| HS Code | 463415 |
| Polymer Type | Maleic Anhydride Modified Linear Low Density Polyethylene |
| Base Resin | Linear Low Density Polyethylene (LLDPE) |
| Functional Group | Maleic Anhydride |
| Form | Pellets |
| Color | Natural |
| Density | 0.91 g/cm³ |
| Melt Flow Index | 2.0 g/10 min (190°C/2.16 kg) |
| Melting Point | 120 °C |
| Vicat Softening Point | 90 °C |
| Maleic Anhydride Content | 0.9 wt% |
| Tensile Strength At Break | 18 MPa |
| Elongation At Break | 700 % |
| Flexural Modulus | 200 MPa |
| Hardness | Shore D 50 |
| Water Absorption | <0.1 % |
As an accredited Arkema Orevac® 18302 Maleic Anhydride modified LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Arkema Orevac® 18302 modified LLDPE pellets are supplied in 25 kg bags, palletized and stretch-wrapped for industrial use. |
| Container Loading (20′ FCL) | Arkema Orevac® 18302 pellets in 25 kg bags, palletized, approximately 20 MT per 20′ FCL, stretch-wrapped for secure sea transport. |
| Shipping | Arkema Orevac® 18302 Maleic Anhydride modified LLDPE is shipped as dry pellets in 25 kg polyethylene bags or 1000 kg bulk bags, palletized and shrink-wrapped. Transport as non-hazardous cargo in clean, dry vehicles. Keep sealed and away from moisture, heat, ignition sources, and contamination. |
| Storage | Store Orevac® 18302 in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed to prevent moisture ingress and contamination. Avoid prolonged storage above 30°C. Keep separate from oxidizing agents, amines, alcohols, and strong bases. Use original packaging, protect from physical damage, and observe good industrial hygiene. Store away from food and feed. |
| Shelf Life | Typically 24 months from manufacture when stored unopened in original packaging under cool, dry conditions, away from moisture and direct sunlight. |
Five-layer EVOH barrier film coextrusion relies on Orevac® 18302 as the discrete adhesive layer on both sides of the EVOH core to suppress delamination during film collapse, gusseting, and flexural cracking. The tie layers are metered at 8–14 µm per side in a total film thickness of 65–140 µm, placing the adhesive fraction between 12% and 20% of the structure by thickness; the exact ratio is determined by the target oxygen transmission rate and the stiffness of the surface LLDPE grades. Coextrusion is performed on a five-layer blown film line with die lip gaps of 1.6–2.4 mm, blow-up ratios from 1.8:1 to 2.5:1, and die-exit melt temperatures of 210–230 °C. Adhesion is measured on flat-seal specimens under ASTM F904-16, with process capability data from production lines commonly recording 12–30 N/15 mm depending on EVOH grade and seal dwell time, while film tensile properties are checked under ASTM D882-18. Compliance for food contact use in the European Union is designed around Regulation (EU) No 10/2011, with total migration tested per EN 1186-1:2002 and specific migration limits for maleic anhydride assessed under the applicable Annex II provisions; for U.S. structures, the tie layer is typically covered by 21 CFR 175.105 or the laminated structure provisions of 21 CFR 177.1390. Terminal finished formats include thermoformed meat and cheese modified-atmosphere trays, vacuum pouches, high-oxygen-barrier cereal liners, and stand-up pouch side gussets for liquid dairy products. Pre-drying of EVOH to below 0.25 wt% moisture is required before coextrusion, and melt temperatures above 240 °C initiate EVOH gel formation that appears as lens-shaped clear defects in the barrier layer.
