| HS Code | 975065 |
| Productname | Methyl Ethyl Ketone Peroxide |
| Abbreviation | MEKP |
| Chemicalfamily | Organic peroxide |
| Chemicalname | Methyl ethyl ketone peroxide |
| Synonyms | MEKP; 2-butanone peroxide; methyl ethyl ketone hydroperoxide |
| Casnumber | 1338-23-6 |
| Einecsnumber | 215-661-2 |
| Unnumber | 3105 |
| Hazardclass | 5.2 Organic peroxide |
| Subsidiaryrisk | 8 Corrosive |
| Molecularformula | C8H16O4 (representative dimer) |
| Molecularweight | 176.21 g/mol (representative dimer) |
| Physicalstate | Liquid at room temperature |
| Appearance | Colorless to pale yellow liquid as formulated |
| Odor | Pungent, sharp, characteristic peroxide odor |
| Density | Approximately 1.05 to 1.15 g/cm3 at 20 C |
| Flashpoint | Typically above 60 C; formulation dependent |
| Solubilityinwater | Slightly soluble |
| Solubilityinorganicsolvents | Soluble in many organic solvents |
| Activeoxygencontent | Typically 8 to 10 percent |
| Ph | Typically 2 to 5 |
| Viscosity | Low to moderate, formulation dependent |
| Selfacceleratingdecompositiontemperature | Approximately 50 to 60 C, formulation dependent |
| Storagetemperature | Recommended below 30 C, preferably 10 to 25 C |
| Shelflife | Typically 6 to 12 months under recommended storage |
| Oxidizingproperties | Strong oxidizing agent |
| Decompositionhazard | Exothermic decomposition; may be violent if contaminated or heated |
| Incompatibilities | Strong acids, bases, reducing agents, metals, accelerators, combustible materials |
| Primaryuse | Curing agent and initiator for unsaturated polyester and vinyl ester resins |
| Packaging | Approved polyethylene containers with vented closures |
As an accredited Methyl Ethyl Ketone Peroxide (MEKP) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | MEKP is packaged in 5 L high-density polyethylene containers with vented caps and hazard labels, stored upright in secondary containment. |
| Container Loading (20′ FCL) | Methyl Ethyl Ketone Peroxide (MEKP) in 20′ FCL: organic peroxide, IMDG-compliant, temperature-controlled as required, secured, upright, ventilated, segregated; avoid heat, ignition, incompatibles. |
| Shipping | Methyl Ethyl Ketone Peroxide (MEKP) is shipped as a hazardous organic peroxide (Class 5.2, often UN 3105) in approved, compatible packaging. Shipments require proper labels, placards, and documentation. Keep cool, upright, and away from heat, shock, acids, metals, and reducing agents. Temperature control may be required depending on formulation. Follow all transport regulations. |
| Storage | Store MEKP in a cool, dry, well-ventilated, fire-resistant, locked area away from heat, sunlight, ignition sources, acids, bases, metals, and combustibles. Keep in original, vented containers with secondary containment. Maintain stable, monitored temperature; prevent impact, friction, or contamination. Segregate from incompatible materials and use grounding, spill kits, and local regulatory requirements. MEKP is shock-, heat-, and friction-sensitive. |
| Shelf Life | MEKP typically has a shelf life of 3–6 months if stored cool, dry, and away from sunlight, heat, and contaminants. |
In open-mold laminating of orthophthalic and isophthalic unsaturated polyester resins for glass fibre-reinforced transport body panels and leisure marine shells, methyl ethyl ketone peroxide (MEKP) is metered at 1.2–2.0 wt% of resin mass only after the cobalt octoate promoter has been dispersed in the resin phase. Direct addition of MEKP into a concentrated cobalt promoter stream or vice versa creates localized redox decomposition with gas evolution and possible thermal runaway; production lines therefore use separate dosing reservoirs and keep manual mixing vessels rigorously segregated to prevent cross-contamination. The forming process typically alternates between chopper-gun spray lay-up at 0.38–0.45 MPa atomization pressure and vacuum infusion under 20–80 mbar absolute pressure, with consolidation rollers removing trapped air before the resin reaches the gel point. In hand lay-up and spray lay-up sections thicker than 6 mm per pass, the peak exotherm must remain below 150 °C; exceeding that threshold produces thermal expansion of styrene vapour, fibre print-through on the tool-side surface, and a measurable drop in through-thickness Barcol hardness. Mechanical compliance is verified under ISO 527-4:2021 for tensile properties of orthotropic laminates and ASTM D3039/D3039M-17 for polymer matrix composite tensile testing, while small craft hull laminates are qualified against the structural requirements of ISO 12215-2:2002. The terminal components produced under this working window include boat decks, caravan sidewalls, truck body panels, agricultural equipment hoods, and lightweight trailer skins. Because the promoter-to-catalyst ratio is the primary lever controlling gel time, the MEKP fraction is held within the stated range; below 1.2 wt% ambient cure in thin laminate edges can remain incomplete, whereas above 2.0 wt% the exotherm may induce local styrene boil-out in thick ribs and core transitions.
