| HS Code | 911104 |
| Productname | Sodium Persulfate |
| Synonyms | Sodium peroxydisulfate; Sodium peroxodisulfate |
| Chemicalformula | Na2S2O8 |
| Molecularweight | 238.10 g/mol |
| Casnumber | 7775-27-1 |
| Ecnumber | 231-892-1 |
| Unnumber | 1505 |
| Appearance | White crystalline powder |
| Odor | Odorless |
| Physicalstate | Solid |
| Color | White |
| Density | 2.59 g/cm3 |
| Decompositiontemperature | 180 °C |
| Watersolubility | 55.6 g/100 mL at 20 °C |
| Solubilityinothersolvents | Insoluble in ethanol |
| Ph | 2.5-4.5 (5% solution) |
| Assay | ≥98% |
| Vaporpressure | Negligible at 20 °C |
| Oxidizingproperties | Strong oxidizing agent |
| Hazardclass | 5.1 Oxidizing substances |
| Packinggroup | III |
| Storageconditions | Cool, dry, well-ventilated area away from combustibles |
| Incompatibilities | Reducing agents, combustible materials, acids, bases, metals |
| Stability | Stable under normal conditions; decomposes on heating |
| Flashpoint | Non-flammable |
| Hazardstatements | H272, H302, H315, H317, H319, H334, H335 |
| Precautionarystatements | P210, P220, P261, P280, P301+P312, P302+P352, P305+P351+P338, P304+P341, P342+P311 |
As an accredited Sodium Persulfate factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Sodium Persulfate is supplied in 25 kg polyethylene-lined, moisture-resistant fiber drums with sealed lids and clear hazard labels. |
| Container Loading (20′ FCL) | Sodium Persulfate, UN 1505, Class 5.1 oxidizer, loaded in 20′ FCL: palletized, shrink-wrapped, fully secured, labelled, with proper DG documentation. |
| Shipping | Sodium persulfate is shipped as UN 1505, Class 5.1 oxidizing solid, Packing Group III. Use approved UN packaging, oxidizer labels, and proper shipping papers. Keep away from combustible materials, heat, and reducing agents. Follow ADR/IATA/IMDG regulations and carrier requirements. Handle as dangerous goods; ensure compatibility, segregation, and emergency response information. |
| Storage | Store sodium persulfate in a cool, dry, well-ventilated area away from heat, sunlight, and ignition sources. Keep containers tightly closed, clearly labeled, and corrosion-resistant. Separate from combustible, organic, reducing, acidic, alkaline, and metal materials. Avoid moisture, contamination, and physical damage, as these can cause decomposition or hazardous reactions. Use secondary containment where required. Follow local regulations and inventory controls. |
| Shelf Life | Sodium persulfate typically has a two-year shelf life if kept cool, dry, sealed, and away from heat, moisture, and reducing agents. |
In aqueous free-radical polymerization, the thermal decomposition of sodium persulfate follows first-order kinetics with an approximate half-life of 6.3 h at 70 °C and 0.28 h at 90 °C at pH 7.0. The initiator is typically charged at 0.1–0.5 wt% based on total monomer in thermally initiated batch emulsion systems; in redox-initiated variants, the addition level is lowered to 0.05–0.15 wt% sodium persulfate combined with 0.02–0.08 wt% sodium metabisulfite as reducing agent, permitting radical flux at 40–60 °C instead of 75–85 °C. Each persulfate anion decomposes to yield two sulfate radical anions, and those sulfate radical species initiate vinyl polymerization while sulfate ion residues remain in the aqueous phase. Oxygen must be excluded because dissolved oxygen above 0.5 mg/L retards conversion. For large-scale latex production, the process is executed in jacketed 316L stainless steel or glass-lined reactors equipped with pitched-blade turbine agitators at 120–180 rpm and external circulation loops for heat removal. A pre-emulsion is prepared in a separate vessel with a high-shear rotor-stator mixer at 3,000–6,000 rpm, and the initiator solution is introduced either as a single shot after the monomer pre-emulsion reaches 65–75 °C or as a metered stream over 2–4 h. The reaction is conducted under inert nitrogen gas at 0.2–0.5 barg. When monomer conversion reaches 95–99%, the batch is held at 80 °C for 30–60 min to decompose residual initiator and reduce residual monomer, then cooled and filtered through 100–150 µm bag filters.
