Bamberger Polymers Bapolene 133b Lldpe Hexene Film Grade

Bamberger Polymers Bapolene® 133B LLDPE, Hexene Film Grade

    • Product Name: Bamberger Polymers Bapolene® 133B LLDPE, Hexene Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 893248
    Product Bamberger Polymers Bapolene® 133B LLDPE, Hexene Film Grade
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene
    Density 0.918 g/cm³
    Melt Index 1.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 10.3 MPa (1500 psi)
    Tensile Strength At Break 24.1 MPa (3500 psi)
    Elongation At Break 700%
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 12%
    Gloss 70%
    Melting Point 125 °C
    Vicat Softening Point 100 °C

    As an accredited Bamberger Polymers Bapolene® 133B LLDPE, Hexene Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 133B LLDPE Hexene Film Grade is packaged in 25 kg (55 lb) bags, palletized for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL loading: Bamberger Polymers Bapolene® 133B LLDPE Hexene Film Grade, 25 kg bags, palletized, approx. 18–22 MT per container.
    Shipping Bapolene® 133B LLDPE Hexene Film Grade is shipped as non-hazardous solid resin pellets. Standard packaging includes 25 kg (55 lb) moisture-resistant bags on pallets, or bulk trucks/railcars. Store in a cool, dry, ventilated area away from sunlight and ignition sources. No special DOT/IMDG/IATA hazardous classification applies.
    Storage Store Bapolene® 133B LLDPE, hexene film grade, in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep original bags sealed and palletized off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure, excessive stacking, and incompatible chemicals. Maintain stable ambient conditions and follow FIFO stock rotation.
    Shelf Life Bapolene® 133B has a shelf life of 24 months from manufacture when stored cool, dry, and in original packaging.
    Application of Bamberger Polymers Bapolene® 133B LLDPE, Hexene Film Grade

    High-speed cast stretch film conversion places Bapolene 133B in the structural layer of pallet unitization films where pre-stretch ratios routinely exceed 200% and line speeds reach 450–600 m/min on chill-roll cast coextrusion lines. The base resin blend is compounded at 65–80 wt% Bapolene 133B with 15–25 wt% metallocene ethylene-octene plastomer of 0.870–0.902 g/cm³ density and 5–10 wt% long-chain-branched LDPE for shear thinning; polyisobutylene cling additive is injected at 1.5–2.5 parts per hundred resin through a heated liquid port downstream of the feed zone. On a 90 mm single-screw extruder with 30:1 L/D and a Maddock shear mixer, barrel zones are set from 205–250 °C and die-lip melt temperature is held at 238–260 °C. The cast die gap is maintained at 0.5–0.8 mm, air-knife pressure at 0.2–0.4 bar, primary chill-roll temperature at 18–24 °C, and secondary roll at 22–28 °C. The governing process conflict is draw resonance; because the linear hexene-copolymer backbone stores less extensional strain than branched LDPE, draw-down ratio above 35:1 becomes unstable unless plastomer loading exceeds 25 wt%. Chill-roll temperatures below 16 °C are avoided because condensation on the cast web creates haze bands and intermittent cling slip. Edge-trim regrind above 15 wt% is also constrained because non-uniform polyisobutylene migration shifts peel-cling behavior. Film verification is anchored to ASTM D882 for tensile at break, ASTM D5748 for puncture resistance at 0.5 mm probe radius, ASTM D5458 for peel cling, and ISO 4593 for thickness. Terminal articles include pre-stretched hand rolls, automated wrapper machine film, and heavy-load bundling wrap at 15–30 µm nominal thickness.

    Representative comparative data for butene-copolymer and hexene-copolymer LLDPE blown film at 25 µm and 0.918 g/cm³ resin density are shown in the table; actual Bapolene 133B film values depend on screw design, additives, and draw ratio.

    PropertyTest methodC4 LLDPEC6 LLDPE
    Dart drop impact, method AISO 7765-190–120 g130–180 g
    Elmendorf tear, machine directionISO 6383-2300–400 g450–600 g
    Elmendorf tear, transverse directionISO 6383-2350–450 g500–700 g
    Tensile at break, machine directionISO 527-335–40 MPa40–48 MPa
    Protrusion puncture resistanceASTM D574835–45 N50–65 N

    Why Does Bapolene 133B Appear in the Core Layers of Heavy-Duty Blown Film Sacks Rather Than as a Monolayer Stiffness Resin?

