| HS Code | 279168 |
| Product Name | Amoco PEN Raw Material NDC Monomer |
| Chemical Name | 2,6-Naphthalenedicarboxylic acid |
| Synonyms | 2,6-NDCA; NDC; naphthalene-2,6-dicarboxylic acid |
| Cas Number | 1141-38-4 |
| Molecular Formula | C12H8O4 |
| Molecular Weight | 216.19 g/mol |
| Product Grade | PEN raw material monomer grade |
| Appearance | White to off-white crystalline powder |
| Physical State | Solid |
| Color | White to off-white |
| Odor | Odorless |
| Melting Point | >300 °C (decomposes) |
| Boiling Point | 437.3 °C at 760 mmHg (predicted) |
| Density | 1.5 g/cm³ (estimated) |
| Flash Point | 232.4 °C (predicted) |
| Water Solubility | Insoluble in water |
| Solubility | Soluble in alkaline aqueous solutions |
| Purity | ≥99.0% (typical) |
| Acid Value | ≈519 mg KOH/g |
| Moisture Content | ≤0.5% (typical) |
| Bulk Density | 0.6–0.9 g/cm³ (typical) |
| Particle Size | Typically 100 mesh pass |
| Storage Conditions | Store dry and sealed at ambient temperature |
As an accredited Amoco PEN Raw Material NDC Monomer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Amoco PEN Raw Material NDC Monomer is packaged in 25 kg net moisture-resistant bags, palletized for safe industrial storage and handling. |
| Container Loading (20′ FCL) | Loading a 20-foot FCL container with securely packed and labeled Amoco PEN Raw Material NDC Monomer for safe chemical shipment. |
| Shipping | Amoco PEN Raw Material NDC Monomer is shipped as a non-hazardous solid and is not classified as dangerous goods for transport. Use secure, moisture-resistant packaging and labeled containers. Store away from heat and incompatible materials. Follow the SDS, carrier requirements, and applicable national/international shipping regulations. |
| Storage | Store Amoco PEN Raw Material NDC Monomer in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and incompatible oxidizers. Keep containers tightly closed to prevent moisture ingress and contamination. Use appropriate secondary containment, label clearly, and follow local SDS and regulations. Avoid dust generation and keep storage segregated from acids, bases, and flammables. |
| Shelf Life | Amoco PEN Raw Material NDC Monomer typically has a 12-month shelf life when stored in tightly closed original containers in a cool, dry, well-ventilated area. |
Competitive Amoco PEN Raw Material NDC Monomer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Amoco PEN Raw Material NDC Monomer is the dimethyl ester of 2,6-naphthalenedicarboxylic acid, CAS 840-65-3, supplied as a crystalline solid with molecular formula C14H12O4 and molecular weight 244.24 g/mol. The trade designation refers to the naphthalene-dicarboxylate monomer used in melt-phase production of polyethylene naphthalate and high-NDC-content copolyesters; it is not a formulated resin, a masterbatch, or a finished barrier additive. Because the monomer is a dimethyl ester, its polymerization route proceeds by transesterification with ethylene glycol and releases methanol rather than the water released by purified terephthalic acid in direct esterification. The structural distinction between the fused bicyclic naphthalene ring and the monocyclic benzene ring in dimethyl terephthalate is the central variable controlling final polymer thermal, mechanical, and transport properties. Representative procurement specifications reported in supplier literature include ester content at or above 99.5 wt%, methanol below 0.05 wt%, acid number below 0.5 mg KOH/g by ASTM D664, moisture below 0.1 wt% by ASTM E203, ash below 0.01 wt%, and a melting point between 187 °C and 190 °C by ASTM D3418. The color of a methanol solution is typically controlled at or below 20 APHA by ASTM D1209. Because the monomer is not a food-contact article, compliance for final packages must be demonstrated on the finished PEN or copolymer under U.S. FDA 21 CFR 177.1632 or Commission Regulation (EU) No 10/2011, with migration testing appropriate to the intended food type and temperature.