On production lines equipped with five-layer dies, the most frequent adhesion-loss signature is not gross delamination but micro-voiding at the EVOH/tie interface after film ageing, detected when bond strength under ASTM F904-16 falls below 8 N/15 mm after 14 days at 38 °C and 90% relative humidity. This failure mode is addressed by maintaining EVOH pellet moisture below 0.25 wt% and purging the EVOH extruder with a polyolefin transition material for at least 10 min during shutdown. The tie resin extruder should not be operated above 240 °C because maleic anhydride graft degradation increases head pressure and produces a burnt odour at the die lips. Batch-to-batch variation in tie-layer thickness across the web is controlled by gravimetric hopper loaders and automatic die-bolt profile systems, with thickness recorded by a non-contact capacitance gauge and held within ±1.5 µm of target on the tie layers.
At extrusion lamination line speeds above 150 m/min, Orevac® 18302 is extruded between corona-treated aluminium foil and a polyolefin sealant web at a coating weight of 14–22 g/m², equivalent to a film thickness of roughly 15–24 µm under the extruder die. The line uses a single-screw extruder with an L/D ratio of 30:1 and a barrier screw, a coat-hanger die with internal deckles, and an air gap of 150–250 mm; die-exit melt temperature is held at 270–290 °C to generate the oxidative carbonyl species required for adhesion to aluminium foil. Lower melt temperatures below 260 °C produce inconsistent peel adhesion below 4 N/15 mm on unprimed foil, a failure mode observed as discontinuous transfer of the tie layer to the metal surface during high-speed slitting. The structure is tested under ASTM F904-16 for bond strength and under ASTM D882-18 for laminate tensile properties. Food-contact compliance is engineered under Regulation (EU) No 10/2011 and 21 CFR 177.1390 or 21 CFR 175.105 for the adhesive function. Terminal finished products include retort pouches processed at 121 °C for 30 min, stand-up pouches with aluminium foil barrier, pharmaceutical lidding foils, and high-barrier sachets for liquid concentrates.
When the same foil lamination line switches from a conventional LDPE coating grade to Orevac® 18302, the first production-shift adjustment is normally a 10–15 °C reduction in die temperature to prevent smoke evolution while maintaining adhesion. Edge-bead formation at the internal deckle increases if the melt curtain is not maintained within the 150–250 mm air gap; the resulting edge trim can reach 12 mm per side and must be kept out of the regrind stream if foil has already been laminated. Adhesion failures in retort pouches often present after steam sterilization when the aluminium foil picks off from the sealant web with a fibrous surface, indicating that the tie layer was applied below its oxidative activation window. For low-temperature foil lamination below 260 °C, published data for this specific product configuration is limited, and a primer or in-line corona treatment of the foil at a wetting tension above 42 mN/m is normally required.
Three-layer polyethylene pipe coating lines apply an epoxy primer, Orevac® 18302, and a high-density polyethylene topcoat onto steel pipe preheated to 180–220 °C. The adhesive layer is specified at 200–350 µm, between a fusion-bonded epoxy layer of 80–120 µm and a topcoat of 2.5–3.5 mm, depending on pipe diameter and service temperature. Steel surface preparation is blast cleaning to Sa 2½ under ISO 8501-1:2007, with an anchor profile of 50–100 µm. The adhesive is extruded through a side-wrap cross-head die with an internal spiral mandrel, using barrel temperatures from 190 °C to 230 °C and a screw speed selected to deliver a melt pressure below 250 bar; the FBE flash-off and gel time is set between 15 s and 25 s so the adhesive exits the die at the point where the primer has entered the rubbery cure plateau. If steel preheat drops below 180 °C, the FBE remains undercured and peel failure occurs within the epoxy layer, while preheat above 230 °C can cause the maleic anhydride graft to discolour and increase back pressure through micro-crosslinking. Compliance is governed by ISO 21809-1:2018 and DIN 30670:2012, with cathodic disbondment testing under the relevant annex, peel adhesion testing at 23 °C often specified at or above 35 N/cm in project documents, and holiday detection performed at 25 kV depending on coating thickness. Terminal finished products are buried and submerged transmission pipelines for oil, gas, water, and firewater service, where the tie resin’s function is to maintain adhesion between the non-polar polyethylene topcoat and the polar epoxy primer under soil stress and wet cathodic protection conditions.
