Arkema Orevac Oe807 Maleic Anhydride Modified Lldpe

Arkema Orevac® OE807 Maleic Anhydride modified LLDPE

    • Product Name: Arkema Orevac® OE807 Maleic Anhydride modified LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 810326
    Density 0.920 g/cm³
    Melt Flow Index 190 C 2 16 Kg 3.0 g/10 min
    Maleic Anhydride Content 0.9 wt%
    Melting Point 122 °C
    Vicat Softening Point 92 °C
    Tensile Strength At Break 12 MPa
    Elongation At Break >500%
    Flexural Modulus 250 MPa
    Hardness Shore D 50
    Water Absorption <0.1%
    Processing Temperature 200–250 °C
    Appearance White to off-white pellets

    As an accredited Arkema Orevac® OE807 Maleic Anhydride modified LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Arkema Orevac® OE807 is supplied as pellets in 25 kg polyethylene bags, 40 bags per 1000 kg pallet.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Arkema Orevac OE807 maleic anhydride modified LLDPE, 25 kg bags, palletized, shrink-wrapped, securely loaded for export.
    Shipping Arkema Orevac® OE807 (maleic anhydride-modified LLDPE) is shipped as non-hazardous solid polymer pellets in 25-kg bags, big bags, or bulk containers. It is not regulated for transport under DOT, IMDG, IATA, or ADR; no UN number, hazard class, or packing group is assigned. Keep dry and away from heat.
    Storage Store Orevac® OE807 in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep packaging tightly closed and off the floor to prevent moisture pickup. Protect from water, amines, alcohols, and strong oxidizers to avoid hydrolysis or reactions. Maintain clean conditions and avoid prolonged storage above supplier-recommended temperatures. Follow the SDS and local regulations.
    Shelf Life Typically 24 months when stored unopened, dry, cool, away from direct sunlight and heat in original packaging.
    Application of Arkema Orevac® OE807 Maleic Anhydride modified LLDPE

    A five-layer blown-film line with a 250 mm spiral mandrel die, 2.0 mm die gap, and blow-up ratio of 2.2:1 places Arkema Orevac OE807 as a discrete tie stream between EVOH barrier resin and LLDPE skins. The tie layer is not a compounded additive; it is metered at 100% resin through a 60 mm 24:1 L/D single-screw extruder with zone setpoints from 180 °C in the feed zone to 230 °C at the adapter. In a total film thickness of 75 µm, two tie layers of 6–8 µm each represent 16–21% of the structure. Food-contact conformity is established under EU Regulation (EU) No 10/2011 using overall migration per EN 1186-1:2002 and specific migration for maleic anhydride per EN 13130-1:2004; U.S. structures reference FDA 21 CFR 177.1520 for the olefin polymer construction and 21 CFR 175.105 where adhesive-layer migration is assessed. Medical packaging is validated to ISO 11607-1:2019, with seal strength measured as N/15 mm under ASTM F88/F88M-21. On-line controls include air-ring pressure at 2.5–3.5 kPa, frost-line height 250–350 mm, and die melt temperature below 245 °C to limit anhydride ring-opening and gel formation. Terminal products include vacuum barrier pouches, stand-up pouch inner tie layers, modified-atmosphere lidding films, and terminally sterilized medical barrier pouches.

    How Is Pipe Coating Adhesion Maintained After Cathodic Disbondment Testing at 65°C?

    At the pipe plant, the steel substrate is blast-cleaned to Sa 2.5 with an angular profile of 50–90 µm and preheated to 200–230 °C before fusion-bonded epoxy powder is applied at 60–120 µm. OE807 is then extruded through a 120 mm 30:1 L/D side extruder with a flat die at 180–220 °C between the partially cured FBE layer and the high-density polyethylene topcoat. The adhesive layer is specified at 170–300 µm for pipe diameters from 219 mm to 1220 mm, and the topcoat thickness is 2.0–4.0 mm. Qualification testing under ISO 21809-1:2018 covers peel resistance, cathodic disbondment, hot-water immersion, and impact resistance; DIN 30670:2012 and CSA Z245.21-18 provide regional supplementary acceptance values, and corrosion control selection follows NACE SP 0169-2013. Cathodic disbondment is commonly run at 65 °C for 28 days at −1.5 V versus an Ag/AgCl reference cell, with radial disbondment acceptance below 8 mm. Peel adhesion is tracked at 23 °C and 50 °C after 24 h conditioning; field delamination at cutback is frequently associated with FBE surface temperature falling below 175 °C before OE807 application. Terminal products are buried onshore gas transmission pipelines, crude oil gathering lines, water injection pipelines, and insulated line-pipe spools.