| Parameter | Test method | Typical procurement limit |
|---|---|---|
| Chemical name | — | Dimethyl naphthalene-2,6-dicarboxylate |
| CAS registry number | — | 840-65-3 |
| Ester content | Gas chromatography | ≥ 99.5 wt% |
| Methanol content | Headspace gas chromatography | ≤ 0.05 wt% |
| Acid number | ASTM D664 | ≤ 0.5 mg KOH/g |
| Moisture | ASTM E203 | ≤ 0.1 wt% |
| Ash | ASTM D482 | ≤ 0.01 wt% |
| Melting point | ASTM D3418 | 187 °C–190 °C |
| Color in methanol solution | ASTM D1209 | ≤ 20 APHA |
In continuous polyester polymerization, NDC monomer is slurried or melted with ethylene glycol and fed to a transesterification reactor maintained at 160 °C–220 °C under atmospheric or mild vacuum. Manganese acetate or zinc acetate is typically used as the transesterification catalyst at metal concentrations ranging from 20 ppm to 200 ppm relative to the dimethyl ester. Methanol generated in this stage is removed through a distillation column and condensed in a refrigerated recovery system; the vent stream must be designed for methanol’s lower flammability limit, reported at 6.0 vol% in air. After transesterification, the bis(2-hydroxyethyl) naphthalate intermediate is transferred to a polycondensation finisher operating at 280 °C–300 °C and absolute pressure below 1 mbar. Antimony trioxide or titanium alkoxide catalysts promote chain extension, while phosphorus-based stabilizers are added to control color and oxidation. Because the naphthalene ring increases melt viscosity at a given intrinsic viscosity relative to PET, the finisher requires high-torque agitation and a short-residence surface-renewal design such as a wiped-film or cage-type reactor. Published data for this specific Amoco monomer configuration in a single reactor train is limited; producers generally derate throughput by 10–20% relative to PET when running high-NDC melts to maintain acceptable melt temperature and residence-time distribution.
Unlike DMT-based PET production, the presence of NDC in the melt increases the lowest feasible crystallization temperature. Preform injection molding of PEN homopolymer and high-NDC copolyesters commonly uses barrel and hot-runner temperatures between 290 °C and 320 °C, mold temperatures of 120 °C–160 °C, and longer cooling times than PET at the same wall thickness. A reciprocating screw with a low compression ratio, typically 2.2:1–2.8:1, and a free-flow check ring reduces shear heating. Published production-scale data for specific injection molding clamp force settings is limited because cavity pressure is affected by gate size, preform weight, and intrinsic viscosity; however, processors report that clamp force per square centimeter of projected area is higher than for PET at the same melt temperature.
The naphthalene ring has a larger planar aromatic system than the benzene ring, which reduces segmental mobility and free-volume available for gas transport. In oriented films, oxygen permeability coefficient per ASTM D3985 is reported near 0.9–1.5 cm³·mm/(m²·day·atm) for PEN homopolymer at 23 °C and 0% RH, compared with 3.0–6.0 cm³·mm/(m²·day·atm) for PET. Carbon dioxide transmission rate by ASTM F2476 is roughly 4–5 times lower for PEN than for PET, which is the primary reason for carbonated soft drink preforms and beer bottles containing high naphthalate levels. Water vapor transmission rate by ASTM F1249 is similarly reduced to approximately one-third of the PET value at 38 °C and 90% RH. The polymer glass transition temperature rises to 118 °C–122 °C by ASTM D3418, allowing hot-fill exposure at 85 °C–95 °C without the paneling that occurs with standard PET at equivalent blow-molding orientation. Tensile modulus of PEN film reaches 5.5–6.0 GPa under ASTM D882, compared with 2.8–4.1 GPa for PET film. These differences are not always linear with NDC content in PET/PEN copolymers; published data for specific copolyester grades show nonlinear barrier response with naphthalate mole fraction, and converters should verify final formulations against the intended package specification.
| Property | Test method | PET | PEN |
|---|---|---|---|
| Glass transition temperature | ASTM D3418 | 70–80 °C | 118–122 °C |
| Melting point | ASTM D3418 | 245–265 °C | 265–270 °C |
| Tensile modulus, oriented film | ASTM D882 | 2.8–4.1 GPa | 5.5–6.0 GPa |
| Oxygen permeability coefficient, 23 °C, 0% RH | ASTM D3985 | 3.0–6.0 cm³·mm/(m²·day·atm) | 0.9–1.5 cm³·mm/(m²·day·atm) |
| Carbon dioxide transmission rate, normalized to PET | ASTM F2476 | 1.0 | 0.2–0.3 |
In PET/PEN copolymer formulations, NDC monomer is added to the esterification or transesterification feed in molar proportions from 1 mol% to 15 mol% for barrier-enhanced PET bottles. At low levels the material reduces oxygen and carbon dioxide transmission without forcing the melt processing temperature to PEN homopolymer levels. Intrinsic viscosity measured by ASTM D4603 is typically maintained between 0.60 dL/g and 0.80 dL/g for bottle grades, with solid-state polymerization used after melt pelletizing to raise molecular weight. The presence of naphthalene rings slows solid-state polymerization relative to PET; the polycondensation rate at 220 °C under vacuum is reported to be lower, so reactors may require extended residence time or higher temperature. This is a process conflict at high NDC content: the same ring that raises barrier also reduces chain-end mobility and solid-state advancement rate. Published data for this specific monomer in a given solid-state reactor is limited, so pilot-scale trials are used to define residence time.