    Core-layer placement is driven by the need to combine hexene-copolymer dart impact with high-density polyethylene modulus. A monolayer LLDPE sack lacks secant modulus and collapses during filling; a monolayer HDPE sack fails Elmendorf tear along machine-direction creases. In a 3-layer coextruded structure, the core contains 60–80 wt% Bapolene 133B and 20–40 wt% high-molecular-weight HDPE at 0.956–0.960 g/cm³; the skins are a lower-modulus hexene LLDPE/metallocene blend to support seal strength. On a 200 mm coextrusion die with 1.4–2.0 mm gap and 2.2:1–3.0:1 blow-up ratio, the frost line is positioned at 5–7 die diameters. The principal process failure appears as bubble tremor when high-stalk height exceeds 8 die diameters, producing gauge bands visible at haul-off speeds above 80 m/min. A 65 mm grooved-feed extruder with 28:1 L/D processes the core at a 180–220 °C barrel profile and 230–240 °C melt temperature; residence time at melt temperature is kept below 3 min. Camera-based gel inspection uses 3×3 cm sample fields with an acceptance limit of 5 gels larger than 200 µm. Filled sack qualification for polymer granule or fertilizer service uses a 1.2 m drop height at 25 kg fill weight according to ISO 7965-1; the seal should retain 80% of parent film tensile strength. Terminal articles include gusseted valve sacks for pet food, fertilizer sacks, and form-fill-seal bags for densified plastic pellets.

    Agricultural silage and greenhouse cover coextrusions place Bapolene 133B in a service window of −10 °C to 60 °C and continuous UV exposure. The resin is extruded as the core layer of a 3-layer blown film with a stabilizer package of 0.8–1.2 wt% hindered amine light stabilizer, 0.2–0.4 wt% hydroxybenzophenone or hydroxyphenyltriazine UV absorber, and 0.5–1.0 wt% precipitated silica antiblock in the skin layers. The die diameter is 1,600–2,000 mm, the blow-up ratio is 1.8:1–2.5:1, and the structure is run in a low-stalk configuration to reduce fold creasing and gusset weakness. Field failures on silage clamps are dominated by puncture from maize stubble and abrasion against trench walls; silage clamp covers are therefore specified at 120–150 µm minimum thickness, while greenhouse side rolls are specified at 150–200 µm. Sulfur-containing agricultural chemicals and chlorine-based fumigants can accelerate oxidation at the polyethylene surface; if such contact is planned, the converter must pre-qualify the formulation under EN 13206 and ISO 4892-2 accelerated weathering for 3,600–5,000 h. Published long-term field data for Bapolene 133B in silage covers specifically is limited; conversion trials should therefore include Xenotest and buried-panel testing rather than density extrapolation. Light transmission for greenhouse service is measured by an integrating sphere spectrophotometer per ISO 13468-1 and should remain above 75% in the photosynthetically active radiation band. Terminal articles include silage bags, clamp covers, greenhouse side rolls, and temporary tunnel covers.

    When Frozen Food Packaging Must Retain Seal Integrity After a −25 °C Drop

    Conditioning of sealed pouches at −25 °C for 24 h followed by a 1.5 m free-fall drop onto concrete is the governing qualification test for IQF vegetables, seafood, and frozen dough. In a 7-layer coextruded barrier film, Bapolene 133B is used as the sealant layer at 20–30 wt% of total thickness; the structure includes a central EVOH barrier layer and maleic anhydride-grafted tie layers, with skin layers composed of 70–80 wt% hexene LLDPE and 20–30 wt% LDPE. On a 55 mm blown film line with 25:1 L/D, the die gap is 1.2–1.6 mm, the blow-up ratio is 2.0:1–2.8:1, and melt temperature is maintained below 240 °C. Seal initiation is measured by ASTM F1921 method A and is specified at 95–110 °C for the sealant blend. Seal strength after 0.5 s dwell is evaluated by ASTM F88; at −18 °C, values below 18 N/25 mm are cause for rejection because frozen transport punctures initiate at the seal edge. The limiting degradation pathway is thermal oxidation in the die; if melt remains above 245 °C for more than 3 min, the C6 branch sites form gel streaks that reduce low-temperature dart impact by 20–30%. Food-contact compliance is verified under 21 CFR 177.1520 and EU 10/2011 with an overall migration limit of 10 mg/dm²; the finished structure must be tested because EVOH and tie resin migration are not accounted for by the LLDPE resin alone. Terminal articles are pillow pouches for frozen shrimp, zipper-reclosed vegetable bags, and lidding film for frozen dough trays.