On a side-extrusion line producing 508 mm diameter pipe at 1.2 m/min, the adhesive layer residence time between die exit and topcoat contact is typically less than 2 s; longer residence times allow the steel temperature to cool the adhesive below 190 °C before topcoat compression, producing a weak boundary layer. The overlap region where the extruded sheet wraps around the pipe creates a local thickness peak of +40%, and this ridge is a known site for holiday detection signals above 25 kV. Operators control this by adjusting the side-wrap angle and die gap, not by raising adhesive melt temperature, because exceedance of 230 °C increases the concentration of free maleic anhydride at the die exit and causes die-lip yellowing. Cathodic disbondment testing under ISO 21809-1:2018 after 30 days at 23 °C and −1.5 V relative to a copper/copper-sulfate reference electrode is used to validate that the tie layer does not lose adhesion at the FBE interface.
Where sterile barrier systems replace solvent-based adhesive lamination, a three-layer cast coextrusion of polyamide, Orevac® 18302, and a linear low-density polyethylene sealant web is used for film widths up to 1,600 mm. The tie layer is set at 10–18 µm within a total thickness of 60–120 µm, balancing bond strength against sealant puncture resistance. Cast film equipment includes extruder melt temperatures of 230–250 °C, a feedblock with layer encapsulation, and a chill roll held at 18–25 °C to limit post-crystallisation haze; thickness variation is maintained within ±2%. Seal strength is evaluated under ASTM F88/F88M-21, and the formed pouch is validated for sterile barrier performance under ISO 11607-1:2019 with package testing according to EN 868-5:2019; biological evaluation of the final packaging material follows ISO 10993-5:2009 where the device manufacturer requires cytotoxicity data. Terminal finished products include sterile barrier pouches, header bags, and forming webs for ethylene oxide, steam, and gamma-sterilised medical devices. The maleic anhydride functional layer must be shielded from excessive humidity before extrusion, and converters should not rely on the tie resin alone to compensate for excessive polyamide moisture above 0.15 wt%, which produces gel flecks in the barrier ply.
For gamma-sterilised medical pouches, the converter qualification usually includes exposure to 25–50 kGy followed by seal-strength testing per ASTM F88/F88M-21; a loss of more than 20% relative to unirradiated controls indicates that the polyamide grade or tie-layer thickness must be adjusted. The maleic anhydride layer should not be combined with amine-containing printing primers or solventless laminating inks on the same surface, because the acid-amine interaction can cause a visible yellow tint and a measurable increase in seal initiation temperature. On cast-film lines, plate-out on the chill roll can appear when the polyamide and tie resins are processed above 250 °C; this is controlled by maintaining the feedblock temperature no higher than 250 °C and cleaning the roll with a polyolefin purge between product runs.
Halogen-free flame retardant compounds based on LLDPE, high-density polyethylene, and 60–65 wt% alumina trihydrate or magnesium dihydrate use Orevac® 18302 at 2–5 wt% of the total compound to react with filler surface hydroxyl groups and reduce melt fracture at high filler loading. Compounding is executed on a co-rotating intermeshing twin-screw extruder with an L/D ratio of 44:1–52:1, screw speeds of 400–700 rpm, and a barrel profile of 150–190 °C; pelletising is performed on an underwater die-face cutter to handle the high melt viscosity. Melt flow rate is determined according to ISO 1133-1:2022, tensile properties under ISO 527-2:2012, and limiting oxygen index under ISO 4589-2:2017. Finished cables are classified for construction products under EN 50575:2014+A1:2016, with flame spread tested per IEC 60332-1-2:2015 and halogen acid gas release per IEC 60754-1:2011. Terminal product types include sheathing for building wire, control cable, renewable energy cable, and data-communication riser cable where low-smoke and halogen-free performance is mandatory. Process limitations include accelerated screw and barrel wear from ATH at the feed zone, which requires hardened screw elements, and the avoidance of amine-based hindered amine light stabilisers or melamine-based flame retardants that can react with the maleic anhydride group and cause a torque rise above 10% during steady-state extrusion.