Exterior gelcoats for swimming pool shells, shower trays, bathtubs, and marine topsides are formulated with styrene-suppressed unsaturated polyester, fumed silica thixotrope at 1.0–2.0 phr, and either paraffin wax or a non-wax air-inhibition suppressant to achieve a tack-free surface after cure. MEKP dosage is maintained at 1.5–2.5 wt% of resin mass, not including pigment paste or thixotrope, because the applied wet film is only 0.4–0.8 mm thick and is particularly vulnerable to air inhibition at the surface. Spray application is performed through HVLP cup guns at 0.15–0.25 MPa fluid pressure or air-atomized guns with a 0.12–0.18 MPa atomization stream; gelcoat is usually applied in two passes to avoid sag on vertical surfaces. When workshop temperature remains below 18 °C, the induction time is extended and the surface conversion can be incomplete even after 24 h; forced-air heating or infrared panels set at 40–50 °C are therefore used to bring the mould surface into the acceptable cure window before spraying. Surface hardness is checked with a Barcol impressor under ASTM D2583-13a, with supplier bulletins commonly specifying a minimum of 35 after 24 h for waxed gelcoats; pull-off adhesion to the subsequent laminate is assessed under ISO 4624:2016 after the laminate has been postcured. The terminal parts include in-ground swimming pool shells, moulded shower trays, bathtub skins, and marine deck gelcoats. In wax-free gelcoats, the surface remains deliberately tacky for subsequent lamination, and the use of MEKP alone without paraffin wax is not sufficient to overcome oxygen inhibition in the outermost 10–20 µm layer. A reduction below 1.5 wt% is generally not permissible for gelcoat because residual styrene remains in the film and acts as a solvent that reduces hardness and may cause primer or antifouling paint delamination later.
Trowel-applied unsaturated polyester body filler pastes for sheet metal repair are initiated with 2.0–3.0 wt% MEKP based on total filled paste mass, not on resin solids alone, because talc and calcium carbonate loadings of 30–50 phr and 20–40 phr respectively act as thermal mass that moderates peak exotherm while also reducing shrinkage. The paste is mixed at 20–25 °C for 1.5–2.5 min with a flat spatula or pneumatic stirrer at 150–300 rpm until the peroxide is evenly distributed into the styrene-monomer-rich paste; once mixed, the pot life is 6–10 min and the compound must be trowelled onto the metal substrate before the viscosity build-up prevents wetting of sanded steel. Sanding can begin after 20–30 min with P80–P120 abrasives provided the repair is below 5 mm thickness; thicker applications require a two-layer technique because the exotherm in the centre of a single thick layer can exceed the solvent-pop threshold. Adhesion and cohesive integrity are measured under ISO 2409:2013 cross-cut testing on degreased steel, with acceptance at classification 1 or better for most automotive aftermarket repair specifications, and ASTM D3359-17 Method B is used when North American body shop adhesion records are required. The terminal product range includes automotive door skins, roof seams, quarter panel repairs, bumper repair compounds, and truck cab fairing fillers. Batch-to-batch variation in talc moisture or styrene monomer isomer balance can shift gel time by approximately ±3 min on the production floor; therefore each paste batch is qualified with a 50 g cup gel test before release. The working boundaries are equally narrow: below 2.0 wt% MEKP, unpolymerized styrene may remain entrapped and later migrate through waterborne basecoat during bake cycles above 80 °C, while above 3.5 wt% the repair becomes brittle, sands unevenly, and can transfer a yellow peroxide degradation product into light-coloured topcoats.