    Unsupported Industrial Liners and the Case for Hexene-Copolymer Tear Resistance in Geomembrane-Like Service

    Unsupported industrial liner conversion relies on the improved slow-crack resistance of the C6 structure under folded storage and repeated flexing. Bapolene 133B constitutes 95–98 wt% of the film compound, with carbon black masterbatch at 2.0–3.5 wt% and processing stabilizer at 0.3–0.8 wt%. The film is produced on high-output blown film towers with internal bubble cooling, a 300–400 mm die diameter, a die gap of 2.0–2.8 mm, a blow-up ratio of 1.8:1–2.2:1, and tower height of 6–8 m. The primary failure mode is seam splitting at impulse welds, not burst; heat-sealed seam specimens must retain 80% of parent film tensile strength per ISO 527-3. Tear resistance for a 250 µm monolayer liner is measured by ISO 6383-2 Elmendorf tear and ISO 6383-1 trouser tear; typical converter specifications require a trouser tear value of at least 300 N/mm in the machine direction. Crease whitening after five flex cycles on a 180° fold is an early indicator of orientation-induced fibrillation; formulations with high HDPE content fail this test, which is why the hexene-copolymer backbone is preferred for unsupported liners. The application boundary excludes aromatic hydrocarbons, chlorinated solvents, and continuous service above 50 °C; chemical resistance after immersion is evaluated by ASTM D543 practice using 7-day exposure at 23 °C. Industrial packaging compliance is governed by REACH 1907/2006 and, when used as a liner in rigid plastics drums, the assembly is certified under UN 1H2. Terminal articles are drum liners, collapsible IBC liners, and secondary containment films for pesticide and fertilizer storage.

    Extrusion lamination positions Bapolene 133B as the sealant layer in flexible packaging structures where the hot-tack window sets filling-line speed. On a coextrusion coating line running at 250–350 m/min, a 90 mm extruder with 30:1 L/D and a 2.8:1–3.2:1 compression ratio feeds the resin to a flat die lip maintained at 305–325 °C. The resin is blended at 60–80 wt% with long-chain-branched LDPE to suppress draw resonance and reduce neck-in; the LDPE fraction also raises melt-curtain sag resistance during lamination to aluminium foil and polyester. Hot tack is measured by ASTM F1921 method A and is specified at 95–115 °C; seal strength after 0.3 s dwell is measured by ASTM F88 with a target of 15–20 N/25 mm at 121 °C filling temperature. The primary process defect is surging caused by the higher backpressure of the linear backbone in the screw feed section; a shallow-grooved feed bushing and a barrier screw of 25:1 L/D feed section reduce melt-temperature fluctuation to within ±3 °C. The grade is not automatically suitable for full retort; exposure to 121 °C steam for 30 min can produce more than 2% sealant-layer shrinkage in multi-layer laminates unless the converter qualifies the structure under FDA 21 CFR 177.1395. Food-contact compliance is determined by EU 10/2011 overall migration and 21 CFR 177.1520 for the olefin layer. Terminal articles are stand-up pouches, quad-seal coffee bags, and high-speed cup lidding webs.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 133B LLDPE, Hexene Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bapolene® 133B is a linear low density polyethylene supplied by Bamberger Polymers for blown film extrusion. The nominal melt flow rate is 1.0 g/10 min at 190°C under 2.16 kg load (ASTM D1238 Procedure A or ISO 1133-1), and the nominal density is 0.918 g/cm³ (ASTM D1505 or ISO 1183-1). These specification points place the resin in the medium-flow LLDPE film category, but the hexene designation is the principal differentiator from butene-based LLDPE grades of identical melt index and density. Published data for the complete film property matrix of Bapolene 133B is limited; the supplier technical data sheet and lot certificates for slip, antiblock, and antioxidant levels are required before incoming quality limits are established. Differential scanning calorimetry (ASTM D3418) can characterize melting behavior if extrusion or seal modeling requires crystallinity input, but no product-specific thermogram is reproduced here.

