    Specifications
    HS Code 890983
    Polymer Type Low Density Polyethylene (LDPE)
    Grade Film Grade
    Density 0.922 g/cm³
    Melt Index 2.0 g/10 min
    Tensile Strength At Yield 10.0 MPa
    Tensile Strength At Break 24.0 MPa
    Elongation At Break 600%
    Tensile Modulus 0.200 GPa
    Flexural Modulus 0.200 GPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 7.0%
    Gloss 75%
    Melting Point 110 °C
    Vicat Softening Point 95 °C

    As an accredited Bamberger Polymers Bapolene® 122B Polyethylene, Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Bamberger Polymers Bapolene® 122B Polyethylene, Film Grade is supplied in 50 lb moisture-resistant bags, palletized and stretch-wrapped for industrial shipment.
    Container Loading (20′ FCL) Bamberger Polymers Bapolene® 122B Polyethylene, Film Grade, in 25 kg bags, palletized, stretch-wrapped, loaded into a 20′ FCL.
    Shipping Bamberger Polymers Bapolene® 122B Polyethylene, Film Grade is a non-hazardous, non-regulated thermoplastic resin supplied as pellets. It typically ships in 25 kg bags, bulk bags, or bulk containers, palletized and stretch-wrapped. Store in a cool, dry, clean area away from direct sunlight, heat, and moisture. No special transport placards required.
    Storage Store Bamberger Polymers Bapolene® 122B Polyethylene, Film Grade, in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original packaging closed, palletized, off the floor, and protected from moisture, dust, and contamination. Maintain ambient temperature, avoid excessive stacking, use FIFO, and follow SDS/local regulations. Store away from incompatible materials and ignition sources.
    Shelf Life Shelf life is approximately 24 months when stored in a cool, dry, well-ventilated area in original, unopened packaging.
    Application of Bamberger Polymers Bapolene® 122B Polyethylene, Film Grade

    Bapolene 122B enters heavy-duty shipping sack lines as a monolayer blown film with a nominal density of 0.922 g/cm³ (ASTM D1505) and a melt flow rate of 0.55 g/10 min (ASTM D1238, 190 °C/2.16 kg). Film extrusion is carried out on single-screw blown-film lines with screw L/D ratios between 24:1 and 30:1, annular die diameters from 250 mm to 400 mm, and die gaps between 1.8 mm and 2.5 mm. Volumetric throughput on a 90 mm extruder with a 400 mm die typically ranges from 120 kg/h to 180 kg/h when internal bubble cooling is used; the specific output is limited by bubble stability rather than plastication. Melt temperatures at the die are held between 160 °C and 190 °C, and frost line heights are maintained from 600 mm to 900 mm by adjusting the IBC air volume. Blow-up ratios of 2.0:1 to 2.8:1 are applied to balance machine-direction and transverse-direction tensile properties; values below 2.0:1 produce MD-oriented film with low dart impact, while values above 2.8:1 increase gauge scatter on conventional external cooling rings.

    Sack converters specify 100 µm to 200 µm film for filling masses between 10 kg and 50 kg. The required mechanical performance is verified through ASTM D1709-16a Method A dart impact, ASTM D1922-15a Elmendorf tear, and ASTM D882-18 tensile testing. Published minimum values for specific sack constructions are not standardized across converters; however, a 150 µm monolayer structure is frequently accepted when dart impact exceeds 200 g, MD tear exceeds 250 gf, and tensile strength is at least 15 MPa in the machine direction at 500 mm/min. Elongation at break is typically above 300%; lower values indicate excessive orientation or oxidative degradation during extrusion. The seal side of the film is left untreated, while the outer surface may be corona-treated to 38 mN/m to 42 mN/m (ASTM D2578) for solvent-based printing or thermal transfer overprint.

    On production-scale lines equipped with rotating nip rolls and automated gauge scanners, gauge variation has been observed to increase from ±5% to ±12% when the frost line is raised above 900 mm because the melt is still partially oriented at the nip, generating irregular draw-down. The failure mode is not bulk melt fracture but localized thinning in the bubble transition region; the resulting film shows low dart impact at those thin bands and can rupture during 1.2 m drop tests. Die land length ratios below 10:1 combined with throughput above 150 kg/h produce sharkskin on the outer film surface, which appears as parallel transverse ridges and reduces printing adhesion. Processing corrections include increasing die gap to 2.5 mm, raising the die exit temperature to 180 °C, or reducing screw speed by 5% to 10%; each intervention changes the draw-down ratio and must be validated with a full property panel.

    What Limits Film Gauge Uniformity in High-Stalk Greenhouse and Mulch Film Production?

