packagingFDA 21 CFR 177.1520Olefin polymer specificationConforms for food contact
    Agricultural cover filmsEN 13206:2017Cover film classification and weatheringSite-specific UV ageing validation
    Construction sheetingASTM D4397-16Polyethylene sheeting specificationThickness, tensile, and tear minimums
    Collation shrink filmREACH / RoHS Directive 2011/65/EUArticle 33 and substance restrictionsNo listed substances above threshold
    Medical sterile barrierISO 11607-1:2019Seal strength, integrity, and microbial barrierValidated sterile barrier performance

    Temporary Protective Film for Coil-Coated Metals Requires Controlled Peeling Forces

    For temporary protection of coil-coated steel and aluminum composite panels, Bapolene® 133F is extruded at thicknesses of 50 µm–100 µm, with corona treatment at 38 dyn/cm–42 dyn/cm applied immediately before pressure-sensitive adhesive coating on a separate lamination line. The base film is blown on lines with die diameters of 150 mm–250 mm and melt temperatures of 165°C–190°C; subsequent adhesive lamination is run at 40 m/min–80 m/min with solvent-based acrylic or water-based adhesive systems. The formulation uses 100 wt% Bapolene® 133F for low-peel applications or 85 wt%–95 wt% Bapolene® 133F with 5 wt%–15 wt% LLDPE to raise puncture resistance during profile stacking. Peel adhesion to stainless steel is controlled to 0.5 N/25 mm–3.0 N/25 mm using ASTM D3330/D3330M-04; tensile performance is evaluated by ISO 527-3:2018. Regulatory compliance references REACH, RoHS Directive 2011/65/EU for electronics-related coated metals, and GB/T 2792-2014 where Chinese coated-aluminum converters require peel force documentation. Terminal finished products include protective film for aluminum composite panels, coil-coated steel sheets, PVC window profiles, and anodized aluminum extrusions. The film is intended for temporary indoor or covered outdoor storage only; adhesion build and UV degradation above 60°C or under direct weathering can produce adhesive residue, and published data for long-term outdoor exposure beyond 3 months is limited.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 133F Polyethylene, Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bamberger Polymers Bapolene® 133F is a low-density polyethylene homopolymer designed for blown film extrusion. The grade designation separates it from higher-melt-index LDPE film grades, extrusion coating resins, and liner grades within the supplier’s Bapolene portfolio. Unlike linear low-density polyethylene produced by low-pressure copolymerization, the base polymer is polymerized in a high-pressure process, so the molecular architecture contains branched chains. This branching increases transient extensional viscosity and melt tension, which are decisive for bubble stability in air-quenched blown film. The product data sheet lists a nominal melt index of 0.25 g/10 min when measured under ASTM D1238 at 190 °C with 2.16 kg; the equivalent ISO 1133-1:2022 melt mass-flow rate test is used for standardized comparison outside North America. The nominal density is 0.923 g/cm³ under ASTM D1505 or ISO 1183-1:2019. These values are not batch release limits; the certificate of analysis for each production lot must be consulted for actual values.

    The resin is intended for monolayer and coextruded film applications where moderate clarity, heat-seal integrity, and bubble robustness are needed. Typical end uses include heavy-duty shipping sacks, industrial liners, construction films, shrink bundling film, and overwrap. In coextruded structures, the material can be placed in the core or sealant layer, but its base resin additive package may not include a designated slip or antiblock level. Film processors must therefore verify whether additional masterbatch is required for the target coefficient of friction and blocking behaviour. Published film properties are generally measured on 50 µm blown film produced with a 2.5:1 blow-up ratio, a 38 µm die gap, and a frost line height appropriate to the equipment.

    Nominal physical properties of Bapolene 133F film grade
    Property Test method Nominal value
    Melt index ASTM D1238 / ISO 1133-1:2022 0.25 g/10 min
    Density ASTM D1505 / ISO 1183-1:2019 0.923 g/cm³
    Tensile yield strength, 50 µm film ASTM D882 9.5 MPa
    Tensile strength at break, MD/TD, 50 µm film ASTM D882 23 MPa / 18 MPa
    Elongation at break, MD/TD, 50 µm film ASTM D882 300% / 550%
    Dart impact resistance, F50 ASTM D1709A 85 g
    Elmendorf tear resistance, MD/TD ASTM D1922 4.0 N / 2.5 N
    Haze, 50 µm film ASTM D1003 7.5%
    Gloss at 60° ASTM D2457 60
    Vicat softening temperature ASTM D1525 91 °C

    Values in Table 1 are nominal physical properties from conditioned blown film specimens; they are not to be interpreted as specification limits, and ASTM D882 tensile data vary with extrusion conditions and gauge.