    TestStandardConditionTypical acceptance
    Cathodic disbondmentISO 21809-1:201865 °C, 28 days, −1.5 V≤ 8 mm radial disbondment
    Hot-water immersionISO 21809-1:201870 °C, 30 daysno blistering
    Peel adhesionDIN 30670:201223 °C, 50 °Clot-to-lot SPC trend
    Blast cleanlinessISO 8501-1:2007—Sa 2.5

    Compounding of halogen-free sheathing compounds on a co-rotating twin-screw extruder with L/D 44:1 and a side-stuffer at barrel zone 7 requires a coupling resin that remains processable at the 145–175 °C barrel setpoints used for high filler loadings. OE807 is metered at 5–12 wt% of the polymer phase in a formulation where aluminum trihydrate or magnesium dihydrate occupies 60–65 wt%; the polymer phase is 35–40 wt%, so the corresponding total compound level is 1.8–4.8 wt%. Flame-safety compliance is established under IEC 60754-1:2011 for halogen acid gas content, IEC 60754-2:2019 for combustion-gas pH and conductivity, and IEC 61034-2:2019 for smoke density. Mechanical properties are tested to EN 60811-501:2012, and reaction-to-fire classification in the European market is declared under EN 50575:2014+A1:2016 with testing per EN 50399. Filler is pre-dried to 0.1 wt% residual moisture in a desiccant dryer at 80–90 °C; barrel setpoints are 145–175 °C, the die is held at 165 °C, and melt temperature must remain below 190 °C to avoid anhydride ring-opening and secondary acid evolution. Vacuum venting at −0.06 MPa removes bound water released at zone 6. When filler moisture exceeds 0.15 wt%, torque instability and screen-pack pressure above 8 MPa are observed, and elongation under EN 60811-501:2012 may drop below 150%. Terminal products are sheathing for building distribution cables, industrial control cables, automotive charging cables, and flame-retardant flexible conduit.

    Aluminium/PE Core Lamination Through Flat-Die Coextrusion

    In manufacture of aluminium composite panels, OE807 is coextruded as the bonding layer between the polyethylene core and the aluminium skin. The aluminium coil, 0.3–0.5 mm thick, is degreased and conversion-coated, then heated to 80–120 °C immediately before the lamination nip; surface energy is verified at 42–48 mN/m by dyne test according to ISO 8296:2003. The PE core is extruded through a 2400 mm flat die at 220–250 °C, while OE807 is supplied through a secondary extruder to the feedblock to generate a tie layer of 30–60 µm on each aluminium skin. Nip pressure is controlled at 3–6 N/mm² across the roll face, and peel strength is measured by 180° peel after 24 h conditioning under ASTM D1876. Fire classification of the finished panel is assessed under EN 13501-1:2018; surface-burning characteristics are tested to ASTM E84-23a where North American cladding requirements apply, and aluminium-plastic panel specifications in China reference GB/T 17748-2016. Adhesion failures traced to residual rolling oils or dew point excursions below the conversion-coating line indicate insufficient surface preparation rather than tie-resin deficiency. Terminal products include exterior curtain-wall spandrel panels, interior wall cladding, signage board, and column covers.

    Wood-fibre moisture above 0.8 wt% suppresses maleic anhydride coupling efficiency.