    What Consequence Does Hexene Short-Chain Branching Have on Solid-State Film Properties?

    Hexene incorporation in a linear polyethylene backbone produces a butyl branch of four carbon atoms, while butene produces an ethyl branch of two carbon atoms and octene produces a hexyl branch of six carbon atoms. The longer hexene branch disrupts the orthorhombic polyethylene lattice more effectively at equivalent comonomer molar content, increasing the probability of tie-chain formation between adjacent lamellae during blown film crystallization. Tie-chain concentration is not measured in routine lot release; it is inferred through Elmendorf tear (ASTM D1922 / ISO 6383-2) and dart drop impact (ASTM D1709 / ISO 7765-1). A 0.918 g/cm³ hexene LLDPE therefore tends to show higher toughness than a butene LLDPE of identical density and melt index, particularly in films below 50 μm where puncture and brittle tear are limiting failure modes. Because Bapolene 133B is a conventional Ziegler-Natta grade, its comonomer distribution is broader than that of a metallocene hexene LLDPE. The broad distribution supports shear thinning in the die but may widen the heat-seal range and increase extractable fractions relative to narrow-dispersion metallocene resins. Molecular weight distribution, branching index, and tie-chain concentration for this specific resin are not publicly specified.

    Hexene Versus Butene at Constant Density and Melt Index

    When a converter replaces a butene LLDPE of 1.0 g/10 min melt flow rate and 0.918 g/cm³ density with Bapolene 133B on the same blown film line, the expected differences usually appear first in transverse-direction tear and dart drop. Actual film performance values for Bapolene 133B are not supplied in this document; direct substitution should not be based solely on density and melt index. In industrial comparisons of 0.918 g/cm³ hexene and butene Ziegler-Natta films, hexene grades commonly show a dart drop advantage at 25 μm, but the magnitude depends on die gap, blow-up ratio, frost line height, and melt temperature. At heavy-duty sack film gauges between 50 μm and 125 μm, the hexene architecture generally provides better low-temperature toughness, although field performance still depends on bag geometry, closure mechanism, and fill temperature. Compared with an octene LLDPE of equal density, hexene can approach most of the toughness benefit in many packaging applications; against metallocene hexene grades, Bapolene 133B may show lower clarity and lower dart drop at thin gauges because metallocene resins often have a narrower molecular weight distribution and more uniform comonomer placement. These comparisons are structural and should not be interpreted as guaranteed specifications for Bapolene 133B.

    On monolayer blown film lines, the resin is processed with a LLDPE-specific barrier screw and a die gap from 1.0 mm to 1.5 mm. A barrel profile of 180°C, 195°C, 205°C, and 215°C with a die set-point of 220°C is a common starting point for a 45 mm to 65 mm grooved-feed extruder having L/D 24:1 to 28:1. Melt temperature at the die should be maintained between 190°C and 225°C. Above 230°C, residence-time-driven oxidative gel formation becomes increasingly likely; below 190°C, excessive melt viscosity can destabilize the bubble. Blow-up ratios from 2.0:1 to 3.0:1 are typical. Above 3.2:1, transverse-direction tear usually increases while machine-direction tear and puncture resistance may decline because orientation shifts toward the transverse direction. Below 1.8:1, haze may improve but dart drop can lose consistency because machine-direction orientation increases. If the frost line is set too low, the film may be quenched before stress relaxation is complete, producing machine-direction brittleness. If the frost line is too high, bubble sag can increase gauge variation. The sharkskin melt fracture threshold for Bapolene 133B has not been published. On die gaps below 0.8 mm, elevated shear stress may exceed the critical onset for this product class; the onset should be mapped on the production die by stepwise increases in screw speed with a clean screen pack and constant melt temperature.

    Rheological assessment of the melt can be performed by capillary rheometry at 190°C and 230°C to define apparent shear-rate limits. LLDPE film resins are shear-thinning, but the critical shear rate for sharkskin is a function of die gap, temperature, and molecular weight distribution. For Bapolene 133B, no product-specific flow-curve data or critical shear stress are publicly available. On a production die, the onset of surface roughness should be identified by deliberately increasing screw speed while holding melt temperature and screen-pack condition constant. If sharkskin appears, the first corrective actions are to raise the die temperature within the allowable range, widen the die gap, or reduce throughput. Raising the die temperature above 230°C should be avoided because oxidative degradation may increase gel formation and reduce film appearance ranking.

