Bamberger Polymers Bapolene 122f Polyethylene Film Grade

Bamberger Polymers Bapolene® 122F Polyethylene, Film Grade

    • Product Name: Bamberger Polymers Bapolene® 122F Polyethylene, Film Grade
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 148634
    Density 0.922 g/cm³
    Melt Flow Rate 2.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 10.0 MPa
    Tensile Strength At Break 20.0 MPa
    Elongation At Break 500%
    Flexural Modulus 200 MPa
    Dart Drop Impact 100 g
    Elmendorf Tear Strength Md 200 g/mil
    Elmendorf Tear Strength Td 300 g/mil
    Haze 8%
    Gloss 70%
    Vicat Softening Point 90°C
    Melting Point 110°C
    Recommended Extrusion Temperature 160-190°C

    As an accredited Bamberger Polymers Bapolene® 122F Polyethylene, Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 122F Polyethylene, Film Grade is supplied in 55 lb bags, 40 bags per pallet (2,200 lb total).
    Container Loading (20′ FCL) 20′ FCL container loaded with Bamberger Polymers Bapolene® 122F Polyethylene, Film Grade, palletized bags secured for ocean transport.
    Shipping Bamberger Polymers Bapolene® 122F Polyethylene, Film Grade is a non-hazardous solid resin shipped as pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Pallets are stretch-wrapped and labeled. Transport in clean, dry, ambient conditions; avoid moisture, contamination, heat, and direct sunlight. Standard freight; no hazardous placards required.
    Storage Store Bapolene® 122F in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Maintain temperatures below recommended limits, use first-in, first-out stock rotation, inspect containers regularly, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Bapolene 122F polyethylene film grade has indefinite shelf life when stored cool, dry, sealed, and protected from direct sunlight and contaminants.
    Application of Bamberger Polymers Bapolene® 122F Polyethylene, Film Grade

    Blown film lines producing direct food-contact bags from Bapolene® 122F typically operate with an air-cooled annular die at a die gap between 0.9 mm and 1.5 mm, a blow-up ratio of 2.0:1 to 3.0:1, and a frost-line height of 250 mm to 400 mm. The resin, a low-density polyethylene homopolymer with nominal melt flow rate 2.2 g/10 min at 190°C/2.16 kg under ASTM D1238-23 and nominal density 0.922 g/cm³ under ASTM D792-20, is blended with a slip masterbatch at 0.5 wt% to 1.5 wt% and an antiblock masterbatch at 2.0 wt% to 5.0 wt%, both carried in low-density polyethylene to prevent viscosity mismatch at the die lip. Extruder barrel zones are set from 160°C to 190°C, adapter temperature at 180°C, and die temperature at 185°C; melt temperature should not exceed 232°C, above which oxidative chain scission can generate extractable oligomers that impair organoleptic performance. Gauge control at 25 µm to 50 µm is maintained by a dual-sensor thickness scanner with closed-loop control, while haze is measured according to ASTM D1003-21 and tensile properties according to ASTM D882-18. Finished bags are used for fresh produce, bakery film, and retail bread bags. Compliance relies on FDA 21 CFR 177.1520 for olefin polymers in contact with aqueous, acidic, and fatty foods up to specified temperature limits, and on EU Regulation No 10/2011, Annex I, with overall migration below 10 mg/dm² under test conditions OM2 for short-time high-temperature contact. Extractables testing is commonly performed according to ISO 17716 or using a 40°C, 10-day food simulant protocol. This grade is not recommended for oxygen barrier applications; if oxygen transmission rate below 100 cm³/m²·day·atm is required, coextrusion with an ethylene-vinyl alcohol barrier layer is necessary.

    Why Does Silage Cover Film Extrusion Require UV Stabilizer Masterbatch Pre-Dispersion Before the Final Mixing Stage?

    Agricultural silage cover and greenhouse films use Bapolene® 122F because of its process stability and acceptable tear initiation resistance at 150 µm to 200 µm thickness. The formulation includes a hindered amine light stabilizer masterbatch at 2.0 wt% to 4.0 wt%, a UV absorber masterbatch at 1.0 wt% to 2.0 wt%, and optionally a carbon black masterbatch at 2.5 wt% to 5.0 wt% for silage pit covers where opacity is required. Pre-dispersion is required because direct metering of low-viscosity liquid additives into the main feed port creates localized lubricant-rich zones that reduce screw conveying efficiency and produce melt pressure oscillation. On a single-screw extruder with a 30:1 L/D barrier screw and Maddock mixing section, melt pressure at the screen pack typically remains between 180 bar and 240 bar, but undispersed additive can cause pressure variation exceeding ±15 bar within 10 min. Barrel temperatures from 165°C to 195°C and a die temperature of 190°C are used; coolant air temperature at the frost line is maintained at 12°C to 18°C to stabilize bubble geometry. The finished silage cover retains tensile elongation at break above 500% after 1,000 h of accelerated weathering under ASTM G154-23 when compounded properly, but published full-scale field exposure data for this specific film grade is limited. Compliance for agricultural film falls under EN 13206:2002 for covering films, heavy-metal restrictions under REACH Annex XVII, and dimensional stability evaluation under ASTM D1204-20. Greenhouse films additionally require light transmittance and haze measurement per ASTM D1003-21, with total hemispheric transmittance not below 80% for the clear grade.