Compounding at filler loadings of 60–65 wt% shifts the apparent melt viscosity enough that the twin-screw extruder may require side feeding of ATH downstream of the main feed throat to limit torque peaks. The maleated LLDPE is metered into the main feed throat with the base resin at 2–5 wt%; feeding it downstream can reduce early shear heating but may leave unreacted filler surfaces and cause die-face pellet agglomeration. Under-utilisation of the coupling agent below 2 wt% lowers elongation at break below typical project thresholds under ISO 527-2:2012, while loadings above 5 wt% can shift the limiting oxygen index downward under ISO 4589-2:2017 because the polyolefin fraction increases. The finished cable jacket is often tested for thermal ageing at 100 °C for 7 days, and the compound should be designed with a stabiliser package that does not contain amine-functional antioxidants that react with the maleic anhydride graft.
| Downstream application | Compliance standards and test methods | Assessed property |
|---|---|---|
| Five-layer EVOH barrier film | Regulation (EU) No 10/2011, EN 1186-1:2002, 21 CFR 175.105, ASTM F904-16, ASTM D882-18 | Total migration, tie-layer adhesion, laminate tensile |
| Aluminium foil extrusion lamination | Regulation (EU) No 10/2011, 21 CFR 177.1390, ASTM F904-16 | Bond strength after lamination and retort |
| Three-layer PE pipe coating | ISO 21809-1:2018, DIN 30670:2012, ISO 8501-1:2007, NACE SP0169 | Peel adhesion, cathodic disbondment, surface preparation |
| Polyamide/PE medical packaging | ISO 11607-1:2019, EN 868-5:2019, ISO 10993-5:2009, ASTM F88/F88M-21 | Sterile barrier integrity, seal strength, cytotoxicity |
| Halogen-free cable sheathing | EN 50575:2014+A1:2016, IEC 60332-1-2:2015, IEC 60754-1:2011, ISO 4589-2:2017 | Flame spread, acid gas release, limiting oxygen index |
| Wood-plastic composite profiles | ASTM D7031-11, EN 15534-1:2014, ISO 178:2019, EN 317:1993 | Flexural properties, water absorption |
In wood-plastic composite profiles, Orevac® 18302 is added at 2–6 wt% of the compound to improve interfacial adhesion between a polyolefin matrix and dried wood flour. Production uses a counter-rotating conical or parallel twin-screw extruder with melt temperatures restricted to 160–185 °C to limit wood fibre discolouration and furfural emissions, followed by profile calibration in a vacuum water tank. The wood flour is dried to below 1.5 wt% moisture before feeding; higher moisture contents produce steam voids at the profile surface and reduce the effectiveness of the maleic anhydride coupling reaction. Compliance and test methods include ASTM D7031-11 and EN 15534-1:2014, with flexural properties tested under ISO 178:2019 and water absorption under EN 317:1993. Terminal products include exterior decking, cladding, railing profiles, and fence slats where the acid-modified polyolefin improves dimensional stability and reduces water uptake at exposed edges. Published data for Orevac® 18302 in wood-plastic composite formulations is limited compared with coextrusion tie-layer applications; converter-run DOE trials should confirm flexural modulus and water uptake for the specific wood species and particle size distribution before full production.
Competitive Arkema Orevac® 18302 Maleic Anhydride modified LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Arkema Orevac® 18302 is a maleic anhydride grafted linear low-density polyethylene (LLDPE-g-MAH) supplied as pelletized tie resin for coextruded multilayer film, sheet, and extrusion coating structures. The maleic anhydride functionality is present as pendant graft sites on the polyethylene backbone, not as a uniform random comonomer insertion. That molecular architecture leaves the base polymer with a published typical density of 0.912 g/cm³ and a melt flow rate of 1.0 g/10 min at 190 °C / 2.16 kg. The product is primarily used to bond polyolefin skins to ethylene-vinyl alcohol copolymer, polyamide, and other polar barrier layers in five- and seven-layer packaging systems. The LLDPE backbone controls bulk toughness, tear behavior, and melt viscosity matching with film-grade polyethylene skins, while the grafted anhydride provides interfacial reactivity with polar substrates. The product is not designed for use as a sealant skin or as a direct replacement for random polar copolymers in all barrier structures.