For indirect food-contact papers and paperboard coatings, residual persulfate-derived sulfate is controlled within the use limitations of FDA 21 CFR 176.170; for adhesives and coatings, the applicable food-contact clearance is FDA 21 CFR 175.105 or FDA 21 CFR 175.300. Persulfate salts are classified as oxidising solids under EU CLP Regulation (EC) No 1272/2008, and workplace exposure assessment falls under REACH Annex I. Residual sulfate and persulfate in finished latex are measured by ion chromatography according to ISO 10304-1:2007, with the latex coagulated and extracted to avoid column fouling. The process yields carboxylated styrene-butadiene latex for coated paper and packaging, all-acrylic and styrene-acrylic architectural coatings, pressure-sensitive adhesives, vinyl acetate-ethylene adhesives, and nonwoven binders used in hygiene and filtration media. Operational limitations include batch-to-batch radical flux variation when dissolved iron exceeds 0.5 mg/L Fe²⁺ or when recycled process water contains copper from cleaning operations; ethylenediaminetetraacetic acid disodium salt or an equivalent chelating agent is therefore added at 0.01–0.05 wt%. Sodium persulfate solutions should not be brought into contact with amine-containing monomers at high pH without evaluation because protonated amines can accelerate decomposition and release oxygen, which creates a premature initiator consumption profile.
In high-density interconnect printed circuit board production, sodium persulfate microetch is applied after alkaline cleaning and before dry film lamination to remove chromate conversion layers, eliminate copper oxides, and roughen copper foil surfaces. The bath is formulated with 80–180 g/L sodium persulfate and 1–5 vol% sulfuric acid, operated at 35–50 °C in a conveyorized spray etching module constructed from polyvinyl chloride or 316L stainless steel. Under these conditions, copper etch rate is typically 0.5–1.5 µm/min on 35 µm electrodeposited copper foil, but the rate decreases as dissolved copper accumulates above 15–20 g/L because cupric sulfate complexes lower free persulfate activity. The spray module uses nozzle pressures of 1.5–3.0 bar and conveyor speeds of 2–5 m/min; a post-etch deionized water rinse, acid dip, and hot-air knife drying are required before dry film lamination. On production lines, etch rate drift is commonly compensated by raising persulfate feed rate until copper sulfate approaches its solubility boundary near 30 g/L, beyond which sludge precipitation and nozzle blockage occur.
| Parameter | Lower boundary | Upper boundary | Measurement method |
|---|---|---|---|
| Sodium persulfate concentration | 80 g/L | 180 g/L | Iodometric titration |
| Sulfuric acid concentration | 1 vol% | 5 vol% | Acid-base titration |
| Copper loading | 5 g/L | 30 g/L | Atomic absorption or UV-Vis |
| Bath temperature | 35 °C | 50 °C | Inline thermocouple |
| Spray nozzle pressure | 1.5 bar | 3.0 bar | Pressure transducer |
| Copper etch rate | 0.5 µm/min | 1.5 µm/min | Gravimetric coupon test |
Finished PCB qualification is performed under IPC-A-600H for acceptability and IPC-6012D for rigid board performance; copper surface roughness after microetch is measured by contact profilometry per ISO 4287:1997, with typical arithmetic mean roughness of 0.25–0.60 µm on low-profile foil. The process supports rigid multilayer boards, high-density interconnect boards, IC substrates, and flexible printed circuits. Terminal product types depend on subsequent imaging and plating steps: fine-pitch rigid packages with line width/spacing below 50/50 µm, chip-on-film substrates, and double-sided flex circuits. A limitation encountered on manufacturing lines is the reduction in etch rate when the bath is operated beyond 30 g/L copper or below 35 °C; moreover, hydrochloric acid or chloride-containing cleaners must be excluded from the persulfate bath because acidic chloride can generate chlorine gas and alter the etch profile. Published data for the exact upper copper loading limit across different spray chamber geometries is limited, so pilot trials are required to establish the breakpoint for each etching machine configuration.
