Tert Butyl Peroxybenzoate Tbpb

tert-Butyl Peroxybenzoate (TBPB)

    VTB
    Specifications
    HS Code 713216
    Productname tert-Butyl Peroxybenzoate
    Abbreviation TBPB
    Casnumber 614-45-9
    Einecsnumber 210-382-2
    Molecularformula C11H14O3
    Molecularweight 194.23 g/mol
    Appearance Colorless to light yellow liquid
    Density 1.04 g/cm3 at 20 °C
    Meltingpoint 8 °C
    Boilingpoint 75-76 °C at 0.2 mmHg
    Flashpoint 93 °C
    Refractiveindex 1.4990 at 20 °C
    Activeoxygen 8.24%
    Assay ≥98%
    Decompositiontemperature 60 °C (SADT)
    Solubility Insoluble in water; soluble in organic solvents
    Viscosity 7.4 mPa·s at 20 °C
    Halflife 10 h at 104 °C
    Unnumber 3103
    Hazardclass 5.2 (Organic peroxide)

    As an accredited tert-Butyl Peroxybenzoate (TBPB) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TBPB is packaged in 25 kg net UN-approved polyethylene drums with vented closures, labeled as organic peroxide, stored cool and upright.
    Container Loading (20′ FCL) Load tert-Butyl Peroxybenzoate in a clean, dry 20′ FCL, palletized and secured, away from heat/ignition, per IMDG organic peroxide rules.
    Shipping TBPB is shipped as UN 3103, Organic Peroxide Type C, Liquid (tert-Butyl Peroxybenzoate), Class 5.2, Packing Group II. Use approved organic peroxide packaging. Store cool, dry, ventilated, away from heat, sunlight, acids, bases, and reducing agents. Temperature control not normally required; follow SADT limits.
    Storage Store in a cool, dry, ventilated, fire-resistant area, ideally refrigerated or below 30°C, away from sunlight and ignition sources. Keep in original, labeled, compatible, vented containers. Separate from acids, bases, reducing agents, accelerators, metals, and combustibles. Use grounded equipment; avoid friction, impact, and contamination. Monitor temperature; follow supplier SDS. Do not return unused material to container if contaminated.
    Shelf Life TBPB has a limited shelf life: store below 30°C, protect from heat, light, and contaminants; typically three to six months.
    Application of tert-Butyl Peroxybenzoate (TBPB)

    In compression moulding of glass-reinforced unsaturated polyester compounds, tert-butyl peroxybenzoate acts as the high-temperature initiator because its half-life in dilute solution is approximately 10 h at 105°C, 1 h at 125°C, and 1 min at 166°C. This decomposition profile aligns the practical cure window with press temperatures between 135°C and 160°C, whereas ambient-cure systems based on methyl ethyl ketone peroxide and cobalt accelerators gel at room temperature but can leave higher residual styrene in thick sections. Typical dosage in SMC and BMC resin paste is 1.0–1.5 wt% based on resin, corresponding to 0.8–1.2 phr on resin solids. The peroxide is dispersed in the unsaturated polyester/styrene phase of a low-profile formulation containing 25–30 wt% glass fibre, 40–50 wt% calcium carbonate filler, 3–5 wt% thermoplastic low-profile additive, and magnesium oxide thickener at 1.5–2.5 wt%. After compounding on an SMC machine with doctor blades set to 1.5–4.0 mm film thickness, the sheet is matured at 25–35°C for 48–120 h until thickening reaches 30–50 million mPa·s. TBPB remains essentially dormant during maturation, but storage above 40°C can initiate slow radical generation and reduce the available active oxygen before moulding. Moisture in filler above 0.2% alters magnesium oxide thickening and can shift the maturation curve by ±20%, producing variable mould contact and incomplete filling on the press.