Maleic anhydride grafting introduces reactive anhydride groups without converting the backbone into a highly polar random copolymer. The graft level is generally not published as a release specification; it is balanced to provide reactive adhesion while limiting moisture uptake and excessive melt-phase odor. The material remains fundamentally an LLDPE in its crystalline melting range, with a melting endotherm near 126 °C under ISO 11357-3. This is a key operational difference from ethylene–vinyl acetate–maleic anhydride or acid-modified ethylene copolymers, where polar comonomer placement alters seal initiation, stiffness, and moisture barrier more broadly.
Table 1 consolidates manufacturer-published typical values for Orevac® 18302. The values are lot-average reference points, not contractual release limits, and should not be used as a substitute for a certificate of analysis.
| Property | Unit | Published typical value | Test procedure |
|---|---|---|---|
| Density at 23 °C | g/cm³ | 0.912 | ISO 1183-1 |
| Melt flow rate, 190 °C / 2.16 kg | g/10 min | 1.0 | ISO 1133-1 |
| Melting temperature, DSC second heating | °C | 126 | ISO 11357-3 |
| Tensile stress at yield | MPa | 9.0 | ISO 527-2 |
| Elongation at break | % | 800 | ISO 527-2 |
| Hardness | Shore D | 54 | ISO 868 |
Batch-to-batch differences, thermal history, and specimen preparation can shift tensile and hardness values. For film converters, the more useful control is therefore not anhydride content alone but peel adhesion on the target barrier structure. ASTM F904-16 adapted for T-peel geometry is a common starting point, with jaw speed of 50 mm/min often used for flexible packaging laminates. When testing coextruded film rather than laminate stock, the failure mode must be reported because peel force alone cannot distinguish weak interfacial bonding from cohesive failure in the tie layer.
Relative to EVA-based maleic anhydride tie resins, Orevac® 18302 contains no vinyl acetate. The absence of acetate removes a source of acetic acid during prolonged high-temperature extrusion and elevates the seal initiation of the tie resin compared with many EVA-based grades. EVA-g-MAH products can offer softer feel and lower-temperature sealability, but they often contribute to die-lip buildup and require more intensive purge procedures. The LLDPE backbone of Orevac® 18302 provides an elongation at break near 800 % under ISO 527-2 and improved tear propagation resistance, which is relevant for downgauged packaging films subjected to tensile impact and drop abuse.
Relative to maleic anhydride grafted HDPE, Orevac® 18302 has a density of 0.912 g/cm³ versus typical HDPE-based grades above 0.94 g/cm³. The lower crystallinity reduces modulus and Vicat softening temperature but improves compatibility with LLDPE skins. HDPE-g-MAH tie layers can provide higher temperature resistance and chemical resistance, but they may create interfacial stress mismatch in asymmetric polyethylene/barrier structures and can increase curl. In five-layer blown film with LLDPE skins, Orevac® 18302 generally matches film-grade LLDPE melt viscosity better than HDPE-based anhydride grades at 230 °C, reducing layer disturbance in feedblock and die distribution.
Orevac® 18302 is processed in the polyolefin temperature range. Barrel profiles commonly begin at 160 °C in the feed zone and rise to 210–230 °C in the metering zone; adapter and die zones are usually held at 225–240 °C. Because the LLDPE backbone melts near 126 °C, rear barrel temperatures below 150 °C can cause pellet slippage in grooved-feed extruders, while melt temperatures above 250 °C increase the release of free maleic anhydride vapor and may reduce adhesion after excessive heat history. General-purpose polyolefin screws with 24:1 to 30:1 L/D and compression ratios of 2.8:1 to 3.5:1 are usually adequate. High-shear barrier screws with aggressive Maddock or similar mixer sections can generate excessive melt temperature; if such screws are used, screw speed should be trimmed to keep melt temperature below 245 °C at the die.