    How Does Low Melt Index and Long-Chain Branching Dictate Processing Conditions?

    At the stated melt index, the resin exhibits high shear viscosity. The pressure drop across a 100 mm spiral die at an output of 80 kg/h can be 15–25 MPa on a 50 mm extruder depending on die gap and melt temperature, although exact values require machine-specific pressure transducer data. The long-chain branching produces strain-hardening behaviour in the bubble, which means that local thinning under air-ring draw does not immediately lead to bubble failure. This is the key difference from linear resins, which have lower strain-hardening response and more abrupt neck-in. The processing window is therefore governed primarily by melt fracture and thermal oxidative degradation rather than bubble instability alone.

    Barrel temperature settings of 150 °C in the feed zone, 160 °C in the compression zone, and 170–180 °C in the metering zone are compatible with 24:1 to 30:1 L/D single-screw extruders. At the die entry, a melt temperature of 165–185 °C is recommended. Below 160 °C, sharkskin may appear as a series of transverse ridges on the film surface because the melt cannot relax entrance stresses in the die land. Above 195 °C, the risk of gel particles and oxidative odor increases, particularly at long residence times on high-output lines with low throughput fluctuations.

    Across production-scale runs, the most frequently observed bottleneck is bubble instability caused by air-ring turbulence, not by viscosity alone. Variations in ambient temperature or plant humidity, especially when relative humidity exceeds 60%, alter frost line position and can increase gauge scatter. Batch-to-batch differences in additive loading, if slip/antiblock masterbatch is introduced at the hopper, can further shift the coefficient of friction and blocking force; therefore, feeders must be calibrated for each lot when 2–5 wt% masterbatch is added.

    Surface moisture should be removed by hopper drying at 60 °C for 2 h when resin has been stored in unheated silos or bags exposed to condensation. No hydrolytic drying is required for the base LDPE polymer. Residence time and melt filtration are critical when the resin is processed on lines with excessive barrel temperatures or start-stop schedules. Because high-pressure LDPE contains long-chain branching and some high-molecular-weight fraction, gel formation can be observed if the resin is exposed to 190 °C for more than 20 min in stagnant zones. Screen packs with 20/60/100/20 mesh combinations are common downstream of the breaker plate to trap oxidized gel particles; a pressure rise of more than 5 MPa across the screen pack indicates screen replacement or reduced throughput. Batch-to-batch variation in high-pressure reactor conditions can shift the molecular weight distribution enough to require ±5 °C melt temperature adjustments, even when the melt index remains within specification. This sensitivity is smaller than for metallocene LLDPE but larger than for high-MI LDPE grades.

    According to typical equipment logs from production lines running 70 wt% of this grade in a monolayer structure, the coefficient of friction without added slip can remain above 0.50, which is too high for high-speed vertical form-fill-seal machines. Addition of 0.5–1.5 wt% erucamide-based slip masterbatch lowers the kinetic COF to 0.12–0.20, as measured by ASTM D1894, but migration equilibrium is not reached until 24–48 h after film production. Lines that handle freshly extruded film with automatic filling equipment must therefore account for this aging period. For printing and lamination, surface treatment by corona discharge is used to raise surface energy to 38–42 mN/m, as measured by ASTM D2578; the treated film should be used within a limited time because treatment decay accelerates under high humidity and temperature.

    Blown Film Die, Air Ring, and Frost Line Interactions

    Die gap selection should follow draw-down and film thickness. For film thicknesses from 30 µm to 80 µm, a die gap of 0.8–1.2 mm is typical; for 80–150 µm, gaps up to 1.5 mm reduce orientation-induced stresses. The die gap is not an adjustable parameter during production, but its interaction with blow-up ratio and frost line height controls the balance between machine-direction and transverse-direction properties. Low frost line settings of 100–150 mm from the die face increase quench rate and improve optical clarity but reduce tear resistance; high frost line settings of 250–400 mm increase crystallinity and can improve stiffness but produce haze and gauge bands.