    Polyethylene-based wood-plastic composite profiles use OE807 at 2–5 wt% of total formulation to esterify hydroxyl groups on wood flour surfaces and reduce interfacial water absorption. In a formulation with 55 wt% hardwood flour, 40 wt% high-density polyethylene, and 5 wt% additives, the OE807 level is adjusted between 2 wt% and 4 wt% according to wood species and particle-size distribution below 180 µm. Compliance is demonstrated under EN 15534-1:2014+A1:2017 for material characterisation and ASTM D7031-11(2019) with ASTM D7032-17 for product performance; flexural modulus is measured by ISO 178:2019. Processing is carried out on a counter-rotating conical twin-screw extruder with wood flour pre-dried to 0.8 wt% maximum in a rotary dryer at 105 °C; barrel zones are 150–170 °C, the die is set at 165 °C, and screw speed is limited to hold melt pressure below 15 MPa. When residual wood moisture exceeds 0.8 wt%, the anhydride group is consumed by hydrolysis before fibre coupling, which produces a measurable drop in interlaminar shear strength and outdoor creep resistance. Terminal products are solid and hollow decking planks, railing profiles, fencing elements, and exterior cladding boards.

    When a 7 µm Aluminium Foil Web Is Extrusion-Coated Without a Tie Layer, T-Peel Delamination Occurs After 121°C Retort

    Before a retortable laminate reaches the pouch converter, the aluminium foil web must be extrusion-coated or laminated to a polyolefin sealant; OE807 is introduced as the adhesion-promoting melt between 7–12 µm foil and an LLDPE sealant. The foil is annealed and surface treated, then corona-discharged at line speeds from 30 m/min to 80 m/min. OE807 is applied at a coating weight of 12–20 g/m², corresponding to approximately 12–20 µm, through a 900 mm slot die at 230–260 °C. For food-contact compliance, the laminate is validated under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011; adhesion is tested as T-peel after retort at 121 °C and 0.1 MPa for 30 min. Pouch seal strength is recorded under ASTM F88/F88M-21, and channel-leak integrity is checked by dye penetration under ASTM F1929-15. If adhesion loss exceeds the control limit after retort, the peel failure mode is examined to distinguish cohesive sealant rupture from adhesive loss at the foil interface. Terminal products are retortable stand-up pouches, pet-food laminate structures, pharmaceutical strip-pack laminates, and high-barrier lidding films for ambient shelf-stable foods.

    Free Quote

    Competitive Arkema Orevac® OE807 Maleic Anhydride modified LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Arkema Orevac® OE807 is a maleic anhydride-modified linear low density polyethylene supplied as a reactive polyolefin intermediate for melt-compounded formulations and multilayer structures. The base polymer is an LLDPE backbone, while the grafted maleic anhydride groups provide polarity and the capacity to form covalent ester or amide linkages with hydroxylated mineral fillers, aminosilane-treated glass fibre, aluminium hydroxide, magnesium hydroxide, and polyamide chain ends. Because the product is intended for compounding or tie-layer let-down rather than as a standalone packaging resin, its specification sheet is written around melt rheology, melting behaviour, and anhydride functionality rather than final film or moulded-part properties. The manufacturer’s current technical bulletin lists a melt mass-flow rate of 2.5 g/10 min measured with a 2.16 kg load at 190 °C in accordance with ISO 1133-1:2022, and a density of approximately 0.912 g/cm3 determined by ISO 1183-1:2019. The melting peak recorded by differential scanning calorimetry per ISO 11357-3:2018 is typically near 124 °C. Exact values are lot-dependent and should be taken from the certificate of analysis issued for the specific delivery.

    The grafted maleic anhydride content is not always expressed as a single nominal percentage in regional datasheets because it is controlled by titration of saponified samples or by Fourier transform infrared spectroscopy, and the value is compared against an internal Arkema specification. When a formulation model requires a stoichiometric anhydride concentration, the lot-specific certificate of analysis provides the relevant value; published data for this specific configuration is limited without access to the manufacturer’s current technical bulletin. In compound screening, the effective reactive content is often judged from the torque response in a Brabender mixer at 190 °C and 50 rpm, where an increase in steady-state torque relative to unmodified LLDPE indicates grafting-induced polarity and molar mass changes.

    Relative to non-functional LLDPE, OE807 is not a drop-in viscosity modifier. The anhydride groups introduce melt-state moisture sensitivity, potential reactions with amine stabilisers, and a higher melt polarity that alters wetting on metal and mineral surfaces. These differences are intentional: they allow the resin to bind mineral fillers to the polyolefin matrix and to improve interfacial adhesion in coextruded barrier structures. The grade is differentiated from maleated high-density polyethylene coupling agents by its LLDPE backbone, which retains a lower crystalline fraction and a different balance between modulus and environmental stress crack resistance. Compared with lower-viscosity maleated polyolefins, the melt index of OE807 is in a medium-flow range, which supports dispersive mixing of high-surface-area fillers without excessive pressure drop in strand pelletising heads.