    Scaling from laboratory cast film to production blown film is not valid for this product class. Blown film orientation and thermal history influence crystalline morphology and mechanical properties; a film produced on a small laboratory line with a 20 mm extruder may not reproduce the dart drop or tear performance of a production line with a 65 mm extruder and internal bubble cooling. Internal bubble cooling can stabilize large-diameter bubbles and improve output, but it also affects frost line height and quench rate. No product-specific scale-up factors for Bapolene 133B are published.

    Sealing behavior on form-fill-seal lines should not be inferred from melt index alone. Starting dwell times from 0.5 s to 1.0 s and jaw pressures from 300 kPa to 500 kPa are common for LLDPE sealant layers, but each machine requires its own response curve. Seal strength after conditioning at 23°C and 50% RH for 24 h is commonly measured with ASTM F88; hot tack is measured with ASTM F1921. Bapolene 133B is not marketed specifically as a low-seal-initiation grade, so converters requiring a narrow seal window should compare it with metallocene or octene-based sealants. No product-specific seal initiation or hot tack data are currently published.

    When Bapolene 133B Is Combined with LDPE or High-Density Polyethylene in Coextruded and Blended Structures

    Blending 10–30 wt% high-pressure LDPE into Bapolene 133B raises low-shear viscosity and improves bubble stability on high-stalk extrusion lines, but it also reduces dart drop and Elmendorf tear compared with the neat LLDPE layer. A discrete HDPE skin layer is generally preferred when stiffness and toughness are both required, because the skin preserves the core tear resistance while the HDPE layer contributes modulus. Coextrusion die feedback must be designed without stagnant flow paths. Hexene LLDPE held above 230°C for long residence times can undergo oxidative degradation, generating gel particles and visible speck defects. For satellite extruders of 35–45 mm diameter, the LLDPE temperature profile should be lower than the HDPE profile to prevent excessive shearing and local melt-temperature overshoot. Layer adhesion and interlayer thickness distribution must be confirmed by cross-sectional microscopy on the specific die geometry; monolayer film data cannot be transferred directly to coextruded structures. Published data comparing Bapolene 133B to other hexene film resins in coextrusion lines is limited.

    Film blocking and coefficient of friction are influenced by the additive package rather than the base resin alone. Hexene LLDPE films without sufficient slip or antiblock can block on the roll after winding, especially at gauge above 50 μm. Coefficient of friction is measured by ASTM D1894, and blocking force by ASTM D3354. Surface treatment for printing or lamination is measured by ASTM D2578 wetting tension. No Bapolene 133B-specific additive concentrations or surface-energy decay rates are published. Converters should specify target COF, blocking load, and dyne level in the incoming resin or finished film specification and verify them after storage, because slip migration to the film surface is time- and temperature-dependent.

    Incoming lot testing typically includes melt flow rate (ASTM D1238) and density (ASTM D1505) to confirm that the resin is within normal specification. Film converters may also perform gel count analysis by extruding a thin film and counting visual defects under a standardized light table. Lot-to-lot variation in comonomer content can shift seal initiation and tear properties even when density remains within specification; control charting of supplier lot certificate values is recommended. Bapolene 133B-specific standard deviation values are not publicly available. Without control charts, small changes in hexene content or molecular weight may remain undetected until downstream packaging lines experience seal failures or field returns.

    Food-contact suitability is evaluated under 21 CFR 177.1520 for olefin polymers. The finished article must meet extractable fraction limitations and end-use conditions appropriate for the intended food type and temperature. When the film is used as a component of paper or paperboard packaging, 21 CFR 176.170(c) may also apply. For European Union applications, the supplier’s declaration under Regulation (EU) No 10/2011 must be obtained; that declaration should state overall migration limits, specific migration limits, and dual-use additive compliance. The standard Bapolene 133B grade should not be used in medical or pharmaceutical contact applications unless the supplier has issued a specific statement for those end uses. For outdoor agricultural film, the base resin must contain an adequate UV stabilizer package. If moisture condensation is observed on pellets, pre-drying at 60°C for 2 h is sufficient because polyethylene is not hygroscopic in normal storage. The resin should be stored away from direct sunlight, strong oxidizing agents, and excessive heat to prevent free-radical degradation before extrusion.