For low-temperature hydraulic fracturing fluids containing borate-crosslinked guar at bottomhole static temperatures below 49 °C, unencapsulated sodium persulfate is generally combined with a tertiary amine activator to generate sulfate radicals before viscosity reduction is needed. The addition rate ranges from 0.05–5.0 lbm/1,000 gal (6–600 mg/L) of gelled fracturing fluid, with encapsulated grades more commonly applied at 0.25–1.0 lbm/1,000 gal (30–120 mg/L) to delay gel break until after proppant placement. In the mixing plant, sodium persulfate is introduced as a dry powder through a high-shear hydration unit or as a mineral-oil-encapsulated particulate during proppant addition, while the fracturing slurry is pumped at 2–5 m³/min by high-pressure positive-displacement pumps. Downhole, the thermal decomposition of persulfate and subsequent oxidative scission of guar polymers reduce fluid viscosity, allowing fracture closure on the proppant pack. Viscosity break is evaluated on a high-pressure high-temperature rheometer at 100 s⁻¹ and bottomhole static temperature; the terminal target is commonly below 10 cP at 100 s⁻¹. Performance is measured in accordance with ISO 13503-1:2011 for completion fluid viscosity testing, and formation water compatibility is screened in bottle tests before the treatment. The terminal process outputs are the broken gel return fluid, retained proppant pack, and produced water containing sulfate and degraded polymer fragments. Below 35 °C, unencapsulated persulfate may require excessive activator and cause premature viscosity loss; contact with ferrous iron in tanks or transfer lines should be avoided because iron-catalyzed decomposition accelerates breaker consumption. Pre-mixing in freshwater holding tanks for longer than 6 h is not recommended due to activity loss.
Alkaline oxidative destruction of free cyanide in electroplating rinse water is carried out with sodium persulfate at pH 10.0–11.5, maintained by sodium hydroxide metering. The applied oxidant dose for free cyanide is typically 2.5–5.0 g sodium persulfate per gram of free cyanide; for rinse streams containing weak-acid dissociable metal-cyanide complexes such as zinc or copper cyanides, the effective ratio may rise to 8–12 g/g because the metal-cyanide complex must be destabilized before oxidation. Treatment is performed in a continuously stirred tank reactor with 30–60 min hydraulic residence time, equipped with an ORP electrode and maintained at 300–400 mV vs Ag/AgCl. Persulfate is metered as a 20–30 wt% aqueous solution through a diaphragm pump with a pulsation dampener to avoid pH swings; the reactor and circulation piping are constructed of 316L stainless steel or polypropylene. Free cyanide is measured by ISO 14403-1:2012, and discharge compliance is evaluated against the electroplating categorical standards in 40 CFR Part 413 or applicable municipal limits. The output is cyanate- and sulfate-rich treated rinse water suitable for discharge or further polishing. If sulfide or thiosulfate is present, it consumes persulfate and lowers oxidation efficiency; pH below 9.5 must be prevented to avoid hydrogen cyanide release. The process is unsuitable for concentrated cyanide baths unless pretreated by oxidation or cyanide recovery because persulfate consumption becomes uneconomical and heat release may require cooling capacity.
During oxidative desizing of starch-laden cotton warps, sodium persulfate is applied in a pad-steam range at 2–6 g/L with a nonionic wetting agent at 0.5–2 g/L and steaming temperature 80–95 °C for 30–90 s. The fabric is padded to a wet pickup of 70–90%, steamed in a roller steam box, and then washed in multi-box open-width washers at 60–90 °C. Size removal is verified by starch-iodine spot test, and residual sulfate on fabric is measured by ISO 10304-1:2007; finished fabric residue compliance is assessed against OEKO-TEX Standard 100. Fabric tensile strength retention is evaluated per ISO 13934-1:2013; excessive persulfate dosage or iron contamination can depolymerize cotton cellulose and reduce strength below 85% of greige fabric. The process yields desized and scoured cotton and cotton/polyester woven or knitted goods for subsequent dyeing, printing, and finishing. Sodium persulfate should not be combined with reducing agents in the same formulation tank because exothermic decomposition can occur during storage.
Competitive Sodium Persulfate prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618963613625 or mail to sales10@ascent-petrochem.com.
We will respond to you as soon as possible.
Tel: +8618963613625
Email: sales10@ascent-petrochem.com
Flexible payment, competitive price, premium service - Inquire now!
Sodium persulfate (Na2S2O8; CAS 7775-27-1) is an anhydrous white crystalline oxidizer with molecular mass 238.10 g/mol and theoretical active oxygen 6.72% by mass. Industrial supply forms include free-flowing powder and granular solid; the product is specified by chloride and iron limits rather than by trade model, with common classes being technical grade, low-chloride grade, and low-iron electronics grade. Low-chloride grade is selected when chloride above 0.005% would be detrimental to stainless steel feed skids or to catalyst performance in polymerization.