In cultured marble and solid surface casting, alumina trihydrate at 55–68 wt% of the filled mix is combined with unsaturated polyester resin and MEKP at 1.0–2.0 wt% of resin mass; the filler acts as a thermal sink that suppresses peak exotherm but also as a viscosity modifier that changes the required mixing energy. The production process begins with vacuum mixing at 50–80 mbar for 3–5 min to remove entrained air, followed by vibratory casting into closed or open moulds at 0.2–0.6 mm amplitude and 35–50 Hz vibration frequency. Ambient cure is carried out at 25–35 °C for 4–8 h, and demoulded parts are postcured at 50–60 °C for 4 h to complete conversion before polishing. Hardness development is measured under ASTM D2583-13a, with typical Barcol hardness values of 40–55 on polished surfaces; water absorption and dimensional stability are evaluated under ASTM D570-22 and ANSI Z124.1-2017 for plastic tub and shower units where applicable. Terminal products include vanity tops, wet wall panels, freestanding tubs, basin bowls, and tabletop surfaces. At the lower end of the catalyst window, 1.0 wt% MEKP can produce adequate cure in thin castings but may leave resin-rich veins under-cured inside complex sink bowl radii; mixing must therefore maintain a tip speed above 1.5 m/s to avoid localized peroxide-starved regions. At the upper end, loadings above 65 wt% alumina trihydrate may require the catalyst to be raised toward 2.0 wt%, but it must not exceed 2.5 wt% because the exotherm can then generate microcracks that appear only after thermal shock testing under ANSI Z124.1-2017. Published data for this specific configuration is limited; qualification on the production floor therefore relies on 10 mm cube specimens cured under identical vacuum and vibration conditions before full batch release.
Resin concrete and chemical-resistant screed formulations based on unsaturated polyester binders are initiated with MEKP at 1.0–2.0 wt% of binder after the cobalt promoter has been dispersed into the resin phase; aggregate-to-binder ratios of 8:1–12:1 by mass produce low-slump mortars that are compacted by power trowel or vibratory screed. Continuous mixing is carried out in a forced-action paddle mixer at 20–40 rpm with the aggregate and resin components combined under a controlled sequence: resin, promoter, MEKP, then dry quartz filler, because adding the peroxide before the promoter is fully dispersed causes local gel particles that cannot be re-wet. The mixed material is placed at floor temperatures above 15 °C; at 20 °C the pot life is 15–25 min, and early walk-on strength develops within 8–12 h. Compressive strength is tested under EN 13892-2, and the finished screed is classified under EN 13813:2002; quartz-filled unsaturated polyester screeds commonly exceed 45 MPa at 7 days when the aggregate is dry. Terminal product types include drainage channels, pump foundations, secondary containment curbs, manhole bases, trench covers, and plinth toppings in chemical processing buildings. Aggregate moisture above 0.3 wt% is a critical operational boundary: water retards the MEKP-initiated cure and promotes hydrolytic attack on the polyester binder, reducing long-term compressive strength and chemical resistance. On production lines where quartz sand is stored in unheated silos, condensation on aggregate surfaces in winter months must be controlled by pre-drying at 80–100 °C until the moisture threshold is restored.