    Extrusion Coating and Paperboard Lamination Process Parameters for Liquid Packaging Pre-Cuts

    Extrusion coating of paperboard and aluminium foil with Bapolene® 122F is conducted on a coater equipped with a flat die, a water-cooled chill roll at 10°C to 18°C, and a vented extruder with L/D 33:1. The resin is processed at a melt temperature between 320°C and 335°C to achieve adequate oxidation and adhesion to the paperboard substrate; this is above typical blown film temperatures but below the 350°C threshold at which severe gel formation occurs. The additive package is limited to 0.5 wt% antioxidant masterbatch to reduce gel formation at high coating temperature. In this application, low-density polyethylene homopolymer is used as the moisture barrier and heat-seal layer, not as a primary oxygen barrier. Coat weight is controlled at 15 g/m² to 30 g/m², and line speed typically ranges from 120 m/min to 250 m/min. Adhesion to aluminium foil is promoted by applying an ethylene-acrylic acid copolymer primer or by using an air-gap oxidation distance of 100 mm to 200 mm. The finished board is die-cut into liquid packaging pre-cuts and processed on filling lines. Peel adhesion between the polyethylene layer and aluminium foil is measured per TAPPI T-590, with values generally above 200 g/25 mm. Water vapour transmission through the coating is evaluated by ASTM F1249-22; at 25 g/m² coat weight, WVTR is typically below 5 g/m²·day at 38°C/90% RH. Compliance for food contact is under FDA 21 CFR 177.1520, EU No 10/2011, and GB 9685-2016 for exports to China. Thermal sealing is performed at jaw temperatures 120°C to 150°C with dwell time 0.5 s to 1.2 s; seal strength is measured per ASTM F88/F88M-21. A limitation is the moderate melt strength relative to high-pressure polyethylene grades that require higher neck-in resistance; published data for this specific configuration is limited, but stable coating is achieved with die-to-chill-roll gap below 250 mm.

    Where heavy-duty industrial liners require impact resistance and weld integrity at 100 µm to 200 µm gauge, film converters commonly blend 70 wt% Bapolene® 122F with 30 wt% linear low-density polyethylene butene copolymer having a melt flow rate of 1.0 g/10 min at 190°C/2.16 kg under ASTM D1238-23. The LLDPE fraction raises dart drop values under ASTM D1709-22 from the homopolymer baseline to above 300 g at 125 µm, while the 122F fraction maintains bubble stability and permits lower extruder head pressure. A twin-station winder with centre-driven surface winding is used; winding tension is set between 5 N and 12 N per 100 cm width to avoid telescoping without stretching the film. Extruder profile is 160°C, 175°C, 185°C, and 190°C across four zones, with die temperature at 190°C. Die gap is widened to 1.2 mm to 2.0 mm relative to food film to accommodate the higher melt viscosity of the LLDPE blend. Finished liner products include FIBC liner inserts, drum liners, and pallet containment covers. Weld seams are manufactured by thermal impulse sealing, with seal temperature between 150°C and 180°C and jaw pressure 3 bar to 5 bar. Puncture resistance is measured by ASTM D3420-21 or EN 14477, and tensile properties by ASTM D882-18. The blend complies with the heavy metals restrictions under REACH Annex XVII and with CONEG model legislation for packaging. A potential incompatibility is the addition of recycled post-consumer content above 15 wt%, which can produce dimensional instability and gels at the die lip due to trapped volatiles; pre-drying of recycled material is required at 80°C for 2 h if ambient relative humidity exceeds 60%.