    The melt viscosity of OE807 can be shifted by blending with the host LLDPE; the shear-thinning behaviour of the blend follows typical polyolefin melt behaviour. In capillary rheometry at 190 °C, apparent shear rates from 100 s−1 to 1000 s−1 are relevant to die flows in profile extrusion and injection moulding. The esterification reaction between the anhydride and surface hydroxyl groups is kinetically limited; in a twin-screw extruder the reaction window is often 20 to 45 s after filler incorporation, depending on screw speed. Production lines with very short residence times may require a slightly higher let-down ratio to achieve the same coupling effect.

    What Limits Melt Processing Stability in High-Filler Compounding with OE807?

    In halogen-free flame-retardant compounds, OE807 is commonly added at 1 to 3 wt% of total formulation during twin-screw extrusion. The residence time distribution and shear history are set by screw configuration as much as by barrel temperature. A co-rotating twin-screw extruder with an L/D ratio of 40:1 or higher is typically operated with filler side-feeding after a melt seal, followed by atmospheric venting and vacuum devolatilisation at pressures at or below −0.08 MPa. When precipitated magnesium hydroxide or fine-precipitated aluminium hydroxide is run at loadings above 50 wt%, vent-port fouling can occur if low-molecular-weight maleated species are drawn from the melt surface before dispersion is complete. This is a production-scale maintenance issue controlled by adding the coupling agent upstream of the filler feed, using a distributive mixing section before the vacuum port, and maintaining vacuum-line knock-out capacity.

    The processing temperature window is bounded by melting point on the low side and anhydride degradation or crosslinking on the high side. Barrel settings from 170 °C to 220 °C are common, with short exposure to melt temperatures above 240 °C avoided because gel particles may form and the carbonyl functionality can be chemically altered. In reactive extrusion, melt temperature at the die should be measured with an immersion thermocouple or infrared pyrometer rather than inferred from barrel setpoints alone. The melt index of OE807 can drift if the material remains in the extruder at high temperature for excessive residence time; lot-to-lot viscosity differences are generally small but should be monitored by the melt mass-flow rate method in ISO 1133-1:2022.

    Moisture control is less demanding than for condensation polymers, but sacks exposed to high-humidity storage should be dried at 60 °C to 80 °C for 2 to 4 h in desiccant air if surface condensation is visible. This precaution reduces steam-induced porosity in the compounded strand and limits hydrolysis of the anhydride to the corresponding diacid. The diacid form remains polar but does not have the same ring-opening reactivity toward hydroxylated fillers; therefore, excessive moisture uptake can reduce interfacial coupling efficiency.

    Primary and secondary amine-based additives should be avoided or evaluated at low concentrations because amines react rapidly with the succinic anhydride ring during compounding, consuming the functional site before filler coupling can take place. Metal stearates and certain acid scavengers can also compete for anhydride reactivity; formulations should be screened by torque rheometry and by mechanical testing of the final compound rather than by single-point melt index alone. The product is generally not recommended for processes requiring a high-clarity monolayer film because the polar graft can increase surface haze and gel sensitivity in thin-gauge cast film, especially after multiple heat histories.

    In polyethylene/polyamide and polyethylene/EVOH coextrusion, OE807 is used as a tie-layer component. A typical tie layer is a let-down of OE807 into a neat LLDPE carrier at 10 to 30 wt% active resin, depending on the barrier resin, layer thickness, and line speed. Peel adhesion measurements on flat film are carried out using ASTM F904 or ISO 11339:2022; the observed adhesion is sensitive to nylon amine-end concentration, EVOH ethylene content, corona treatment, and the thermal history of the coextruded structure. Published data for this specific configuration is limited when non-standard layer ratios or recycled barrier trim are used.