Vinyl ester resin systems used for corrosion-resistant FRP tanks, piping, scrubber shells, and ductwork are ambient-gelled with MEKP at 1.0–2.0 wt% of resin after the cobalt promoter is pre-dispersed; the working window is set by the need to obtain sufficient room-temperature green strength before the thermal postcure step. Contact molding and filament winding are the dominant production processes, with the inner corrosion barrier applied as a resin-rich layer of 0.5–1.0 mm thickness before structural glass layers are wound at 55–65° wrap angle under fibre tension. After ambient cure for 12–24 h, the laminate is postcured at 93 °C for 4 h or at 104 °C for 2 h, depending on the supplier formulation; the postcure is considered mandatory to achieve full crosslink density and corrosion resistance. Fabrication is qualified under ASME RTP-1-2021 for reinforced thermoset plastic corrosion-resistant equipment and ASTM C582-09(2016) for contact-molded corrosion-resistant laminates; GRP piping systems are additionally tested under ISO 14692-1:2017. Barcol hardness after postcure is routinely specified at a minimum of 35 on interior surfaces, with lower readings indicating undercure or insufficient styrene conversion. The terminal products include acid storage tanks, chlor-alkali scrubber shells, flue gas ductwork, header pipes, and inline flanges for chemical process plants. The most critical processing boundary is single-pass laminate thickness: if one structural pass exceeds 6 mm wall thickness, the MEKP exotherm can drive the laminate core above 120 °C, creating microcracks and potential delamination at the corrosion barrier even before postcure. Fabricators therefore split structural laminates into multiple passes with an interpass window of 1–2 h and monitor surface temperature during winding with infrared thermography. The catalyst dosage is not reduced below 1.0 wt% solely to moderate exotherm, because ambient undercure then leaves unreacted styrene that exudes during postcure and compromises the resin-rich corrosion barrier.
Competitive Methyl Ethyl Ketone Peroxide (MEKP) prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618963613625 or mail to sales10@ascent-petrochem.com.
We will respond to you as soon as possible.
Tel: +8618963613625
Email: sales10@ascent-petrochem.com
Flexible payment, competitive price, premium service - Inquire now!
Methyl ethyl ketone peroxide (MEKP), CAS 1338-23-4, is a phlegmatized organic peroxide supplied as a clear, low-colour liquid. The commercial product is not a single compound but a multi-component equilibrium mixture containing monomeric and dimeric peroxide species, methyl ethyl ketone, hydrogen peroxide, water, and a phlegmatizer such as dimethyl phthalate, dibutyl phthalate, or an aliphatic ester. Active oxygen content, rather than nominal peroxide concentration, defines cure performance. Industrial grades are specified according to active oxygen in the range 8.0–10.0%, with water content typically below 1.5% and density at 20 °C between 1.10 g/cm³ and 1.20 g/cm³ when determined by ISO 2811. The product is classified as an organic peroxide Type D liquid under UN 3105 for transport, with a self-accelerating decomposition temperature (SADT) usually reported between 45 °C and 60 °C depending on packaging volume and phlegmatizer level. These values are release specifications controlling shelf life, storage configuration, and resin-system design.
In unsaturated polyester and vinyl ester processing, MEKP is used as a room-temperature radical initiator after the resin has been accelerated with cobalt octoate or cobalt naphthenate. The product is selected where a practical balance between gel time, peak exotherm, and through-cure is required in open-mould laminating, gel coat application, resin transfer molding, and solid surface casting. Supplier model designations such as MEKP-9, MEKP-50, and MEKP-LA are not harmonized; the relevant comparator is the certificate of analysis for active oxygen, residual hydrogen peroxide, water content, and viscosity under the methods shown below.
Commercial MEKP is differentiated by phlegmatizer chemistry, active oxygen content, and residual hydrogen peroxide. Low-water grades are preferred for vinyl ester laminating because water can interfere with interfacial wetting of carbon or glass reinforcement. Dimethyl phthalate-diluted grades remain standard in general-purpose orthophthalic and isophthalic unsaturated polyester resins. Low-monomer grades are specified for closed-mould processes where styrene emissions and phase separation in dosing lines are controlled.
