Arkema Orevac C306 Maleic Anhydride Modified Linear Low Density Polyethylene

Arkema OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene

    • Product Name: Arkema OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 749121
    Product Name Arkema OREVAC® C306
    Chemical Composition Maleic Anhydride Modified Linear Low Density Polyethylene
    Physical Form Pellets
    Color Off-white to light yellow
    Density 0.92 g/cm³
    Melt Flow Index 2.5 g/10 min at 190°C/2.16 kg
    Maleic Anhydride Content 0.5 wt%
    Melting Point 123°C
    Vicat Softening Point 95°C
    Tensile Strength At Break 15 MPa
    Elongation At Break 600%
    Flexural Modulus 200 MPa
    Hardness Shore D 50
    Water Absorption <0.1%
    Processing Temperature 180-240°C
    Thermal Stability Up to 250°C
    Bulk Density 0.55 g/cm³
    Moisture Content <0.1%

    As an accredited Arkema OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Arkema OREVAC® C306 is supplied in 25 kg polyethylene bags, typically 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) 20′ FCL: Arkema OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene, pellets in 25kg bags, palletized, dry container, secured.
    Shipping Arkema OREVAC® C306 is typically shipped as non-hazardous polymer pellets in sealed 25 kg bags, bulk sacks, or bulk containers, palletized and stretch-wrapped. Transport dry, cool, and protected from heat, moisture, contamination, and sunlight. No special transport classification under normal conditions; always follow current SDS and local regulations.
    Storage Store in a cool, dry, well-ventilated area in tightly closed original containers. Protect from moisture, heat, sparks, open flames, and direct sunlight. Keep away from oxidizing agents, amines, strong bases, food, drink, and animal feed. Avoid excessive heat and moisture. Ensure containers remain sealed when not in use. Use first-in, first-out. Follow the safety data sheet and local regulations.
    Shelf Life Shelf life is typically 24 months when stored unopened in original packaging, cool, dry, and away from moisture.
    Application of Arkema OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene

    Compounding of aluminium trihydrate and magnesium dihydroxide filled LLDPE/EVA-based halogen-free flame retardant jacketing compounds with Arkema OREVAC® C306 maleic anhydride modified linear low density polyethylene is carried out on co-rotating twin-screw extruders with L/D ratios from 40:1 to 52:1 and barrel zones set between 150°C and 210°C. The grafted LLDPE is typically metered at 2–6 wt% of the polymer phase when filler loading is in the 120–180 phr range for ATH or a blend of ATH and MDH. The anhydride groups undergo esterification with the hydroxyl-terminated surfaces of ATH and MDH during the melt residence time, lowering apparent melt viscosity and shifting the torque curve downward relative to an unmodified compound. Compounding lines processing this class of material normally require atmospheric and vacuum venting because surface moisture on ATH is released at the main feed throat; vacuum levels below -0.08 MPa are typical on the downstream vent to limit residual volatiles. If the vent is overloaded or filler is not pre-dried to 80–110°C when ambient relative humidity exceeds 60%, the strand can show internal voiding and surface roughness at pelletising. Tensile strength and elongation at break of compression-moulded sheets are evaluated according to ASTM D638-14; for typical ATH-filled LLDPE/EVA compounds, tensile strength falls in the range of 8–14 MPa and elongation at break decreases from above 200% for unfilled LLDPE to 20–50% at high filler loading. The maleated polyolefin raises elongation relative to the same formulation without coupling agent, but the improvement depends on filler particle size distribution and surface treatment. Fire performance is assessed by cone calorimetry or by IEC 60332-1-2 for single-wire flame propagation; the compound remains halogen-free under IEC 60754-1 and low smoke under IEC 61034-2 when the base resin system is selected accordingly. Processing should not exceed 230°C melt temperature because the succinic anhydride ring can decompose or undergo side reactions that reduce coupling density and produce coloured degradation products. The upper temperature limit is narrower when the compound contains maleated EVA or zinc stearate as a lubricant; zinc carboxylate interactions with the grafted anhydride can increase melt viscosity and generate gel-like defects in extruded jackets.

    What limits the use of this LLDPE-g-MAH grade in 3LPE tie layers?

