Arkema Orevac 18302n Maleic Anhydride Modified Linear Low Density Polyethylene

Arkema OREVAC® 18302N Maleic Anhydride Modified Linear Low Density Polyethylene

    • Product Name: Arkema OREVAC® 18302N Maleic Anhydride Modified Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 845271
    Density 0.91 g/cm³
    Melt Flow Index 2.5 g/10 min (190°C/2.16 kg)
    Maleic Anhydride Content 0.8 wt%
    Melting Point 123°C
    Vicat Softening Temperature 93°C
    Tensile Strength At Break 18 MPa
    Elongation At Break 700%
    Flexural Modulus 200 MPa
    Hardness Shore D 50
    Water Absorption <0.1%
    Appearance Pellets
    Color White to off-white

    As an accredited Arkema OREVAC® 18302N Maleic Anhydride Modified Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Arkema OREVAC 18302N is typically supplied in 25 kg bags, palletized, and 1000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL: Arkema OREVAC® 18302N pellets in 25 kg bags, palletized, shrink-wrapped, secured in dry container; non-hazardous cargo.
    Shipping Arkema OREVAC® 18302N is supplied as solid thermoplastic pellets, typically packaged in moisture-barrier bags or boxes and palletized. Ship in clean, dry, ventilated transport, away from heat, moisture, oxidizers, and ignition sources. Keep containers closed, protect from sunlight/damage, and follow SDS/local regulations. Consult supplier for specific packaging, documentation, and transport classification.
    Storage Store OREVAC® 18302N in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, moisture, and oxidizing agents. Keep containers tightly closed to prevent contamination. Use original packaging, avoid extreme temperatures, and maintain clean, dust-free conditions. Follow local regulations and the manufacturer’s safety data sheet for safe handling and storage.
    Shelf Life Store sealed in original packaging, dry, below 30°C; shelf life is typically two years from manufacturing date.
    Application of Arkema OREVAC® 18302N Maleic Anhydride Modified Linear Low Density Polyethylene

    In five-layer coextruded blown film lines producing polyamide/EVOH barrier structures for modified atmosphere packaging, OREVAC 18302N is introduced as a continuous tie layer between the LLDPE sealant or skin layer and the EVOH or polyamide core. The adhesive extruder melt temperature is controlled between 190°C and 230°C; the barrier extruder is run at set points high enough to melt the polyamide or EVOH without causing residence-time degradation. Blow-up ratios from 2.0:1 to 2.5:1 and die gaps from 1.8 mm to 2.6 mm are used to maintain bubble symmetry when the tie layer is diluted with regrind or non-grafted LLDPE. Tie-layer gauge is normally specified at 4 µm to 12 µm within a total film thickness of 50 µm to 120 µm. The dilution threshold is not universal: production runs on a 65 mm single-screw adhesive extruder with an L/D of 30:1 have shown that replacing more than 30 wt% of the grafted polymer with non-grafted LLDPE can reduce interlayer T-peel adhesion measured per ASTM D1876 at 300 mm/min, but the exact drop depends on EVOH ethylene content, polyamide end-group concentration, and die residence time. Compliance for finished EU food-contact laminates is determined under Regulation (EU) No 10/2011, including the overall migration limit of 10 mg/dm² and specific migration verification in the appropriate food simulant for the actual packaged food class; for U.S. structures, the adhesive function may be evaluated under 21 CFR 175.105, while the olefin backbone falls under 21 CFR 177.1520. EVOH and polyamide must be pre-dried before coextrusion; EVOH drying at 80°C for 4 h and polyamide drying at 80°C for 6 h to 8 h are used to keep residual moisture below 0.08 wt%. Moisture above this level produces microbubbles at the tie-layer interface that visible inspection records as haze bands and often coincide with interlayer delamination during thermoforming. Terminal products include vacuum pouches for processed meat, retortable lidding film, shrink bags for cheese and poultry, and thermoformed trays for fresh pasta.