    Agricultural greenhouse film based on Bapolene 122B is processed at thicknesses from 150 µm to 200 µm, while mulch film is extruded at 25 µm to 50 µm. UV stabilizer masterbatches containing hindered amine light stabilizers and UV absorbers are added at 2 wt% to 5 wt% for greenhouse service and at 3 wt% to 8 wt% for mulch films where carbon black or titanium dioxide controls photodegradation. The masterbatch carrier resin and mineral fillers shift melt viscosity upward by 10% to 20% at constant melt temperature, so the screw speed on a 65 mm barrier screw with a Maddock mixing section is reduced 5% to 10% to keep melt pressure below 350 bar. High-stalk bubble geometry, with the frost line raised to 800 mm to 1,000 mm, is used to improve bubble stability, but this reduces the rapid quenching that produces high clarity; greenhouse film therefore requires a compromise between gauge uniformity and light transmission.

    Accelerated weathering is evaluated by ISO 4892-2:2013 using a xenon-arc source with a 0.35 W/m² irradiance at 340 nm; specifications for multi-season greenhouse films commonly require tensile elongation retention above 50% after 3,000 h to 5,000 h, though published data for this specific grade is limited. Mulch film must fragment rather than embrittle into large pieces; photodegradation control is confirmed by field exposure rather than accelerated testing because soil temperature and moisture affect oxidation kinetics. The main process failure mode is die lip residue from low-molecular-weight stabilizer fractions, which appears after 48 h to 72 h of continuous extrusion and produces longitudinal die lines. Manual die cleaning is required at intervals determined by masterbatch quality; no chemical purge completely removes the deposit. REACH Article 33 communication applies only if the finished agricultural film contains a substance of very high concern above 0.1 wt%, which is not expected for standard UV masterbatches.

    Lamination Sealant Webs and the Food-Contact Compliance Thresholds That Govern Layer Ratios

    Blown film of Bapolene 122B is converted into sealant webs of 30 µm to 60 µm for adhesive lamination to BOPET or BOPP print webs. Corona treatment on the adhesive side is set to 38 mN/m to 42 mN/m (ASTM D2578), while the seal side remains untreated to preserve heat-seal performance. Solventless polyurethane adhesives are applied at 1.5 g/m² to 2.5 g/m² and cured for 24 h to 48 h at 40 °C; laminate bond strength after cure typically exceeds 2.5 N/15 mm when the polyethylene surface energy remains above 38 mN/m. Seal initiation temperature falls between 95 °C and 110 °C, and heat-seal strength measured per ASTM F88/F88M-21 reaches 20 N/25 mm to 30 N/25 mm at 130 °C. These values apply to monolayer sealant webs; if coextruded with a lower-melting metallocene polyethylene skin, the seal initiation drops further.

    Food-contact compliance for the sealant web is anchored to FDA 21 CFR 177.1520(c), which permits olefin polymers for use in contact with food, subject to conditions of use assigned to the final laminate and extractive testing where required. For the EU market, Regulation (EU) 10/2011 applies to the finished laminate, and overall migration must remain below 10 mg/dm² when tested in the food simulant assigned to the packaged food category. Slip and antiblock loadings are critical: erucamide is added from 500 ppm to 1,500 ppm and synthetic silica from 800 ppm to 1,200 ppm to reduce the coefficient of friction below 0.20 (ASTM D1894) on high-speed pouch machines. Process limitation: erucamide migration above 1,500 ppm has been associated with reduced adhesive anchorage and interlayer delamination in tropical storage because the bloomed amide interferes with the polyurethane curing reaction; when film is intended for hot-climate distribution, the upper slip loading is validated by laminate bond strength testing after 30 days at 40 °C.

    ApplicationStandard / Test MethodTypical Specification or Measured Range
    Heavy-duty sacksASTM D1709-16a Method A180 g–250 g at 150 µm
    Agricultural greenhouse filmISO 4892-2:201350% retained elongation after 3,000 h–5,000 h
    Lamination sealant webFDA 21 CFR 177.1520(c), EU 10/2011overall migration < 10 mg/dm²
    Collation shrink filmASTM D2732-1415%–25% MD free shrink at 100 °C
    High-speed FFS packagingASTM F1921-18> 2 N/25 mm hot-tack at 120 °C

    When Collation Shrink Film Demands Low Free Shrink Temperature and Abrasion Resistance