    Application sectorRegulatory boundaryVerification method
    Direct food-contact filmFDA 21 CFR 177.1520; EU No 10/2011; GB 9685-2016Overall migration EN 1186-1:2002; extractables ISO 17716
    Agricultural silage coverEN 13206:2002; REACH Annex XVIIWeathering ASTM G154-23; tensile ASTM D882-18
    Extrusion coating for paperboardFDA 21 CFR 177.1520; EU No 10/2011WVTR ASTM F1249-22; adhesion TAPPI T-590
    Heavy-duty industrial linersREACH Annex XVII; CONEGPuncture ASTM D3420-21; dart impact ASTM D1709-22
    Shrink collation filmFDA 21 CFR 177.1520; EU No 10/2011Shrinkage ASTM D2732-20; haze ASTM D1003-21
    Medical overwrapISO 11607-1:2019; ISO 10993-12:2021Seal ASTM F88/F88M-21; particulates ISO 14644-1

    Controlled Low-Temperature Shrink Collation Film Extrusion Requires a Narrow Orientation Window

    Shrink collation film made from Bapolene® 122F is formulated with a high molecular weight low-density polyethylene or LLDPE modifier at 10 wt% to 25 wt% to increase transverse direction shrinkage, and a nucleating agent masterbatch at 0.5 wt% to 1.0 wt% to control crystal size and haze. The blown film is produced with a high blow-up ratio of 3.5:1 to 4.5:1 and a die gap of 0.8 mm to 1.2 mm, followed by machine-direction orientation at 80°C to 100°C and transverse-direction orientation at 90°C to 110°C on a double-bubble line. Melt temperature during primary extrusion is kept at 180°C to 200°C; residence time must remain below 10 min to prevent gel formation. Shrinkage is measured by immersion in a 150°C oil bath according to ASTM D2732-20, with target values of 20% to 35% in the machine direction and 15% to 25% in the transverse direction at 150°C for 30 s. The shrink force at 125°C should not exceed 0.4 N/cm to avoid crushing lightweight corrugated trays during tunnel passage. Haze is measured per ASTM D1003-21, with typical values below 12% for 40 µm film. Finished goods include bottle multipack collation film and display overwrap. Compliance includes FDA 21 CFR 177.1520 for indirect food contact where the film is used over packaged articles, and EU No 10/2011 for food-contact packaging if shipping foodstuffs. Sealability is assessed per ASTM F88/F88M-21; hot-tack strength is measured by ASTM F1921-20 at 115°C. Published data for this specific grade on a double-bubble line is limited; the above parameters reflect standard polyethylene shrink film extrusion practice rather than a proprietary datasheet.

    During manufacture of non-sterile temporary cover film and patient gown overwrap from Bapolene® 122F, the resin is processed on a cast film line with chilled roll temperatures from 15°C to 25°C, melt temperature 225°C to 245°C, and screw speed 60 rpm to 90 rpm on a 75 mm extruder with 30:1 L/D. The formulation avoids slip agents and restricts antiblock to below 1.0 wt% to minimize particulate contamination, and uses a silica antiblock masterbatch with median particle size below 5 µm to comply with particulate limits. Film gauge is 20 µm to 40 µm. Terminal products include temporary cover bags, instrument protection sleeves, and non-critical surface barriers. Requirements for medical packaging are governed by ISO 11607-1:2019 and ISO 13485:2016, but Bapolene® 122F as a raw material is not certified for direct implant contact. Bioburden control is process-related, not resin-related. Tensile seam strength is measured per ASTM D882-18; seal integrity per ASTM F88/F88M-21. Extractables are evaluated using ISO 10993-12:2021 for devices with transient contact. Halogen content is assessed per IEC 61249-2-21 if the film is used in electronic component packaging. The film is not radiation-sterilized above 25 kGy because the homopolymer can undergo crosslinking and discoloration; published data for this specific resin under gamma irradiation is limited.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 122F Polyethylene, Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bamberger Polymers Bapolene® 122F is a low-density polyethylene film grade supplied as pellets for blown and cast film extrusion. The resin is characterized by a nominal melt index of 2.0 g/10 min determined under ASTM D1238 at 190 °C with a 2.16 kg load and a base density of 0.922 g/cm³ determined under ASTM D1505. These values place the grade in the medium-flow segment of the LDPE film class, a range selected where converter throughput and draw-down must be balanced against melt strength and film toughness. The long-chain branching formed during high-pressure polymerisation distinguishes this material from linear low-density polyethylene and from HDPE; the molecular architecture produces shear-thinning behaviour and melt elasticity that support stable bubble formation on air-cooled blown film lines. Because the grade is a general-purpose film resin rather than a fractional-melt extrusion-coating material, it is not typically used for high-melt-strength applications such as heavy industrial liners that require 0.8 g/10 min or lower melt index.

    What Melt Temperature and Die Gap Boundaries Govern Blown Film Conversion?