    During compression moulding, charge coverage of the tool is held at 40–70% to allow flow and fibre orientation before gelation. Hydraulic press closing speed is normally set to 5–10 mm/s until the gap reaches 2–4 mm, followed by 0.5–1.0 mm/s final closing to avoid glass fibre resin enrichment or weld-line formation. Cure time is commonly 40–90 s/mm of part thickness at 140–155°C under 60–120 bar cavity pressure. Low-profile SMC exterior body panels tested per ASTM D790-17 at 23°C exhibit flexural modulus of 8–12 GPa and flexural strength of 150–220 MPa. Electrical BMC enclosures specified under UL 94 are formulated with flame-retardant synergists and must achieve V-0 at 3.0 mm, while dielectric strength per IEC 60243-1 is commonly 12–15 kV/mm on 3.0 mm coupons. Terminal products include automotive body panels, lighting housings, electrical distribution boxes, and dishwasher inner tubs. TBPB is not a room-temperature initiator; if an accelerated ambient gel time is required, the formulation must include a conventional MEKP/cobalt promoter system, but such combinations can generate redox heat and must not be used for mature SMC. The deep process conflict in this segment is the simultaneous requirement for high final conversion above 90% and low flow time before gelation. Too low a TBPB charge below 0.8 wt% produces undercured edges and low Barcol hardness below 40, while too high a charge above 1.8 wt% can generate a peak exotherm above 220°C in thick ribs, leading to internal cracks and styrene vapour voids.

    How Is Pull Speed Constrained by Die Zone Temperatures in TBPB-Initiated Pultrusion?

    Pultruded profiles present a kinetic conflict between die residence time and TBPB decomposition. A translucent or filled unsaturated polyester matrix is impregnated into continuous glass rovings with tracer fibres, then drawn through a heated die with typical temperature zones of 120°C, 150°C, and 160°C. Because the peroxide half-life at 150°C falls in the minute range, the peak die zone acts as the primary conversion trigger, while the upstream 120°C zone serves to raise the matrix to the gelation threshold without premature gel on the die walls. TBPB dosage in pultrusion is usually 0.8–1.5 wt% of resin, with a resin viscosity at 25°C controlled to <2.5 Pa·s to permit wet-out at speeds up to 1.0 m/min. Fillers are limited to 5–10 wt% of resin because higher loadings increase die pull resistance and can abrade the chrome-plated die surface. For profiles with cross-sections between 6 mm and 20 mm, pull speed is normally held at 0.2–0.8 m/min, yielding a residence time of 1.5–4.0 min in a 1.0 m heated die. The upper speed boundary is set by the time required to reach at least 95% radical conversion; exceeding 0.8 m/min on a 10 mm solid round tends to move the exotherm front past the die exit, producing a soft core that can tear on the pulling grips. The lower speed boundary is equally hazardous: below 0.2 m/min, the matrix can reach full gelation too early inside the die, causing die seizure and filament breakage at the entrance. Tapered dies with entrance angle 2–5° and die hardness HRC 60–65 are standard for glass-reinforced profiles. The process is validated by ASTM D7957-22 for GFRP reinforcing bar, with a glass transition temperature by ISO 11357-2:2020 not less than 100°C. Terminal products include FRP rebar, cable trays, ladder rails, window profiles, and cooling tower structural members. The central process failure mode is die-lock initiated by excessive gelation in the first heated zone; therefore zone temperatures must be recalibrated when back-pressure rises more than 15% above baseline for a given reinforcement weight fraction.

    Chemical Service Laminates Demand a Post-Cure Ramp Above the Perester Half-Life Threshold

    Vinyl ester laminates for chemical storage operate under a different constraint: the peroxide must deliver a fully crosslinked network with low residual styrene, but the exotherm of thick laminates can exceed the decomposition temperature of the peroxide and form voids. TBPB is added at 1.0–2.0 wt% of the liquid resin, often a bisphenol A epoxy vinyl ester with styrene content of 35–45 wt%. In wet layup and filament winding operations, the resin is applied at 20–30°C and heated in an oven or electric blanket to 80–100°C for initial gelation, followed by post-cure at 120°C for 1–2 h. The post-cure ramp is critical because TBPB has a 10 h half-life at 105°C; below 120°C the terminal styrene conversion proceeds too slowly and residual monomer by ISO 4901 may remain above 0.1%, reducing chemical resistance. For laminate thickness above 10 mm, the peak exotherm can exceed 200°C and must be managed by staged lay-up or external cooling, otherwise volatile styrene creates microvoids at the resin/glass interface. The process conflict is most acute in tank linings: the surface exposed to acid must be hard and fully cured, while the structural backup laminate must not exotherm enough to crack at the liner-substrate bond. Chemical resistance is tested with ASTM C581-20 coupons exposed to the service medium at design temperature for 6 months; a commonly specified acceptance criterion is retention of Barcol hardness within 10% of the unexposed reference. Pipe and ducting are additionally specified under ISO 14692-2 for glass-reinforced plastic piping systems in oil and gas service. Terminal parts include hydrochloric acid tanks, bleach scrubbers, desulfurization ducts, and brine piping. TBPB is not suitable for ambient-cure field repairs on these structures; the required heat source is absent in open field environments, and cobalt-promoted MEKP must be used only for temporary patch applications with restricted immersion service. In this application the most common industrial failure is an undercured inner corrosion barrier; therefore oven temperature uniformity must be maintained within ±5°C during post-cure.