Pre-drying is not required under normal indoor storage. When sacks have been exposed to high humidity or condensation, drying at 70 °C for 4 h removes surface moisture that can cause surging, bubbles, or optical defects. The product is not hygroscopic in the manner of polyamide or EVOH, but surface water on pellets is a direct cause of feed instability. Local exhaust at the die and feed throat should be provided when running long campaigns at the upper end of the temperature range, because maleic anhydride vapor can condense on cold metal surfaces and promote corrosion over time.
Reverse temperature profiles are not recommended for grooved-feed extruders, because early melting in the grooves can reduce solids conveying. Instead, the first zone should be maintained between 160 °C and 180 °C to soften pellets before compression. For shutdown and start-up, polyethylene purge is preferred. Halogenated purge compounds should be avoided because residual halogen can react with anhydride groups and leave surface defects at the die. On cast film and blown film lines, tie-layer pressure variation should be minimized; a fluctuation of more than ±2 bar at stable throughput can produce visible interfacial bands. If tie-layer thickness variation exceeds ±1 µm in a 15 µm layer, feed-zone temperature or screw cooling should be adjusted before increasing die temperature.
EVOH grades with ethylene content below 32 mol% provide high oxygen barrier but require a narrow processing window and usually process between 205 °C and 225 °C. When Orevac® 18302 is coextruded against such EVOH, the tie layer should not leave the die above 230 °C. EVOH degradation can create cross-linked gel particles that reduce interface clarity and weaken peel strength. A die temperature of 220 °C ± 5 °C is a practical target for five-layer blown film. Lower ethylene content EVOH grades also exhibit higher melt viscosity, so the tie layer may require an increase from 10 µm to 15–20 µm to maintain continuous interfacial coverage under shear. Published data for this specific configuration is limited; pilot-line trials should define the minimum tie thickness for the target EVOH grade and package size.
With polyamide barrier layers, the limiting temperature is typically the polyamide, not Orevac® 18302. Aliphatic polyamide processed at 240–260 °C can coexist with this grafted LLDPE, but residence time in transfer lines and feedblocks should be minimized. At prolonged melt residence above 245 °C, the adhesive contribution of the anhydride can decay before the interface is formed, especially if the line is stopped and restarted. After a stoppage, the tie-layer extruder should be purged with fresh LLDPE until melt temperature and pressure return to target before restarting barrier coextrusion.
Five-layer and seven-layer barrier films for processed meat, cheese, and snack packaging are typical application areas. In symmetrical polyethylene/tie/EVOH/tie/polyethylene films, the two tie layers together commonly represent 8–14 wt% of total film mass. The material is also used in heavy-duty sacks and collation shrink structures where the tie layer is buried and must tolerate machine-direction orientation without delamination. Orevac® 18302 should not be formulated with amine-based antifog, amine-based slip concentrates, or unneutralized acid scavengers without adhesion trials, because amine species can quench anhydride groups and reduce peel values. In food-contact structures, a regulatory compliance statement must be obtained from the manufacturer for the specific composition, food simulant, and migration conditions; Orevac® 18302 is not a universal food-contact polymer for all global jurisdictions.
Converters replacing an acid-modified EAA or EMAA tie resin with Orevac® 18302 should validate that downstream corona treatment, lamination, and thermal tunnel settings remain compatible with the lower surface energy of the LLDPE backbone. Acid-modified polyethylenes often bond more readily to aluminum foil and can seal at lower temperatures, while Orevac® 18302 contributes higher tear resistance and reduced moisture sensitivity at the die. Published data for direct substitution on high-speed cast film and extrusion coating lines is limited; plant-scale adhesion tests with the actual barrier layer and final lamination structure are required before commercial release.