    Adhesive interlayer response to cathodic disbondment and hot water immersion in three-layer polyethylene pipe coatings

    At the adhesive boundary between fusion-bonded epoxy (FBE) primer and the high-density polyethylene topcoat, the grafted LLDPE must wet the gelled epoxy surface during the narrow time window between FBE film formation and topcoat coverage. Steel pipe is blast-cleaned to Sa 2½ per ISO 8501-1 and preheated to 180°C–220°C; FBE powder is applied at 60 µm to 120 µm, after which the adhesive layer is extruded through a side-fed die at 150 µm to 300 µm while the pipe rotates at 1.0 m/min to 3.5 m/min. In production coating plants, edge waviness and adhesive striping are the principal failure modes when the adhesive viscosity is not matched to the topcoat: a high-melt-index grafted layer sags on large diameters and can thin at the pipe crown, while a low-melt-index layer does not penetrate FBE gel texture and yields isolated adhesion voids that become visible only after 24 h water immersion. The complete coating system is qualified under ISO 21809-1:2018 and DIN 30670:2012; acceptance testing includes peel adhesion before and after hot water immersion, cathodic disbondment resistance, impact resistance, and hot water soak performance. Formulation uses OREVAC 18302N as the reactive constituent in a blend with a non-grafted linear medium-density polyethylene carrier at a mass ratio between 25:75 and 60:40; the ratio is adjusted against topcoat melt index and pipe preheat to prevent sag or poor wetting. If the adhesive melt temperature exceeds 240°C, the maleic anhydride functionality can participate in gel-forming reactions that produce hard specks and screw pressure variation. The grafted resin must be pre-dried at 80°C for 3 h when ambient relative humidity is above 60%; moisture not removed before extrusion causes steam pinholes at the FBE-adhesive interface. Terminal products include buried gas and oil transmission pipelines, above-ground insulated pipe systems, and steel water main rehabilitation.

    Continuous double-belt press lamination of fire-retardant polyethylene core stock to coil-coated aluminium requires adhesion that survives panel trimming, bending, and building-movement stress, and the grafted LLDPE is therefore incorporated directly into the core compound rather than applied as a separate film. Core stock based on low-density polyethylene and 60–70 wt% mineral filler incorporates OREVAC 18302N at 2–5 wt% of total compound; when the aluminium coil enters without chemical conversion coating, the dose is raised to 8 wt% to restore peel force on degreased substrates. Published data for this specific grade in aluminium composite panel core stock is limited; therefore the addition level must be confirmed on the production laminator with the actual mineral filler, line speed, and coil pre-treatment. Building façade applications are regulated under EN 13501-1 reaction-to-fire classification at the assembled panel level; the tie resin itself carries no fire class and cannot be treated as a fire-performance additive. Processing takes place on a co-rotating twin-screw extruder at melt temperatures between 170°C and 210°C with a flat sheet die feeding a double-belt press at 0.5 bar to 1.2 bar nip pressure; filler moisture must remain below 0.15 wt% to prevent hydrolytic deactivation of the anhydride and blistering at the metal-polymer interface. In continuous campaigns, the first 3 m of each coil are peel-tested at the line; increases in peel force variability after filler changeover are often traced to moisture adsorbed on the replacement filler during hopper residence. Terminal products include exterior façade panels, interior wall panels, signage boards, and cabinetry.

    What coupling-agent dose avoids embrittlement in wood–LLDPE extrusion without sacrificing flexural modulus?