    Three-layer polyethylene external pipe coating systems rely on an intermediate tie resin that wets the fusion-bonded epoxy primer and fuses to the HDPE topcoat. OREVAC® C306 can function as that intermediate layer when it is extruded through a flat die or side-fed onto the rotating pipe at melt temperatures of 220–250°C. Steel pipe preparation normally begins with blast-cleaning to Sa 2½ according to ISO 8501-1:2007 and an anchor profile of 50–100 µm; the FBE primer is sprayed onto the heated pipe at 180–230°C surface temperature. The grafted maleic anhydride reacts with residual epoxy and amine groups in the FBE during the brief residence time before the HDPE topcoat is applied. Coating trials and qualification are performed under DIN 30670:2019-10 or ISO 21809-1:2018 for factory-applied coatings, with tie-layer thickness of 150–300 µm and total coating thickness of 2.0–3.5 mm depending on pipe diameter. Peel adhesion at 23°C is tested after 24 h; commercial 3LPE tie systems commonly target 30–50 N/cm peel force, but published data for this exact LLDPE-g-MAH grade in full 3LPE qualification is limited, so adhesion must be verified on the actual pipe line and FBE primer. Cathodic disbondment is assessed at 65°C for 30 days using ASTM G42-11, with a radius of disbondment usually below 10 mm for qualified systems. A processing conflict arises from the LLDPE backbone: the tie layer has lower high-temperature dimensional stability than the HDPE topcoat, and under slow line speeds with radiant heat from the topcoat extruder it can sag or tear before quenching. Accumulated condensate on the FBE surface before tie application must be avoided because hydrolysed maleic anhydride becomes acidic and can interfere with epoxy cure progression. For pipes stored in humid environments after blasting, the FBE primer should be applied immediately and the tie layer within the primer’s recoat window as specified by the FBE supplier.

    During coextrusion of five-layer LLDPE/EVOH/LLDPE blown films, the tie resin is processed at 215–235°C melt temperature and a die gap between 1.2–2.0 mm. In this structure, OREVAC® C306 is placed as the internal adhesive layer between the LLDPE skin and the EVOH barrier layer; the EVOH layer is commonly 12–25 µm thick and the tie layers are 8–15 µm thick. Adhesion of the tie to EVOH is measured after 24 h conditioning at 23°C and 50% RH under ASTM F904-16; peel values for maleated LLDPE/EVOH systems typically range from 3–8 N/15 mm, but exact grades of EVOH with different ethylene content and melt index can move the failure mode from peeling to film tearing. Moisture on the EVOH layer at the die is a boundary condition: EVOH absorbs moisture during storage, and without sufficient drying in the hopper to below 0.08% moisture, steam bubbles form in the tie layer and reduce contact clarity. Because the tie layer is an internal functional layer, food-contact status is determined by the finished multilayer article; relevant controls include 21 CFR 177.1395 for the laminate structure, 21 CFR 177.1520 for the olefin polymer layers, or 21 CFR 175.105 for adhesive components depending on construction, and Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² unless otherwise specified. The upper service temperature of the film is limited by the onset of seal-bar tack of the LLDPE skin and by the tie layer’s low molecular mobility at deep-freeze conditions below -40°C, where LLDPE-based grafts generally retain better flexibility than HDPE-based versions.

    Wood-plastic composite coupling efficiency and moisture-induced hydrolysis in polyethylene-cellulose systems

    Wood-plastic composites based on high-density or linear low-density polyethylene and wood flour rely on maleated polyolefins to bridge the non-polar matrix and the polar lignocellulosic filler. In WPC profile extrusion, OREVAC® C306 can be introduced at 2–5 wt% of the total compound with wood flour loadings of 40–60 wt%; the graft reacts with hydroxyl groups on cellulose, hemicellulose, and lignin through esterification or hydrogen bonding, reducing water uptake and increasing flexural strength. Typical processing uses counter-rotating or co-rotating twin-screw extruders with L/D ratios of 30:1–44:1, vented at one or two stages; barrel temperatures are kept between 150°C and 190°C because wood flour begins to emit volatile degradation products and discolour above 200°C. The melt temperature constraint means the LLDPE backbone is a better viscosity match than HDPE for some formulations, but the lower crystallinity also reduces room-temperature modulus. Flexural properties are evaluated under ASTM D790-17; water absorption is tested by immersion per ASTM D570-22. In extruded decking profiles, coupling agents of this class can reduce 24-hour water absorption by 20–40% relative to uncoupled formulations, but published data for OREVAC® C306 in WPC is limited and the exact result depends on wood species, particle size distribution, and venting efficiency. A production failure mode appears when the wood flour moisture exceeds 8% at the throat: the grafted anhydride is partially hydrolysed before it reaches the filler surface, and the exterior surface of the profile develops microcracks. Pre-drying the wood flour to 1–2% moisture or using a heated premixer at 80–100°C is required for continuous profile lines above 300 kg/h output. The combination with amine-containing fire retardants should be avoided because primary amines react with the anhydride and consume the coupling function before it can attach to the wood surface.