    Compliance checklist for TBPB-cured thermoset applications
    ApplicationTest standardTypical specification
    SMC/BMC electrical enclosureUL 94, IEC 60243-1V-0 at 3.0 mm; dielectric strength 12–15 kV/mm
    FRP rebar pultrusionASTM D7957-22, ISO 11357-2:2020Tg ≥100°C; solid round bar requirements per standard
    Chemical service vinyl ester laminateASTM C581-20Barcol retention ≥90% after exposure
    Engineered quartz slabASTM D790, ASTM D2583Flexural strength 30–50 MPa; Barcol hardness 50–70

    Engineered Quartz Slabs and Solid Surface Cure in Vacuum Compression Presses

    Engineered quartz and solid surface slabs use a vacuum-compression process in which TBPB is dissolved in the unsaturated polyester binder at 0.8–1.5 wt% of resin. The binder fraction is only 7–10 wt% of the total slab mass, the balance being quartz aggregate, glass chips, or aluminum trihydrate filler. Resin-to-filler ratio therefore shifts the exotherm: at 7 wt% resin, the peak exotherm during cure is modest and the cycle can be run at the upper temperature limit; at 10 wt% resin, the same peroxide charge can produce an exotherm that exceeds the boiling point of styrene and creates internal porosity. Mixing is conducted in planetary or high-intensity mixers under vacuum 90–95 kPa to remove air entrainment from the wet mix. The mat is then distributed in a mould frame and compacted in a vacuum vibro-compression press at 80–120 bar, followed by curing at 90–110°C for 30–60 min. TBPB is selected over lower-temperature peroxides because slab thickness commonly reaches 20–30 mm; faster initiators would gel the surface before the core is fully compacted. Filler moisture above 0.1% retards the cure at the resin-filler interface and can reduce final Barcol hardness by 5–10 units. Finished slabs are tested by ASTM D790 for flexural strength, with typical values between 30–50 MPa, and by ASTM D2583 for Barcol hardness, commonly 50–70. Solid surface material for vanity tops and work surfaces is also specified under ISO 19712-1. TBPB above 1.8 wt% in this segment does not improve final conversion; it increases volatile decomposition by-products and can discolour white or translucent slabs, particularly when the cure oven overshoots above 120°C. The main terminal articles are kitchen countertops, vanity tops, wall cladding, and floor tiles.

    During continuous lamination of flat glass-reinforced panels, TBPB is mixed into unsaturated polyester resin at 0.8–1.2 wt% because the gel point must coincide with the fourth heating zone of a double-belt press. The resin is applied to a carrier film at 250–450 g/m² per glass mat layer and then consolidated through nip rollers before entering the heated zone. Typical heating zones are set at 100°C, 130°C, and 140°C, with a line speed of 3–8 m/min for panel thicknesses from 1.5 mm to 4.0 mm. TBPB permits the high line speed because its half-life at 140°C is short enough to complete gelation within the available residence time of 60–180 s, but the front and back surfaces must be heated symmetrically; otherwise the panel warps after trimming. Compliance for flat panels includes ASTM D638-14 tensile strength of 70–100 MPa at 23°C and ISO 75-2 deflection temperature under load. Typical end uses are truck trailer liners, RV side panels, shower surrounds, and agricultural building cladding. Because the resin contains no wax or monomer-barrier additive, oxygen inhibition at the exposed edges must be controlled by enclosing the open edge zone or by adding a paraffin wax to the surface resin; otherwise the edge cure remains tacky and can delaminate under moisture cycling.