Comparison with dimethyl terephthalate is explicit. DMT has a molecular weight of 194.19 g/mol and a melting point of 140 °C–141 °C, so it can be stored and melted at lower temperatures than NDC. Purified terephthalic acid has a much higher melting point and is fed as a solid to direct esterification, whereas NDC monomer is fed as a dimethyl ester to transesterification. This difference changes the overhead system: methanol rather than water is recovered. Methanol recovery requires flame-proof condensers and a sealed receiver, while water removal in PTA-based plants uses a distillation column that manages glycol dehydration. In addition, the naphthalene ring absorbs UV radiation more strongly than the benzene ring; oriented PEN film exhibits an absorbance edge near 380 nm, which can reduce photodegradation in packaged light-sensitive products but also influences reheat behavior in blow molding. The higher melting point and lower volume availability of NDC monomer relative to DMT and PTA affect supply logistics and feed-system design.
Incoming quality-control failures in polyester plants are most frequently associated with moisture excursions, elevated acid number, and particle size changes. When ambient relative humidity exceeds 60%, improperly closed bulk bags or silo vent dryers can admit enough water to hydrolyze the dimethyl ester to free 2,6-naphthalenedicarboxylic acid. The resulting acid number drift above 0.5 mg KOH/g by ASTM D664 alters transesterification stoichiometry and can increase filter pressure in a continuous prepolymer line. Karl Fischer titration per ASTM E203 should be performed on each incoming lot, not only on the certificate of analysis. Particle size distribution is normally specified between the supplier and converter; a laser diffraction analyzer is used to monitor mass-median diameter. Published data for the specific Amoco/BP grade’s particle size distribution is limited, but the material is commonly described as a crystalline powder or flake that may require delumping before transfer. Color in methanol solution above 20 APHA can indicate oxidative degradation or contamination and should be tracked against the supplier’s certificate of analysis using ASTM D1209. Residual methanol above 0.05 wt% can generate volatile organic compounds in the esterification overhead and may require a larger condenser capacity.
Purity is commonly determined by gas chromatography with flame-ionization detection. The critical chromatographic separation is between dimethyl 2,6-naphthalenedicarboxylate and other naphthalenedicarboxylate isomers; the monomer grade must not be confused with the 2,7- or 1,5-isomers, which disrupt chain symmetry and crystallinity in the final polyester. The ester content specification of ≥99.5 wt% implies that isomer and monoester impurities are controlled to low levels, but users should confirm the isomer profile on the certificate of analysis. Acid number by ASTM D664 and moisture by ASTM E203 are more sensitive to storage and transfer than to initial production variability. Melt point by ASTM D3418 is used as a screening test; a depressed melting point or broad endotherm may indicate contamination with monomethyl ester or other naphthalene isomers. Trace metal analysis by inductively coupled plasma optical emission spectrometry can detect catalyst residues relevant to film-grade polymer where hydrolytic stability is critical. These methods do not replace performance testing in the final polymer but reduce the probability of lot-to-lot variation reaching the polymerization vessel.
Melt processing of PEN and high-NDC copolyesters requires tighter residence-time control than PET because the naphthalene ring increases melt viscosity and the finisher temperature is closer to decomposition. Thermogravimetric analysis shows measurable mass loss above 300 °C under nitrogen, and processing above 310 °C narrows the acceptable residence-time window. In injection molding, barrel residence time above 310 °C should be kept below 2 min to avoid color shift and intrinsic viscosity loss. This operational boundary is based on standard polyester thermal degradation behavior; published data for this specific monomer formulation is limited. Processors report that screw speed and back pressure must be reduced relative to PET to limit shear heating, and hot-runner channels should be polished to avoid dead spots. These limits arise from the combination of high melt temperature, residence-time distribution, and the hydrolysis and thermo-oxidative reactions common to all polyester melts.
Storage vessels and transfer lines for NDC monomer should be purged with dry nitrogen when the product is held for more than 48 h in an environment above 60% RH. The dust is an organic particulate and can form an explosible cloud if dispersed in air at sufficient concentration; local exhaust ventilation, bonding, and grounding are required during bag emptying and screening. Avoid contact with strong oxidizers, strong bases, and water sprays because hydrolysis of the ester groups can raise the free acid content. The monomer should not be mixed with amine-based additives or alkaline catalysts outside the polymerization recipe, as acid-base reactions can degrade the ester before transesterification. Prolonged storage above 40 °C may cause caking or volatilization of residual methanol. Published toxicological data for dimethyl 2,6-naphthalenedicarboxylate itself is limited; hazard communication should rely on the current safety data sheet for the supplier’s grade and should not be extrapolated from the polymer. Occupational exposure limits for dust apply, and respiratory protection is required where total dust exceeds applicable threshold limit values.