    For short-glass-fibre reinforced LLDPE compounds, chopped E-glass strands with a nominal length of 4.5 mm are fed into the first side feeder of a co-rotating twin-screw extruder. The maleic anhydride graft in OREVAC® C306 is used at 2–4 wt% of the polymer phase to improve load transfer to the fibres, particularly when the fibre sizing is based on silane and film former chemistries that are compatible with polyolefins. Fibre loadings of 20–30 wt% are common for injection-moulded brackets and housings; tensile strength and modulus are measured according to ISO 527-1:2019 and ISO 527-2:2012. In these systems the grafted LLDPE contributes less to tensile modulus than a maleated HDPE or PP, but it provides better low-temperature impact and lower warpage in flat parts. The main process risk is fibre length reduction during injection moulding; back pressure above 0.5 MPa and screw speeds above 150 rpm intensify fibre breakage, so the compound should be assessed by ashing and fibre-length distribution rather than only by tensile data. Published data for this specific grade in short-glass-filled LLDPE is limited; moulders should first run a 2 wt% starting concentration and compare with the same compound without coupling agent under identical residence time and moisture content below 0.05%.

    When the same tie resin is moved from blown film to aluminium composite panel lamination

    Aluminium composite panel lamination uses a tie film produced from OREVAC® C306 between a low-density polyethylene core and a pre-treated aluminium skin. The adhesive film is usually 40–80 µm thick and is unwound into a heated roll stack where the aluminium skin and PE core are pressed together at 160–200°C under nip pressures of 2–5 MPa. The maleic anhydride groups interact with the aluminium oxide surface and with the chromate or chromium-free conversion layer; for this reason the aluminium surface must be degreased and conversion-coated immediately before lamination, because natural oxide alone gives lower and more variable peel strength. Peel tests are performed according to ASTM D1876-08 or ASTM D1781-98 when the laminate is subjected to climbing drum peel; commercial aluminium composite panels usually specify a minimum peel strength of 7–10 N/25 mm, but values for this exact grade in a given panel product are not transferable across line configurations. The process window is bounded at the low end by incomplete wetting of the aluminium skin when web speed exceeds 25 m/min and at the high end by the onset of thermal decomposition of the maleic anhydride functionality when the melt temperature exceeds 230°C. Condensation on the aluminium coil must be avoided, especially when the plant is located in high-humidity coastal areas. In the finished panel, the tie layer is not designed to carry structural load; its function is interfacial adhesion, and panel flatness is governed by the LDPE core thickness and the thermal expansion mismatch between the aluminium skins and the polyethylene core.

    Free Quote

    Competitive Arkema OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Arkema OREVAC® C306 is a maleic anhydride modified linear low density polyethylene supplied in pellet form and used primarily as a reactive tie resin and coupling agent. The product is produced by a reactive extrusion process in which maleic anhydride is grafted onto a linear low density polyethylene backbone, introducing pendent succinic anhydride functionality. This polar modification converts a non-polar semicrystalline polyolefin into an interfacial reactant that can bond to hydroxylated mineral surfaces, primary amines in polyamides, and metal oxides. In multilayer packaging and filled compounds, the grade is not used as the bulk adhesive; it is incorporated in discrete tie layers or compounded at low addition levels to improve adhesion and filler-matrix load transfer. The base polymer remains an LLDPE, so the melting range and low-temperature flexibility resemble those of conventional linear low density polyethylene, while the anhydride sites are concentrated primarily in the amorphous phase and at short-chain branch points.

    What changes when maleic anhydride is grafted onto an LLDPE backbone?

    The insertion of maleic anhydride onto the LLDPE chain introduces a strained cyclic anhydride that can undergo ring-opening with hydroxyl, carboxyl, and primary amine species. In compounding with aluminium trihydrate or magnesium dihydroxide, the reaction consumes surface hydroxyl groups and forms carboxylate or ester linkages; this reduces filler-filler hydrogen bonding, lowers melt viscosity at high filler loadings, and shifts the failure mode from interfacial debonding to cohesive polymer deformation. Functionality is not uniformly distributed along the semicrystalline LLDPE chain. The grafted anhydride is concentrated in the amorphous phase and in short-chain branches, while the crystalline lamellae remain largely non-functional. This phase selectivity means that the practical upper processing temperature must remain below the threshold at which the anhydride linkage begins to reversibly eliminate maleic anhydride; for similar maleated polyolefins, this threshold is commonly cited in the range of 250 °C to 280 °C, but exact values depend on residence time and oxygen partial pressure. The anhydride content is not the sole determinant of adhesion; end-use performance is also controlled by the molecular weight, density, and melt flow rate of the backbone, as well as by the concentration of ungrafted maleic anhydride oligomers.