    Dual-lip air rings with chilled air at 8–15 °C are frequently used for this grade to increase output while maintaining bubble neck geometry. On monolayer lines, the recommended blow-up ratio range is 2.0:1 to 3.0:1; below 2.0:1, transverse-direction tensile properties decline, and above 3.2:1, bubble oscillation and contact with the air-ring lip can occur. These boundaries are observed on conventional extruders with output rates of 0.8–1.2 kg/h per mm of die circumference; larger dies or internal bubble cooling systems can shift the upper limit but do not fundamentally alter the resin’s strain-hardening response.

    At a screw speed of 70 rpm on a 50 mm 30:1 L/D barrier screw, the melt pressure at the die entry is often recorded between 18 MPa and 25 MPa. Higher pressure increases melt temperature through viscous dissipation; therefore, screw cooling or lower screw speed may be necessary on lines that are not equipped with high-pressure dies. Because the resin’s viscosity curve is shear-thinning, increasing screw speed does not produce a proportionate output increase at high speeds; this is a limitation in high-throughput operations.

    When High-MI LDPE, LLDPE, and Metallocene Resins Are Compared for the Same Film Application

    Relative to a 2.0 g/10 min LDPE film grade of similar density, 133F offers higher melt tension and a wider bubble stability window but lower maximum drawdown. Thin-gauge cast film or rapid-cycle blown film operations that require ≤25 µm gauge at high line speed are therefore more often served by high-MI LDPE or LLDPE. Compared with a conventional C4 LLDPE at 1.0 g/10 min and 0.918 g/cm³, the 0.923 g/cm³ LDPE grade shows lower dart impact and puncture resistance but superior clarity, gloss, and lower extruder backpressure.

    In applications such as heavy-duty sacks where tear propagation and impact energy are critical, LLDPE may be blended with the 133F at 20–40 wt% to improve toughness while retaining bubble stability; however, the addition of LLDPE increases torque and die pressure, and may require a wider die gap of 1.2–1.5 mm to avoid melt fracture. Compared with metallocene-catalyzed LLDPE, the LDPE long-chain branched architecture provides higher melt strength but lower puncture and downgauging capability, so downgauging below 30 µm requires verification of dart impact and tear data on the specific film line.

    Compared with high-density polyethylene film, the lower density and higher branching reduce moisture barrier and stiffness but improve tear and impact at similar gauge. The heat-seal initiation temperature for LDPE is typically 105–115 °C, whereas HDPE film requires higher temperatures and a narrower sealing window. In barrier structures, HDPE film provides lower water vapour transmission rate and higher modulus; 133F is preferred when heat-seal initiation and optical clarity are more critical than moisture barrier.

    Comparative profile of film resin families at a 50 µm blown film reference point
    Resin family Nominal melt index Nominal density Dart impact F50 Haze Relative melt tension
    Bapolene 133F LDPE 0.25 g/10 min 0.923 g/cm³ 85 g 7.5% High
    High-MI LDPE film 2.0 g/10 min 0.922 g/cm³ 60 g 6.0% Low
    C4 LLDPE 1.0 g/10 min 0.918 g/cm³ 130 g 12% Moderate
    Metallocene LLDPE 0.8 g/10 min 0.918 g/cm³ 180 g 10% Moderate-low

    The relative melt tension values in Table 2 are qualitative rankings based on bubble stability and extensional viscosity, not normalized test values. Lot-specific data for 133F in Table 1 should prevail over the representative values in Table 2.

    Food-contact packaging produced from this resin must be validated against FDA 21 CFR 177.1520 for olefin polymers and, where applicable, Commission Regulation (EU) No 10/2011 with its specific migration limits. The base polymer is generally not considered hygroscopic, so no pre-drying is required at relative humidity below 60%; if surface condensation is suspected after storage in unheated silos, hopper drying at 60 °C for 2 h is sufficient. The resin should not be stored in direct sunlight for prolonged periods or in outdoor conditions that allow temperature cycling above 50 °C, because additive migration and pellet blocking can occur. As with all high-pressure LDPE film grades, the final extrusion setting must be derived from the certificate of analysis, the specific blown film line, and the target film specification, not from nominal data alone.

    Top