    The extrusion temperature profile for Bapolene® 122F is normally set between 160 °C and 190 °C at the adapter, with the feed zone kept below 160 °C to prevent premature melting and bridging. The lower thermal boundary is governed by screw torque and melt pressure; the upper boundary limits the accumulation of oxidised gel particles that form when free radicals generated at elevated temperature react with unsaturation in the polymer chain. On single-screw extruders of 50 mm to 75 mm screw diameter and 24:1 to 30:1 L/D ratio, barrier screws with Maddock mixers are preferred because the resin’s 2.0 g/10 min melt index does not require an intensive dispersive mixing section. A die gap of 0.8 mm to 1.5 mm is used for monolayer blown film; at blow-up ratios from 2:1 to 3:1, the bubble diameter is stabilised by a single-lip or dual-lip air ring. Frost-line height is maintained between 5 and 8 die diameters for most gauge targets, but the exact setting is adjusted with air-flow rate and room dew point.

    Melt index testing under ASTM D1238 averages shear rates below 10 s-1; blown film die lips operate at apparent shear rates of 100 s-1 to 1000 s-1. Because LDPE is shear-thinning, the pressure drop at the die lip is not linear with melt index. The power-law coefficient for a branched LDPE of this density is typically between 0.35 and 0.45 at 190 °C over the film-extrusion shear-rate range; the value must be confirmed by capillary rheometry on the specific lot because molecular-weight distribution and long-chain branching content vary with reactor conditions.

    When the same resin is run on a cast film line, melt temperatures of 200 °C to 230 °C are possible because the chill-roll quenching step removes heat more rapidly than air cooling. Chill-roll temperatures are set from 20 °C to 30 °C; roll temperatures above 24 °C can improve gloss but may initiate blocking when no antiblock concentrate is present. Antiblock or slip concentrates are dosed gravimetrically at 1 to 3 wt%; loss-in-weight feeders are required to avoid additive variation that appears as transverse haze bands and differential coefficient-of-friction behaviour in downstream converting.

    Mechanical, Optical, and Barrier Data Anchored to Standardised Film Tests

    Film tensile properties are measured under ASTM D882 using 25 mm-wide strip specimens conditioned at 23 °C and 50% relative humidity. Machine-direction and transverse-direction tensile values diverge with blow-up ratio because melt draw orients the polymer chains; for LDPE film at 2:1 bubble expansion, transverse-direction elongation at break usually exceeds machine-direction elongation. Bapolene® 122F has a density of 0.922 g/cm³, so its crystallinity and modulus are lower than those of HDPE. This lower crystallinity reduces haze but also reduces tensile stiffness and water-vapour barrier. The 2.0 g/10 min melt index lowers the molecular-weight tail compared with fractional-melt LDPE, which can reduce dart impact and machine-direction tear resistance at equal film thickness; actual values must be taken from the certificate of analysis because additive package, die gap, and frost-line position control the final balance.

    Dart drop impact is evaluated under ASTM D1709; tear propagation is evaluated under ASTM D1922. The lower melt tension of a 2.0 g/10 min LDPE can reduce machine-direction orientation at high draw ratios and preserve some transverse-direction tear, but it can also reduce pin-hole resistance in thermoforming operations. When comparing against a 0.8 g/10 min LDPE of identical density, no universal numerical offset is valid because downgauging shifts the failure mode from ductile puncture to crack propagation. Oxygen transmission is determined under ASTM D3985 and water-vapour transmission under ASTM F1249. Polyethylene film of this density is not a high-barrier material; coextruded EVOH, PVDC, or metallisation is required when oxygen transmission below 100 cm³/(m²·day·atm) at 23 °C is specified.

    When Coextrusion Layer Ratios and Reclaim Levels Are Modified

    Bapolene® 122F is frequently blended with LLDPE in the same extruder or placed as a separate layer in coextruded film. Additions of 10 to 30 wt% LDPE to an LLDPE layer increase melt elasticity and can reduce draw resonance on cast lines; the exact effect depends on the LLDPE melt index and the die-gap setting. When the LDPE fraction exceeds 30 wt% of a given layer, the overall tensile modulus drops and the seal-initiation temperature may decrease slightly because the lower crystallinity of LDPE melts over a broader temperature interval. Coextrusion feedblocks and dies must account for the viscosity ratio between LDPE and metallocene LLDPE at the relevant shear rate; layer thickness non-uniformity can increase if the die is operated below the critical shear stress for interfacial stability. No tie layer is required for adjacent polyolefin layers.