The release ranges in Table 1 represent typical values obtained from supplier technical bulletins for medium-reactivity, phlegmatized MEKP; procurement specifications should be fixed against the actual certificate of analysis.
| Property | Test method | Typical release range |
|---|---|---|
| Appearance | Visual inspection | Clear, colourless to pale yellow liquid |
| Active oxygen | ASTM E298 | 8.0–10.0% |
| Density at 20 °C | ISO 2811 | 1.10–1.20 g/cm³ |
| Viscosity at 20 °C | ISO 2555 | 15–70 mPa·s |
| Water content | ISO 760 | ≤ 1.5% |
| Flash point | ISO 3679 | > 70 °C |
| SADT | UN Test H.4 | 45–60 °C |
Residual hydrogen peroxide is controlled because it affects accelerator demand and exotherm shape. A product with hydrogen peroxide above 2.5 wt% can produce longer gel times than the active oxygen value suggests, followed by a rapid exotherm when the promoted resin reaches critical free-radical flux. In a 50 L vacuum-assisted resin infusion tool maintaining a glass-fibre volume fraction of 0.45, changing from a standard medium-reactivity MEKP to a low-hydrogen-peroxide grade at fixed 1.25 phr and 0.30 phr cobalt octoate 12% shifted gel time from 18 min to 24 min at 23 °C and reduced peak exotherm by 35–45 °C. Published data for this specific configuration is limited; the exact shift must be established by cup gel tests under plant-specific reinforcement fraction and mould temperature.
Phlegmatizer type changes total volatiles, plasticizer migration, and flash point. Dimethyl phthalate has a boiling point near 282 °C and a flash point near 146 °C; it reduces volatility but can contribute to volatile organic emissions in high-temperature postcure. Aliphatic ester-diluted grades offer lower viscosity and lower plasticizer migration but may require recalibration of peroxide metering pumps because viscosity at 20 °C can fall below 20 mPa·s. A gear pump calibrated for 50 mPa·s MEKP may underfeed a 15 mPa·s grade if internal slip increases; peristaltic dosing with calibration by mass per stroke is specified for low-viscosity grades.
The limiting variables in ambient cure are accelerator availability, resin unsaturation, inhibitor package, laminate thickness, and workshop temperature. MEKP dosage is typically held between 1.0 phr and 2.5 phr in open-mould laminating; cobalt octoate 12% is added between 0.2 phr and 0.5 phr. Raising MEKP above 2.5 phr does not produce a proportional increase in final conversion; it mainly accelerates exotherm and increases the risk of foaming and cracking in sections thicker than 10 mm. Gel time measured by ISO 2535 in a 25 °C water bath typically falls from 22 min to 11 min when workshop temperature rises from 18 °C to 27 °C at fixed accelerator loading. This 8–14 min shift per 10 °C is observed in cobalt-promoted orthophthalic laminating resin; vinyl ester resins may show stronger sensitivity.
Decomposition in cobalt-promoted resin follows a redox cycle: cobalt(II) is oxidized by peroxide to cobalt(III), which re-oxidizes MEKP to alkoxy and peroxy radicals. The rate depends on cobalt concentration and temperature. The apparent activation energy for gelation in unsaturated polyester resins is typically between 60 kJ/mol and 90 kJ/mol, which explains the large gel-time shifts over narrow temperature windows. This range is derived from ISO 2535 gel-time measurements at multiple temperatures; exact values vary with inhibitor package and resin unsaturation.
In open-mould spray-up with resin output of 4.5 kg/min, gel-time control is normally adjusted through cobalt dosage rather than MEKP because changes in MEKP level above 2.0 phr generate exotherm with limited working-time benefit. Equipment operating in relative humidity above 60% without paraffin wax or film closure can exhibit surface tack from oxygen inhibition, particularly in air-backed laminates. This is a processing boundary, not a property of the peroxide alone.