Routine commercial certificates of analysis for low-chloride material list assay ≥99.0% as Na2S2O8 by iodometric titration, moisture ≤0.05% by Karl Fischer titration, chloride ≤0.002% by silver nitrate titration adapted from ISO 9297, iron ≤0.0005% by ICP-OES, and heavy metals as Pb ≤0.001%. The product is classified as UN 1505, Packing Group III. Maximum recommended storage temperature is 40°C; excursions above 60°C can lead to self-accelerating decomposition if fines or transition-metal contamination are present.
Aqueous solubility of sodium persulfate is approximately 550 g/L at 20°C, which allows concentrated stock solutions for continuous dosing. Unheated transfer lines often operate at 100–150 g/L sodium persulfate to avoid winter crystallization. The pH of a 5% solution is typically 3.0–5.0; decomposition acidifies the solution through sulfate and hydrogen sulfate formation. Differential scanning calorimetry data on dry solid show exothermic decomposition onset near 180°C, but transition-metal contamination reduces the apparent onset by 20–40°C. Storage and metering lines therefore use 316L stainless steel or HDPE, with copper and brass excluded.
Sodium persulfate solutions are not stable indefinitely. At 50°C, a 10% solution loses measurable active oxygen within 24 h; therefore, stock solutions are prepared daily and cooled when ambient plant temperature exceeds 35°C. Batch-to-batch variance in solution clarity is not a reliable quality indicator because sulfate microcrystals and trace silica from packaging can produce haze without affecting iodometric assay.
Thermal decomposition of persulfate ion in aqueous media yields sulfate radical anions that initiate vinyl polymerization at kettle temperatures of 65–85°C. Sodium persulfate is selected over ammonium persulfate when ammonia release is unacceptable or when latex pH must be controlled independently. A feed solution of 10–20 wt% is typically metered into the reactor at 0.1–0.5 phm on monomer. At 70°C, the persulfate half-life in dilute aqueous solution is several hours, so fed-batch or staged initiator addition is required rather than a single initial charge.
Continuous stirred-tank reactor lines demonstrate that dissolved oxygen below 1 ppm in the monomer pre-emulsion reduces induction-time variability. Iron contamination in dilution water above approximately 2 ppm can prematurely activate persulfate in the feed preheater and produce localized oligomer formation. Residual monomer after polymerization is monitored by GC according to ISO 13741-1 for styrenic polymers; substituting sodium persulfate for ammonium persulfate does not relax the target residual monomer specification but removes the ammonia buffering effect.
In styrene-butadiene latex production, decomposition rate is influenced by pH and temperature; plant-process data from calorimetric monitoring show that an increase in initiator feed from 0.3 phm to 0.5 phm shortens total reaction time but also raises coagulum if the latex stabilizer is below 1.0 phm. Consequently, process engineers rely on reaction calorimetry rather than assuming linear scaling from pure-water decomposition data. In acrylonitrile-butadiene-styrene latex systems, the retained sodium cation alters electrolyte balance; anionic emulsifier is often adjusted in the range of 0.5–1.0 phm to maintain particle size distribution.
In horizontal conveyorized printed circuit board pretreatments, sodium persulfate baths are used to generate a uniform copper surface for photoresist lamination. Common bath formulations contain 50–100 g/L sodium persulfate and 1–2 vol% sulfuric acid at 30–40°C; copper etch rate is maintained near 0.5–1.0 µm per pass in spray equipment operating at nozzle pressure 1.0–2.0 kg/cm². Surface roughness is verified by contact profilometry according to ISO 4287, with typical target values of 0.20–0.45 µm Rz on 18 µm copper foil. Sodium persulfate avoids ammonium complexation in alkaline waste treatment, reducing copper precipitation problems compared with ammonium persulfate microetchants.
A practical boundary is sulfate build-up. At bath density above 1.25 g/cm³ or copper loading beyond 30 g/L, etch uniformity degrades and sludge may settle in spray nozzles. Published data for specific nozzle configurations is limited; therefore, line setup uses foil-loss coupons and profilometry rather than universal parameters. Rinsewater from sodium persulfate microetch contains sulfate and copper; ion-exchange recovery of copper is less effective when the bath is fortified with high sulfuric acid above 3 vol% because acid load reduces resin selectivity. Neutralization with sodium hydroxide precipitates copper hydroxide; sludge dewatering characteristics depend on sulfate-to-chloride ratio, with chloride-limited systems producing denser filter cake.