    When wood flour is compounded at 50–65 wt% with LLDPE, OREVAC 18302N is metered gravimetrically into the main feed throat at 2–4 wt% of total formulation; maleated polyolefin addition below 2 wt% produces insufficient esterification at the lignocellulosic fibre surface, while levels above 6 wt% can produce melt strength reduction at the die and low-temperature impact failures in the finished board. Counter-rotating conical twin-screw extruders with an L/D ratio of 32:1 to 36:1 are used to limit shear heating; wood flour is side-fed after the polymer melting zone, and the melt temperature is held at 160°C to 185°C. Wood flour moisture must be dried below 1.0 wt% before side-feeding; excursions above 1.5 wt% cause steam pressure in the downstream vent section and surface blisters on the extruded profile. Compliance testing for decking and railing is governed by ASTM D7031-11 for flexural properties, creep, and freeze-thaw durability, and by EN 15534-1:2014 for wood-polymer composite decking and cladding; the coupling agent dose is optimized to retain the standard’s required impact performance after weathering. Production experience with tropical hardwood fillers shows that extractives can act as anhydride scavengers, requiring a shift from 2 wt% toward 4 wt% before a measurable flexural modulus plateau is reached. Terminal products include exterior decking boards, railing, fencing, and window profiles.

    When magnesium dihydroxide surface silanization is combined with maleated LLDPE-bearing compounds

    In low-smoke zero-halogen sheathing compounds where magnesium dihydroxide or alumina trihydrate loadings are pushed to 55–65 wt%, the grafted polyolefin is added at 2–8 wt% relative to mineral filler, not total compound; the lower end of this range is evaluated where the filler has a complete silane surface treatment, while the upper end is reserved for coarse or poorly treated grades that exhibit high surface moisture. The objective is to retain elongation at break above 150% on dumb-bell specimens tested per ISO 527-2 while maintaining limiting oxygen index above 35% per ISO 4589-2. Cable sheathing compounds are qualified against IEC 60754-2 for acid gas evolution, IEC 61034-2 for smoke density, and ISO 4589-2 for limiting oxygen index; the maleated resin must contribute no halogen or heavy-metal residues. Compounding is performed on a co-rotating twin-screw extruder with an L/D ratio above 40:1 and a side feeder downstream of the primary melting zone; melt temperature must not exceed 200°C because alumina trihydrate begins endothermic dehydration near 190°C and off-gassing creates porosity at the pellet centre. In production campaigns, batch-to-batch variation in the silane treatment of magnesium dihydroxide has been observed to invert the expected viscosity build-up at constant grafted resin dosage, requiring pelletizer die face pressure adjustments; if the pelletizer strand diameter becomes erratic, the silane treatment level and filler moisture are tested before adjusting the maleated polyolefin content. Terminal products are building riser cable sheathing, marine power cable jackets, and rail transit control cable jackets.

    Extrusion coating tie-layer behavior on corona-treated aluminum foil

    In extrusion coating of OREVAC 18302N onto corona-treated aluminium foil for pharmaceutical lidding and liquid sachet laminates, the polymer is cast through a flat die at a coating weight of 8–20 g/m² and a melt temperature of 230°C to 260°C; the air gap between die exit and nip is maintained between 150 mm and 250 mm, and the chill roll is held at 15°C to 20°C. Higher air gaps increase oxidation of the grafted polyolefin surface but improve aluminium oxide wetting; lower air gaps reduce neck-in and improve gauge uniformity at the edges. The ratio of grafted resin to non-grafted LLDPE in the coating layer ranges from 40:60 to 100:0; dilution is adjusted against foil temper and corona treatment level. Compliance for pharmaceutical laminates is often assessed under 21 CFR 175.105 adhesive components and 21 CFR 177.1520 olefin polymers; EU food-contact laminates may require overall migration testing under Regulation (EU) No 10/2011. Production experience indicates that corona-treated foil must be laminated immediately after treatment; exposure to relative humidity above 70% for more than 2 h reduces adhesion and causes uneven coating thickness at the edges. Terminal products are blister lidding foil, stick pack sachet laminates, and aseptic packaging barrier plies.