    For mineral-filled polyolefin compounds, OE807 can be introduced upstream of the filler feed to allow the anhydride groups to react with the hydroxylated filler surfaces during dispersion. The resulting mechanical improvement is commonly assessed after injection moulding of tensile bars and impact specimens. Tensile tests according to ISO 527-2:2012 at 50 mm/min and notched Charpy impact tests according to ISO 179-1:2010 are appropriate indicators of coupling efficiency. Unfilled reference plaques of OE807 itself are rarely used for final part approvals because the product is an intermediate; instead, the filled compound is tested against the same formulation prepared with a non-functional LLDPE carrier. The relative increase in tensile strength at break and the reduction in filler agglomerate size in scanning electron microscopy images provide evidence of interfacial adhesion.

    For steel or aluminium lamination, OE807 can be used as a tie layer in extrusion coating or as a component of a hot-melt adhesive when blended with tackifiers and waxes. Peel adhesion to aluminium foil is measured by ASTM D1876 or internal T-peel methods after conditioning. The anhydride groups bond to metal oxide or hydroxide surface layers; cleaning and corona or flame treatment determine the failure locus. Published data for this specific configuration is limited when substrate surface energy is not controlled to the same level as the laboratory trial.

    Thermal Degradation Boundaries, Regulatory Checks, and Lot-Release Parameters

    Thermogravimetric analysis of maleated LLDPE under nitrogen typically shows the main degradation onset well above 350 °C, but this is a laboratory stability guide and not a melt-processing target. The functional groups can be monitored by infrared spectroscopy: the anhydride carbonyl band near 1710 cm−1 and a carboxylic acid shoulder near 1730 cm−1 can indicate hydrolysis or ring-opening after prolonged storage. A ratio shift toward the acid band suggests exposure to moisture or reaction with basic additives. The melt mass-flow rate, density, melting peak, and titrated anhydride content are the key lot-release parameters; the certificate of analysis should be requested for each batch because storage age and ambient humidity can change surface moisture while leaving the grafted functionality essentially intact.

    Regulatory compliance depends on the final article and the converter’s use conditions. OE807 is supplied as a reactive polymer intermediate and is not automatically certified as a food-contact resin. In food-contact adhesive applications, converters may need to demonstrate compliance with US FDA 21 CFR 175.105 or with Commission Regulation EU No 10/2011 for the finished structure, including overall migration and specific migration limits. Electrical and electronic market users typically request documentation for EU RoHS Directive 2011/65/EU and REACH SVHC status; the supplier’s regulatory datasheet lists the applicable declarations, and the user is responsible for verifying that the final compound meets the specific end-market standard.

    Control pointReference method or regulationTypical requirement or check
    Melt mass-flow rateISO 1133-1:2022Report at 190 °C/2.16 kg; compare to lot certificate
    DensityISO 1183-1:2019Measure on compression-moulded plaque at 23 °C
    Melting behaviourISO 11357-3:2018Report peak melting temperature from second heating at 10 K/min
    Tensile properties of filled compoundISO 527-2:2012Test conditioned type 5A or type 1B specimens; modulus at 1 mm/min, break at 50 mm/min
    Notched impact of filled compoundISO 179-1:2010Test at 23 °C and, where required, −20 °C; compare with unmodified carrier control
    Food-contact adhesive migrationUS FDA 21 CFR 175.105; EU 10/2011 as applicableValidate finished structure migration limits; do not assume direct food-contact approval for the neat resin

    The principal operational boundary in using OE807 instead of a non-functional LLDPE is that the anhydride group is reactive, not inert. Storage conditions should prevent prolonged exposure to moisture-laden air, and formulations should not combine the product with primary or secondary amine antistatic concentrates unless the user has verified that the amine does not reduce coupling efficiency. In high-speed coextrusion, the tie-layer let-down ratio should be adjusted to avoid melt instability at the die; edge trim containing EVOH or polyamide should be dried if it is returned to the polyethylene skin layer because hydrolytic degradation products can react with the anhydride and increase interfacial haze. These limitations define the process boundaries within which the functional performance is reproducible.

    In filled systems where property retention after water immersion is critical, the compound should be tested after conditioning in water at 80 °C for 7 days or per the relevant end-product standard, because interfacial bonds formed by anhydride coupling can be attacked by hot water over time. The choice of OE807 versus an unmodified LLDPE or a higher-melt-flow maleated grade should therefore be based on a designed experiment that includes filler type and particle size, base resin melt index, extruder screw profile, and final part test method rather than on melt index alone.

    Top