    When Oven-Cured Gel Coats Must Survive Thermal Cycling, Perester Dosage Tightens to a Narrow Window

    Oven-cured gel coats formulated with TBPB exhibit a pronounced sensitivity to dosage. The gel coat resin is sprayed or flow-coated at 0.4–0.8 mm wet film thickness into a mould prepared with release agent, then cured in a forced-air oven at 80–120°C for 20–40 min before laminate backup is applied. TBPB loading is held at 0.5–1.0 wt% of the gel coat resin. At loadings above 1.2 wt%, the cured film develops microcracking after repeated thermal cycling between -20°C and 80°C, with gloss reduction measured by ISO 2813 exceeding 10%. At loadings below 0.5 wt%, the surface remains undercured after the oven cycle and can develop blisters after 24 h water immersion at 65°C per ASTM D570. The finished gel coat is used on sanitary ware, bathtubs, shower trays, and vanity basins. Oven curing must hold temperature uniformity within ±5°C across the part to avoid localised overcure. Direct contact with cobalt promoters is not recommended because the redox decomposition of TBPB is incomplete at ambient temperature and produces a tacky, low-hardness film before the oven ramp begins.

    Free Quote

    Competitive tert-Butyl Peroxybenzoate (TBPB) prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618963613625 or mail to sales10@ascent-petrochem.com.

    We will respond to you as soon as possible.

    Tel: +8618963613625

    Email: sales10@ascent-petrochem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    tert-Butyl peroxybenzoate (TBPB; CAS 614-45-9) is an aromatic peroxyester supplied as a clear, colorless to pale-yellow liquid with a molecular weight of 194.23 g/mol and a theoretical active oxygen content of 8.24 wt%. Commercial material is typically specified at ≥98.0% assay by iodometric titration (ASTM E298), a density at 20 °C of 1.035–1.045 g/cm³ (ASTM D4052), and a refractive index n20D of 1.498–1.502. Trade designations such as Trigonox C and Luperox P are encountered in procurement, but specification equivalence should be established against CAS registry, peroxide assay, and active oxygen content rather than the trade name alone. At 98.0% assay, the calculated active oxygen is 8.08 wt%.

    Thermal decomposition proceeds by homolytic scission of the O–O bond adjacent to the carbonyl group, generating benzoyloxy and tert-butoxy radicals. The tert-butoxy radical undergoes β-scission to acetone and a methyl radical at temperatures above 100 °C, while the benzoyloxy radical may decarboxylate to a phenyl radical and carbon dioxide. This radical profile differs from dibenzoyl peroxide (BPO), which does not generate tert-butoxy species, and from dicumyl peroxide (DCP), which produces cumyloxy and methyl radicals plus acetophenone as a decomposition by-product. These mechanistic distinctions affect cure temperature selection, odor generation, and migration behavior in finished polymer matrices.

    Representative commercial specification envelope for TBPB
    ParameterSpecification rangeTest method
    Peroxide assay≥98.0 wt%ASTM E298
    Active oxygen8.0–8.3 wt%Calculated from assay
    Density at 20 °C1.035–1.045 g/cm³ASTM D4052
    Refractive index n20D1.498–1.502Refractometric method
    Flash point, closed cup≥88 °CISO 3679
    SADT60 °CPackaging-dependent test
    Maximum storage temperature30 °CManufacturer technical bulletin

    How Does TBPB’s Half-Life Profile Compare with Other Organic Peroxides?

    The selection criterion for high-temperature curing is usually the temperature at which the peroxide exhibits a 10 h half-life in a specified solvent. For TBPB, published technical bulletins commonly list a 10 h half-life of 104 °C in benzene; the corresponding values for benzoyl peroxide and dicumyl peroxide are approximately 73 °C and 117 °C in equivalent media. tert-Butyl peroxy-2-ethylhexanoate (TBPEH), a lower-temperature peroxyester, has a 10 h half-life near 72 °C. TBPB therefore occupies an intermediate stability window: it can be stored at 30 °C without the stringent refrigeration demanded by TBPEH, but it requires mold or bath temperatures above 120 °C to produce sufficient radical flux within typical cycle times.