    Free Quote

    Competitive Arkema OREVAC® 18302N Maleic Anhydride Modified Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Arkema OREVAC® 18302N is a maleic anhydride modified linear low density polyethylene supplied as a pelletized reactive extrusion grade. Its linear low density backbone is grafted with polar maleic anhydride groups; the polyolefin segment remains co-crystallizable with polyethylene seal layers, while the anhydride reacts with terminal amines in polyamides and with hydroxylated mineral surfaces. The material is used as a tie layer in polyolefin/polyamide and polyolefin/EVOH coextrusion, as a coupling agent in filled polyethylene compounds, and as a reactive blend component where higher melt-flow and low-temperature flexibility are required. Unlike unmodified LLDPE, the resin is moisture sensitive during melt processing because hydrolysis of the anhydride to carboxylic acid reduces interfacial reactivity and can change the shear viscosity under production-scale conditions.

    What Processing Envelope Prevents Anhydride Hydrolysis and Gel Formation?

    Melt processing is typically maintained between 190 °C and 240 °C; die zones are kept near the lower bound to limit anhydride degradation. On a corotating twin-screw extruder with an L/D ratio of 44:1, the resin is fed at the main feed throat, while mineral fillers are side-fed after the primary melting zone. Vacuum devolatilization at −0.08 MPa is applied downstream to strip moisture and low-molecular-weight reaction residues. If ambient relative humidity exceeds 60%, pre-drying in a desiccant dryer at 70–80 °C for 4 h is required, with residual moisture below 0.02 wt% before extrusion. Subjecting the melt to temperatures above 250 °C can generate crosslinked gel particles and discolouration, while hydrolysed anhydride alters the FTIR carbonyl absorption region near 1785 cm⁻¹. Residence time above 45 s at 230 °C should be avoided on production lines with narrow die passages because localized viscosity rises when coupling reactions occur prematurely.

    Lot release documentation should be reviewed for melt mass-flow rate, density, melting endotherm, and grafted maleic anhydride content. The melt flow rate is measured under ISO 1133-1:2022 at 190 °C with a 2.16 kg load; density is measured under ISO 1183-1:2019 at 23 °C; and the melting peak is determined by differential scanning calorimetry under ISO 11357-3:2018. Commercial LLDPE-grafted maleic anhydride tie resins of this class are commonly controlled to a density between 0.910 g/cm³ and 0.915 g/cm³, with a melting peak between 120 °C and 126 °C. Published melt mass-flow values for OREVAC 18302N are generally in the 1.0 g/10 min to 2.0 g/10 min range; the exact figure is lot-specific and appears on the certificate of analysis. Graft content is frequently controlled within 0.5 wt% to 1.0 wt%, with acid-base titration or FTIR used for lot-release verification. Tensile and impact values are not fixed design limits because the graft level, molecular weight distribution, and conditioning state affect the result. Unfilled compression-moulded specimens of commercial LLDPE-g-MAH in this class generally show ductile tensile behaviour under ISO 527-2, but end-use testing on the final compound or film is required to establish fitness for a given construction.

    Primary Characterization Methods for OREVAC 18302N
    PropertyMethodUnit
    Melt mass-flow rateISO 1133-1:2022g/10 min
    DensityISO 1183-1:2019g/cm³
    Melting endothermISO 11357-3:2018°C
    Maleic anhydride contentFTIR or acid-base titrationwt%
    Tensile stress at breakISO 527-2MPa
    Notched Charpy impactISO 179-1kJ/m²

    Filler Coupling Efficiency in Mineral-Filled Low-Density Polyethylene Compounds

    In halogen-free flame-retardant cable compounds filled with aluminum hydroxide or magnesium hydroxide at 55–65 wt%, OREVAC 18302N is used at 2–5 wt% of the total compound. The grafted maleic anhydride reacts with surface hydroxyl groups on the filler, reducing agglomeration and improving stress transfer from the polyethylene matrix to the mineral particles. On a corotating twin-screw line with side-fed filler and vacuum devolatilization, replacement of an unmodified LLDPE by this grade in the same formulation generally raises elongation at break and notched impact energy, as determined by ISO 527-2 and ISO 179-1. Flame-retarded cable sheathing is additionally evaluated under IEC 60332-1-2 for vertical flame spread and ISO 4589-2 for limiting oxygen index. Scanning electron micrographs of tensile fracture surfaces at 500× magnification often show less exposed filler pull-out with the maleated LLDPE than with a non-functional LLDPE control. If the filler surface is contaminated or heavily hydrated above 0.3 wt% moisture, the coupling reaction may be incomplete and batch-to-batch tensile variation can increase on production-scale compounding lines.