    Collation shrink film from Bapolene 122B is extruded at die gaps of 1.2 mm to 2.0 mm and blow-up ratios of 2.5:1 to 4.0:1 to generate the orientation required for controlled shrink around grouped bottles or cans. The frost line is held at 400 mm to 600 mm from the die face, which is substantially lower than in heavy-duty sack film and produces greater transverse orientation while retaining bubble stability. Free shrink measured per ASTM D2732-14 at 100 °C is typically 15% to 25% in the machine direction and 10% to 20% in the transverse direction; at 120 °C, free shrink may exceed 30%, but shrink force increases and can deform thin-walled PET containers. The process conflict is immediate: raising the blow-up ratio above 3.5:1 increases transverse shrink but also increases gauge spread unless a segmented external air ring and internal bubble cooling are precisely balanced; without that control, thickness variation exceeds ±10%, producing dog-ear seals and torn open corners. Annealing downstream of the freeze line is not performed because it would reduce free shrink; orientation is locked by rapid cooling and a controlled collapse frame geometry.

    Impulse sealing parameters are set at 120 °C to 160 °C jaw temperature and 0.5 s to 1.0 s dwell time. Seal strength is evaluated by ASTM F88/F88M-21, with minimum values of 10 N/25 mm to 15 N/25 mm required for collation packs above 2 kg. Hot-tack force is less critical than in form-fill-seal because sealing occurs on a static collation line, but seal release at high temperatures can delaminate the film. Abrasion resistance in transit is controlled by adding a slip/antiblock masterbatch at 5% to 10%, which lowers coefficient of friction but slightly reduces hot-tack and interlayer seal strength; the upper limit is set by packaging line speed and pack weight. A particular failure mode on high-shrink lines is the formation of transverse gauge bands when the collapsing frame is misaligned; these bands shrink at different rates and create visible distortion bands on printed shrink film.

    Bapolene 122B converted into 55-gallon drum liners uses tubular film of 75 µm to 125 µm and thermal impulse bottom seals at 130 °C to 150 °C. Blocking at wind-up is controlled with 800 ppm to 1,200 ppm silica antiblock; no orientation threshold or critical processing window applies beyond standard blown-film melt temperatures of 160 °C to 180 °C. Where indirect food-contact liners are specified, FDA 21 CFR 177.1520(c) conditions of use govern the extractive testing, but most drum liner applications are industrial packaging outside food-contact scope.

    Seal Strength Falls When Dwell Time Drops Below 80 ms on High-Speed Form-Fill-Seal Lines

    On vertical and horizontal form-fill-seal machines running at 60 to 120 cycles/min, film from Bapolene 122B at 40 µm to 80 µm is sealed at jaw temperatures of 115 °C to 140 °C. Dwell time is often limited to 20 ms to 80 ms; the seal must develop sufficient hot-tack force before the product loading station, so hot-tack strength is specified above 2 N/25 mm per ASTM F1921-18. Gauge uniformity must be held within ±5%; thin spots below 35 µm fail by seal tearing during product drop, and thick spots above 90 µm increase seal jaw heat transfer variability. Slip-modified film with erucamide levels near 1,000 ppm yields a coefficient of friction of 0.10 to 0.20 (ASTM D1894) for reliable film transport over forming shoulders; levels below 500 ppm produce blocking and machine stops.

    The critical limitation for Bapolene 122B is seal initiation temperature relative to metallocene LLDPE formulations. Blending more than 20 wt% of this LDPE film grade into an mLLDPE formulation can raise heat-seal initiation by 5 °C to 10 °C, which on a high-speed line may require an increase in jaw temperature beyond the thermal distortion limit of the packaging film. Excess erucamide above 1,500 ppm deposits on seal jaws and reduces seal strength below 15 N/25 mm (ASTM F88/F88M-21) after several hours of continuous operation. The problem is not bulk resin degradation but additive bloom on jaw surfaces; cleaning intervals are therefore determined by accumulated slip residue rather than polymer melt contamination. Process validation includes seal strength after 4 h and 8 h of continuous cycling, because the first-hour seal value overestimates long-run performance.

    Free Quote

    Competitive Bamberger Polymers Bapolene® 122B Polyethylene, Film Grade prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Bapolene® 122B is classified as a high molecular weight high-density polyethylene (HMW-HDPE) film extrusion resin with a nominal density of 0.949 g/cm³ when tested in accordance with ASTM D1505-18 and a high-load melt index of 8.0 g/10 min at 190 °C/21.6 kg using ASTM D1238-20 Procedure B or ISO 1133-1:2022. The conventional melt index at 2.16 kg is typically below 0.1 g/10 min, which excludes the material from injection molding and most cast film operations and defines its processing niche in air-cooled or water-quenched blown film lines. The high molecular weight architecture produces a high zero-shear viscosity and pronounced shear thinning; these characteristics support bubble stability at relatively low frost-line heights while requiring grooved-feed extruder sections and controlled melt pressure. Actual lot-specific values are governed by the supplier's certificate of analysis, not by general literature values.