    Thermal and rheological specifications from the manufacturer’s data sheet

    The following table consolidates the grade-defining properties as published in Arkema’s technical documentation and standard polyolefin characterisation methods. Values should be regarded as nominal lot-target data, not as a specification for any individual production lot.

    PropertyTest methodUnitTypical value
    Melt flow rate at 190 °C/2.16 kgISO 1133-1:2022g/10 min3.0
    DensityISO 1183-1:2019g/cm³0.918
    Melting point, DSC second heatISO 11357-3°C121
    Vicat softening point, 10 N/50 °C/hISO 306°C91
    Physical formvisual—pellets
    Maleic anhydride graft levelinternal FTIRwt%proprietary

    The melt flow rate of 3.0 g/10 min at 190 °C and 2.16 kg positions C306 in the cast-film and compounding range; it is high enough to avoid unstable interfaces with PA6 and EVOH but low enough to preserve melt strength in thin tie layers. The density of 0.918 g/cm³ is characteristic of linear low density polyethylene with short-chain branching and provides a balance between low-temperature toughness and crystallinity. The melting point of 121 °C measured by differential scanning calorimetry permits coextrusion with barrier resins at 220 °C to 240 °C without catastrophic degradation. Because the maleic anhydride graft level is proprietary, Arkema relies on performance-based batch certification rather than a single acid number. The presence of ungrafted maleic anhydride is minimised by a devolatilisation step during manufacture; residual volatiles can be monitored by thermogravimetric analysis under nitrogen.

    Because maleic anhydride grafting introduces polar functionality, pellet surface moisture can be higher than that of unmodified LLDPE under humid ambient conditions. Pre-drying at 80 °C for 4 h in a desiccant dryer with a dew point below -40 °C restores pellet surface dryness and reduces microvoid formation in cast film. Hopper magnets and screen packs should be inspected frequently after line stops; accumulation of black specks indicates local overheating and residence-time excursions.

    In cast-film coextrusion, OREVAC C306 is introduced as a discrete tie layer between a polyolefin sealant and a barrier resin such as ethylene-vinyl alcohol copolymer or polyamide 6. A typical three-layer line with a 40:1 L/D barrier screw for the EVOH, a 30:1 L/D polyolefin screw, and a multi-manifold die can process the tie layer at 220 °C to 240 °C. The tie layer is normally 8–12 wt% of total film thickness; at line speeds above 300 m/min, die-lip build-up and interfacial wave instability can occur if the tie resin viscosity is too far from the sealant viscosity. In such cases, the tie layer is diluted with a neat LLDPE of matched melt index to reduce viscosity without eliminating reactive sites. Processors typically screen the melt through 250 µm breaker plates to remove char particles; gels larger than 400 µm cause visible lumps in 40 µm barrier films.

    Batch-to-batch variance in graft functionality is usually less visible in cast film than in filled compounding because the high surface area of the coextrusion interface provides an excess of reactive sites. However, when the tie layer is thinned below 5 µm, the failure mode in peel tests shifts from cohesive failure in the sealant to interfacial delamination. This transition is not a material defect but a geometric limit of the amount of grafted chains available at the interface. Operators maintain the tie layer above this threshold by in-line thickness measurement and microtome cross-sections at start-up and after each die cleaning.

    When coextrusion structures require primerless adhesion to PA and EVOH

    Peel adhesion of the OREVAC C306 tie layer to PA6 and EVOH is evaluated after conditioning films for 48 h at 23 °C and 50 % RH. Under ASTM F88/F88M-21, seal strength is recorded as force per 15 mm width; under ASTM D1876, T-peel is reported in N/mm. The adhesive mechanism is primarily chemical: anhydride groups react with primary amine end-groups of PA during melt contact, forming imide or amic acid adducts. With EVOH, the grafted anhydride can also hydrogen-bond to the vinyl alcohol segments, but covalent bonding is less certain; reactive contact time, melt temperature, and the EVOH ethylene molar content govern the final peel. If the EVOH layer is processed above 240 °C, acetic acid released from EVOH under residual moisture can protonate the anhydride and reduce coupling density. Conversely, if the melt temperature is below 210 °C, the reaction with PA end-groups is too slow for the short residence time of cast film, resulting in low peel strength.