    In three-layer blown film structures with a polyamide 6 barrier layer and an LLDPE seal layer, OREVAC 18302N is processed as the middle tie layer. The melt temperature at the extruder is maintained at 220–240 °C, with a die gap between 1.8 mm and 2.2 mm and a blow-up ratio of 2.2:1 to 2.8:1. Interlayer adhesion is measured by T-peel testing under ISO 8510-1 or seal-strength methods under ASTM F88. The chemical reaction between maleic anhydride and polyamide terminal amine groups forms block copolymer in situ at the tie-layer interface; this interfacial copolymer is necessary for adhesion in retort and vacuum packaging. A tie-layer thickness below 3 µm can produce uneven interfacial coverage in the bubble, particularly when polyamide film layers are thin, leading to visual delamination and loss of oxygen barrier measured under ASTM D3985.

    Assessing Coextruded Tie-Layer Adhesion in Five-Layer EVOH Barrier Structures

    In symmetrical five-layer EVOH barrier structures, the use of OREVAC 18302N as the adhesive layer on both sides of the EVOH core provides adhesion to polyolefin skins. The maleated LLDPE is chosen because its lower melting point permits a broad heat-seal window with LLDPE skin layers and lower die pressure than a maleated HDPE tie resin. Layer distribution is usually set to 10–15% of total film thickness for the combined tie layers, with the EVOH layer at 5–10% to balance oxygen barrier and flex-crack resistance. Barrier properties are tested using ASTM D3985 for oxygen transmission rate and ASTM F1249 for water vapour transmission rate. When high-humidity converting conditions above 60% relative humidity occur without pre-drying, the tie layer can retain surface moisture that disrupts interfacial wetting, producing streaks in the coextruded film. The resulting defects are not eliminated by increasing die temperature alone; a separate purge with low-MFI LDPE is necessary before restarting the line.

    In three-layer external coating systems for steel pipe, OREVAC 18302N can serve as the tie layer between an epoxy primer and an LLDPE or high-density polyethylene topcoat. The grafted anhydride reacts with unreacted amine or hydroxyl groups in the epoxy, while the LLDPE backbone fuses with the polyolefin topcoat. Application is by side-wrapped or cross-head extrusion, with barrel temperatures between 200 °C and 230 °C. Adhesion of the three-layer system is typically evaluated through peel testing under ISO 21809-1:2018 or CSA Z245.21, with minimum peel values set by the project specification. The lower melting point of the LLDPE-g-MAH layer can reduce the risk of powder sag during side-wrap application compared with a HDPE-g-MAH tie layer, but published data for exact field application rates is limited. Ambient humidity at the pipe surface must be controlled below 4% moisture on the primer before tie-layer application to prevent interfacial blistering.

    When a Maleic Anhydride Grafted HDPE Would Impose a Low-Temperature Impact Penalty

    OREVAC 18302N is selected over a maleic anhydride grafted HDPE grade when end-use operations require flexibility, low-temperature impact resistance, or a lower sealing initiation temperature. The LLDPE backbone exhibits a lower flexural modulus than HDPE-based grafted resins under ISO 178, and notched Charpy tests under ISO 179-1 at −40 °C are more likely to retain ductile failure. Conversely, maleic anhydride grafted HDPE provides higher heat deflection temperature under ISO 75-2 and better creep resistance, which may be required for pipe-coating adhesion layers exposed to sustained elevated service temperatures. The melting point difference is roughly 10–15 °C between the LLDPE-based and HDPE-based tie resin classes. Replacing one with the other without a full line trial is not recommended because the viscosity, interfacial reaction rate, and bubble stability differ; published comparative data for all exact film constructions is limited, and full-scale trial runs on the target line are used to confirm stable bubble geometry and peel strength.