    In monolayer blown film, the grade is specified for thin-gauge merchandise bags, T-shirt bags, can liners, industrial inner liners, and other packaging structures where downgauging from low-density polyethylene demands higher secant modulus at equivalent thickness. Typical film gauges range from 10 µm to 50 µm. The material is not intended for high-clarity packaging because the semicrystalline character of HDPE produces haze levels that exceed those of LDPE and many metallocene LLDPE grades. Processors should verify the supplier's lot-specific additive declaration before blending with LLDPE or LDPE; small additions can modify tear resistance but also influence haze, bubble stability, and blocking behavior.

    Rheological basis for film-grade melt strength and low-shear viscosity control

    The shear thinning behavior of Bapolene® 122B is a critical variable in bubble formation. Although the high-load melt index is 8.0 g/10 min, the zero-shear viscosity remains sufficiently high to resist sag in the free bubble above the die. On air-cooled monolayer lines with a blow-up ratio of 3:1 to 5:1 and a frost-line height of 6 to 10 die diameters, this viscosity reduces gravitational and aerodynamic distortion of the molten tube. The resin should be processed with die gaps between 1.0 mm and 1.5 mm; narrower gaps used for LDPE can generate excessive die-lip shear and initiate sharkskin or melt fracture. When surface defects appear at high line speeds, a fluoropolymer processing aid at 400–800 ppm is often evaluated, but compatibility with the resin's stabilizer package must be confirmed by the supplier.

    On a 65 mm grooved-feed extruder with 30:1 L/D and a 250 mm spiral mandrel die, a representative temperature profile of 180 °C in the rear zone, 200 °C in the middle zones, 210 °C in the front zone, and 215 °C at the adapter and die has been used in production-scale trials. These setpoints are not universal; they must be adjusted for screw geometry, output rate, and ambient cooling capacity. Rear-zone temperatures below 190 °C may cause granule bed blockage in grooved-feed sections, while die temperatures above 240 °C increase the probability of oxidative degradation, die-lip plate-out, and film odor.

    Pre-drying is not required for Bapolene® 122B under normal indoor storage conditions below 50% RH. If pellets are transferred from cold outdoor silos to a warm production area, surface condensation can occur. In such cases, a hopper dryer at 70 °C for 2 hours removes surface moisture. At relative humidity above 70%, residual surface water can create steam streaks and bubble instability. Extended shutdowns should be preceded by purging with a lower-viscosity HDPE or LLDPE carrier to prevent stagnant high-viscosity melt in the adapter and die from degrading during heat soak. Mixing with polypropylene or PET contaminants should be avoided because incompatible melt phases produce gels and hole formation in thin film.

    When film is drawn to 25 µm and conditioned for 40 hours at 23 °C and 50% RH according to ASTM D618-21, the mechanical response differs from low-density film grades in both tensile and tear behavior. Tensile properties are determined by ASTM D882-18 using a grip separation rate of 500 mm/min. HMW-HDPE films in the 0.947–0.951 g/cm³ density class typically exhibit machine-direction tensile strength at break of 40–60 MPa and transverse-direction values of 30–45 MPa; elongation at break commonly falls between 500% and 800%. These ranges reflect a thicker semicrystalline network than that of LDPE and are not a substitute for lot-specific measurements.

    Typical mechanical and barrier ranges for HMW-HDPE blown film in the 0.947–0.951 g/cm³ density class
    PropertyTypical range for 25 µm filmTest method
    Density0.947–0.951 g/cm³ASTM D1505-18
    High-load melt index7.5–8.5 g/10 min at 190 °C/21.6 kgASTM D1238-20 Procedure B
    Tensile strength at break, MD40–60 MPaASTM D882-18
    Tensile strength at break, TD30–45 MPaASTM D882-18
    Elongation at break, MD500–800%ASTM D882-18
    Elmendorf tear, MD10–25 gASTM D1922-15a
    Elmendorf tear, TD200–400 gASTM D1922-15a
    Dart drop impact, Method A150–300 gASTM D1709-16a
    Water vapor transmission rate4–8 g/(m²·day) at 38 °C/90% RHASTM F1249-20

    Film-level data vary with blow-up ratio, frost-line height, output rate, and laboratory sample preparation. Published data for this specific configuration is limited, and the ranges above should be used for preliminary material selection only. The controlling mechanical values are those reported on the supplier's lot-specific certificate of analysis and should be confirmed on the actual production line.

    What restrains downgauging below 12 µm on monolayer lines?