    Comparative thermal stability and storage limits for selected organic peroxides
    Peroxide10 h half-life temperature (°C, benzene)SADT (°C)Maximum storage temperature (°C)
    TBPB1046030
    Benzoyl peroxide (BPO)738040
    Dicumyl peroxide (DCP)1178040
    tert-Butyl peroxy-2-ethylhexanoate (TBPEH)723515

    During sheet molding compound (SMC) and bulk molding compound (BMC) compression molding, TBPB is introduced at 1.0–2.0 phr into unsaturated polyester resin formulations containing 35–55 wt% calcium carbonate filler and 25–32 wt% glass fiber. The initiator is pre-dissolved in the styrene or acrylic monomer phase before filler addition to avoid localized concentration gradients. Production presses operating at 145–155 °C achieve cure times of 60–120 s for 2.5–3.0 mm flat panels, while thicker sections above 6 mm require a staged initiator package because the low thermal conductivity of the compound delays the internal temperature rise by 25–40 s. A 70:30 blend of TBPB and TBPEH reduces the peak exotherm temperature by 8–12 °C and shortens the final cure zone without extending total cycle time beyond 180 s. Formulations containing hydroquinone or methyl ether of hydroquinone may delay gel time by 15–30% compared with uninhibited resin; the initiator dose is adjusted upward by 0.2–0.5 phr to compensate, but the response is not linear because inhibitor consumption occurs during the induction period.

    Acrylic syrup polymerization for cast sheet and unsaturated polyester-acrylic hybrids uses TBPB at 0.3–1.0 wt% in combination with azo initiators or lower-temperature peroxyesters. The peroxide is added after mercaptan chain-transfer agents have been mixed to avoid premature radical attack on the thiol group. In continuous casting lines with belt speeds of 1.5–2.5 m/min and bath temperatures of 70–90 °C, TBPB alone is generally insufficient; it functions as the high-temperature finishing initiator to reduce residual monomer after the primary initiator has been depleted. Gel effect onset at 20–30% conversion raises the local temperature by 15–25 °C, which can activate TBPB and shorten the final cure zone.

    When TBPB Replaces Dicumyl Peroxide in EPDM Extrusion Grades

    Peroxide-cured EPDM compounds used in automotive coolant hoses and window seals are crosslinked with 5–8 phr of dicumyl peroxide or 6–10 phr of TBPB on a 100 phr polymer basis, depending on ethylene content and the presence of co-agents such as triallyl cyanurate. TBPB’s decomposition products include tert-butanol and benzoic acid; benzoic acid can accumulate as surface bloom at addition levels above 8 phr, a limitation not observed with DCP at equivalent crosslink density. The scorch time at 125 °C, measured by moving-die rheometer (ISO 6502), is typically 3–5 min shorter for TBPB than for DCP in comparable compounds, which narrows the processing window in long-die extrusion. Compounders therefore hold maximum extrusion head temperature at 115 °C or use a co-agent to delay premature crosslinking. Published data for direct exothermic comparison across all EPDM grades is limited, and compound-specific cure curves should be generated on the production rheometer before lot approval.

    Cure Kinetics, Solvent Dependence, and Radical Flux Boundaries

    Published half-life data for TBPB are solvent-dependent. In aromatic solvents such as benzene or xylene, the 10 h half-life is near 104 °C; in polar media the decomposition rate may shift because radical recombination and cage escape are influenced by viscosity and solvent polarity. In styrenated unsaturated polyester resin, the effective half-life at 140 °C is shorter than the benzene-derived value because the monomer participates in chain transfer and the polymerization exotherm adds to the temperature rise. Molding compounds containing 1.5 phr TBPB can exhibit peak exotherms of 190–210 °C in thick sections; this is a critical boundary because thermal degradation of the cured matrix may begin above 220 °C. The radical flux is also sensitive to dissolved oxygen, which acts as a radical scavenger during the early stages of cure. Closed-mold processes suppress oxygen inhibition, but open-surface applications may develop an incompletely cured tacky layer unless a paraffin wax or nitrogen blanket is applied.

    Because TBPB is classified as an organic peroxide, the transport classification is UN 3103, Division 5.2, Type C, with a self-accelerating decomposition temperature of 60 °C. Storage areas must maintain product temperature at or below 30 °C, and bulk tanks require independent high-temperature alarms set at 40 °C with automatic cooling interlocks. The compound is incompatible with strong acids, alkalis, amines, transition metal salts, and reducing agents; contact with cobalt accelerators in the absence of a diluent can initiate rapid decomposition below 40 °C. Firefighting media should be water spray or water fog; dry chemical and carbon dioxide are ineffective for cooling bulk containers. Ventilation must be explosion-rated because decomposition vapors include acetone and benzene derivatives.

    Top