    Compared with PP-g-MAH, OREVAC 18302N co-crystallizes with polyethylene seal layers and does not embrittle the LLDPE sealant; PP-g-MAH has better heat resistance but creates a distinct interface with polyethylene that reduces seal integrity under ASTM F88 after thermal treatment. Another comparison is with EVA-based or ethylene-acrylate-based tie resins. The LLDPE-grafted maleic anhydride resin contains no acetate or acrylate comonomer, so it does not release acetic acid during extrusion at temperatures above 200 °C. EVA-based tie resins may offer stronger adhesion to aluminium foil and some polar substrates, but they have a lower continuous-use temperature limit and require more aggressive odour management in converting plants. OREVAC 18302N also differs from unmodified linear low density polyethylene by its ability to bond to polyamide, EVOH, and mineral surfaces; without the grafted anhydride, a standard LLDPE layer exhibits low T-peel adhesion under ISO 8510-1 and can delaminate during film slitting or bag-forming operations.

    Concentrate producers occasionally use OREVAC 18302N as a carrier in high-graft letdown blends, diluting it with unmodified LLDPE at ratios from 1:1 to 1:4 depending on the target graft level in the formulated compound. This dilution practice must be validated because the grafted anhydride can form hydrogen-bonded clusters that increase melt viscosity relative to a linear blend prediction. Capillary rheometry under ISO 11443 at 190 °C with a die of 1 mm diameter and 30 mm length is used to record apparent melt viscosity at apparent shear rates from 100 s⁻¹ to 1000 s⁻¹. Blends outside the specified dilution ratio can exhibit unstable melt pressure in blown film dies, especially when the letdown reduces the graft content below the level needed for interfacial coverage on EVOH or polyamide. On a modular corotating twin-screw line, a low-shear screw configuration is preferred for letdown blending to limit shear heating and gel formation.

    Comparative Differentiation Among Maleic Anhydride Grafted Polyolefin Tie Resins
    CharacteristicOREVAC 18302N (LLDPE-g-MAH)HDPE-g-MAHPP-g-MAHEVA-g-MAH
    Backbone flexibilityHighModerateLow-moderateHigh
    Typical melting or softening range120–126 °C130–135 °C160–165 °C70–90 °C
    Practical extrusion upper limit250 °C260 °C280 °C220 °C
    Primary adhesion targetsPA-6, PA-66, EVOH, mineral fillerPA, epoxy-coated steelPA, EVOH at elevated temperaturealuminium foil, polar films
    Low-temperature flexibilityGood below −30 °CModerateReduced below 0 °CGood

    Application-specific qualification is necessary because table values represent typical commercial class data, not lot-specific product specifications. The exact grade-specific behaviours should be confirmed using the certificate of analysis and full-scale equipment trials.

    Material compliance documentation should request Arkema's REACH registration confirmation under Regulation (EC) No 1907/2006. For electronic applications, a supplier declaration against Directive 2011/65/EU as amended by (EU) 2015/863 should be obtained from the producer. If a converter evaluates multilayer films with an olefin polymer layer, the relevant food-contact regulation may include 21 CFR 177.1520, provided all layer components and migration limits are cleared. These statements are not a substitute for lot-specific certification; converter responsibility remains with the final article.

    Storage in sealed 25 kg moisture-barrier bags at temperatures below 40 °C is specified to preserve anhydride functionality. Partially used containers should be resealed and protected from relative humidity above 60%; otherwise pre-drying is required before extrusion. The product should not be dry-blended with amine-based stabilizers or polyamide masterbatch prior to metering because the acid-base reaction can occur in the feed zone and generate localized high-melt-viscosity regions. In a production-scale 75 mm twin-screw line operating at 300 kg/h, the material is typically metered with a gravimetric feeder and processed with a flat temperature profile of 200–230 °C across the first two barrel sections.