    Below 12 µm, the film enters a process window in which bubble instability increases sharply because melt thickness per unit area decreases and gauge uniformity becomes highly sensitive to air-ring turbulence. The high zero-shear viscosity of HMW-HDPE helps retain bubble stiffness but does not eliminate the requirement for controlled air-ring performance and precise collapsing-frame geometry. When die gaps exceed 1.2 mm, drawdown ratios can exceed 100:1, producing strong machine-direction molecular orientation and tear anisotropy. Elmendorf tear in the machine direction may fall below 10 g, while transverse tear remains high; this property conflict is a primary technical limit for downgauging on monolayer equipment.

    Blocking also intensifies in films below 10 µm, requiring an antiblock masterbatch. Inorganic antiblocks reduce optical clarity and, when poorly dispersed, increase gel count and film defects. Where puncture resistance and tear must be improved simultaneously, a three-layer coextrusion with LLDPE skins and an HDPE core is used. That structure preserves the core resin's modulus while placing tougher LLDPE at the surfaces. However, the high melt temperature of HMW-HDPE can create interfacial viscosity mismatch if the skin resin has a much higher melt index, leading to interfacial instability and layer thickness variation.

    When 122B replaces a 0.922 g/cm³ LDPE on an existing monolayer line

    Conventional LDPE film grades with density near 0.922 g/cm³ and melt index near 2.0 g/10 min process at melt temperatures of 160–190 °C and die gaps of 0.8–1.0 mm. A direct substitution with Bapolene® 122B requires raising barrel and die setpoints by approximately 20–40 °C and increasing the die gap to 1.2–1.5 mm to prevent melt fracture. Extruder drive load can increase because of the higher melt viscosity; the line must have a grooved-feed section and adequate motor torque. In return, the film secant modulus at 1% strain increases by a factor of 2–3 relative to LDPE, permitting gauge reduction at equivalent stiffness. Clarity decreases and film feel becomes stiffer and noisier, which may be acceptable for utility packaging but unsuitable for retail display films requiring gloss.

    The following comparison provides material-selection context. The values are representative of commercial blown film grades and are not batch-specific.

    Comparative processing and performance profile for blown film extrusion
    ParameterBapolene® 122B HMW-HDPETypical LDPE film resinTypical butene LLDPE film resin
    Density, ASTM D1505-180.949 g/cm³0.922 g/cm³0.918 g/cm³
    Melt flow value8.0 g/10 min HLMI2.0 g/10 min MI1.0 g/10 min MI
    Typical die melt temperature210–230 °C160–190 °C180–220 °C
    Film clarityHigh haze, translucentHigher clarityModerate haze
    Secant modulus at 1% strain600–900 MPa150–250 MPa180–300 MPa
    Typical dart drop impact, 25 µm150–300 g80–150 g200–400 g

    Bapolene® 122B should not be confused with HMW-HDPE blow molding resins of similar density. Blow molding grades are formulated for parison sag control and often carry different stabilizer packages and gel-level requirements. Film-grade material may have lower additive levels optimized for surface quality, blocking resistance, and bubble stability. In injection molding, the conventional melt index below 0.1 g/10 min is insufficient to fill small gates and thin-wall molds. The product's processing envelope is therefore limited to blown film and, in some configurations, simple slit-die sheet where the machine can handle the high melt viscosity.

    For food-contact applications, a statement of compliance should be obtained from the supplier for the exact product code and lot. HMW-HDPE films of this class are typically referenced under FDA 21 CFR 177.1520(c) for olefin polymers, with extractable fraction limits specified in the applicable table of that section, and under Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for general food-contact plastics. The exact compliance status of Bapolene® 122B depends on the antioxidant and slip/antiblock additives present; the supplier's lot-specific regulatory declaration is the controlling document. RoHS Directive 2011/65/EU restrictions on lead, cadmium, mercury, hexavalent chromium, PBB and PBDE are typically satisfied by polyethylene homopolymers, but compliance must be confirmed by the resin manufacturer for the specific lot.

    Lot-to-lot variation in high-load melt index and density is normally controlled within narrow supplier limits. Processors should nevertheless monitor extruder head pressure, bubble position, and film gauge after silo changes because shifts in molecular weight distribution can alter shear thinning behavior and output rate. The most stable production performance is obtained when incoming resin is segregated by lot and when film property verification follows ASTM D882-18 for tensile properties and ASTM D1709-16a for dart impact. Where film is printed or laminated, corona treatment levels should be controlled after surface oxidation develops; HMW-HDPE films typically require higher treater power than LDPE at equivalent line speed to reach the 38–42 dyn/cm wetting tension range commonly specified for water-based inks.