    Reclaim handling influences gel content and film appearance. Screen packs of 60/100/60 mesh are common on packaging lines; a continuous screen changer is specified when post-industrial reclaim exceeds 15 wt% of the extruder feed. Oxidised polypropylene residues in mixed reclaim can produce visible specks and interfacial weakness in coextruded structures; silo and conveying lines should therefore be purged after polypropylene campaigns. Long residence times above 220 °C should be avoided because thermo-oxidative chain scission and crosslinking generate gel particles that pass conventional melt filters and appear as undispersed defects in thin film.

    Compared with fractional-melt LDPE film grades of similar density, Bapolene® 122F provides lower extruder motor load and faster screw recovery because the higher melt index reduces melt viscosity at typical processing shear rates. However, bubble stability at high blow-up ratios is generally lower than with 0.8 g/10 min LDPE, and the material is less suitable for very thick shrink film or heavy-duty sacks where a high molecular-weight tail is needed. Compared with LLDPE of 0.918 g/cm³ density, Bapolene® 122F typically offers lower dart impact at equal thickness but improved optical clarity and higher melt strength. Compared with HDPE of 0.960 g/cm³, Bapolene® 122F has lower stiffness, lower temperature resistance, and higher permeability, but greater flex-crack resistance and higher elongation. These distinctions position the grade for medium-gauge packaging film, liners, and coextruded seal or bulk layers rather than for barrier or load-bearing structural film.

    AttributeBapolene® 122FFractional-Melt LDPELLDPEHDPE
    Melt index under ASTM D12382.0 g/10 min0.8 g/10 min1.0 g/10 min0.5 g/10 min
    Density0.922 g/cm³0.922 g/cm³0.918 g/cm³0.960 g/cm³
    Melt strengthmoderatehighlowmoderate
    Dart impact resistancemoderatehighhighlow
    Optical clarityhighmoderatemoderatelow
    Water-vapour barrierhigh transmissionhigh transmissionhigh transmissionlow transmission

    Regulatory Documentation Is Required Before Food-Contact Clearance

    Bapolene® 122F can be assessed for food-contact use as an olefin polymer, but the base-resin compendial status does not automatically clear a finished film. Extraction, migration, and additive-package documentation are required for the final article. The following compendial and regulatory references are applied in converter specifications:

    Regulatory referenceSubjectTest or condition
    FDA 21 CFR 177.1520(c)Olefin polymers for food contactDensity and extractable fraction; final article subject to end-use limitations
    EU Regulation (EU) No 10/2011Plastic materials and articles intended for food contactOverall migration limit 10 mg/dm²; specific migration depends on additives
    REACHRegistration, evaluation, authorisation of chemicalsPolymer substance registration obligations are distinct from monomer and additive duties
    RoHS Directive 2011/65/EURestriction of hazardous substancesApplicable only to electrical/electronic equipment; not relevant to plain LDPE but customer may request confirmatory Pb, Cd, Hg, Cr(VI), PBB, PBDE screening

    Slip additives such as erucamide migrate slowly to the film surface over hours to days after extrusion. The coefficient of friction measured under ASTM D1894 will therefore drift after conversion; initial values are higher and fall as the amide blooms. Antiblock concentrates based on synthetic silica or diatomaceous earth increase surface roughness; addition at 1 to 3 wt% is typical, but excess reduces clarity and can increase die-lip build-up. Bapolene® 122F may be supplied without these additives or with a standard package; the converter should specify the required additive type and quantity on the purchase order to prevent mismatched slip performance in high-speed form-fill-seal lines.

    Bubble stability in a 2.0 g/10 min LDPE is more sensitive to ambient air currents than in a fractional-melt grade. At BUR 2:1, a stable frost line can be achieved with internal bubble cooling when the tower is fitted with an upper nip and no internal stabiliser baskets; at BUR 3:1, external air-ring venturi angle and lower tower temperature become critical. The frost-line height should be raised if transverse-direction gauge variation exceeds ±5% because rapid quenching increases freezeline set and reduces bubble deformation. For gauge control below ±3%, gravimetric throughput control, die-gap uniformity, and die temperature balancing are required; melt-temperature variation across the die should be kept below 5 °C.

    Storage and handling conditions affect film performance. Pellets should be kept in closed silos or lined boxes to prevent condensation on the granule surface; drying is generally unnecessary when the resin is stored below 30 °C and protected from dew-point cycling. If exposed to ambient humidity above 60% relative humidity for prolonged periods, hopper dryers with an inlet-air dew point of −10 °C are used to avoid surface moisture and attendant bubble instability. The product is insensitive to normal outdoor ultraviolet exposure only during storage; finished film intended for agricultural or construction exposure requires a UV stabiliser masterbatch because the base resin contains insufficient light stabiliser for long-term weatherability.

    Top