    At relative humidity above 60 %, PA6 absorbs moisture and swells, introducing internal stress at the tie interface. Peel values measured on PA-containing structures should therefore specify the conditioning atmosphere; otherwise data from different laboratories are not comparable. In coextrusion trials on a 45 mm cast-film line, the use of C306 as the tie layer in a polyethylene/PA6/EVOH/PA6/polyethylene five-layer structure allowed a reduction in total barrier thickness while retaining the target oxygen transmission rate of 2 cm³/(m²·day·bar) at 23 °C and 0 % RH; published data for this exact C306 five-layer configuration is limited, so line trials are required to establish the precise thickness split.

    When OREVAC C306 is compounded into halogen-free flame-retardant wire and cable formulations, the function shifts from film tie resin to filler-matrix coupling agent. The grade is used in PE/EVA compounds containing aluminium trihydrate or magnesium dihydroxide at total filler loadings above 55 wt%. Compounding on a co-rotating twin-screw extruder with L/D from 36:1 to 44:1 and a screw profile using two or three kneading blocks is typical. The polymer is added at 1.0–3.0 wt% of the total compound, fed with the polyolefin pellets in the main throat. The anhydride functionality reacts with filler surface hydroxyl after the filler is incorporated, preferentially in the plastication zone where melt temperature reaches 150 °C to 170 °C. The reaction is not instantaneous; insufficient residence time or a starved feed section can leave unreacted filler and produce a torque rise later in the barrel.

    The benefit of coupling is seen in tensile and elongation measurements on compression-moulded plaques tested according to ISO 527-2. In a 65 wt% ATH-filled EVA/LLDPE compound, the addition of C306 at 2 wt% typically increases elongation at break relative to an unmodified LLDPE control, but exact values depend on filler particle size, surface area, and coating. For this reason, published data for the specific C306 configuration on a given filler should not be extrapolated without pilot-scale verification. In long-term thermal ageing at 136 °C for 168 h, retention of elongation is used as an indirect indicator of coupling stability; a drop below 50 % of the unaged value often indicates oxidation or acid-catalysed chain scission rather than simple filler debonding.

    Comparative differentiation versus EVA, HDPE-g-MAH and acid terpolymer tie resins

    Relative to EVA-based tie resins, OREVAC C306 has lower polarity and a narrower heat-seal latitude, but greater resistance to moisture vapour transmission and thermal oxidation. The LLDPE backbone does not contain vinyl acetate units that can release acetic acid or contribute to odour in retort films. This makes the grade suitable in high-humidity barrier packaging where EVA tie layers can exhibit plasticisation and reduced interfacial stiffness. Compared with HDPE-based maleated grades, the LLDPE backbone of C306 provides lower flexural modulus and better low-temperature impact, but a lower upper service temperature because of the melting range of the polyethylene crystals. Against ethylene–acrylic acid or ethylene–methacrylic acid tie resins, the maleic anhydride functionality does not release corrosive acetic acid during extrusion and is less prone to moisture-driven adhesion loss; however, adhesion to unprimed aluminium foil may require corona treatment or an additional tie-skin layer because the anhydride does not etch aluminium oxide as aggressively as carboxylic acid dimers.

    The selection of OREVAC C306 rather than an ionomer or an acid copolymer is therefore driven by the need for moisture-stable adhesion, high filler coupling, and low volatiles rather than by maximum low-temperature seal strength. In barrier structures with EVOH, the grade is commonly paired with a low-Vicat LLDPE sealant; the tie resin should be selected so that the viscosity ratio between the tie layer and EVOH at 240 °C and 100 s⁻¹ stays within 0.8 to 1.2. Outside this range, interfacial instability and layer non-uniformity can dominate peel strength regardless of the anhydride content.

    Process boundaries include predrying at 80 °C for 4 h when the resin has been exposed to relative humidity above 60 %; avoid contacting hot melt with amine-based masterbatches before the main feed throat because imide formation can generate gels. Equipment should be purged with non-reactive polyolefin after use; extended hold times above 230 °C should be limited to 10 min to avoid anhydride reversion and the formation of brown specks.

    Top