For closed-mould resin transfer molding, low-exotherm MEKP grades are specified to delay gelation until the flow front has filled the reinforcement. Injection pressures are typically controlled between 1.5 bar and 3.0 bar. Higher pressures do not alter MEKP decomposition kinetics, but they can create resin-rich channels if preform permeability varies. Neat resin casts of 20 mm thickness cured with standard MEKP at 2.0 phr can exceed 160 °C internally; the same system may not crack at 4 mm because heat is dissipated. Low-active-oxygen grades reduce peak exotherm but also reduce final conversion unless postcure at 60–80 °C for 2–4 h is applied.
Peroxide dosing lines for MEKP require stainless steel or polypropylene construction; brass, copper, and iron components are excluded because transition-metal contamination can initiate peroxide decomposition. Static mixers with dead zones have shown premature gelation when MEKP and promoted resin are partially mixed; low-dead-volume mixers are specified to prevent peroxide pooling.
MEKP is not interchangeable with other organic peroxide initiators. The selection depends on accelerator type, laminate thickness, required working time, and surface quality. Table 2 compares typical ambient-cure initiator systems using representative ranges from supplier technical bulletins; actual values depend on resin unsaturation, inhibitor content, filler loading, and part geometry.
| Initiator system | Typical dosage | Gel time at 20–25 °C | Peak exotherm in 4 mm neat resin cast | Primary limitation |
|---|---|---|---|---|
| MEKP + cobalt octoate 12% | 1.0–2.5 phr MEKP; 0.2–0.5 phr Co | 10–30 min | 130–180 °C | Exotherm cracking above 10 mm thickness |
| BPO + tertiary aromatic amine | 1.5–3.0 phr BPO; 0.5–1.0 phr amine | 20–90 min | 90–140 °C | Slower surface cure; moisture sensitivity |
| AAP + cobalt octoate 12% | 1.0–2.0 phr AAP; 0.1–0.4 phr Co | 5–15 min | 150–200 °C | Short pot life; high exotherm |
| CHP + cobalt octoate 12% | 1.5–3.0 phr CHP; 0.2–0.6 phr Co | 60–240 min | 60–110 °C | Low conversion as sole initiator |
MEKP provides a broader ambient-cure window than AAP and more complete through-cure than CHP alone. BPO/amine systems are used where lower exotherm is required or where cobalt promotion is not acceptable, but the surface cure is slower and humidity sensitivity is greater. Cobalt-promoted MEKP cure becomes impractically slow below 12 °C; BPO/amine systems are selected for cold-weather laminating down to 5 °C. In gel coat formulations, MEKP is often preferred because it can be formulated with low-hydrogen-peroxide grades to reduce porosity and with CHP as a secondary initiator to improve surface cure; this blend approach modifies gel time without raising MEKP concentration into the exotherm-cracking range.
Differences in water content and phlegmatizer also alter migration kinetics in polymer matrices. Dimethyl phthalate-diluted MEKP can plasticize thin gel coats slightly at 2.0–3.0 phr, whereas aliphatic-ester-diluted grades are specified where phthalate migration is restricted under EU 10/2011 food-contact conditions. This distinction is operational, not cosmetic.
Storage of MEKP requires vented containers maintained between 2 °C and 20 °C and segregated from accelerators, strong acids, strong bases, amines, and reducing agents. Direct mixing of MEKP with cobalt octoate or tertiary amines is prohibited; the accelerator must be dispersed into the resin before peroxide addition. Metal contamination from iron, copper, and brass fittings must be eliminated from dosing lines because transition-metal ions lower the decomposition onset temperature. The maximum recommended storage duration under 20 °C is 6 months; product withdrawn from bulk storage should be kept in original vented containers and not returned to inventory after dispensing. Containers exposed to temperatures above 30 °C should be checked for pressure build-up and active oxygen retention before use. The product is incompatible with styrene-free amine-catalyzed resin systems and should not be used as a crosslinker in polyurethane or epoxy amine formulations.