Sodium persulfate is applied as an in situ chemical oxidation reagent for chlorinated ethenes and petroleum hydrocarbons. The persulfate ion is relatively stable at ambient groundwater temperatures, but contaminant destruction requires activation to sulfate radical. Activation methods include alkaline addition to pH 10–12, chelated ferrous iron at 1–5 mM, or thermal treatment at 40–60°C. Field dosages are site-specific and commonly reported as 5–30 g/kg of saturated soil. Groundwater monitoring is performed using EPA 8260 for volatile chlorinated compounds and EPA 8015 for gasoline- and diesel-range hydrocarbons.
Matrix oxidant demand is the primary limitation. In soils with total organic carbon above 2 wt%, natural organic matter competes for radical species and decreases the fraction of persulfate available for contaminant oxidation. Bicarbonate alkalinity above 400 mg/L can scavenge sulfate radical and increase persulfate demand; published data for site-specific configurations is limited, so treatability studies using site groundwater and soil cores are required before full-scale injection.
Sodium persulfate injection in low-permeability zones may require pneumatic fracturing or direct-push injection at pressures below 5 bar to avoid daylighting. Oxidation of chlorinated ethenes can release chloride and temporarily increase dissolved cobalt or nickel from aquifer solids; monitoring of secondary contaminants is therefore included in treatability protocols. Published data on metal mobilization for this reagent is matrix-specific and should not be extrapolated from one site to another without core leaching tests.
Differences among persulfate products are controlled by cation content, solubility, and nitrogen release. Potassium persulfate has a solubility of approximately 52 g/L at 20°C, restricting it to direct solid addition where slow dissolution is acceptable. Ammonium persulfate is highly soluble but contains approximately 15.8% ammonium ion by mass, and decomposition can release ammonia. Sodium persulfate has 19.3% sodium content and introduces no nitrogen, which is advantageous in electronics-grade etch baths and in discharge-regulated wastewater treatment. Compared with hydrogen peroxide, sodium persulfate provides a solid, non-venting oxidizer with different radical kinetics and longer subsurface persistence, although pH and transition-metal compatibility differ.
| Parameter | Sodium persulfate | Ammonium persulfate | Potassium persulfate |
|---|---|---|---|
| CAS registry | 7775-27-1 | 7727-54-0 | 7727-21-1 |
| Molecular mass | 238.10 g/mol | 228.20 g/mol | 270.32 g/mol |
| Water solubility at 20°C | ~550 g/L | ~582 g/L | ~52 g/L |
| Typical assay | ≥99.0% | ≥98.5% | ≥99.0% |
| Cation content | 19.3% Na | 15.8% NH4 | 28.9% K |
| Nitrogen release | None | Ammonia | None |
In continuous microetch and polymerization systems, sodium persulfate decomposition generates sodium sulfate and sulfuric acid. For each kilogram of sodium persulfate consumed, approximately 0.59 kg of sodium sulfate is produced by the sulfate pathway; this increases conductivity in etch baths and sludge loading in wastewater neutralization. In polymer latex, sodium sulfate introduced by initiator decomposition at 0.2–0.8 phm can alter particle size and mechanical stability, requiring adjustment of emulsifier or initiator feed strategy.
Sodium persulfate cakes when exposed to plant air above 60% relative humidity; opened packages are used within 24–48 h or transferred to sealed stainless steel or HDPE hoppers with desiccated purge air. Caking does not materially reduce assay but changes gravimetric feed screw accuracy. Moisture films on crystal surfaces dissolve residual chloride and iron impurities, creating localized acidic conditions that can corrode carbon steel screw conveyors. Rotary valves and screw conveyors are therefore specified in 316L stainless steel with PTFE seals.
Incompatibility segregations are mandatory. Sodium persulfate is separated from sulfites, metabisulfites, powdered metals, amines, and concentrated acids. Contamination with sodium metabisulfite can initiate rapid exothermic reaction at ambient temperature; bulk storage areas therefore use separate containment dikes and oxidizer-rated fire-suppression systems. Spill handling is performed by dry vacuum with HEPA filtration rather than wet sweeping because water accelerates localized persulfate decomposition on contaminated surfaces.
Commercial low-iron electronics grade is produced through high-purity synthesis and recrystallization, with iron ≤0.0005% and chloride ≤0.002%. In copper microetch, iron above 5 ppm can promote localized copper pitting; the electronics grade is specified when roughness uniformity must remain below 0.3 µm Rz on thin foil. Technical grade is typically applied in soil remediation and water treatment where pitting is not a downstream concern. Shelf life in original sealed packaging is typically 12 months when stored below 40°C and 50% relative humidity; retest intervals of 6 months are common for inventory held in non-climate-controlled warehouses.